Part 8 · Chemistry
Identifying Substances
How to find out what something is made of with a flame, a blowpipe, a charcoal block and a rack of test tubes — which metal is in an ore, whether a well is fouled by sewage or a pot glaze leaks lead, whether milk has been watered or flour cut with chalk. Every test is checked against a reference set of known samples you build yourself.
- Difficulty
- ●●●●●
- Time
- An evening to learn the flame and blowpipe tests; weeks to months to gather a full set of reagents and reference samples
- Steps from zero
- 10 prerequisites →
The full path from nothing — 10 steps before this one
- Fire
- Finding and Preparing Clay
- Pottery
- The Kiln
- Lime
- Lye and Potash
- Fermentation
- Glass
- Acids, Bases and Testing
- Laboratory Glassware
- Identifying Substances
Do them roughly in this order. See it on the tech tree →
Why it matters
Sooner or later every chapter asks what is this stuff? Is this heavy grey rock lead ore? Is the well safe for a baby's bottle? Has the miller cut the flour with chalk, does the new glaze leak lead into the soup, did your batch of soda come out as soda?
Qualitative analysis — finding which substances are present, rather than how much — answers these questions with heat, a few chemicals, glass tubes and careful eyes. It is how chemists found most of the elements, how miners found ore and how food inspectors cleaned up adulterated bread and milk.
It also keeps you honest. A reaction that "worked" proves nothing until a test shows you made what you meant to make (The Scientific Method).
How it works
Every element behaves in its own way when it is heated or meets certain other chemicals. Analysis is a set of signatures:
- Colour in a flame. Some metals colour a hot flame: sodium yellow, copper green, potassium lilac.
- Behaviour under the blowpipe. A blowpipe turns a lamp flame into a small, hot jet whose tip oxidises (adds oxygen) and whose inner blue cone reduces (takes oxygen away, like a furnace — Iron (the Bloomery)). On charcoal, many ores reduce to a bead of metal and leave a coloured coating; in a bead of melted borax, metal oxides colour the glass.
- Precipitates. Add the right reagent (a chemical used for testing) to a solution and a solid — a precipitate — appears with a telling colour: white for chloride with silver, blue-black for iron with tannin.
- Gases and smells. Carbonates fizz with acid; ammonium salts smell of ammonia when warmed with lime.
No single test is proof. Two things make it reliable:
- A reference set — known, pure samples of each substance, tested side by side with your unknown. You learn what "brick-red" means by seeing calcium next to your sample, not by reading it.
- A blank — the same test done on clean distilled water and clean reagents. If the blank also turns cloudy, the cloudiness came from your reagents, not your sample.
What you need
| Item | Notes |
|---|---|
| Spirit lamp | A nearly colourless flame, burning strong alcohol or wood spirit (Laboratory Glassware, Ether, Acetone and Solvents) |
| Mouth blowpipe | A tapered brass or glass tube about 20 cm long, tip about 0.5 mm (Bellows) |
| Charcoal blocks | Dense hardwood charcoal ground flat, about 10 × 4 × 3 cm, a shallow hollow at one end (Charcoal) |
| Wire loop | Best: 5 cm of fine platinum wire sealed into a glass rod (Platinum and the Platinum Metals). Otherwise thin iron wire cleaned in Hydrochloric Acid before each test, or a hard carbon rod (The Battery). |
| Cobalt-blue glass | A small deep-blue piece (Glass, Glazes, Nickel and Cobalt), for the potassium test |
| Test tubes | 12–24, with droppers, a white glazed plate and filter papers (Laboratory Glassware, Paper) |
| Distilled water | Several litres; every test uses it (Distillation) |
| Balance, magnet | Measurement from Scratch, Magnets |
| Notebook | Every test, result and blank, written down (Writing and Numbers) |
Reagents
Make these up in small, labelled, stoppered bottles. Most come from other chapters.
