◆ Rebuild

Part 12 · Transport

Roads and Bridges

How to build roads that stay firm in the wet — drainage, camber and layers of broken stone, from a simple gravel track to Roman, Telford and Macadam roads — and how to cross water by ford, log and plank bridges, stone arches, rope suspension bridges and timber trusses.

Difficulty
●●●●●
Time
A few days for a log bridge; a season for a kilometre of gravel road; years for a stone arch bridge
Steps from zero
12 prerequisites →

You need first

Quarrying and Cutting StoneMortar and ConcreteSurveying and Levelling

This unlocks

The Post
The full path from nothing — 12 steps before this one
  1. Stone Tools
  2. Fire
  3. Finding and Preparing Clay
  4. Simple Machines
  5. Measurement from Scratch
  6. Writing and Numbers
  7. Quarrying and Cutting Stone
  8. The Kiln
  9. Arithmetic and Fractions
  10. Lime
  11. Surveying and Levelling
  12. Mortar and Concrete
  13. Roads and Bridges

Do them roughly in this order. See it on the tech tree →

Why it matters

A cart on a good road needs about a fifth of the pull it needs on a muddy track (The Wheel and Axle). The same horse that drags 500 kg through mud pulls 2 tonnes on a hard, smooth road. Roads decide whether a farm can sell its grain, whether ore reaches the furnace, whether a doctor reaches a sick child in winter. A road that turns to mud every spring cuts a village off for months.

Bridges matter even more. A river without a bridge is a wall: in flood it cannot be crossed at all, and in normal times crossing it costs hours and risks lives. A single good bridge can join two valleys into one community.

This chapter starts with the cheapest thing that works — a drained gravel road and a log bridge — and goes on to the paved roads and stone bridges that last for centuries.

How it works

Water is the enemy

Almost all soil is strong when dry and weak when wet. Clay soaked with water turns to paste; wheels sink, ruts form, the ruts hold water, and the road gets worse with every cart. Every rule of road building is really about water:

  1. Shed rain off the top. The road surface is built higher in the middle than at the edges — this is called the camber — so rain runs off sideways instead of soaking in. A fall of about 1 in 25 to 1 in 40 from the centre to the edge is right for gravel (4–2.5 cm for every metre of width).
  2. Carry the water away. A ditch on each side, at least 30 cm deeper than the bottom of the road's stone layer, takes the water away. Where a stream or ditch must cross the road, build a culvert — a pipe or a stone-lined channel under the road (Tiles and Clay Pipes). Ditches are dug and graded as in Field Drains, Terraces and Erosion Control.
  3. Keep the base dry. Raise the road a little above the ground around it on an embankment of its own spoil from the ditches. The Romans called this raised bank the agger.

Spreading the load

A wheel presses down on a small patch of road. A layer of stones spreads that weight over a wider area of soil underneath, the way a snowshoe stops you sinking. Angular, broken stones lock together under traffic into a firm crust; rounded river pebbles roll over each other like marbles and never lock. This is why road builders break stone rather than using it as found.

Gradients

Animals tire quickly on hills, and loaded wagons run away going down them. Keep main roads to a slope of no more than 1 in 20 (5 m of rise in 100 m) — steeper only for short stretches. On a hillside, zigzag up in switchbacks rather than going straight up. Lay out the grade with a level as described in Surveying and Levelling.

What you need

Job Materials Tools
Gravel road, per 100 m of 4 m road About 80–120 m³ of gravel or broken stone (160–240 tonnes) Spades, picks, rakes, baskets or carts, a level (Surveying and Levelling)
Macadam surface Hard stone broken to 2–5 cm Hammers, a 5 cm ring gauge, a heavy roller
Log footbridge Two sound logs, 25–40 cm thick; planks; posts for a handrail Axe, adze, auger, wedges, rope
Stone arch bridge Dressed stone (Quarrying and Cutting Stone), lime mortar (Mortar and Concrete), timber for centering Masonry tools (Stone Masonry), lifting gear (Cranes and Lifting)
Rope suspension bridge 4–6 heavy ropes (Cordage and Rope), planks or poles for the deck Anchors, a capstan or block and tackle

Where to find it

  • Road stone. The best is hard, tough rock that breaks into sharp-edged lumps and does not crumble or turn to mud when wet: basalt and other dark, heavy volcanic rocks, granite, hard sandstones, and flint. Test a lump: hit it with a hammer; good road stone rings, breaks with sharp edges, and the fragments do not powder between your fingers. Soft limestone and chalk wear down fast but will do on lightly used roads. See Rocks and Minerals.
  • Gravel lies in river beds, old stream terraces and the gravel hills left by glaciers. Pit gravel with a little clay in it packs harder than clean river gravel.
  • Bridge timber. Oak, larch, chestnut and other rot-resistant woods; see Timber Framing and Log Building. Choose logs straight, sound and without rot at the heart (tap them: a hollow log sounds dull and booming).
  • Fords are found at wide, shallow stretches where the water ripples over a gravel bed (a riffle), usually just downstream of a pool. Animal trails often lead to them.

