◆ Rebuild

Part 4 · Food and Farming

Sickle, Scythe and Hand Harvest Tools

The tools that bring the harvest in — flint and steel sickles, the long scythe and how to set it up, mow with it and keep it razor sharp by peening and honing — plus rakes, pitchforks, flails and a threshing floor.

Difficulty
●●●●●
Time
A day to make a flint sickle; a week to fit and learn a scythe; a season to mow well
Steps from zero
15 prerequisites →

You need first

Farming from SeedAxes, Chisels, Knives and Planes

This unlocks

Hay and Silage
The full path from nothing — 15 steps before this one
  1. Stone Tools
  2. Fire
  3. Cordage and Rope
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Charcoal
  9. Farming from Seed
  10. Hides and Leather
  11. Bellows
  12. Iron (the Bloomery)
  13. Blacksmithing
  14. Steel
  15. Axes, Chisels, Knives and Planes
  16. Sickle, Scythe and Hand Harvest Tools

Do them roughly in this order. See it on the tech tree →

Why it matters

Grain ripens all at once. A field of wheat that is ready today will start dropping its seed in a week or two, and a storm can flatten it overnight. Hay must be cut, dried and stacked between rains. Whatever your field can grow, you can only keep what you can cut and carry in time. Harvest is the bottleneck of every farming year, and for most of history it was the one time when everyone — children, the old, the smith and the priest — went to the fields.

Better harvest tools let fewer people bring in more. A person with a sickle cuts about 0.1–0.2 hectares of grain a day. With a scythe, a good mower cuts about 0.4 hectares of grass a day, and with a grain cradle on the scythe, 0.8–1 hectare of wheat. That difference decides how large a field one family can sow — and how much hay they can store to keep animals through the winter (see Keeping Animals).

This chapter covers the cutting tools, the rakes and forks for handling the crop, and the tools and floor for threshing — knocking the grain from the straw. How to judge ripeness, stook sheaves, winnow and grind is in Grain, Flour and Bread.

How it works

Grass and grain stalks are tough, springy tubes. A blade cuts them in one of two ways:

  • Sawing. A serrated (toothed) edge drawn across a bunch of stalks held in the hand. The teeth catch and tear each stalk. A toothed edge stays working even when dull. This is the sickle: you grab a handful and pull the blade toward you.
  • Slicing at speed. A very thin, very sharp edge moving fast through standing stalks, which are held upright only by their own stiffness and roots. The edge must be thin enough to pass through before the stalk bends away. This is the scythe: a long blade swung close to the ground, slicing with a drawing cut as it sweeps.

The scythe's edge is so thin it would chip if it were hard like a knife. Instead the blade is steel tempered softer than a knife — springy rather than hard — and the edge is thinned by hammering (peening) rather than grinding. Cold hammering squashes the steel out into a feather-thin edge and also work-hardens it a little. A few strokes of a stone (honing) then make it razor-sharp. When it dulls, you peen it again. A well-kept blade lasts a lifetime.

What you need

Tool Material Size
Flint sickle Wooden haft; 4–8 flint blades; birch tar or resin glue Haft 30–45 cm
Steel sickle Steel or iron bar; wooden handle Blade 40–50 cm round the curve
Scythe blade Spring-tempered steel 55–75 cm for grass; 80–100 cm for grain
Snath (handle) Ash, willow or spruce, or a naturally curved sapling 1.5–1.8 m, two hand grips
Whetstone Fine sandstone or other natural fine abrasive 20–25 cm long, cigar-shaped
Stone holder Cow horn, wooden or clay pot, worn on the belt Holds water
Peening anvil and hammer Hard steel Anvil face 2–3 cm, hammer 300–500 g
Hay rake Ash or willow handle, hardwood head and teeth Handle 1.8 m, head 60 cm
Pitchfork Naturally forked ash, hazel or willow; or iron tines 1.5–2 m
Flail Ash handle; holly, blackthorn or other heavy hardwood beater; rawhide Handle 1.2–1.5 m, beater 70–90 cm