| Reagent | How to get it | What it tests for |
|---|---|---|
| Hydrochloric, nitric and sulfuric acids, dilute (1 part in 5–10 of water) | Hydrochloric Acid, Nitric Acid, Sulfuric Acid | Carbonates (fizz), dissolving samples |
| Ammonia water | Ammonia | Copper (deep blue), many precipitates |
| Lime water | Slaked lime shaken in water, left to settle; use the clear liquid (Lime) | Carbon dioxide (turns milky) |
| Silver nitrate, 2–5% | Silver dissolved in nitric acid, dried to crystals, redissolved in distilled water. Keep in a dark bottle (Nitric Acid). | Chloride, iodide, phosphate |
| Barium chloride, 5% | Heavy spar (barite) heated with charcoal, then dissolved in hydrochloric acid — outdoors, it gives off hydrogen sulfide. Poisonous. | Sulfate |
| Tannin (oak-gall extract) | Crushed oak galls soaked in water (Ink, Dyes and Mordants) | Iron (blue-black) |
| Green vitriol (iron sulfate) | Sulfuric Acid, Dyes and Mordants | Nitrate (brown ring) |
| Liver of sulfur | 2 parts dry potash melted with 1 part sulfur in a covered crucible to a brown cake; dissolve a little in water as needed (Lye and Potash, Sulfur) | Lead, copper, silver, mercury (dark precipitates) |
| Salt of sorrel (oxalate) | Juice of wood sorrel or rhubarb leaves, boiled down and crystallised | Calcium (white) |
| Starch water and iodine | Iodine | Starch, and iodine itself |
| Soap solution | Shavings of pure soap dissolved in alcohol and water (Soap) | Water hardness |
| Fehling's solution, in two bottles | A: 7 g copper sulfate in 100 ml water. B: 35 g Rochelle salt (from wine-barrel tartar and soda — Beer, Wine and Cider, Soda Ash and Baking Soda) and 10 g caustic soda in 100 ml water. Mix equal parts just before use. | Sugars (red) |
| Borax and soda ash | Soldering and Brazing, Soda Ash and Baking Soda | Blowpipe fluxes |
| Molybdate (advanced) | Molybdenite ore roasted, the white oxide dissolved in ammonia water (Molybdenum) | Phosphate (yellow) |
Where to find it
Most reagents come from earlier chapters. The few new raw materials: barite (heavy spar — pale, glassy, flat-bladed crystals in lead and zinc veins, startlingly heavy for a pale stone), cobalt ore for blue glass (Glazes), wood sorrel (sour, clover-like woodland plants; rhubarb leaves hold the same oxalate but are poisonous to eat) and molybdenite (soft, greasy, lead-grey flakes in granite veins — Rocks and Minerals).
Method 1: Flame tests
- Clean the loop. Dip it in dilute hydrochloric acid and hold it in the hottest part of the flame. Repeat until the flame shows no colour at all. Even a fingerprint gives a sodium flash.
- Load it. Dip the hot loop in acid, then in a pinch of the powdered sample, so a little sticks. Acid turns the metal into its chloride, which vaporises easily and gives the brightest colour.
- Look. Hold the loop in the edge of the flame, in a dim place. Watch the first flash and what follows.
- Compare with your reference samples.
| Colour of flame | Means |
|---|---|
| Strong yellow-orange, lasting | Sodium — almost everything shows a trace. Only a strong, long flare matters. |
| Lilac (pale violet), short | Potassium. Through cobalt glass: pinkish-violet, while sodium vanishes. |
| Brick-red / orange-red | Calcium (lime, chalk, gypsum) |
| Crimson | Strontium or lithium |
| Pale apple-green | Barium |
| Green to blue-green | Copper (blue with a green edge if moistened with hydrochloric acid) |
| Vivid green | Boron: borax moistened with sulfuric acid; or boric acid in burning alcohol |
| Pale grey-blue | Lead, arsenic or antimony — check with the blowpipe, and see Dangers |
Method 2: Blowpipe on charcoal
Learning to blow. Puff out your cheeks and breathe through your nose while your cheeks keep pushing air through the blowpipe — a steady jet, not puffs. It takes an afternoon. Lay the tip just inside the flame of a candle or lamp and blow along the wick: a long, pointed, roaring flame forms. Its outer pale tip is the oxidising flame; the inner blue cone is the reducing flame, and the hottest point is just beyond the blue cone's tip.