Method 1: An earth and gravel road

This is the road that will serve most of your traffic for a long time. Done well, it carries carts all year.

  1. Lay out the line. Follow the contours, avoid wet ground, and keep the slope under 1 in 20. Peg the centre line every 20 m.
  2. Clear it. Remove trees, roots and all the dark topsoil — it holds water and never firms up — down to firm subsoil, over a width of about 5 m for a road that two carts can pass on (3 m for a single lane with passing places).
  3. Dig the ditches. On each side, a ditch about 60 cm deep and 60 cm wide at the top, with sloping sides. Throw the spoil into the middle of the road.
  4. Shape the base. Rake and stamp the base into a camber, highest in the middle. For a 4 m road, the centre should stand about 8–10 cm higher than the edges.
  5. Spread the stone. Lay 15–25 cm of gravel or broken stone, thickest in the middle. On soft ground, use more.
  6. Compact it. Ram it with a heavy wooden rammer, roll it with a stone or log roller pulled by people or animals, or simply let traffic do it — but fill the ruts every few days while it beds in.
  7. Build culverts wherever water will cross the road. A culvert of flat stones — two walls and a slab lid — or a large clay pipe, laid on a slope so water runs through, with stones at each end so the water does not scour.

Maintenance is most of road building. After every heavy rain, walk the road: clear blocked ditches and culverts, rake loose stone back into ruts, and fill potholes as soon as they appear. A hole left for a month becomes a pit.

Method 2: Macadam and Telford roads

In the early 1800s two Scottish engineers found how to build fast, hard roads without the Romans' enormous depth of masonry.

EARTH AND GRAVEL ROAD Camber 1 in 25 to 1 in 40 Gravel 15–25 cm on firm subsoil Side ditch 30 cm below the stone MACADAM Fine top 5 cm stone 2–2.5 cm Two layers, 10 cm each angular stone under 5 cm Drained, cambered soil carries the load TELFORD Gravel top Broken stone 15 cm Large stones set on edge 15–18 cm, by hand ROMAN ROAD (TEXTBOOK FORM) Paving slabs, kerbs Gravel and lime concrete Rubble in lime Large stones on a raised bank rain runs off
Fig. 1 Road cross-sections. An earth and gravel road; John McAdam's road of small broken stone on a cambered, drained base; Thomas Telford's road with a foundation of hand-set stones; and a classic Roman road with several layers under a paved surface.

The Macadam road

John McAdam's insight was that well-drained native soil carries any load, so long as it is kept dry by a waterproof crust of small, angular stones.

  1. Shape and drain the soil base with a camber, and dig ditches, exactly as for the gravel road.
  2. Break the stone. Workers with light hammers break hard rock into pieces that pass through a ring 5 cm across (McAdam's famous test was that each stone should fit in a man's mouth). Reject dust, earth and anything round. Piece size matters more than anything: big stones work loose and roll, small ones lock.
  3. Lay it in layers. Spread a first layer of about 10 cm and let traffic or a roller compact it. Then another 10 cm. Then a final layer of 5 cm of smaller stone (2–2.5 cm). Total about 25 cm.
  4. Bind it. Later builders swept stone dust and sand into the top layer, watered it and rolled it with a heavy roller — 2–3 tonnes of stone or iron pulled by horses — so the fines wedged the stones tight. This water-bound macadam is far smoother.

The Telford road

Thomas Telford built heavier roads for the busiest routes and soft ground. He first laid a foundation of large flat stones, 15–18 cm high, set by hand on edge, close together like books on a shelf, with the gaps filled with stone chips. On top went about 15 cm of broken stone and a top layer of gravel. It is more work, but it carries heavy traffic over poor soil.

Paving

In towns, on steep slopes and at the approaches to bridges, lay setts — roughly cubic stone blocks 10–15 cm across — or flat slabs on a bed of sand or lime mortar over a stone foundation. Joints filled with sand, or with lime mortar on the heaviest streets (Mortar and Concrete).

