◆ Rebuild

Part 5 · Cloth and Clothing

Knitting, Crochet and Netting

Making fabric from one continuous strand of yarn by pulling loops through loops — with two needles (knitting), a hook (crochet) or a flat needle and knots (netting and nålbinding). The way to make socks, sweaters, hats, bags and fishing nets without a loom.

Difficulty
●●●●●
Time
An evening to learn the basic stitches; a hat in 1–2 days; a pair of socks in a week of evenings; a sweater in 3–6 weeks
Steps from zero
2 prerequisites →

You need first

Spinning and Weaving Cloth

This unlocks

Hats, Gloves, Scarves and Stockings
The full path from nothing — 2 steps before this one
  1. Cordage and Rope
  2. Spinning and Weaving Cloth
  3. Knitting, Crochet and Netting

Do them roughly in this order. See it on the tech tree →

Why it matters

A loom (Spinning and Weaving Cloth, The Loom) makes flat, firm cloth, but it is big and stays at home. Knitting, crochet and netting need only a stick or two and a ball of yarn; the work goes in a pocket and can be done by firelight or while minding animals.

Knitted fabric stretches and springs back, so it hugs the body: socks that stay up, hats and mittens that fit anyone, sweaters that trap a thick layer of warm air. It is shaped as you go — a sock heel, a mitten thumb — with no cutting or seams (Hats, Gloves, Scarves and Stockings gives more patterns). In cold country, warm dry feet and hands are the difference between working through winter and losing toes (Surviving Cold and Heat).

Netting is the knotted cousin: open meshes held by knots that cannot slip, for fishing nets (Fishing), bird and rabbit nets (Hunting and Trapping), bags and hammocks (Cradles, Hammocks, Sofas and Folding Chairs).

How it works

All of these fabrics are made of one long strand pulled through itself in loops. They differ only in how the loops are held:

  • Knitting keeps a whole row of open loops ("stitches") waiting on one needle. With the second needle you pull a new loop through each old one, moving them across to the other needle. Each row hangs from the row before it. Because the loops are not knotted, a cut or a dropped stitch can unravel — a run, or "ladder", that runs down the fabric.
  • Crochet keeps only one live loop on a hooked stick. Each new stitch is completed before the next begins, so crochet is easier to fix and to shape into round things, but it is thicker, less stretchy and uses about a third more yarn than knitting.
  • Netting ties each loop to its neighbour with a knot (the sheet bend), so the mesh holds its size under load and does not unravel when one cord breaks.
  • Nålbinding ("needle-binding", the older Scandinavian word) uses a single flat needle and short lengths of yarn, passing each new loop through several earlier ones. It is slow but extremely tough and cannot run. It is how socks and mittens were made in northern Europe and the Middle East for well over a thousand years before knitting arrived.
1. Inright needle into the frontof the first loop, behindthe left needle 2. Roundwrap the yarn round theright needle tip,anticlockwise 3. Throughdraw the new loop backthrough the old one 4. Offslip the old loop off theleft needle: one stitchis done left needleyarn HOW KNITTED FABRIC HANGS TOGETHER Needleholds the live loops of the newest row Row 3Row 2Row 1 Each loop is pulled up throughthe head of the loop below it.No knots: one escaped loopcan run down the whole fabric.
Fig. 1 The knit stitch in four moves. The right needle goes into the front of the first loop, the yarn is wrapped round it, the new loop is drawn back through, and the old loop drops off. Below: how the rows of loops hang from each other.

Yarn and gauge

Use two-ply yarn (Spinning and Weaving Cloth): it is round and does not kink. Wool is best — springy, warm when wet, and holds its shape. Linen and cotton have no stretch; use them for bags and summer clothes.

Gauge is how many stitches fit into 10 cm, and it decides the size of everything. Hands differ, so always knit a test square first.

Yarn thickness Needle diameter Stitches per 10 cm Good for
Fine ("fingering") 2–3 mm 28–32 Socks, gloves, baby clothes
Medium ("worsted") 4–5 mm 18–20 Sweaters, hats, mittens
Thick ("bulky") 6–9 mm 12–14 Fast warm outer layers, blankets

What you need

Item Size Made from
Straight needles (a pair) 25–35 cm long, 3–6 mm thick Hardwood, bamboo, bone, or later steel or brass wire
Double-pointed needles (a set of 4 or 5) 15–20 cm long, 2–3 mm thick Same; for knitting tubes — socks, sleeves, hats
Crochet hook 12–15 cm long, 3–6 mm thick Hardwood or bone, with a hook notch at one end
Netting needle (shuttle) 15–25 cm long, 1.5–3 cm wide Thin hardwood or bamboo slat
Mesh gauge Flat stick as wide as half a mesh, 15 cm long Any smooth wood
Nålbinding needle 8–12 cm long, flat, with a big eye Wood, bone or antler
Yarn Hat 150–200 m; pair of socks 400 m fine yarn (about 100 g); adult sweater 1,000–1,400 m medium yarn (500–700 g) Wool, linen, cotton
Twine for nets 1–3 mm, hard-twisted Hemp, flax, nettle (Cordage and Rope)

