◆ Rebuild

Part 14 · Electronics and Computing

Fibre Optics

A thread of glass thinner than a hair, with a slightly denser core inside a slightly lighter skin, traps light by total internal reflection and carries it round corners. Made of glass pure enough, it carries laser pulses a hundred kilometres before they need help, and a single fibre carries more messages than every copper telephone line once built. How it works, the glass-clad fibre a workshop can draw, how ultra-pure silica fibre is really made, splicing, cables, and why fibre carries the internet.

Difficulty
●●●●●
Time
A week for glass-clad fibre and a short light link; years and a chemical and glass industry for long-distance silica fibre
Steps from zero
47 prerequisites →

You need first

Glass Fibre and Glass WoolLasers

This unlocks

The Internet
The full path from nothing — 47 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Sulfur
  7. Hunting and Trapping
  8. Basic Woodworking
  9. The Kiln
  10. Pottery
  11. Charcoal
  12. Hides and Leather
  13. Lime
  14. Bricks
  15. Salt
  16. Mercury
  17. Lye and Potash
  18. Fermentation
  19. The Wheel and Axle
  20. Glass
  21. Firebrick and Refractories
  22. Bellows
  23. Saltpeter
  24. The Lathe
  25. Gears
  26. Glass Fibre and Glass Wool
  27. Copper Smelting
  28. Iron (the Bloomery)
  29. Laboratory Glassware
  30. Sulfuric Acid
  31. Pumps
  32. The Waterwheel
  33. Lenses
  34. Blacksmithing
  35. Hydrochloric Acid
  36. The Battery
  37. The Vacuum Pump
  38. Magnets
  39. The Spectroscope
  40. The Light Bulb
  41. Copper Wire
  42. The Generator
  43. The Vacuum Tube
  44. The Electric Arc Furnace
  45. Pure Silicon
  46. Semiconductors and the Transistor
  47. Lasers
  48. Fibre Optics

Do them roughly in this order. See it on the tech tree →

Why it matters

A copper telephone wire carries a few conversations, fades every few kilometres and picks up noise from lightning and motors. A thread of glass carries light, whose waves swing hundreds of trillions of times a second, so it can carry vastly more information. In good glass it travels 100 km or more before it needs amplifying, picks up no electrical noise, carries no lightning into a building, and is made from sand.

That is why almost every long-distance telephone call and nearly all internet traffic, across land and under the oceans, now travels as flashes of laser light in glass fibre (The Internet).

Humbler uses come much earlier: bundles that carry an image round corners into a stomach or a boiler, light pipes, and short data links immune to lightning. This chapter starts with the fibre a glass workshop can draw from two ordinary glasses (Glass Fibre and Glass Wool covers drawing), then explains honestly what the real thing takes.

How it works

Light trapped in glass

When light passes from glass into air, it bends away from the straight line (Lenses). The more steeply it strikes the surface, the more it bends. Beyond a certain angle, the critical angle, it cannot get out at all: all of it reflects back into the glass, more perfectly than from any silvered mirror. This is total internal reflection. You can see it by looking up at the surface of still water from below in a swimming pool: beyond a certain slant the surface becomes a silver mirror.

Shine light into the end of a long glass rod and it bounces from side to side, zig-zagging along inside, and comes out of the far end even if the rod is bent. A jet of water from a hole in a bucket does the same: light a lamp behind the hole and the curved jet glows along its length.

Why fibre needs a skin

A bare glass thread works only while its surface is perfectly clean and touches nothing. A fingerprint, a drop of water or a neighbouring fibre lets light leak out at every touch. The cure is to give the fibre a skin of glass with a slightly lower refractive index (refractive index: how much a material slows and bends light; air 1.00, water 1.33, ordinary glass about 1.5). The light now reflects from the boundary between the inner core and its cladding, buried safely inside, and the outside can be handled, glued and bundled.

The smaller the difference in index, the shallower the angle the light must travel at to stay trapped. The range of angles a fibre accepts is its numerical aperture: a glass-clad workshop fibre with a big index difference accepts light from a wide cone; a telecom fibre accepts only a narrow one, and needs a laser aimed into it.

Total internal reflection air glass Steep ray escapes (and bends away) Slanting ray reflects completely beyond about 42° from the dashed line An optical fibre, cut lengthways Plastic coating Claddinglower refractive index Corehigher index Single-modecore 9, glass 125, coat 250 Multimodecore 50, glass 125, coat 250 Workshop fibrelead-glass core 80 in 100 Human hairabout 70 sizes in micrometres
Fig. 1 Left: light meeting the boundary between glass and air. A steep ray escapes; a ray striking at more than the critical angle reflects completely. Right: an optical fibre. The core has a slightly higher refractive index than the cladding, so light zig-zags along the core; a plastic coating protects the glass. Below, the cross-sections of common fibres, drawn to scale.