Tip Tar macadam. Mix hot tar (Tar, Pitch and Glue, or tar from Coal and Coke) into the top layer of broken stone and roll it. It stops dust and keeps water out completely. This is the "tarmac" of the 20th century.

Crossing bogs

Where the ground is too soft for any stone, lay a corduroy road: logs 15–20 cm thick laid side by side across the line, on long logs laid lengthways underneath, and covered with brushwood and gravel. Bundles of brushwood (fascines) laid on the bog spread the load in the same way.

Fords

A ford is a bridge you do not have to build. Choose a wide, straight stretch where the bed is firm gravel or rock, not mud or sand. For people on foot, keep to water below knee depth (about 50 cm) in a gentle current; for carts, below the axle (about 60 cm). Pave a muddy bed with large flat stones, mark each side of the safe line with tall posts, and set up a depth post — a pole marked in rings — at the entrance, so people can see when the water is too high.

Bridges

LOG BEAM BRIDGE STONE ARCH BRIDGE KING-POST TRUSS ROPE SUSPENSION BRIDGE Criblogs and stones Logs 25–40 cm thickspan 5–8 m on foot highest flood Keystone Arch stones(voussoirs) Spandrelrubble fill abutment on firm ground or rock Strutspushed (compression) King post Tie beampulled (tension) spans to about 10 m Deadman logburied 1.5 m deep Handrail ropes Sag ≈ 1/10of the span
Fig. 2 Four bridges. A log beam bridge on stone-filled crib abutments; a stone arch bridge; a king-post timber truss; and a rope suspension bridge, its cables anchored into the ground at each end.

Log beam bridges

The simplest bridge is one or more logs laid across a stream.

  1. Build abutments. At each bank, build a firm seat for the logs above the highest flood level you can find (look for flood debris caught in trees and the line of dead grass on the banks). A crib of logs laid log-cabin fashion and filled with stones makes a strong abutment; so does dry-stone walling (Stone Masonry).
  2. Size the logs. As a rough guide for sound, straight hardwood or larch: a log 25 cm thick safely spans about 5 m for foot traffic; 35–40 cm for about 8 m. For carts, use four or more logs 40 cm thick or more, spanning no more than 6 m, and plank across them. Longer spans need a pier in the middle or a truss.
  3. Flatten the tops with an adze. Lay the logs, pin them to the abutments with hardwood pegs, and peg planks or split poles across them for a deck. Add a handrail.
  4. Keep the ends dry. Logs rot first where they rest on wet ground. Seat them on flat stones and leave air around them.

A clapper bridge does the same with long stone slabs laid on stone piers. Stone is weak when bent: slabs much over 2 m long will crack under load.

Stone arch bridges

An arch turns the weight of the bridge and its load into pure compression, which stone takes easily. A well-built stone arch bridge lasts many centuries. Read Arches, Vaults and Domes for how arches work and how to build the wooden centering they are built on.

  1. Foundations are everything. Build piers and abutments on solid rock if possible. On gravel or clay, dig deep inside a cofferdam — a ring of driven timber piles packed with clay to keep the river out while you work — and drive oak piles to spread the load (Foundations and Floors). Most old bridges that fell were undermined by the river scouring away the ground under a pier.
  2. Piers in the river should be about a quarter to a third of the span thick, with pointed cutwaters on the upstream side to part the current and the ice.
  3. Build the arches on centering, from both sides at once, finishing with the keystone. Leave the centering for several weeks while the lime mortar hardens.
  4. Fill the spandrels (the spaces above the arch at each side) with rubble or lighter material, cover the arch with a layer of clay to keep water out, then the road surface. Add parapets.
  5. Give the river room. The arches must pass the biggest flood with room to spare. A bridge that blocks a flood acts as a dam, and the water pushes it over.

Timber trusses

A truss is a frame of triangles. A triangle cannot change shape without one of its sides stretching or shortening, so a truss is far stiffer and stronger than a single beam of the same timber. How to design and join trusses is in Trusses and Frames.

  • King-post truss (spans to about 10 m): two sloping struts meet over the middle of the span; a vertical post hangs from their peak and holds up the middle of the bottom beam.
  • Queen-post truss (spans to about 15 m): the peak is replaced by a horizontal top beam between two vertical posts, making a longer frame.
  • Longer trusses repeat the triangles many times. With iron rods for the parts in tension (Blacksmithing), 19th-century trusses spanned 50 m and more.

A roof over a timber bridge keeps rain off the joints, and roofed (covered) bridges last 80–100 years against 15–20 for open ones.

Rope suspension bridges

Where a gorge is too deep for piers and too wide for logs, hang the deck from ropes. The Inca built such bridges of woven grass rope across the Andes.

