Pass a direct current through a liquid and it pulls the liquid apart — water into hydrogen and oxygen, salt water into chlorine, caustic soda and hydrogen, and impure copper into copper pure enough for wire. How it works, Faraday's laws for working out how much you get, and how to design electrodes and cells.

Difficulty
●●●●●
Time
An afternoon to split water; a week to set up a copper refining tank; weeks to run a brine works
Steps from zero
15 prerequisites →

You need first

The BatterySalt

This unlocks

Chlorine and BleachHydrogen, Oxygen and GasesHydrogen Peroxide and Oxygen BleachSodium and Potassium MetalFuel CellsLithium BatteriesAluminiumCorrosion and Its PreventionElectroplatingMagnesiumNickel and Cobalt
The full path from nothing — 15 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Charcoal
  9. Pottery
  10. Hides and Leather
  11. Salt
  12. Fermentation
  13. Bellows
  14. Copper Smelting
  15. The Battery
  16. Electrolysis

Do them roughly in this order. See it on the tech tree →

Why it matters

Fire can pull oxygen out of iron ore, copper ore and lead ore. It cannot split salt, or water, or the ores of the most stubborn metals. An electric current can. Electrolysis — splitting a substance by passing electricity through it while it is dissolved or molten — is the second great chemical tool after fire.

With it you can make:

  • Pure copper, 99.9% or better, the only copper good enough for long Copper Wire coils and lines. All electrical copper in the modern world is refined this way.
  • Caustic soda (sodium hydroxide), the strong alkali for Soap, Paper, refining bauxite for Aluminium, and much more — and from the same cell, chlorine for Chlorine and Bleach and safe drinking water.
  • Hydrogen and oxygen, very pure, from water (Hydrogen, Oxygen and Gases).
  • Thin coats of metal on other metals: Electroplating.
  • Metals no fire can free: sodium, potassium, magnesium, calcium and Aluminium.

In 1807–08 Humphry Davy used electrolysis to discover six new elements in two years. It turned chemistry from guesswork into a science.

How it works

+− −−− +++ Anode (+)carbon, platinum orthe metal to dissolve Gas at the anodeoxygen or chlorine Cathode (−)iron, copper,lead or carbon At the cathodemetal is laiddown, or hydrogenbubbles off Electrolytesalt, acid or alkali in water − particles drift to the anode, + particles to the cathode
Fig. 1 An electrolysis cell. The positive plate (anode) and negative plate (cathode) stand in an electrolyte. Positively charged particles drift to the cathode, where metal or hydrogen comes out; negatively charged particles drift to the anode, where oxygen or chlorine is given off, or the anode metal dissolves.

When salt, acid, alkali or a metal salt dissolves in water, it falls apart into electrically charged particles called ions. Common salt, for example, becomes positive sodium ions and negative chloride ions. A liquid full of ions conducts electricity and is called an electrolyte. (Pure water has almost none and barely conducts.)

Dip two plates — electrodes — into it and connect them to a source of direct current:

  • The plate joined to the positive (+) side is the anode.
  • The plate joined to the negative (−) side is the cathode.

Positive ions (metals and hydrogen) drift to the cathode, take electrons from it, and turn back into metal or hydrogen gas. Negative ions drift to the anode, give up electrons, and come off as oxygen or chlorine — or, if the anode is made of a metal that dissolves easily, the anode itself dissolves into the liquid instead.

Alternating current does nothing useful: whatever is done in one half of each cycle is undone in the next. Electrolysis needs DC, from a The Battery, a The Rechargeable Battery or a The Generator with a commutator.

What comes out where

Electrolyte At the cathode (−) At a carbon or platinum anode (+) At a copper anode (+)
Water with washing soda, lye or a little sulfuric acid Hydrogen Oxygen Copper dissolves
Salt water (brine) Hydrogen, and caustic soda forms in the liquid Chlorine Copper dissolves, green-blue mess
Copper sulfate Copper Oxygen (liquid turns to acid) Copper dissolves — refining and plating
Molten salt (no water, over 800 °C) Sodium metal Chlorine —

Two rules cover most cases:

  1. Metals that do not react with water — copper, silver, gold, nickel, tin, lead and (with care) zinc — come out at the cathode from a water solution of their salts.
  2. Very reactive metals — sodium, potassium, calcium, magnesium, aluminium — never do. From water, hydrogen comes out instead. To get these metals you must electrolyse the molten salt, with no water at all.

