◆ Rebuild

Part 2 · Earth and Fire

Abrasives and Grinding Stones

Hard grit — sand, sandstone, emery, garnet — wears away anything softer than itself. This chapter covers finding and shaping whetstones and grindstones, sorting grit into exact grades by letting it settle in water, polishing powders like rouge and tripoli, and how to put a keen edge on a blade.

Difficulty
●●●●●
Time
An afternoon to make a whetstone; a day to grade a batch of grit; weeks to cut and mount a grindstone
Steps from zero
1 prerequisite →

You need first

Stone Tools

This unlocks

Industrial Diamond and Hard AbrasivesGem Cutting and LapidaryQuartz Crystals and Frequency ControlPrecision GrindingSharpening and Honing
The full path from nothing — 1 step before this one
  1. Stone Tools
  2. Abrasives and Grinding Stones

Do them roughly in this order. See it on the tech tree →

Why it matters

Every cutting tool goes blunt. Without a way to sharpen it, an axe, knife, sickle, chisel or razor is a lump of metal. Abrasives — hard grains that scratch away softer material — are how you:

How it works

Hardness decides everything. An abrasive grain scratches only a material softer than itself. Mineral hardness is compared on the Mohs scale, from 1 (talc) to 10 (diamond). Some useful points:

Hardness Material Field test
2–2½ Fingernail
3–3½ Copper coin, calcite
5–5½ Ordinary glass, iron knife
6–6½ Feldspar; hard steel file Scratches glass
7 Quartz (sand, flint, sandstone grains) Scratches glass and steel easily
6½–7½ Garnet Scratches glass
9 Corundum (in emery) Scratches quartz
10 Diamond Scratches everything

Hardened steel is about 6–7, so quartz (7) — the grain of sand and sandstone — will sharpen it, slowly. Emery (9) cuts hardened steel, glass and quartz fast. See Rocks and Minerals for more field tests.

Grit size decides the finish. Big grains cut fast and leave deep scratches. Small grains cut slowly and leave fine ones. So every job goes coarse to fine: each finer grit removes the scratches left by the one before. A good rule is to roughly halve the grain size at each step. If a single coarse grain gets into a fine stage, it leaves a deep scratch, and you must go back.

Polishing is the last stage: very fine, often softer powders (rouge, tripoli, chalk, tin oxide) on a soft backing — leather, felt, wood or pitch — that rub away the last tiny scratches until the surface shines.

What you need

Item Notes
Whetstones A coarse and a fine stone, each about 20 × 5 × 2.5 cm
A flat lapping slab A large flat stone, 40 × 30 cm or more, for flattening whetstones
Loose grit Sand, crushed flint or quartz, garnet sand or emery
Settling vessels 5–6 tall jars or pots, 30 cm deep, and a ladle or a cloth siphon
Polish Rouge, tripoli, chalk or fine wood ash
A leather strop A strip of leather 5 × 40 cm, glued to a flat board, or hung from a hook
For a grindstone A sandstone wheel, a wooden frame, an axle, a crank or treadle, a water trough

Where to find it

  • Sandstone — layered cliffs and stream boulders of grey, buff or red rock that feel like sandpaper. Coarse, even-grained sandstone makes grindstones. Look for blocks with no cracks, no pebbles, and no soft or clay-rich layers. See Quarrying and Cutting Stone.
  • Whetstone rocks — the best natural hones are very fine-grained, even, hard rocks: dense siltstones, fine slates, quartz-rich schists (the Vikings traded hones of grey schist from Norway across all of northern Europe), and the very fine white quartz rock novaculite. Test any likely stone: rub a steel knife on it with water. A good hone "bites" — you feel a slight drag — and quickly makes a grey slurry. A stone that feels glassy and slick is too hard or too fine; one that crumbles is too soft.
  • Quartz and flint — crush pebbles after heating them red-hot and dropping them in water, which cracks them. See Stone Tools.
  • Garnet — dark red, brownish or black, glassy, heavy grains. They gather in reddish or purplish streaks on beaches and in river bends where water has sorted out heavy minerals, like gold. Pan the sand in a shallow dish under water: light quartz washes over the edge and the heavy garnet (and black iron sand — remove it with a lodestone) stays behind. Garnets also sit as round crystals in mica schist.
  • Emery — dark grey to black, granular rock, very heavy for its size, so hard it scratches quartz. It forms lenses in old marble and metamorphic rock. Rare; prized.
  • Pumice — pale grey volcanic rock full of bubbles, so light it floats. Found in volcanic regions and washed up on beaches far away. Ground fine, it is a mild abrasive for wood, horn and paint.
  • Tripoli (also called rottenstone) — light, soft, porous, buff, grey or pinkish rock, made of extremely fine silica, often where limestone or chert has rotted. It crumbles to a fine powder between the fingers that feels smooth, not gritty, and makes no fizz with acid. The classic polish for brass and other soft metals.
  • Rouge — fine red iron oxide. Grind red hematite or red ochre, roast iron rust, or heat green vitriol to a red powder (see Lenses).
  • Chalk — soft white rock that fizzes with vinegar. Washed fine, it polishes silver, pewter and horn without scratching.
  • Horsetail — the scouring rush, a jointed, hollow, leafless green plant of wet places. Its stems are full of silica; bundled, they scour pots and polish wood and pewter.