Loss, counted in decibels

Glass absorbs and scatters a little light in every metre. Fibre losses are counted in decibels (dB): every 10 dB means the light is cut to one tenth, 20 dB to a hundredth, 30 dB to a thousandth; 3 dB is about half.

Glass Loss Light left after 1 km
Good window glass about 1,000 dB per km nothing measurable
Glass-clad fibre from a workshop (lead-glass core) about 1 dB per metre usable to 10–30 m
Plastic fibre 0.15–0.2 dB per metre usable to 50–100 m
First low-loss silica fibre (1970) 17–20 dB per km 1–2 %
Modern silica fibre at 1,550 nm about 0.2 dB per km 95 %; 1 % left after 100 km

Where the loss comes from:

  • Impurities. Iron, copper, chromium and other metal atoms absorb light strongly. A few parts per billion matter. So does water: hydroxyl groups in the glass absorb strongly near 1,380 nm.
  • Scattering. Tiny unevenness frozen into the glass scatters light, as dust in a sunbeam. It falls steeply with longer wavelength (with the fourth power), which is why long-distance fibre uses invisible infrared at 1,310 and 1,550 nm, not visible light.
  • Bending. Bent too sharply (tighter than a few centimetres radius for telecom fibre), light leaks out at the bend.

Pulses that spread

In a thick core (50 micrometres or more) light can take many zig-zag paths of slightly different lengths, so a short flash arrives smeared out; flashes sent too close together blur into each other. This multimode fibre is cheap and easy to connect but is limited to a few kilometres at high speed. A single-mode fibre has a core so thin (about 9 micrometres) that light can only travel straight down the middle. It needs lasers and precise alignment, but carries tens of billions of flashes a second over a hundred kilometres.

What you need

For What From
Glass-clad fibre A lead (flint) glass rod for the core, a soda-lime glass tube for the cladding, matched in expansion Glass, Optical Glass and Achromatic Lenses, Lead
A small furnace or burner, a drawing drum Glass Fibre and Glass Wool
A light link A lamp or light-emitting diode, a photocell or photodiode, an amplifier Arc Lamps, Neon and Fluorescent Lights, Photocells and Sensors, Amplifiers and Oscillators
Silica fibre Distilled silicon tetrachloride and germanium tetrachloride, dry oxygen, fused-quartz tubes Pure Silicon, Liquid Air, Nitrogen and the Noble Gases, Distillation
A glassworking lathe with an oxy-hydrogen burner; a draw tower with a 2,000 °C furnace; coating resin and an ultraviolet lamp Hydrogen, Oxygen and Gases, Machine Tools, Petrochemicals and Modern Plastics
Long links Laser diodes at 1,310 or 1,550 nm, fast photodiodes, and later optical amplifiers Lasers, Semiconductors and the Transistor

Where to find it

  • Silica for fused-quartz tubes and for silicon: clear vein quartz and the whitest quartz sand, washed and acid-cleaned (Rocks and Minerals).
  • Lead for flint glass: galena ore (Lead).
  • Germanium, used to raise the index of the core: a trace in zinc ores (sphalerite), collected from the flue dust and residues of zinc smelting, and in the ash of some coals.
  • Chlorine, to turn silicon and germanium into distillable liquids: from salt by Electrolysis (Chlorine and Bleach).
  • Borax and potash adjust soft glasses so core and cladding match (Borax and Boric Acid).

Method 1: Glass-clad fibre (workshop)

This is how the first practical fibres were made in the 1950s, and it needs only good glassworking.

Choose two glasses. The core must have the higher refractive index: a lead (flint) glass, about 1.6. The cladding: ordinary soda-lime glass, about 1.52 (Optical Glass and Achromatic Lenses gives recipes). They must also shrink by the same amount as they cool, or the finished fibre shatters or peels apart. Test this with the old glassworker's thread test: soften the end of a rod of each glass, press them together side by side, and pull out a thread of the two fused together, about 30 cm long. As it cools, a matched pair stays straight; a badly mismatched pair curls into a bow towards the glass that shrinks more. Adjust the cladding glass (more potash or borax to change its expansion) and repeat until the thread stays nearly straight.

Rod in tube.