The voltage needed

Each process needs a minimum push before anything happens, plus extra to drive the current through the liquid:

Process Volts per cell, in practice
Copper refining (copper anode, copper cathode) 0.2–0.4 V
Copper plating from a copper anode 0.5–1.5 V
Splitting water 1.8–2.5 V
Brine to chlorine and caustic soda 3.5–4.5 V
Aluminium from molten alumina and cryolite 4–5 V

Copper refining needs so little because nothing is really being split: copper dissolves at one plate and an equal amount comes out at the other. The voltage only has to overcome the resistance of the bath.

Faraday's laws: how much you get

In 1833–34 Michael Faraday showed that electrolysis obeys two exact laws.

  1. The amount of substance produced is proportional to the quantity of electricity that has passed — amps × hours. Twice the current for the same time, or the same current for twice the time, gives twice as much. Nothing else matters: not the size of the plates, the voltage or the strength of the liquid.
  2. The same quantity of electricity always releases the same "chemical amount": 26.8 ampere-hours release 1 g of hydrogen, 8 g of oxygen, 31.8 g of copper, 35.5 g of chlorine, 23 g of sodium or 108 g of silver. These are the atomic weights divided by the number of charges each ion carries.

The practical table, per ampere flowing for one hour:

Substance Grams per ampere-hour Notes
Hydrogen 0.0376 g About 0.45 litres at room temperature
Oxygen 0.298 g About 0.23 litres — half the hydrogen
Copper (from copper sulfate) 1.186 g The standard of Measuring Electricity
Silver 4.02 g
Nickel 1.09 g
Zinc 1.22 g
Lead 3.87 g
Chlorine 1.32 g
Caustic soda 1.49 g Formed with the chlorine
Aluminium 0.336 g From molten salt (Aluminium)

Real cells waste some current on side reactions, so you get less than the table: 90–97% for copper refining, 60–90% for a homemade brine cell. The ratio of what you get to what the table says is the current efficiency.

Energy. Watt-hours = volts × ampere-hours. So:

  • Refining 1 kg of copper takes 843 Ah; at 0.3 V that is only about 0.25 kWh — cheap.
  • Splitting water at 2 V takes about 54 kWh for 1 kg of hydrogen (about 4.8 kWh per cubic metre) — expensive.
  • Making 1 kg of chlorine at 4 V takes about 3 kWh, with 1.1 kg of caustic soda as a bonus.

A hand-cranked dynamo gives perhaps 50 W; a good The Waterwheel dynamo 500 W, about 12 kWh a day. Plan accordingly.

Designing a cell

Electrodes

Material As anode (+) As cathode (−)
Graphite, retort carbon, dense coke Good in brine and acid; slowly crumbles where oxygen comes off Good
Platinum Survives nearly everything; very rare Good
Lead Good in sulfuric acid: grows a brown skin of lead dioxide and lasts Good in acid
Iron, nickel Good in alkaline liquids (soda, lye) for splitting water; dissolves in brine or acid Good almost everywhere
Copper Dissolves — use only when you want it to (refining, plating) Good

The anode is the hard part, because whatever comes off it attacks it. The cathode can be almost any metal.

Current density

The current per area of electrode — amps per square decimetre (1 dm² = 10 × 10 cm = 100 cm²) — controls the quality of a deposit and the life of electrodes. Copper refining: 1.5–2.5 A/dm². Copper plating: 1–4 A/dm². Brine: 3–10 A/dm² on the anode. Too high and metal deposits come out dark, rough and spongy; too low and the work goes slowly. To get more production, use more electrode area, not more current per area.

Spacing, heat and separation

  • Spacing. The liquid between the plates has resistance, and every volt lost there turns into heat. Plates 2–5 cm apart are usual. Closer saves power but risks short circuits from growing deposits.
  • Heat. A cell takes volts × amps of power; all of it that is not stored as chemicals warms the bath. Refining tanks run best warm (50–60 °C); brine and bleach cells must be kept cool.
  • Keeping products apart. Hydrogen and oxygen must never mix; chlorine and caustic soda react if they meet. Separate them with a diaphragm: a wall of unglazed, lightly fired clay, which lets the current and a slow seep of liquid through but stops the gases and bulk mixing. Or let gases rise into separate hoods.

