◆ Rebuild

Part 10 · Machines

Scientific Instrument Making

Science runs on scales and circles divided more finely than an eye can see. How to work brass into instruments, divide a straight scale and a circle by hand to a fraction of a minute of arc, build a dividing engine that does it by screw, cut and fill fine lines, read them with a vernier, graduate glass, and make a spirit level.

Difficulty
●●●●●
Time
A week for a brass scale divided by hand; a month to divide a 30 cm circle by hand; several months to build a dividing engine
Steps from zero
22 prerequisites →

You need first

Machine ToolsGeometry and Trigonometry

This unlocks

Rules, Squares, Callipers and Gauges
The full path from nothing — 22 steps before this one
  1. Stone Tools
  2. Cordage and Rope
  3. Fire
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Writing and Numbers
  7. Basic Woodworking
  8. Hunting and Trapping
  9. Charcoal
  10. Pottery
  11. Arithmetic and Fractions
  12. Hides and Leather
  13. The Wheel and Axle
  14. Geometry and Trigonometry
  15. Bellows
  16. The Lathe
  17. Iron (the Bloomery)
  18. Copper Smelting
  19. Blacksmithing
  20. Steel
  21. The Steam Engine
  22. Machine Tools
  23. Scientific Instrument Making

Do them roughly in this order. See it on the tech tree →

Why it matters

A The Telescope shows you a star; a divided circle under the telescope tells you exactly where it is. The difference between looking and measuring is fine lines on brass. Navigation by the stars (Navigation), maps (Maps and Mapmaking, Surveying and Levelling), the calendar (Astronomy, The Calendar), chemistry by weight and volume (Atoms, Elements and Reactions, Laboratory Glassware), the The Thermometer and The Barometer, the electrical meters of Measuring Electricity, the The Spectroscope and the The Microscope — every one of these is only as good as its scale.

This chapter is about making those scales and the brass bodies that carry them. It builds on two things you already have: flat plates, straightedges and squares (Machine Tools), and the geometry of dividing lines and circles with compass and dividers (Geometry and Trigonometry, Measurement from Scratch). Here we push those methods from millimetres to hundredths of a millimetre, and from degrees to seconds of arc.

How it works

What "fine" means

On a circle of radius R, one degree of arc is R × 0.01745 long. So:

Radius of circle 1 degree is 1 minute of arc is 10 seconds of arc is
10 cm 1.75 mm 0.029 mm 0.005 mm
30 cm 5.24 mm 0.087 mm 0.015 mm
1 m 17.5 mm 0.29 mm 0.048 mm

A careful hand with sharp dividers and a magnifier can place a point to about 0.02–0.03 mm. That is about 1 minute of arc on a 10 cm circle, or 15 seconds on a 30 cm one. Bigger circles are more accurate, which is why old observatories built huge quadrants, and why a dividing engine — which removes the hand — was such a leap.

Three principles every instrument maker uses

  1. Bisection is exact; stepping accumulates error. Halving a length or an arc with arcs from each end needs no measurement, and its errors do not add up. Stepping dividers round a circle 360 times adds every small error together. So divide by bisection wherever you can, and step only small numbers of spaces.
  2. Reversal cancels errors. Measure, turn the instrument end-for-end or upside down, and measure again: half the difference is the instrument's own error. This is how you check a square, a level, and the centring of a circle without any better tool (Machine Tools).
  3. Read both sides. If a circle's centre is not exactly on its axis (eccentricity), readings on one side are too large and on the opposite side too small by the same amount. Two readers (verniers or microscopes) 180° apart, averaged, cancel it completely.

Temperature

Brass grows about 0.019 mm per metre for each degree warmer; steel about 0.012 mm; glass about 0.009 mm. A 30 cm brass scale held in a warm hand for a minute grows by 0.02–0.03 mm — as much as your finest division. Divide and check in a room at an even temperature, with the work left there overnight first, and handle it with a cloth or by its frame.