Making a whetstone

  1. Choose a piece of good hone stone, roughly brick-shaped, with no cracks. Tap it: it should ring, not clunk.
  2. Rough it to shape with a hammerstone, knocking off corners, aiming for about 20 × 5 × 2.5 cm. A pocket hone for a sickle or scythe can be 25 cm long and cigar-shaped.
  3. Flatten the working face. Wet a large, flat sandstone slab, sprinkle on coarse sand, and rub the stone face-down on it in figure-of-eight strokes, pressing firmly. Every few minutes, turn the stone end for end. Keep going until the face is flat all over — check by laying a straight edge across it in several directions against the light.
  4. Finish with finer sand, then rub it on a second flat stone of its own kind.
  5. Use it with water (most stones) or with a little oil or fat (fine, hard stones clog less with oil). Keep it in a wooden box.
  6. Reflatten whenever the face becomes hollow — a dished stone rounds your edges.

Sorting grit by settling

Hand-crushed grit is a mixture of every size, from gravel to dust. To grind lenses or put a fine edge on steel you need grit sorted into grades of nearly equal size. The simplest way is to let it settle in water — larger grains sink faster. This is called levigation or elutriation. Opticians once named their emery grades by the minutes it took to settle.

after 30 safter 2 minafter 15 minafter 1 hour 30 cm of water Coarseover 0.1 mm Medium0.05–0.1 mm Fine0.02–0.05 mm Very fine0.01–0.02 mm Polishingsettles overnight Times are for quartz or flint grit. Heavier garnet and emery settle in about half the time.
Fig. 1 Grading grit by settling. Stir, wait, and pour off the cloudy water into the next jar. What settles in each jar is one grade; the longer the wait, the finer the grit.
  1. Crush the grit as fine as you can on a flat stone with a hammerstone, wet, to keep the dust down. Sieve out anything coarser than the finest sieve or cloth you have; save it for rough grinding.
  2. Fill the first jar with water to a depth of 30 cm, add the grit (a cupful in a big jar), and stir hard until everything is swirling.
  3. Wait, then pour or siphon the cloudy water — not the sediment — into the second jar. Use these times for quartz or flint grit, water 30 cm deep (garnet and emery are heavier: use about half the time):
Wait before pouring off Grains left behind (approx.) Use
30 seconds Coarser than 0.1 mm Rough grinding, sawing stone
2 minutes 0.05–0.1 mm Grinding stone axes; first stage on lenses; coarse sharpening
15 minutes 0.02–0.05 mm Medium grinding
1 hour 0.01–0.02 mm Fine grinding; fine hones
Overnight Finer than 0.01 mm Final smoothing; polishing
  1. Repeat the stir-wait-pour in each jar with the same time, two or three times, to clean each grade.
  2. Dry each grade, and keep it in its own labelled, lidded pot. Never let a coarse grade near a fine one — one coarse grain ruins a polish.

Polishing powders

  • Rouge cuts glass and hardened steel slowly and leaves a mirror finish. Used on leather or pitch (see Lenses).
  • Tripoli with a little oil or fat, on leather or a cloth pad — brass, copper, bronze, pewter, horn, wood finishes.
  • Chalk or whiting with water — silver, pewter, soft metals.
  • Pumice with water or oil on a felt pad — wood, varnish, horn.
  • Fine wood ash, sieved and washed — a gentle polish for glass and metal.
  • Tin oxide (putty powder) — the finest polish for glass and stone; see Lenses.