Where to find it

  • Flint, chert or obsidian for the first sickle blades: see Stone Tools. You want long, thin flakes with one straight sharp edge.
  • Glue: birch tar (made by heating birch bark without air, the same way as Charcoal) or pine resin mixed with powdered charcoal and a little beeswax (about 5 parts resin, 2 parts charcoal dust, 1 part beeswax), melted together. See Glues and Adhesives.
  • Snath wood: a young ash or willow with a gentle natural curve, or a straight pole you steam-bend (see Steam-Bending Wood). Tough, light and springy. Grips are short pegs of the same wood.
  • Whetstone: fine-grained, even sandstone from a river bed or cliff — hard enough not to crumble, gritty enough to bite steel. Test by rubbing a knife on it wet: good stone leaves a grey slurry and a bright, even scratch pattern. Shape it by rubbing on a coarser stone (see Abrasives and Grinding Stones).
  • Forked sticks for pitchforks: look in hazel, ash and willow coppice for stems that split evenly into two or three; or train a growing shoot into a fork over a few years by tying it.

Method 1: The flint sickle

The oldest harvest tool. It works surprisingly well on ripe grain.

Flint sickle pull stroke Flint blades3–5 cm, notchedinto fine teeth Gluebirch tar, or resin +charcoal + beeswax Haft30–45 cm, grooved Steel sickle Backthick Toothed edge2–3 teeth per cm,raked toward the handle pull Blade 40–50 cm round the curve; spring temper.
Fig. 1 Sickles old and new. Flint blades set in a groove make a serrated cutting edge; an iron or steel sickle has fine teeth cut toward the handle so it bites on the pull stroke.
  1. Make the haft. A straight or slightly curved stick of hardwood 30–45 cm long and 3–4 cm thick. Cut a groove 5–8 mm wide and 1–1.5 cm deep along one side for 20–25 cm from the far end.
  2. Knap the blades. Strike 4–8 flakes about 3–5 cm long and 1–2 cm wide, each with one straight sharp edge (see Stone Tools). Lightly notch the cutting edge with small pressure flakes every 2–3 mm to make teeth.
  3. Glue them in. Warm the haft by the fire. Fill the groove with hot glue, then press the blades in one after another, edges outward, overlapping slightly like scales, so their edges make one long line. Smooth the glue with a wet finger. Let it set for an hour.
  4. Use with a pulling stroke: grab a fist of stalks below the heads with your free hand and draw the blades through them low down.

After many days of use the flint takes on a glossy shine from the silica in the straw — the "sickle gloss" archaeologists find on the oldest farming tools.

Method 2: The steel sickle

  1. Forge a bar of steel 3–4 mm thick and 3 cm wide into a curved blade 40–50 cm long around the curve, ending in a tang (see Axes, Chisels, Knives and Planes and Blacksmithing). The curve gathers the stalks toward the handle as you pull.
  2. Grind a single bevel on the inside of the curve.
  3. For a toothed sickle, cut fine teeth along the edge with a sharp cold chisel, 2–3 per centimetre, each angled back toward the handle so it bites on the pull. Teeth stay sharp for a season.
  4. Harden and temper to a spring temper (blue) — see Steel.
  5. Fit a round wooden handle 12–15 cm long on the tang; peen the end over a washer.

A smooth-edged sickle (a "reaping hook" or "bagging hook") is used with a swinging chop and sharpened like a knife; a toothed one is used with a pull.

Reaping with a sickle. Bend at the knees, not the back. Take a handful of stalks in your left hand (if right-handed), pull the sickle through them 10–20 cm above the ground, and lay the cut handful behind you with all the heads pointing one way. Several handfuls make a sheaf; bind it with a twist of straw. A team of three reapers and one binder can cut and bind about half a hectare a day.

Method 3: The scythe

Fitting the scythe to your body

A scythe must fit the person who uses it, like a pair of shoes. A badly fitted scythe is exhausting and cuts badly.