Making the tools

  1. Needles. Split a straight-grained stick of dry, knot-free hardwood (birch, maple, beech, boxwood) or bamboo a little thicker than you need, and shave it round (Basic Woodworking). Taper the last 2–3 cm into a rounded point: sharp points split the yarn, blunt ones won't enter the stitch. Rub smooth with sandstone, then leather, then beeswax or fat. It must be glass-smooth — any roughness snags on every one of thousands of stitches. Put a knob or clay bead on the blunt end so stitches cannot slide off.
  2. Bone needles are ground from a splinter of leg bone exactly as for sewing needles (Sewing, Needles and Thread); they are the smoothest of all.
  3. Crochet hook. Shape a needle as above, then cut a notch 3–4 mm back from the tip, angled back towards the handle like a fish hook's barb. Smooth the inside of the notch with a thread rubbed in sand.
  4. Netting needle. Cut a flat slat 2–4 mm thick. Make a forked tail at one end and a pointed nose at the other with a long open slot inside it, and a thin tongue left standing in the slot to wind twine around (see the drawing below). Wind twine on lengthways, round the tongue and through the fork.

Where to find it

Method 1: Knitting

Hold one needle in each hand; work moves from the left needle to the right. Carry the yarn in whichever hand feels natural.

  1. Slipknot. Leave a 15-cm tail, make a slipknot and put it on the left needle.
  2. Cast on with the knitted cast-on: knit into the slipknot (below), but put the new loop back onto the left needle instead of dropping the old one. Repeat into the newest loop until you have enough.
  3. The knit stitch. With the yarn behind the work, push the right needle into the front of the first loop on the left needle, from left to right, so the right needle lies behind the left one. Wrap the yarn round the right needle anticlockwise. Draw the new loop back through the old one. Slip the old loop off the left needle. That is one stitch. Repeat to the end of the row, then swap the needles between your hands and start again.
  4. The purl stitch is the knit stitch made from the other side: yarn in front, insert the right needle into the front of the loop from right to left, wrap the yarn anticlockwise, push the new loop back and away through the old one, and slip the old one off.
  5. Tension: stitches should slide easily along the needle without hanging loose. Evenness comes after a few hours.
  6. Cast off: knit two stitches, lift the first over the second and off the needle; knit one more and repeat. Pull the cut yarn through the last loop, and darn the tails into the back with a sewing needle (Sewing, Needles and Thread).

The three basic fabrics

Pattern How Behaviour
Garter stitch Knit every row Ridged, thick, lies flat, both sides the same. Best first project
Stockinette Knit one row, purl the next (in the round: knit every round) Smooth V's on the front, bumps behind. Thin and even; the edges curl
Ribbing Knit 2, purl 2, along the row; on the next row knit the knits and purl the purls Very stretchy and springy. Cuffs, hems, the top of socks and hats

Shaping

  • Increase one stitch: knit into the front of a stitch, but do not drop it — knit into its back loop as well, then drop it.
  • Decrease one stitch: knit two stitches together as if they were one ("k2tog"). It slants right. To slant left, slip two stitches one at a time onto the right needle, put the left needle back into their fronts, and knit them together ("ssk").

Knitting in the round

To make a tube with no seam, divide the stitches among three or four double-pointed needles, arrange them in a triangle or square, and knit with a spare one. Make sure the cast-on edge is not twisted round the needles before you join the first stitch to the last. Every round is knit; stockinette needs no purling at all.

Project: a hat

A hat should be about 10% smaller round than the head, so it hugs. For a 56-cm head in medium yarn (18 stitches per 10 cm), cast on 88 stitches in the round. Rib (knit 2, purl 2) for 6 cm — 12 cm to fold up over the ears — then knit plain until it is 18–20 cm long. Crown: knit 9, k2tog all round, then a plain round; then knit 8, k2tog, a plain round; and so on, one fewer plain stitch each time, until 16 stitches remain. Draw the yarn through them and pull tight.

Project: socks

knit downwards Cuffcast on 60, knit 2 purl 2 rib, 5 cm Legplain knitting in the round, 12 cm Heel flap30 rows, back andforth on 30 stitches Heel turnshort rows → 18 Gussetpick up 15 each side (78),decrease back to 60 Footplain, until 5 cm short of the full length Toe4 decreasesper round length of the foot, heel to longest toe
Fig. 2 A top-down sock. The leg is a tube; the heel flap is knitted back and forth on half the stitches, the heel is turned with short rows, stitches are picked up up the sides and decreased away at the gusset, and the toe closes in four lines of decreases.