Abrasive paper and cloth

Brush hot hide glue (see Glues and Adhesives) onto strong paper (Paper) or cloth, sprinkle on one grade of sifted sand, crushed glass or emery, press it down, and let it dry. Shake off the loose grains. This is sandpaper ("glasspaper", "emery cloth"). Wrapped round a block of wood, it shapes and smooths wood, horn and metal.

The grindstone

Sandstone wheel50–80 cm across, 8–12 cm thick Water troughempty it after use Tool restblade meets the wheelturning into its edge Crank60–120 turns a minute Treadle direction of turn
Fig. 2 A treadle grindstone. The sandstone wheel turns slowly through a water trough; the tool rests on a rest and meets the wheel turning toward its edge.

For heavy work — grinding the bevel of an axe or reshaping a chisel — a turning stone wheel is far faster than a hand stone.

  1. Cut the wheel from a block of even, medium sandstone: 50–80 cm across and 8–12 cm thick. Scribe a circle with a cord and peg, then peck and chisel it round (see Quarrying and Cutting Stone). Cut a square hole in the centre, about 5–6 cm across.
  2. Mount it on a square wooden or iron axle, held with wedges on both sides so it runs true. Rest the axle ends in hardwood bearings greased with tallow on a strong wooden frame (see The Wheel and Axle).
  3. Turn it with a crank on one end (see Cranks, Cams and Linkages), worked by a helper, or with a treadle. A 60 cm wheel should turn at about 40–60 turns a minute — the rim then moves at roughly a brisk walk (under 2 m/s). Faster is not safer for natural stone (see Dangers).
  4. Keep it wet. Fix a trough of water below so the bottom of the wheel dips in, or drip water onto it. Water carries away the steel and stone dust, keeps the tool cool, and stops dust flying. Empty the trough after use: a wheel left standing in water goes soft on one side and runs out of balance.
  5. True it when it wears lumpy: hold a hard steel bar or a sharp-edged iron pipe firmly across the turning face on a rest until the high spots are cut away.

Grinding. Hold the tool on a rest so the bevel meets the wheel turning toward the edge (into the edge, not away from it) — this leaves no loose burr and is safest. Use light pressure and keep the tool moving across the face. Dip it in water often. If the steel turns straw, brown or blue, it has softened — the temper is lost (see Steel) and you must grind past it or re-harden.

Sharpening an edge

This is the short version; every kind of edge, with jigs and tests, is covered in Sharpening and Honing.

1. Hold the angle (end view of blade) 2. Raise a burr, then strop it off 20° lift spine≈ ⅓ of width push edge-first, as if slicing a thin layer off Whetstone, wet a 2 cm wide blade: lift about 7 mm for 20°, 1 cm for 30° Burrfeel it with the thumbacross, never along blade, magnified Strop: spine first, edge trailingleather with a little rouge, very light strokes
Fig. 3 Holding the angle. For a 20° bevel on a 2 cm-wide blade, lift the spine about 7 mm. Hone until a burr forms along the whole edge, then work the other side, then strop.

Choose the angle (the angle of one side of the edge):

Tool Angle per side Why
Razor 8–10° Very keen, very delicate
Kitchen and carving knife 15–20° Keen; for soft materials
Chisel, plane iron 25–30° (single bevel) Strong enough to be struck
Axe, hatchet 20–25° (splitting axes more) Must survive hitting knots
Scythe, sickle Thin, honed in the field every half hour

To find the angle without a protractor: for a blade w cm wide, lifting the spine by about a third of w gives roughly 20°; by half of w, roughly 30°. Or cut a wooden wedge to the angle and rest the blade on it while you start.