What you need

Item Notes
Brass sheet and bar About 2 parts copper to 1 of zinc; with 1–2% lead it cuts cleanly (Zinc and Brass)
Beam compass A straight, stiff bar 50–100 cm long with two sliding heads, each carrying a hardened steel point; one head with a fine adjusting screw
Spring dividers Hardened steel points; a screw to set the opening
Gravers Hardened steel bars 3 mm square, ground to a sharp point or a thin knife edge (Axes, Chisels, Knives and Planes)
Magnifiers A hand lens of 5–10 times; later a small microscope with a crosshair (Lenses, The Microscope)
Surface plate, straightedge, square Machine Tools
Lathe with screw-cutting For screws, tubes and the dividing engine (The Lathe)
Black wax Beeswax with a little pine resin and lampblack, for filling lines
Lacquer Shellac dissolved in alcohol, tinted yellow (Glues and Adhesives, Ether, Acetone and Solvents)
Silver Thin strip to inlay for the finest scales (Gold and Silver)
Soft solder Soldering and Brazing

Where to find it

  • Copper and zinc for brass: copper from native copper or green and blue copper ores (Copper Smelting); zinc from calamine (heavy, white to grey, honeycombed lumps, often in limestone) or sphalerite (resinous brown to black crystals that smell of rotten eggs when scratched with acid) — see Zinc and Brass. Tin for solder and bronze comes from cassiterite (Tin and Pewter).
  • Beeswax from hives (Beekeeping), pine resin from wounded pine trees, shellac from the lac insect's resin on trees in South and South-East Asia (Glues and Adhesives). Lampblack: hold a cold plate in a smoky oil flame.
  • Fluorite for etching glass: glassy cubes, often purple, green or yellow, soft enough to scratch with a knife, in veins with lead ores (Rocks and Minerals).
  • Quartz and emery for grinding glass and polishing: see Abrasives and Grinding Stones.

Method 1: Brass instrument work

Brass is the instrument maker's metal: it casts well, cuts cleanly, does not rust, stays still, and polishes beautifully.

  1. Cast and roll or hammer plate. Cast brass into flat ingots in an open mould or sand (Metal Casting), then roll or hammer them out, annealing (heating to a dull red and letting cool) whenever the metal stiffens (Sheet Metal and Rolling).
  2. Planish. Finish a plate by going over it with many light, overlapping blows of a polished hammer on a polished flat anvil. This makes it stiff and springy — hammer-hardened brass holds its shape far better than soft, annealed brass, so a planished instrument limb does not bend when clamped.
  3. Flatten. File and scrape to the surface plate until it shows even contact all over (Machine Tools). Finish with fine emery stone, then charcoal and water, then tripoli.
  4. Turn and fit. Turn bushes, axes and tubes on the lathe; telescope draw-tubes should slide with a smooth, even friction (The Telescope). An instrument's axis — the cone or cylinder it turns on — is lapped into its socket with fine emery and oil until it turns without any shake.
  5. Clamp and tangent screw. To set a telescope or a circle exactly, fit a clamp to lock it roughly and a tangent screw (a fine screw pushing a lug against a light spring) for the last fraction of a degree.
  6. Solder with soft solder for light joints and silver solder for strong ones (Soldering and Brazing).
  7. Lacquer. Clean the brass bright, warm it until it is too hot to hold comfortably, and brush on thin shellac in alcohol, tinted golden with a little turmeric or saffron. It keeps the brass from darkening for years.

Method 2: Dividing a straight scale

With the lathe's screw. If your lathe cuts threads, it is already a dividing machine: the leadscrew moves the carriage a known amount per turn. Clamp the scale on the carriage, fix a graver in a hinged holder on the headstock so it can be drawn across the scale, and advance the carriage by exact turns or fractions of a turn of the leadscrew, read on a dial (Precision and Interchangeable Parts). Every error of the leadscrew goes onto the scale, so check the result as below.

By hand, by bisection.

  1. Lay out the full length between two fine dots made with a sharp, hardened point, using the beam compass set from your standard (Measurement from Scratch).
  2. Bisect: with the beam compass set very nearly to half the length, swing a faint arc from each end dot. If the arcs do not meet, they leave a tiny gap or overlap; the true middle is exactly half-way between them. Mark it with a dot under the lens.
  3. Keep halving: 2, 4, 8, 16 … For tenths, divide into 5 by trial stepping (set the dividers, step five times, adjust by a fifth of the miss, repeat), then halve.
  4. Cut the lines through the dots (Method 5).