  1. Draw a core rod of flint glass about 10 mm thick and 30–40 cm long, and a cladding tube of soda glass that it just slides into, with walls 1.5–2 mm thick.
  2. Clean both inside and out with water, then alcohol; any dust becomes a bubble that scatters light. Slide the rod in.
  3. Heat one end in a small furnace or a ring of burners until it softens (orange, about 900–1,000 °C) and fuses into a blob. Pull the blob away, catch the thread on a drawing drum 30–50 cm across (Glass Fibre and Glass Wool), and turn the drum steadily. The tube collapses onto the rod as they soften, and both draw down together, keeping their proportions.
  4. Feed the rod slowly into the heat as it is used up. The faster the drum turns, the thinner the fibre: aim for 50–100 micrometres for bundles and 0.2–0.5 mm for a single light-carrying fibre.
  5. Coat the fibre at once, before it rubs on anything: run it through a small cup of varnish or molten wax just before the drum.

Uses. A single thick fibre, or a bundle of hundreds, carries light 10–30 m: light into a powder store or a mine without any flame or spark; light to a dozen indicator windows on a control panel from one lamp; a signal link between two buildings that cannot carry lightning or a dangerous voltage.

The fibrescope

A fibrescope carries an image. Wind a single fibre of 20–50 micrometres many hundreds of turns, neatly side by side, round a large drum in one flat layer, then several layers. Soak one short section across all the turns in glue and let it set hard. Cut through the middle of the glued patch. You now have a bundle whose fibres lie in exactly the same order at both ends (a coherent bundle), free and flexible in between. Polish both ends flat. Put a small lens at one end to form an image on the bundle face, and an eyepiece at the other to look at it (The Microscope); a separate loose bundle carries light in to illuminate the scene. The picture is made of dots, one per fibre, like a newspaper photograph. Doctors use fibrescopes to look into the stomach, lungs and joints; engineers into engines and pipes.

Make a light telegraph: a lamp or light-emitting diode at one end of the fibre, switched by the sending key or by a computer's serial output (Networks and the Internet); a photocell or photodiode at the other, feeding an amplifier and a relay or the computer's input. With a filament lamp, expect only tens of switchings a second (the filament is slow to cool); with an LED and a photodiode, thousands to millions.

Method 2: Pure silica fibre (the real thing)

Low-loss fibre is made of nearly pure silica (silicon dioxide, the substance of quartz), with a core made slightly denser by a few per cent of germanium oxide. Silica cannot be melted pure in a pot: no crucible survives 2,000 °C without poisoning it. Instead, the glass is built up from vapour, so that it never touches anything dirty.

Why vapour gives purity. Silicon tetrachloride boils at 58 °C and germanium tetrachloride at 86 °C. The chlorides of iron, copper and the other troublesome metals boil far higher or not at all. Distil the liquids carefully (Pure Silicon describes making and distilling silicon tetrachloride) and then carry them as vapour in a stream of oxygen: the metal impurities simply stay behind in the liquid. That trick, more than anything, is what made fibre possible.

1. Deposition lathe 2. Collapse into a preform 3. Draw tower oxygen + chloride vapours chlorine to scrubber White sootsettles ahead of the flame Clear glass layersmelted as the burner passes Burner1,600–1,900 °C,moving slowly tube turns; burner travels 10–20 cm a minute tube with layers heated to 2,100 °C,it shrinks inward solid rod The preforma scale model of the fibre: 1 m long, 2 cm thick, enough for about 25 km of fibre Preform Furnace2,000 °C Diametergauge: 125 µm Coatingliquid resin UV lampsharden it Capstanpulls Reel
Fig. 2 Making silica fibre. Top: the deposition lathe. Oxygen carrying the chloride vapours flows through a turning quartz tube; a burner moves slowly along it, the vapours burn to white glass soot that settles and melts into clear layers inside the tube, and the tube is finally collapsed into a solid rod, the preform. Right: the draw tower. The preform's tip melts in a furnace and is drawn into fibre, measured, coated and wound.