Vessels and connections

Glass and glazed stoneware (Glazes) suit everything. Wood lined with sheet Lead or coated thickly with pitch (Tar, Pitch and Glue) suits acid baths. Iron suits alkaline baths only. Keep all copper connections above the liquid — a joint in the bath dissolves — and use thick copper bars ("busbars") for large currents.

Matching cells to the supply

Cells can be connected in series, like battery cells, to use up a higher voltage. A 6 V dynamo can feed 15–20 copper refining tanks in series, or one brine cell with a little to spare. The same current then passes through every tank, and each produces its share.

Method 1: Splitting water

For a test tube of each gas, follow Hydrogen, Oxygen and Gases: two strips of iron in washing-soda water, or carbon or lead in dilute sulfuric acid, with tubes inverted over them. For larger amounts:

  1. Use iron or nickel plates in a 20–25% solution of caustic soda or caustic potash (Lye and Potash) in rainwater — the best electrolyte, and the plates do not corrode.
  2. Put a porous clay partition between the plates, and a separate inverted bell or hood over each side, sealed under the liquid, with a pipe from each to its own gasholder.
  3. Run at 2–2.5 V per cell and 1–3 A/dm². One amp for one hour gives about 0.45 litres of hydrogen and 0.23 litres of oxygen.

Never use salt water to make oxygen — you get chlorine instead.

Method 2: Refining copper

This turns fire-refined copper (Copper Wire) — 97–99% pure, with iron, arsenic, sulfur and other metals that ruin its conductivity — into cathode copper of 99.9%. As a bonus, any silver and gold in the copper is collected.

+− Anode (+)impure copper,2–3 cm thick, ina cloth bag Busbarsthick copper Tankwood linedwith lead Cathode (−)thin starter sheet of pure copper, grows Electrolytecopper sulfate+ sulfuric acid,kept at 50–60 °C Anode slimesilver, gold anddirt sink here 4–5 cm, anode to cathode; 0.2–0.4 V per tank
Fig. 2 A copper refining tank. Thick anodes of impure copper alternate with thin cathode sheets of pure copper. All anodes hang from the positive bar, all cathodes from the negative bar. Copper dissolves from the anodes and builds up on the cathodes; insoluble impurities, including silver and gold, sink as slime.
  1. Cast the anodes. Melt fire-refined copper and cast flat plates about 15 × 20 cm and 2–3 cm thick, each with a lug or a copper hook cast in at the top to hang from the bar.
  2. Make starter sheets. The cathodes begin as thin sheets of pure copper. For the first batch, hammer out the purest copper you have to about 0.5 mm. Afterwards, make them in the tank itself: hang a smooth copper or lead sheet, lightly wiped with tallow or a graphite wash, as a cathode for one day, then peel off the thin copper skin.
  3. Make the electrolyte. For each litre of rainwater: 180 g of copper sulfate crystals (The Battery) and about 100 ml (180 g) of strong sulfuric acid, poured slowly into the water (Sulfuric Acid). Add a tiny pinch — about 0.05 g per litre — of boiled bone glue (Glues and Adhesives) and a pinch of salt. These help the copper grow smooth and dense instead of in lumps.
  4. The tank. A wooden tank lined with sheet lead or thick pitch, or a large glazed stoneware vessel. For a start: 60 cm long, 40 cm wide, 40 cm deep, holding about 80 litres.
  5. Hang the plates alternately — anode, cathode, anode, cathode — with 4–5 cm between each anode and the next cathode. All anodes hang from the positive bar; all cathodes from the negative bar. Sew each anode into a loose bag of cotton cloth to catch the slime. Cathodes should be slightly larger than anodes, so that their edges do not grow rough trees.
  6. Current. 1.5–2.5 A for every dm² of cathode (counting both faces). The voltage across the tank will settle at 0.2–0.4 V. A tank with three cathodes of 2 dm² each side needs about 25 A.
  7. Keep it warm and moving. Stand the tank in a warm place or warm it gently to 50–60 °C (hand-hot); stir it or let it circulate slowly a few times a day. A warm bath conducts better and gives smoother copper.
  8. Harvest. At 2 A/dm², each cathode face grows about 0.6 mm a day. After 7–10 days, lift the cathodes out: they will be thick, salmon-pink plates. Each anode lasts about two crops of cathodes. Melt the cathode copper under charcoal and cast it into bars for drawing wire.