The charcoal test.
- Mix a pinch (about the size of a lentil) of powdered sample with two pinches of soda ash and a drop of water. Place it in the hollow of the charcoal block.
- Heat it with the reducing (blue) flame for a minute or two, then let it cool.
- Look at the bead (try it with a knife: does it flatten or shatter?) and the coating on the charcoal around it, both hot and cold.
| Result | Probably |
|---|---|
| Soft grey bead that flattens under a hammer; yellow coating near it | Lead (Lead) |
| Bright white soft bead, no coating | Silver (Gold and Silver) |
| Yellow soft bead | Gold |
| Red metal flakes, no coating | Copper (Copper Smelting) |
| White soft bead; pale coating, white when cold | Tin (Tin and Pewter) |
| Brittle bead; dense white coating close to it, white fumes | Antimony (Antimony and Bismuth) |
| Brittle bead; orange-yellow coating | Bismuth |
| No bead; coating yellow when hot, white when cold | Zinc (Zinc and Brass) |
| No bead; white coating far away; garlic smell | Arsenic — stop at once (Arsenic) |
| Grey powder picked up by a magnet | Iron, nickel or cobalt (Finding and Identifying Ores) |
The borax bead. Heat the wire loop, dip it in borax, and heat until the borax swells and melts to a clear glass bead. Touch it to a tiny speck of sample and heat again in the oxidising flame; let it cool and look through it against the light. Then heat it in the reducing flame and look again.
| Bead colour, cold: oxidising flame | Reducing flame | Metal |
|---|---|---|
| Deep blue | Deep blue | Cobalt |
| Blue (green while hot) | Opaque red-brown | Copper |
| Yellow to brownish | Bottle green | Iron |
| Violet (amethyst) | Colourless | Manganese |
| Green | Green | Chromium |
| Red-brown | Grey, cloudy | Nickel |
A fuller treatment of the borax bead, for the steel-making metals, is in Alloy and Stainless Steels.
Method 3: Tests in solution
Dissolving the sample. Grind it fine. Try, in order: distilled water; warm dilute hydrochloric acid; warm dilute nitric acid. Note what dissolves and what fizzes. Filter, and use the clear liquid. Use a few drops of solution and a drop or two of reagent in a test tube; tap the tube and watch against a white and then a black background.
| Looking for | Add | A positive result |
|---|---|---|
| Carbonate | Dilute acid to the solid | Fizzes; the gas, led or poured into lime water, turns it milky |
| Chloride (salt, brine, sewage) | A drop of nitric acid, then silver nitrate | White curdy precipitate that darkens in sunlight and dissolves in ammonia water |
| Iodide | The same | Yellow, does not dissolve in ammonia |
| Sulfate (gypsum, vitriols, alum) | A drop of hydrochloric acid, then barium chloride | White precipitate that does not dissolve in acid |
| Nitrate (saltpeter, manure-fouled water) | Mix with an equal volume of fresh green-vitriol solution; tilt the tube and slowly run concentrated sulfuric acid down the side so it forms a layer underneath | A brown ring where the layers meet |
| Phosphate | Nitric acid and warm molybdate | Canary-yellow precipitate. Or, in a neutral solution, silver nitrate gives yellow, dissolving in nitric acid |
| Ammonium | Warm with slaked lime or lye | Smell of ammonia; damp red-cabbage paper over the mouth turns green (pH, Indicators and Buffers) |
| Iron | Tannin (oak-gall) solution | Blue-black — the colour of ink |
| Copper | Ammonia water, in excess | Deep royal blue solution. A clean iron nail in the acid solution comes out copper-coated. |
| Lead, copper, silver, mercury | Liver of sulfur solution | Black or dark brown precipitate |
| Calcium | Salt-of-sorrel solution, made slightly alkaline with ammonia | White fine precipitate |
| Starch | Iodine | Blue-black |
| Sugar (glucose, honey, fruit sugar) | Fehling's A + B, boil 1–2 minutes | Blue turns green, yellow, then brick-red |
| Protein (in urine) | Boil the top of a tube of clear urine, then add a few drops of vinegar | Cloudiness that stays after the vinegar |
Arsenic, antimony and mercury — the Reinsch test. Acidify the liquid (or food, finely chopped, with water) with hydrochloric acid, drop in a bright strip of copper and simmer for 10–30 minutes. A dark grey or black film on the copper means arsenic or antimony; a silvery film means mercury. Keep the strip in a sealed tube as evidence; never heat it near your face.