Fitting the snath Snath1.5–1.8 m, ash Upper grip Lower grip Ring and wedgeclamp the tang Blade55–75 cm for grass hip-boneheight elbow tofingertip Mowing, from above uncut grass swath 1.5–2 m step 10–15 cmeach stroke mower Windrowcut grass, laid left The edge, magnified Wornback on the left; edge blunt Peenedfeather-thin 3–5 mm band,hammered thin Peen every 4–8 hours of mowing.Hone every 10–15 minutes: wet stone almostflat on the blade, heel to tip, both sides.
Fig. 2 The scythe and how to fit it. Stood on its heel, the lower grip is at hip-bone height and the upper grip one forearm higher. Right: the mower swings in a crescent and lays the cut grass in a windrow on the left; peening hammers a worn, blunt edge out into a thin band again.
  1. The snath. Cut a pole 1.5–1.8 m long — about your own height. A slight S-curve helps but is not essential.
  2. The lower grip. Stand the snath upright beside you, blade end on the ground. Fix the lower grip (a peg 10–12 cm long, bored and wedged into the snath, pointing to the side) at the height of your hip bone.
  3. The upper grip. Measure from your elbow to your fingertips. Fix the upper grip that far above the lower one, pointing the same way.
  4. Fit the blade. The blade's tang (the bent-up foot at its heel) fits into a slot or against a flat on the end of the snath, and a ring and wedge — an iron ring slid over the end and tightened with a hardwood wedge — clamps it.
  5. Set the angles. Lay the scythe on flat ground in the position you mow in, holding both grips. The whole underside of the blade should lie flat on the ground — the edge just touching, the heel and the tip both down. Adjust the wedge until it does. The tip should point slightly in toward you — a little less than a right angle to the snath. This "closed" set makes the blade slice instead of chop.

Mowing

  1. Stand with feet a shoulder-width apart, knees slightly bent, facing the uncut grass. The blade lies flat on the ground to your right.
  2. Swing by turning your whole body from the hips — not by pulling with your arms. Keep the blade's heel brushing the ground the whole way. The blade sweeps from right to left in an arc in front of you, cutting a crescent about 1.5–2 m wide and laying the cut grass in a row on your left (the windrow).
  3. Step forward 10–15 cm — a half foot — after each stroke, so each crescent overlaps the last slightly.
  4. Rhythm, not force. A good mower swings slowly and steadily, all day. If you are working hard, something is wrong: the blade is dull, set wrong, or you are swinging with your arms.
  5. Mow in the morning dew. Wet grass stands stiffer and cuts much more easily. Dry afternoon grass bends away from the blade.
  6. For grain, mow into the standing crop so the cut stalks fall against it, then gather them into sheaves. A grain cradle — three to five long wooden fingers fixed parallel above the blade — catches the cut stalks and lets you lay them down in a neat row with the heads together.

Honing (every 10–15 minutes)

  1. Stand the scythe on its snath end with the blade up and the edge facing away from you, and hold the back of the blade near the tip.
  2. Wet the stone. Holding it nearly flat against the blade (a few degrees off flat), stroke from heel to tip, alternately on the top and the underside, with light strokes, keeping your fingers behind the stone's back edge. Ten to twenty strokes each side.
  3. Put the stone back in its water holder. Stones must stay wet to cut.

Peening (every 4–8 hours of mowing)

Honing slowly wears the thin edge back into thicker steel. Peening thins it again.

  1. Drive a small peening anvil — a steel peg with a flat or slightly rounded face 2–3 cm across — into the top of a log at sitting height.
  2. Sit with the blade lying across your lap, the edge resting on the anvil face.
  3. With a small hammer, tap the edge with light, overlapping blows, working along the blade from heel to tip, about 3–5 mm back from the edge. Each blow should leave a faint flat mark. You are squeezing the steel thinner, not bending it.
  4. Go along the blade two or three times, each pass a little closer to the very edge. The peened band should end up a bright, even strip about 3–5 mm wide, so thin at the edge that it flexes slightly under a fingernail.
  5. Hone it after peening.