Daily care:

  • Check for short circuits. A cathode growing a lump that touches the anode takes a huge current and stops working. Run a compass along the hangers: a shorted plate swings it violently. Knock the lump off.
  • Keep the acid and copper up. Test a cupful by weighing (Sulfuric Acid). If the blue colour fades, add copper sulfate.
  • Bleed the bath. Iron, nickel and zinc from the anodes stay dissolved and slowly build up. Each week replace a tenth of the bath with fresh electrolyte. Evaporate the old liquid to recover copper sulfate crystals.
  • Collect the slime. Every crop, wash out the anode bags and the bottom of the tank. Dry the black mud. It holds the silver and gold that were in the copper; recover them by cupellation (Gold and Silver).

Method 3: Caustic soda, chlorine and hydrogen from brine

If you want only household bleach or water disinfectant, use the simple single-pot cell in Chlorine and Bleach. This method keeps the products apart, so you get caustic soda to use and chlorine to turn into bleaching powder. It is a works process. Do it outdoors and only once you can handle chlorine safely.

−−+ Carbon anode (+)graphite or retort carbon Brine inlevel kept higher inside Porous potunglazed clay —the diaphragm Iron cathode (−)hydrogen andcaustic soda form brine seepsslowly outward Hydrogenvent high,outdoors Chlorinesealed pipe Absorberslaked lime or causticsoda: makes bleach Cell liquorcaustic soda + salt
Fig. 3 A diaphragm cell for brine. Brine enters the porous clay pot, where chlorine comes off the carbon anode and is led away through a sealed pipe to be absorbed. The brine seeps outward through the pot wall to the iron cathode, where hydrogen comes off and caustic soda forms. The caustic liquor runs out at the bottom.
  1. Purify the brine. Dissolve as much Salt as will dissolve in water (about 310 g per litre). Stir in a little washing soda (Soda Ash and Baking Soda) and a little slaked Lime, let it stand a day, and pour off the clear liquid. This removes calcium and magnesium, which would clog the diaphragm.
  2. The diaphragm. An unglazed, lightly fired clay pot (Pottery) about 12 cm across and 30 cm tall — like the porous pot of a Daniell cell but larger.
  3. The anode. A graphite or retort-carbon rod or plate (Chlorine and Bleach says where to find them) standing in the pot. Any metal anode is destroyed at once.
  4. The cathode. Iron sheet bent round the outside of the pot, 2–3 cm from it, in an outer vessel of iron or glazed stoneware.
  5. Seal the pot. Cover it with a clay or wooden lid luted tight with clay and pitch, with the anode, a brine funnel and a chlorine outlet passing through. Lead the chlorine through a glass, glazed clay or lead pipe to an absorber — a closed pot of slaked lime (for bleaching powder) or of caustic soda solution (for liquid bleach), with its own outlet led into a second pot of lime water.
  6. Feed it. Keep the brine level inside the pot 3–5 cm higher than outside. The liquid then seeps steadily outward through the wall, carrying salt to the cathode and stopping the caustic soda from creeping back to the anode, where it would spoil the chlorine.
  7. Run it. 3.5–4.5 V per cell, about 3–5 A for every dm² of anode. Vent the hydrogen from the outer vessel through a pipe that ends high in the open air.
  8. Draw off the cell liquor from the bottom of the outer vessel. It holds about 8–12% caustic soda and a lot of salt.
  9. Concentrate it. Boil the liquor in an iron pan, outdoors. As it gets stronger, salt crystallises out (salt dissolves poorly in strong caustic); rake it out and put it back in the brine. When the liquid is thick and hot, about half of it is caustic soda. Let it cool to a white solid, or keep it as a strong solution in an airtight iron or stoneware vessel — it greedily drinks water and carbon dioxide from the air.

What to expect: every 100 ampere-hours gives at best about 130 g of chlorine, 150 g of caustic soda and 45 litres of hydrogen. A homemade cell gives perhaps two-thirds of that.

Method 4: Molten salts, in outline

To free the most reactive metals you must electrolyse a melted salt, without water, in an iron or carbon pot at 650–1,000 °C, with heavy currents. Davy first did it with potash and soda in 1807. Sodium is made from molten caustic soda or salt; magnesium from molten magnesium chloride; aluminium from alumina dissolved in molten cryolite (Aluminium). Molten sodium and potassium catch fire in air and explode on touching water. This is work for a well-equipped works with a steady supply of several kilowatts, not a first project.