The systematic scheme (in outline). Professional chemists split an unknown mixture into groups — metals whose chlorides do not dissolve; those thrown down by hydrogen sulfide gas in acid; those thrown down by sulfide in alkali; those thrown down by carbonate; and the rest — then test within each group. It works, but hydrogen sulfide is a deadly gas: learn the single tests first, and attempt the scheme only with a fume cupboard that draws properly to the outside.
Testing water
| Test | How | What it tells you |
|---|---|---|
| Look and smell | A tall clear glass against white; warm a bottle half full, shake and sniff | Cloudiness, colour, rotten-egg or sewage smells |
| Hardness | 40 ml of water in a stoppered bottle; add soap solution a drop at a time, shaking, until a lather lasts 2 minutes. Count the drops. | Rain or distilled water needs only a few drops. Many drops = hard water: scale in boilers (Boilers and Pressure Vessels), soap wasted (Soap). |
| Chloride | Silver nitrate, as above | A faint haze is normal. A well with much more chloride than its neighbours is probably fouled by sewage or urine — or seawater. |
| Nitrate | Brown-ring test | Even a faint ring is a warning. A distinct ring: do not use for babies' feeds, which can turn babies blue and kill them. Look for manure or latrines uphill. |
| Iron | Tannin or strong tea | Blue-black: iron. Harmless, but stains and tastes. |
| Lead | Acidify with a drop of acetic acid, then liver of sulfur | Darkening: a lot of lead, from lead pipes or lead-glazed tanks. A clear result does not prove the water safe. |
Warning No chemical test shows germs. Water can pass every test above and still carry cholera or typhoid. Judge a water source by where it comes from — well-built wells, far (at least 30 m) and uphill from latrines and animal pens (Wells and Cisterns, Sanitation and Germs) — and boil, filter or chlorinate it (Finding and Purifying Water, Water Treatment for a Town). To find germs themselves, you must grow them (Culturing Microbes).
Testing food, pottery and medicine
- Watered milk. Fresh whole milk is a little heavier than water (a litre weighs 1,028–1,034 g). Make a simple floating stick — a thin glass tube or a straight stick weighted with wax at one end — and mark how deep it floats in milk you know is pure. Watered milk lets it sink deeper. Starch or flour added to thicken watered milk turns blue with iodine.
- Chalk, plaster or bone ash in flour. Shake a spoonful in water with a little acid: chalk fizzes. Burn 10 g of flour to white ash in a hot clay dish and weigh the ash: white wheat flour leaves about 0.05 g, wholemeal up to about 0.2 g. Several times more means mineral was added. Test your own known flour alongside.
- Copper in green pickles or peas. Put a bright iron nail in the acidified liquid for an hour: a copper coat means copper salts were added for colour. They are poisonous.
- Lead in pottery glazes. Fill the pot with vinegar (Vinegar and Pickling) and leave it 24 hours. Pour off the vinegar and test it with liver of sulfur: darkening means lead is coming out of the glaze into food. Do not use that pot for acid food, ever (Glazes, Pottery).
- Sugar in urine (sign of diabetes — Chronic Diseases): a few drops of urine boiled with Fehling's turn brick-red. Protein in urine in late pregnancy (boiling test, above) can warn of the dangerous condition called pre-eclampsia (Safe Childbirth, Examining a Patient).
Testing ores
Start cheap and work up (Finding and Identifying Ores, Rocks and Minerals): colour, shine and streak (the colour of the powder scraped on unglazed pottery); density (weight in air ÷ loss of weight when hung in water — quartz about 2.6, iron ores about 5, galena about 7.5); magnet, acid and hardness; then the flame and blowpipe tests above to name the metal. Only an assay — a small trial smelt weighed before and after — tells you whether there is enough of it to mine (Gold and Silver, Lead, Copper Smelting).