A peening jig makes this easier for beginners: a steel peg with a cap that sits over it, guiding the angle. You strike the cap, not the blade. Make two caps with different angles — the first coarse pass, the second fine.

Tip Hammer cold, never hot. Peening is done cold. Heating the blade would destroy its temper. If you crack or tear the edge, you are hitting too hard or the blade is too hard; temper it softer next time you make one.

Rakes, forks and flails

Hay rakehandle 1.8 m,split to brace head 60 cm; teeth 8–10 cm, 4–5 cm apart Pitchforka natural fork,peeled and dried tines fire-hardened Handstaffash, 1.2–1.5 m Swivel jointrawhide caps and a loose loop Swingleholly or blackthorn,70–90 cm; lands flat Threshing floorin section dung-and-clay seal, 2–3 coats clay rammed in 5 cm layers until it rings dry, well-drained ground
Fig. 3 Hay and harvest tools: a wooden rake, a forked-stick pitchfork, and the flail with its swivelling rawhide joint. The threshing floor is beaten clay sealed with dung.

Wooden hay rake.

  1. Head: a straight hardwood bar 60 cm long, 4 cm square. Bore 12–16 holes right through it, 4–5 cm apart.
  2. Teeth: split dry oak, ash or hornbeam into pegs 12–15 cm long and 1–1.5 cm thick, round one end, and drive them through the holes so 8–10 cm stick out below. Dry teeth in a green or damp head grip as the head dries.
  3. Handle: a straight ash or willow pole 1.8 m long. Split the end for 30–40 cm, spread the two halves apart with a small wedge, and fit each into a hole near the ends of the head — the forked brace keeps the head from twisting.

Pitchfork. The simplest is a naturally forked stick of ash, hazel or willow, with two or three tines 30–40 cm long, peeled, dried, and the points sharpened and fire-hardened. Two tines for pitching sheaves; three or more for loose hay. A smith can forge iron tines and socket them onto a handle.

Flail.

  1. Handstaff: a straight ash pole 1.2–1.5 m long, 3–3.5 cm thick.
  2. Beater (the swingle): a heavier, dense hardwood stick 70–90 cm long and 4–5 cm thick — holly, blackthorn, hornbeam or oak.
  3. Joint: this must swivel freely so the beater lands flat. Carve a knob on the end of the handstaff and fit over it a loose cap of thick rawhide or leather, bound on with cord below the knob so it can turn. Tie a similar loop to the beater end. Join the two loops with a third loop of rawhide (see Hides and Leather) or a leather thong so there are 5–8 cm of slack.
  4. Use: swing it over your head so the beater falls flat along the straw. With two or three people, beat in turn in a steady rhythm, never at the same moment.

Threshing technique — how long to beat, turning the straw, then winnowing — is in Grain, Flour and Bread.

Method 4: A threshing floor

A clean, hard floor keeps the grain from getting lost in the dirt or mixed with grit.

  1. Choose a dry, level, slightly raised spot, open to a breeze for winnowing. In a barn, between two opposite doors that let a draught through.
  2. Dig out the topsoil, 10–15 cm deep, over a circle 5–8 m across (or a rectangle 4 × 6 m in a barn). For treading with animals, 10–15 m across.
  3. Fill and ram with damp clay or clay-rich earth in layers 5 cm thick, beating each layer hard with a heavy wooden rammer until it rings.
  4. Seal it: mix fresh cow dung and clay with water into a thin slurry and spread it over the surface with your hands. Let it dry hard in the sun, and repeat two or three times. Cracks are filled the same way each season.
  5. Before threshing, sweep it and let it dry thoroughly.

Large crops can be threshed faster by walking oxen or horses round and round over the sheaves, or by dragging a threshing sledge — a heavy plank 1.5 × 0.6 m, curved up at the front, with sharp flint chips set into its underside — driven by an animal with a person standing on it. The flints chop the straw and knock out the grain. Threshing machines are in Seed Drill and Reaper.