  1. The cables. Four to six heavy ropes of hemp, flax or plant fibre (Cordage and Rope), each as thick as you can make — 5 cm or more for long spans. Two or more carry the deck; one on each side serves as a handrail, tied to the deck ropes with vertical ropes every metre.
  2. The sag. Let the cables hang with a dip in the middle of about one-tenth of the span — 3 m for a 30 m bridge. A tighter cable pulls much harder on its anchors. For a 30 m span carrying 60 kg per metre (deck plus people), the cables together pull on each anchor with more than 2 tonnes — so make each rope several times stronger than its share of that (Cordage and Rope tells you how to test rope).
  3. Anchors. At each end, tie the cables round huge rocks or great logs (deadmen) buried crossways in a trench at least 1.5 m deep and weighted with stone. Anchors fail more often than ropes.
  4. The deck. Lash poles or planks across the deck ropes. Walk across one at a time until you have tested it with a heavy load.
  5. Replace the ropes regularly. Plant-fibre rope rots and weakens in the weather. The last Inca-style grass bridge, Q'eswachaka in Peru, is rebuilt by its villages every year. Iron or steel Wire Rope and Cable lasts far longer and carries much longer spans.

How to tell it worked

  • Roads: after heavy rain, the centre should be firm with no standing water, the ditches running, and ruts shallow. A loaded cart should leave tracks no deeper than 1–2 cm.
  • Bridges: before opening a bridge, test it with a load at least one and a half times the heaviest you expect — stacked stones, or a cart loaded with stones, pushed across from a safe distance with long ropes. Watch the middle of the span against a stretched string: it should sag a little and spring back when the load is removed.
  • After every flood, inspect the piers and abutments for scour (holes under the stone or timber) and fill them with large stones at once.

Note Troubleshooting. Potholes and puddles in the middle of the road → the camber has worn flat. Rake the stone back to the centre and add more. The road breaks up every spring → water is getting into the base. Deepen the ditches and add culverts. Stones roll loose on top → stones too big or too round. Break them smaller and bind with fines. A log bridge sags more each year → the logs are rotting at the ends or inside. Replace them before they fail, and keep the ends dry. Cracks open in an arch → the abutments or piers are moving, usually from scour or soft ground. Stop heavy traffic and investigate the foundations.

Dangers

Danger Moving water is far stronger than it looks. Knee-deep fast water can knock an adult over; about 60 cm of fast water can sweep a cart and its team downstream. Never cross a ford in flood, never let children wade at a ford, and tie a safety line to anyone working in a river.

Danger Bridges fail suddenly. Never use a bridge you have not tested, never overload it, and inspect it after every flood. When removing the centering under an arch, or building any bridge, keep everyone out from under it, and work from the ends with ropes where possible.

  • Cofferdams can burst in a rising river and drown the people inside. Post a lookout upstream in wet weather.
  • Breaking stone throws sharp chips; protect your eyes with a mesh or a slit shield of wood.
  • Cuttings and ditches in loose soil can collapse on the people digging them; slope the sides back.

What this unlocks

Good roads make Wagons and Carriages worthwhile, and good wagons demand good roads. Together they carry the materials for building, industry and trade. Where roads cannot carry enough, people build Canals and Locks — and the engineering of bridges, cuttings and embankments is exactly what Railways later needed. With Portland Cement and Reinforced Concrete, bridges can span far further; with iron and steel (Steel in Quantity), they can cross estuaries.

How it was first done

The Sweet Track, a wooden walkway of planks on crossed stakes across the Somerset marshes in England, has been dated by its tree rings to the winter of 3807–3806 BC. The Persian Royal Road, about 2,700 km long, ran across the Persian Empire in the 500s BC. The Romans began the Appian Way in 312 BC and eventually built about 80,000 km of paved roads, with stone bridges, many still standing; the Inca built about 40,000 km of roads and rope bridges across the Andes without wheels or draft horses.

The Arkadiko bridge in Greece, a corbelled stone arch from about 1300 BC, still carries a track. In China, the engineer Li Chun built the Zhaozhou Bridge around AD 605 — a flat segmental stone arch spanning 37 m with open arches in the spandrels to lighten it and let floods through; it is still in use. Thomas Telford (1757–1834) and John Loudon McAdam (1756–1836) transformed road building in Britain, and the British engineer Edgar Hooley patented tar macadam in 1902. The world's first iron bridge was cast at Coalbrookdale, England, in 1779.

Source: content/entries/transport/roads-and-bridges.md