For an adult foot in fine wool at 30 stitches per 10 cm on 2.5-mm double-pointed needles:

  1. Cuff and leg. Cast on 60 stitches. Join in the round. Knit 2, purl 2 for 5 cm, then knit plain for another 12 cm.
  2. Heel flap. Work back and forth on 30 stitches only (leave the other 30 for the top of the foot). On the outside rows: slip 1, knit 1, repeated. On the inside rows: slip 1, purl to the end. Do 30 rows. The slipped stitches make a thick, hard-wearing pad.
  3. Turn the heel (short rows): Row 1: slip 1, knit 16, ssk, knit 1, turn the work round, leaving the rest unworked. Row 2: slip 1, purl 5, purl 2 together, purl 1, turn. Row 3: slip 1, knit to one stitch before the gap left by the last turn, ssk (joining across the gap), knit 1, turn. Row 4: slip 1, purl to one before the gap, purl 2 together, purl 1, turn. Repeat rows 3 and 4 until every heel stitch has been worked: 18 stitches remain. The heel is now a little cup.
  4. Gusset. Knit across the heel stitches, then pick up and knit 15 stitches along the side of the flap (one in each slipped edge stitch), knit across the 30 instep stitches, and pick up 15 more along the other side: 78 stitches. On every second round, decrease one stitch at each side of the sole where it meets the instep (k2tog before the instep, ssk after it) until you are back to 60.
  5. Foot. Knit plain until the sock measures 5 cm less than the length of the foot, heel to longest toe.
  6. Toe. Divide into sole (30) and top (30). At each of the four corners, decrease one stitch, every other round, until 28 stitches remain; then every round until 16 remain. Cut the yarn and draw it through all the stitches, or graft the two sides together with a sewing needle.
  7. Knit the second sock immediately — otherwise you will never match the gauge again.

Project: a sweater

The simplest sweater is four flat pieces sewn together: two rectangles for the body and two tapering sleeves, with "dropped" shoulders and no shaping.

  1. Body pieces: chest plus 10 cm, halved. For a 100-cm chest: 55 cm, or 99 stitches at 18 per 10 cm. Rib 6 cm, then stockinette to the shoulder (usually 60–70 cm in all). For the front, cast off the middle 20 stitches 8 cm below the top and finish each shoulder separately.
  2. Sleeves: about 40 stitches at the wrist; rib 6 cm, then increase one stitch at each edge every 6th row until about 81 stitches (45 cm wide); continue to the full arm length.
  3. Sew up (Sewing, Needles and Thread): shoulders, then sleeves centred on the shoulder seams, then each underarm and side in one seam. Pick up stitches round the neck and rib 3 cm.

Method 2: Crochet

  1. Chain. Make a slipknot on the hook. Wrap the yarn over the hook ("yarn over") and pull it through the loop. Repeat: each is one chain stitch.
  2. Single crochet. Push the hook into the second chain from the hook. Yarn over, pull a loop through: two loops on the hook. Yarn over, pull through both. Work one into every chain, then chain 1, turn, and work back along the tops of the row below.
  3. Double crochet (twice as tall): yarn over before going into the stitch, pull up a loop (three loops on the hook), yarn over and pull through two, yarn over and pull through the last two.
  4. Working in rounds (bags, hats, pot-holders, baskets of stiff fibre): chain 4, join into a ring, and work 6–8 single crochets into the ring; on each following round, work two stitches into each stitch of the round below at evenly spaced points (6–8 increases per round) to keep it flat.

Crochet makes firm, thick fabric for bags, rugs and edgings — the quickest use for coarse handspun.

Method 3: Netting

THE SHEET BEND meshabove from the gauge free end pull the knot down hard against the gauge Mesh gaugewidth = half the side of a mesh;every loop goes round it Netting needletwine wound on the tongue,through the fork at the tail Knots of the rowbeing made sit ontop of the gauge Head cordtied to a post Next meshto knot
Fig. 3 Netting with a needle and a mesh gauge. Each new loop goes round the gauge, up through the loop above, and is locked with a sheet bend. Every mesh comes out exactly the same size.

The mesh size is set by the gauge, a flat stick whose width equals the length of one side of the finished mesh — half the mesh pulled out straight, knot to opposite knot. For a fish net that holds fish thicker than 4 cm, use a gauge 2 cm wide. A shopping bag might use 3 cm; a rabbit net 4–5 cm.