Keeping a reference set
Your reference set is the most valuable thing in the laboratory. Collect 30–50 pure, known samples — salt, potash, soda, lime, gypsum, saltpeter, alum, the vitriols, borax, sulfur, each metal you make and each ore you have proved — in small stoppered vials, labelled and numbered. Keep a page for each: where it came from, how you know what it is, and how it behaves in every test. Test unknowns side by side with the sample you suspect and with a blank, and date and renew reagents when their blanks stop being clean.
How to tell it worked
You have learned analysis when you can be given five unlabelled samples from your reference set by someone else, and name all five correctly, with blanks clean and notes written. Do this exercise with every new apprentice.
Note Troubleshooting. Every flame is yellow → sodium from dirty wire, fingers or tap water. Clean the loop in acid until the flame is colourless; use distilled water; look through cobalt glass. Blanks go cloudy → dirty glassware or reagents made with ordinary water. Rinse everything three times in distilled water; remake the reagent. Blowpipe flame flickers yellow and smoky → you are blowing in puffs, or the tip is too far out of the flame. Steady pressure from the cheeks; tip just inside the flame. No bead on charcoal → not enough heat or not enough soda; or the metal is one that does not form a bead (iron, zinc). Use the magnet and the coating. Silver nitrate turns everything brown or grey → it has been in the light, or the solution was alkaline. Acidify with nitric acid first; keep the bottle dark. Brown ring test fails with known saltpeter → the green vitriol has turned yellow (oxidised); make it fresh.
Dangers
Danger Arsenic, mercury and lead fumes. Heating ores on charcoal can release them. A garlic smell means arsenic: stop, step back into fresh air, and do not heat that sample again indoors. Work in the open or under a hood that draws to the outside. Wash your hands before eating, and never use laboratory spoons, cups or glasses for food.
Danger Hydrogen sulfide (rotten-egg gas), from sulfides and acid or from making barium chloride, is nearly as poisonous as cyanide. After a few breaths it deadens your sense of smell, so the danger seems to go away while it is still there. Only outdoors or with a working fume cupboard.
- Never taste an unknown, and never put your nose to the tube: waft the air towards you with your hand. Early chemists tasted their samples, and many paid for it.
- Barium salts, oxalate, molybdate and liver of sulfur are poisonous if swallowed. Silver nitrate stains skin black and blinds if splashed in the eyes.
- Acids, lye and hot glass: see Acids, Bases and Testing and Laboratory Glassware.
What this unlocks
Analysis guides all the rest: grading ore (Mining and Tunnelling, Finding and Identifying Ores), checking every batch of acid, soda and fertiliser (Chemical Fertilisers), keeping water safe (Water Treatment for a Town), stopping food fraud and diagnosing illness (Examining a Patient). Measuring how much is present — weighing precipitates and titrating (Acids, Bases and Testing) — is quantitative analysis, the next step; instruments that do both are in Analytical Instruments and Chromatography. Flame colours spread out by a prism become the spectroscope (The Spectroscope), which reads the elements in the Sun (Astronomy).
How it was first done
Robert Boyle, in England in the 1660s–1680s, tested mineral waters with plant colours and a solution of silver. The Swedish mining chemists made the blowpipe a tool: Axel Fredrik Cronstedt in the 1750s, Torbern Bergman and Johan Gottlieb Gahn in the 1770s, and Jöns Jacob Berzelius, whose 1820 book on the blowpipe served mineralogists for a century. Bergman also published one of the first methods for analysing water (1778).
In 1820 Frederick Accum in London exposed chalk in flour, copper in pickles and lead in sweets in his Treatise on Adulterations of Food; British food laws followed from 1860. James Marsh devised his arsenic test in 1836, Hugo Reinsch his copper-strip test in 1841, and Carl Remigius Fresenius published the systematic group scheme the same year. In 1859–1860 Robert Bunsen and Gustav Kirchhoff in Heidelberg looked at flame colours through a prism, found that each element gives its own pattern of bright lines, and with it discovered caesium and rubidium.