Method 3: Dividing a circle by hand

Hand division gave astronomers their best circles until about 1780 and is still worth knowing. The method below follows the 18th-century London makers.

  1. Strike the circle. On the planished, flattened brass limb, strike two concentric arcs a few millimetres apart with the beam compass from the exact centre of the axis. The divisions will run between them.
  2. The first, exact points. With the beam compass set to the radius, step once from the zero point: that point is exactly 60°. Bisect 0–60 to get 30°; bisect again for 15°. For a quadrant, set off 90° as 60° plus 30°.
  3. Bisect down. Halve each 15° into 7½°, 3¾° and so on. Pure halving never gives a whole degree from 15°, so at a convenient stage divide by trial stepping into 3 or 5 (for example, divide 15° into 3 spaces of 5°, then each 5° into 5 of 1°). Step only a few spaces at a time, and correct each by a fraction of its miss.
  4. Use chords for checks. The straight distance (chord) between two points an angle θ apart on a circle of radius R is 2R × sin(θ/2). Work out chords for 30°, 45° and 90° (Geometry and Trigonometry, Algebra), set them on the beam compass from your scale, and check that each falls exactly on its point.
  5. A check scale. The famous maker George Graham divided his great quadrant twice: once into 90 degrees, and on a second arc into 96 parts, because 96 is 3 times 2 × 2 × 2 × 2 × 2 and can be reached almost entirely by bisection. Comparing the two scales by a table showed up errors in either.
  6. Cut the lines (Method 5). Number every 10° with steel number punches or by engraving.
Dividing a quadrant by hand centre 0° 90° Radius stepped oncelands exactly on 60° Bisectarcs from 0° and 60°cross on the 30° line beam compass check: chord of 90°= 1.414 × radius 1° spaces bytrial stepping Read both sides If the circle turns about a point a little off its centre, one reader gains what the other loses. reader A reader B true centre axis Average A and Bthe error cancels exactly
Fig. 1 Dividing a circle by hand. The radius stepped once round the arc marks exactly 60°; bisecting gives 30° and 15°; small spaces are found by trial stepping and checked by chords set off with the beam compass. Two readers 180° apart cancel any error in centring.

Method 4: The dividing engine

A dividing engine replaces the steady hand with a screw. Its heart is a large wheel with teeth round its edge, turned by a worm (a screw lying against the teeth — see Gears). Each whole turn of the worm moves the wheel exactly one tooth, and a dial or a plate of holes on the worm's handle divides that turn finely. The work is clamped to the wheel, and a cutting frame carrying a graver is drawn across it at each step.

The dividing engine, from above Worm wheel30–50 cm, 360 teeth, hobbed equal The workclamped centred on the wheel Worm1 turn = 1 tooth = 1° worm turns the wheel tooth by tooth Index plate60 holes: 1 hole = 1′ Cutting framehinged; lifts between cuts Graverdrawn inward
Fig. 2 The dividing engine. A large worm wheel carries the work; each turn of the worm moves it one tooth — one degree with 360 teeth — and an index plate on the crank divides each turn into 60 parts, so 1 minute of arc. A graver in a hinged cutting frame cuts each line along a fixed guide.

A first engine:

Part Size
Wheel Cast brass or bronze, 30–50 cm across, on a stiff, lapped vertical axis
Teeth 360 (or 180, or 720) fine teeth round the rim
Worm Single-start steel screw of matching pitch, with its shaft in lapped bearings
Index plate A disc on the worm crank with 60 holes and a spring pin: 1 hole = 1 minute of arc with 360 teeth
Cutting frame A graver in a hinged arm that swings down to cut and is drawn along a guide pointing at the axis; stops set the length of short, medium and long lines

Making the teeth equal — the hobbing trick. You cannot cut 360 perfect teeth by hand. Jesse Ramsden, who built the first great engine in London in the 1770s, solved it like this, and so can you:

  1. Divide the wheel's rim by hand (Method 3) into 360 spaces and cut shallow, rough notches.
  2. Turn the worm itself into a cutter: cut grooves across its thread, harden it, and you have a hob.
  3. Press the hob against the wheel and turn it, round and round the whole wheel, for many hours, feeding it in very slowly. Each part of the hob cuts every tooth, so errors in individual teeth are shared out and averaged away — the same principle that makes lapped balls equal (Making Ball and Roller Bearings).
  4. Replace the hob with a smooth, hardened worm of the same thread and lap them together with fine abrasive.