How to tell it worked

  • Water: the hydrogen tube fills twice as fast as the oxygen tube. A glowing splint bursts into flame in the oxygen (Hydrogen, Oxygen and Gases).
  • Faraday check: weigh what you made and compare with the table. If you got close to the expected amount, the cell is efficient. If you got half, look for leaks, short circuits or mixing.
  • Refined copper is salmon-pink, dense and fine-grained. A strip bends double and back without cracking. Drawn into 1 mm wire, 45.6 m should measure 1 Ω at 20 °C (Measuring Electricity) — impure copper reads 5–50% higher.
  • Chlorine bleaches a damp coloured cloth or flower petal at once, and smells sharp and choking even in tiny amounts.
  • Caustic soda solution feels slippery between the fingers (rinse at once), turns turmeric paper red-brown, and dissolves a piece of animal fat when warmed into soapy jelly (Soap).

Note Troubleshooting. No gas, no deposit → AC instead of DC, a broken connection, or a joint dissolving in the liquid. Keep all joints above the liquid. Dark, spongy or powdery copper → current density too high, bath too cold, or too little acid. Lower the current or add cathode area. Copper grows in lumps and trees → add a pinch of glue; check that cathodes are larger than anodes; stir the bath. Tank voltage creeps up over days → anode covered with slime or the cloth bag clogged; scrape the anode and wash the bag. Brine cell gives little chlorine and much oxygen → brine too weak; keep it saturated. Chlorine smells weak but caustic is poor → the diaphragm is cracked or too porous and the two sides are mixing. Fire a new pot slightly harder. Carbon anode crumbling fast → too much current for its area, or weak brine making oxygen. Use more or bigger anodes.

Dangers

Danger Chlorine is a poison gas. A few breaths of strong chlorine damage the lungs and can kill hours later as they fill with fluid. Run every chlorine-producing cell outdoors, upwind, in sealed vessels led to an absorber. If you smell it strongly, switch off and walk away upwind; anyone who has breathed it must rest, sit upright, and be watched for a day. See Chlorine and Bleach.

Danger Hydrogen explodes. Every cell that makes hydrogen — water, brine, even a refining tank — must stand in moving air. Never let hydrogen collect under a roof or in a closed box, never bring a flame or a spark near a cell, and never mix hydrogen with oxygen or chlorine: hydrogen and chlorine explode in sunlight. See Hydrogen, Oxygen and Gases.

Danger Caustic soda blinds. Strong caustic dissolves skin and the clear front of the eye within seconds, and the damage is often permanent. Wear eye protection whenever you handle it, hot or cold. Wash any splash in the eye with running water for at least 30 minutes, holding the eyelids open. Boiling caustic spits — keep the lid half on and stand back. See Lye and Potash.

  • Acid baths — sulfuric acid in refining and coulometer baths burns skin and eyes; always add acid to water (Sulfuric Acid).
  • Heavy currents. The voltage is low, but busbars carrying tens or hundreds of amps get hot, and a ring or metal watch that falls across them can burn to the bone. Take off rings and bracelets.
  • Lead. Lead linings and anodes poison slowly; wash hands before eating (Lead).
  • Arsenic from impure copper ends up in the slime and the old electrolyte. Do not pour them where animals drink.

What this unlocks

How it was first done

In May 1800, within weeks of hearing of Volta's pile, William Nicholson and Anthony Carlisle in London put wires from a pile into water and saw hydrogen and oxygen bubble off — the first electrolysis. In 1807 Humphry Davy, at the Royal Institution, used a huge battery to electrolyse barely damp molten potash and saw globules of a new metal, potassium, burst into flame; within days he had sodium, and by 1808 calcium, barium, strontium and magnesium. Michael Faraday, Davy's former assistant, worked out the laws of electrolysis in 1833–34 and, with the scholar William Whewell, coined the words electrolysis, electrode, anode, cathode, ion and electrolyte. James Elkington in Birmingham, a pioneer of electroplating, patented electrolytic copper refining in 1865 and built a refinery at Pembrey in Wales in 1869, powered by dynamos. Charles Hall and Paul Héroult found the electrolytic route to aluminium in 1886, and the first works making chlorine and caustic soda from brine with diaphragm cells opened in Germany around 1890.