How to tell it worked

  • Sickle: cuts a fistful of ripe wheat stalks in one smooth pull without tearing out the roots.
  • Scythe: leaves an even, close stubble 3–5 cm high, with no tufts or long missed strands, and the cut grass falls in a neat windrow. It cuts with a swishing hiss, not a chopping thump. You can mow for an hour and feel pleasantly tired, not strained.
  • Edge: after peening and honing, the edge catches lightly on a fingernail drawn across it (never along it) and shines evenly.
  • Flail and floor: after two passes, the heads are empty when you rub them between your palms, and the grain on the floor is clean of grit.

Note Troubleshooting the scythe. Blade digs its tip into the ground → tip set too low; adjust the wedge so the blade lies flat, or lift the hands slightly. Leaves long uncut strands → blade dull (hone), or set too open — close the angle so the tip points more toward you. Grass bends over instead of being cut → dull edge, dry grass (mow at dawn), or swinging too slowly at the moment of cutting. Exhausted after half an hour → swinging with the arms; turn from the hips. Or grips are in the wrong place. Edge chips on stones → mow higher on stony ground, clear stones first, and peen out the damage. Small nicks peen out; big ones need grinding. Edge folds over → peened too thin; hone more firmly and peen less far into the edge.

Dangers

Danger A scythe blade can cut to the bone. Carry it over your shoulder with the blade behind you and pointing down, edge outward, or with a sheath of leather or wood over the edge. Never leave a scythe lying in grass, where someone can step or fall on it. Keep at least two scythe-lengths (5 m) from anyone else mowing, and never stand in front of or beside a mower. When honing, keep your fingers behind the stone — honing cuts are the most common scythe injury.

  • Sickle cuts to the gripping hand. Hold the stalks with your thumb on top and your fingers well behind the line of the blade; wear a leather glove or finger guard on the gripping hand.
  • The flail can rebound and hit your head or a partner. Learn slowly, with plenty of space, and keep a steady shared rhythm.
  • Hidden things in long grass: snakes, wasp nests, stones, and animals — mowers have killed ground-nesting birds, hares and fawns. Walk the field first.
  • Farmer's lung. Mouldy hay and grain dust carry fungal spores that, breathed in for years, permanently damage the lungs. Cut and stack hay only when properly dry, and tie a cloth over your nose and mouth when threshing or forking dusty hay.
  • Heat exhaustion at harvest. Drink often, start early, rest in the midday heat.

What this unlocks

Fast, sharp harvest tools let a family farm larger fields and make enough hay to keep animals through the winter (Hay and Silage) — the foundation of Keeping Animals, Draft Animals and Harness and Dairy and Cheese. The scythe's cutting principle, multiplied into a row of small reciprocating blades, becomes the mechanical reaper; the flail becomes the threshing drum (both in Seed Drill and Reaper). Grain gets stored in Granaries and Food Storage and ground in Grain, Flour and Bread.

How it was first done

Sickles came before farming. Hunter-gatherers of the Natufian culture in the Levant were harvesting wild cereals with bone- and wood-handled sickles set with flint blades by about 13,000–11,000 years ago; the glossy polish on those blades is how we know. Egyptian farmers used wooden sickles shaped like an animal's jaw with flint teeth set in them for thousands of years. Metal sickles of copper and bronze, then iron, followed as each metal became available.

The scythe appeared in Iron Age Europe, at first for cutting hay, and was in use by the Romans in the 1st century AD. For grain, the sickle remained usual in much of Europe until the 17th–19th centuries, because the scythe shattered more grain from the heads; the grain cradle and better blades changed that. Austrian and German smiths perfected the light, thin, hammer-peened scythe that is still made today. The flail was used in China in the centuries BC and in Europe probably from late Roman times, and it remained the main way of threshing in Europe until the threshing machine spread in the 1800s.

Source: content/entries/food/sickle-and-scythe.md