  1. Grind the bevel on the grindstone or a coarse stone if the edge is chipped or very dull.
  2. Hone on the coarse whetstone. Wet the stone. Lay the bevel flat on it, then lift the spine to the angle. Push the blade edge-first along the stone, as if slicing a thin layer off it, sweeping so the whole length of the edge passes over the stone. Keep your wrist locked so the angle does not rock. Do 10–20 strokes on one side.
  3. Feel for the burr. Draw your thumb gently across (never along) the edge from the spine outward on the other side. A rough, catching wire of metal along the very edge — the burr — means you have ground right to the edge. Keep honing that side until the burr runs the whole length.
  4. Turn the blade and hone the other side the same way until the burr moves back.
  5. Go to the fine stone. Repeat with lighter pressure and fewer strokes, alternating sides every one or two strokes, until the burr is tiny.
  6. Strop. Rub a little rouge or fine polish into a leather strop. Draw the blade spine-first (edge trailing) along it, 10–20 times each side, very lightly. This removes the last burr and polishes the edge.

Tip The light test. Hold the blade edge-up under a bright light and look straight down at it. A sharp edge is invisible. Dull spots and rolled edges catch the light as bright lines or dots. Hone until no light shows.

How to tell it worked

  • Sharp edge: cleanly slices a sheet of paper held up by one corner; shaves hair from the forearm (knife or razor); the light test shows no shiny line.
  • Good whetstone: flat (no light under a straightedge), bites the steel, makes slurry quickly.
  • Graded grit: a pinch rubbed between glass plates gives an even, uniform frosting with no deeper scratches.
  • Polish: under a raking light, no scratches visible to the eye.

Note Troubleshooting. Edge never gets sharp → you never raised a burr all along it, or your angle rocks; slow down, lock your wrist, use a wedge guide. Edge sharp but dulls at once → angle too low for the job, or a burr left on; raise the angle a few degrees and strop. Stone glazed and slippery → clogged with metal; scrub it with sand and water, or use more water or oil. Edge rounded, belly-shaped → stone dished; reflatten it. Deep scratches in a fine finish → coarse grit contamination; wash everything and go back one grade. Grindstone jumps and bumps → out of round or out of balance; true it, and never leave it standing in water. Steel turned blue at the edge → overheated; lighter pressure, more water.

Dangers

Danger Grindstones can burst. A large stone wheel turning too fast, or one with a hidden crack or a frost-damaged face, can fly apart and kill. Tap a new or stored wheel with a piece of wood before mounting it: a clear ring is good, a dull note means a crack — do not use it. Never turn a natural stone faster than a brisk walk at the rim, never stand in line with the wheel when starting it, and never use a wheel that has been frozen while wet.

Danger Dry grinding kills slowly. Sandstone and quartz dust scar the lungs (silicosis). In 19th-century Sheffield, many dry grinders died before the age of 40. Grind wet, always. Crush and sieve grit wet and outdoors, and cover your mouth and nose with a damp cloth.

  • Eyes. Grit and steel sparks fly from a grindstone. Shield your eyes or turn your face aside.
  • Cuts. Sharpening means fingers near an edge. Stroke away from your hand, keep the stone on a non-slip base, and test sharpness on paper or hair, not on a fingertip.
  • Fumes. Roasting green vitriol to make rouge gives off choking acid fumes; do it outdoors, upwind (see Lenses).

What this unlocks

Sharp tools make all of Basic Woodworking, Axes, Chisels, Knives and Planes, Files and Saws and harvesting practical. Graded grit makes Lenses, Mirrors, the The Microscope and the The Telescope. Grinding and lapping to flatness lead to Precision Grinding, Machine Tools, Bearings and Lubrication and Precision and Interchangeable Parts. Much later, artificial abrasives — silicon carbide made in an The Electric Arc Furnace, Industrial Diamond and Hard Abrasives, and bonded grinding wheels — make precision engineering fast.

How it was first done

People were grinding stone tools to shape with sand and sandstone at least 40,000 years ago; ground-edge axes from northern Australia and Japan are among the oldest known. Egyptian masons cut and drilled granite with copper saws and tube drills fed with wet quartz sand. The Greeks quarried emery on the island of Naxos to carve marble, and the Romans traded whetstones across their empire; Pliny the Elder describes the best kinds. Viking traders carried schist hones from Eidsborg in Norway all over northern Europe. The earliest known picture of a grindstone turned by a crank is in the Utrecht Psalter, made in about AD 830. Glued abrasive paper and emery cloth became common in the 1800s, and in 1891 Edward Acheson made silicon carbide (carborundum) in an electric furnace — the first artificial abrasive harder than almost anything in nature.

Source: content/entries/earth/abrasives.md