  1. Tie a loop of strong cord to a post or a nail at chest height. Wind the netting needle full of twine.
  2. Cast on the first row: tie the twine to the loop, then for each mesh pass the twine down round the gauge and back up, and tie it to the loop with a half hitch. Make as many as the net is wide (for a bag, 20–30). Slide them off the gauge.
  3. The netting knot (sheet bend). Hold the gauge under the row. Pass the needle down in front of the gauge, round behind and up, then up through the next mesh of the row above, from behind. Pull the twine down until the gauge touches the mesh, and pin the crossing with your thumb. Throw a loose loop of twine out to the side, pass the needle behind both legs of the mesh above, and out through the thrown loop. Pull the knot tight downwards: it should snap onto the bottom of the mesh and not slide.
  4. Work across the row, slide the gauge out, turn the work round, and net the next row back the other way.
  5. To make a bag or a round net, net a strip, then join the ends into a tube and continue in a spiral; gather the bottom with a drawstring.
  6. Add a stronger head rope through the top and bottom meshes of a fishing net, with floats (wood, cork, bark) on the top rope and stone or clay sinkers on the bottom (Fishing).

Method 4: Nålbinding

You need a flat needle with a big eye and yarn in lengths of 1–2 m — any longer and the whole length has to be pulled through every loop. Join each new length to the old by spit-splicing: fray both wool ends for 5 cm, overlap them, wet them, and roll hard between your palms until they felt together (Felt).

In the basic Oslo stitch you work around your thumb. Each new loop is made by passing the needle under the loop on your thumb and over the one behind it, then turning back through the loop just formed; pull it snug round the thumb and slide the oldest loop off. Each stitch locks into two before it, and each row passes through the edge of the row below. It is hard to learn from words alone: practise with thick yarn and a fat needle until the motion repeats in your hand. Nålbound socks are slow to make but last years, and will not run when they wear through.

How to tell it worked

  • Knitting: your test square should stretch both ways and recover, and match the gauge table. A vertical ladder of bars means a dropped stitch: catch it with a crochet hook and pull each bar through in turn to climb it back up.
  • Crochet: edges run straight. Flaring or curling means stitches gained or lost at row ends — count every row.
  • Netting: pull hard on one mesh. No knot may slide; all meshes the same size.
  • Socks: the heel sits exactly on your heel with no bunching.

Note Troubleshooting. Stitches too tight to push the needle in → you are pulling the yarn too hard. Wrap it loosely and use a needle 0.5–1 mm thicker. More stitches than you started with → yarn was passed over the needle by accident, or you knitted into a loop of the row below. Count after every row while learning. Edges curl → normal for stockinette. Add 3–4 stitches of garter or ribbing at each edge. Yarn splits → needle points too sharp, or the yarn has too little twist. Blunt the point, or ply your yarn harder. Netting knots slip → you skipped pinning with the thumb, or the twine is too slick and loosely twisted. Use hard-twisted hemp and pull each knot down sharply. Hole at the corner of the sock gusset → pick up one extra stitch in the corner and decrease it away on the next round.

Dangers

Warning Loops and nets can kill. A loop of yarn, cord or net round a small child's neck can strangle it: keep yarn, cords and nets away from babies and toddlers. Nets in water drown people as well as fish: never swim among nets, and carry a knife when setting or hauling them from a boat.

  • Needle points stab in pockets and bedding — cap them with a cork or bead. Hours of knitting inflame wrists and thumbs: stop at the first ache.

Going further

  • Colour knitting (Fair Isle): two colours carried along the row make patterns, and the strand floating behind adds an extra warm layer.
  • Fulled knitting: knit mittens or a cap a third oversize, then wash hot and rub until it shrinks to a windproof felt (Felt).
  • The knitting frame (1589) knits a whole row at once on hooked needles — the ancestor of the knitting machines in Textile Machinery.

How it was first done

Nets are very old. A fishing net of willow bast found at Antrea in Finland has been dated to about 8,500 BC, and net impressions in fired clay in central Europe are older still. Nålbinding was certainly in use by the early centuries AD: socks with a separate big toe from Roman-period Egypt (3rd–5th century AD) are nålbound, and the "Coppergate sock" from Viking-age York (10th century) is a famous example.

True knitting appears later. The oldest pieces we know of are finely patterned blue-and-white cotton socks from Egypt, from about the 11th century AD. Knitting spread through Spain to Europe; by the 1400s and 1500s knitted wool caps and stockings were a major trade, and guilds of knitters existed in many cities. In 1589 an English clergyman, William Lee, built a stocking frame that knitted mechanically. Crochet as we know it became popular in Europe only in the early 1800s; in Ireland during the famine of the 1840s, crocheted lace was an important source of income for many families.

Source: content/entries/textiles/knitting.md