Linear engines divide straight scales the same way, with a long, accurate leadscrew moving a carriage. Lap the screw in a long split nut, end to end and back, to even out its pitch (Precision and Interchangeable Parts).

Method 5: Cutting and reading the lines

  1. The graver. Grind a hardened steel graver to a fine point and hone it on an oilstone and then on leather with rouge until it cuts a clean, bright shaving without tearing. A fine line in brass is about 0.02–0.05 mm wide and as deep.
  2. One stroke, one direction, always along the same straightedge or guide, pulled towards you. Make lines of three lengths — short for units, medium for fives, long for tens — so the eye can count.
  3. Fill the lines by rubbing warm black wax into them and scraping the surface clean with a slip of hardwood. Black lines in bright brass read far more easily.
  4. For the finest scales, inlay a strip of silver in the brass, flatten it, and divide on the silver. Silver is softer and whiter, takes a finer line, and does not darken quickly.
  5. Read between the lines with a vernier: a short sliding scale beside the main scale, with one more (or one fewer) division over the same length. If the circle is divided to half-degrees (30 minutes), a vernier of 30 divisions covering 29 half-degrees reads to 1 minute. How to make and read a vernier is in Precision and Interchangeable Parts; on circles it is the same, curved. For higher accuracy, read each line with a microscope whose crosshair is moved by a fine screw (a micrometer microscope): count turns of the screw from the crosshair to the nearest line.

Method 6: Graduating glass

Burettes, measuring cylinders, thermometer stems and the scales of meters are marked on glass.

  1. Coat the clean glass with a thin, even layer of beeswax with a little resin (dip it warm, let it set).
  2. Scratch the lines through the wax to the glass with a steel point, using the dividing engine, a template, or marks found by filling with weighed water (Laboratory Glassware, The Thermometer).
  3. Mark the lines without acid (preferred): scratch them with a diamond splinter or a sharp chip of hard quartz, or engrave them on the lathe with a small spinning copper disc charged with emery and oil, then fill with black wax or paint (Fluorspar and Fluorine Compounds gives more abrasive methods).
  4. The old acid method, in outline only. Makers once exposed the waxed glass to hydrofluoric acid or its vapour, the only common acid that dissolves glass, then melted off the wax and rubbed pigment into the etched lines. This book gives it only in outline because a small splash can kill; see Fluorspar and Fluorine Compounds.

Danger Hydrofluoric acid is one of the most dangerous chemicals in this book. It passes straight through skin without much pain at first, then destroys deep tissue and bone and pulls calcium out of the blood; a splash the size of a palm can stop the heart. Its vapour burns the lungs and eyes. Do not use it unless trained and with the antidote within reach. First aid for a splash: wash at once with plenty of running water for 5 minutes, then rub in calcium gluconate gel for at least 15 minutes and get medical help; chalk paste is useless and slaked lime burns the skin (Fluorspar and Fluorine Compounds). Scratching or engraving the lines avoids the acid entirely — do that.

Method 7: The spirit level

A bubble in a slightly curved tube of liquid always rises to the highest point. The flatter the curve, the further the bubble moves for a small tilt.

  1. Grind the vial. Take a straight glass tube 1–2 cm across and 8–15 cm long. Grind its inside into a very gentle barrel curve by working a slightly bulging lap of lead or wood back and forth with fine emery, rotating the tube, more in the middle than at the ends.
  2. Fill it with alcohol (Ether, Acetone and Solvents) or ether, which flows fast and does not freeze, leaving a bubble about a fifth of its length. Seal the ends in a flame or with cement.
  3. Mount it in a brass tube with a window, on a true base, with an adjusting screw at one end. Scratch or etch divisions on the glass a few millimetres apart.
  4. Sensitivity. If the inside curve has radius R, a tilt of 1 mm per metre moves the bubble 1/1,000 of R. A gentle curve of R = 20 m moves the bubble 2 mm for a tilt of 1 part in 10,000 (about 20 seconds of arc). Find it by tilting the level on a long beam with a fine screw.
  5. Adjust by reversal. Set the level on a surface, note the bubble, turn it end-for-end in the same place. If the bubble moves, adjust half the difference with the screw and half by tilting the surface; repeat until it does not move.

How to tell it worked

  • Closing error. Step or bisect all the way round a circle: the last division must land exactly on the zero. Note the miss before you cut any lines, and spread it.
  • Compare the halves. With the beam compass, measure the chord of 90° in all four quadrants; they must be equal under the lens.
  • Opposite readings. With two verniers 180° apart, read the circle at a dozen settings. If the difference between the two readings changes as you go round, the centre is off or the divisions are uneven.
  • Against a standard. Compare a scale line by line with your best master scale under a microscope (Measurement from Scratch).
  • Test the instrument on nature. A divided circle used to measure the angles of a large triangle on the ground should give 180° within your expected error (Surveying and Levelling); the altitude of the Pole Star should be the same every night (Astronomy).

Note Troubleshooting. Divisions creep — each a little too long → dividers opening as you step (slack joint), or work warming in your hand; tighten and work cold, and bisect rather than step. Lines ragged or burred → graver dull or cutting the wrong way; hone to a mirror finish and always pull in one direction. Scrape off burrs lightly with a burnisher. Readings disagree on opposite sides → circle off-centre; average both verniers, or re-centre the circle on its axis. Dividing engine gives a pattern of errors repeating every turn of the worm → worm bent or its bearings shaky; true and lap them. Errors repeating every turn of the wheel → wheel off-centre on its axis. Level bubble sticks or jumps → inside of the vial not smooth; grind finer, clean with alcohol. Brass instrument warps after finishing → soft (annealed) brass or stresses from casting; planish, rest it for weeks, then refinish.

Dangers

  • Hydrofluoric acid — see the warning above.
  • Molten brass gives off white zinc oxide fumes that cause "metal fume fever" (shivering, aches, fever for a day). Melt brass outdoors, upwind (Zinc and Brass).
  • Lacquer and alcohol catch fire easily; warm work away from flames.
  • Eyes. Hours with a lens strain the eyes. Work in good daylight, rest every half-hour, and look into the distance.
  • Gravers and points are needle-sharp; keep corks on them.

What this unlocks

Divided circles make the theodolite and the sextant (Measuring Angles: Theodolite and Sextant), the astronomer's transit instrument (Astronomy), and precise Maps and Mapmaking and Navigation. Divided scales make calipers, gauges and micrometers (Precision and Interchangeable Parts), the The Thermometer, The Barometer and burette, and the dials of electrical meters (Measuring Electricity). A dividing engine that cuts thousands of parallel lines per centimetre on glass or polished metal makes a diffraction grating for the The Spectroscope. The same skills make watches, the Chronometers and Stopwatches, orreries and armillary spheres, and the fine mechanisms of the The Typewriter and The Telephone.

How it was first done

Greek and Islamic astronomers divided brass astrolabes by hand, and built huge masonry instruments to get accuracy from sheer size: the meridian arc of Ulugh Beg's observatory at Samarkand (1420s) had a radius of about 40 m. In Denmark in the 1580s Tycho Brahe used slanting transversal lines to read his scales finer. The Portuguese mathematician Pedro Nunes proposed a reading device in 1542; Pierre Vernier described the simpler sliding scale named after him in 1631.

In London, George Graham divided an 8-foot mural quadrant for the Royal Observatory in 1725, with its 90° and 96-part scales; John Bird refined the method of beam compass and bisection and published it in 1767. Jesse Ramsden built his dividing engine, with a wheel about 1.1 m across cut by his hobbing method, in the 1770s; the Board of Longitude paid him to publish its design in 1777, on condition he divide sextants for other makers at a fixed price. From then on, cheap, accurate sextants made navigation by the stars routine. In the 1880s Henry Rowland at Johns Hopkins University in Baltimore built ruling engines with screws lapped to extraordinary accuracy and ruled the diffraction gratings that mapped the spectra of the sun and stars.

Source: content/entries/mechanics/instrument-making.md