1. Building the preform

  1. The tube. A fused-quartz tube, about 20–25 mm across and 1 m long, made by melting pure quartz in an electric furnace. It forms the outer cladding.
  2. The lathe. Mount it in a glassworking lathe that turns it slowly (about one turn a second). A wide oxy-hydrogen burner (Hydrogen, Oxygen and Gases) on a carriage travels slowly along it, about 10–20 cm a minute, heating a short band of the tube white-hot, 1,600–1,900 °C.
  3. The vapours. Bubble dry oxygen through flasks of the liquid chlorides held at a steady temperature (for example in a water bath at 25 °C), and pipe the oxygen, now carrying vapour, into one end of the turning tube. Where the tube is hot, the chlorides burn: silicon tetrachloride + oxygen → silica + chlorine. White silica soot forms and settles on the inside wall just beyond the burner, and the burner, moving on, melts each soot layer into a thin clear glass layer.
  4. Cladding first, then core. Lay down 10–20 layers of pure silica, then switch on the germanium flow and lay down the core layers. A few per cent of germanium oxide raises the index by about a third of a per cent, all a single-mode fibre needs.
  5. Collapse. Turn off the vapours, slow the burner and raise the heat to about 2,100 °C. Surface tension pulls the softened tube inward, pass by pass, until the hole closes completely. The result is a solid glass rod, the preform: an exact scale model of the fibre, with core and cladding in the right proportions.

The chlorine and leftover vapours leave the far end of the tube: lead them through a scrubber of caustic soda solution (Lye and Potash), never into the room.

A preform 1 m long and 2 cm thick draws into about 25 km of fibre. Industry builds preforms 10–15 cm thick by other vapour methods, each drawing thousands of kilometres.

2. Drawing

  1. Hang the preform vertically at the top of a draw tower, its lower tip inside a furnace at about 2,000 °C (a graphite heater in argon, or an induction-heated zirconia tube).
  2. The softened tip drips down as a blob dragging a thread behind it. Cut off the blob and lead the thread down the tower to a pulling wheel (capstan).
  3. Measure the fibre diameter as it passes, by the shadow it casts in a light beam: it must be 125 micrometres, held to within about 1 micrometre. Feed this back to the capstan speed: faster makes it thinner.
  4. Coat it while it is still pristine, before it touches anything: pass it through a cup of liquid acrylic resin and under ultraviolet lamps that harden it in a fraction of a second. Two coats bring it to 250 micrometres.
  5. Wind it onto a reel. Industry draws at 20–50 m a second, from towers 10–30 m tall that give the fibre time to cool before coating. A small tower 4–5 m tall, drawing at 1 m a second, works.
  6. Proof-test every metre: run it over pulleys that stretch it with a force of about 9 newtons, like hanging a 1 kg weight from a hair. Any weak spot breaks then, not under the street.

Splicing and connecting

Fibres are joined end to end, and the joint must line up cores 9 micrometres across.

  1. Strip 3–4 cm of coating (soften it in hot solvent or scrape with a stripping tool with a hole just over 125 micrometres).
  2. Clean the bare glass with alcohol on lint-free paper.
  3. Cleave. Nick the glass with a diamond or hard carbide blade while holding it under slight tension, then bend gently: it snaps with a mirror-flat end square to the axis. Look at it under a microscope at 100–200 times: it should be flat, smooth and clean, tilted less than 1°. A chipped or angled end is cut again.
  4. Fusion splice. Lay the two ends in small V-grooves facing each other, line them up under the microscope with fine screws, and strike an electric arc between two tungsten points across the gap for 1–2 seconds while pushing the ends together by about 10 micrometres. The glass melts into one piece. A good splice loses 0.02–0.1 dB and is almost invisible. Protect it with a sleeve: a steel rod and the fibre inside a heat-shrink tube.
  5. Mechanical splice. Without an arc, lay the cleaved ends nose to nose in a precise V-groove with a drop of index-matching gel between them (pure glycerine, index 1.47, close to silica's 1.46, works) and clamp them. Loss 0.1–0.5 dB; fine for multimode fibre.

Connectors hold the fibre in a hole bored precisely through a ceramic ferrule 2.5 mm across; two ferrules meet nose to nose in a sleeve. Each pair loses 0.3–0.5 dB, and a speck of dust ruins it: cap them always.

Fibre-optic cable

Land cableDeep-sea cable 10–20 mm across, 48–288 fibres17–20 mm across; up to a few dozen fibres Polyethylene jacketblack, sunlight-proof Steel armouragainst rodents and digging Loose tubeup to 12 fibres in water-repelling gel Fibreseach coloured so it can be found at a splice Water-blocking tapeswells if water gets in Strength membersteel wire or glass-reinforced rod: takes the pull Polyethylene insulationkeeps the sea from the copper Copper sleevecarries several thousand volts to power the amplifiers Steel wiresstrength for laying in deep water Welded steel tubekeeps out water and crushing pressure Fibres in gel
Fig. 3 Left: a land fibre-optic cable in section. Colour-coded fibres lie loose in gel-filled tubes, stranded round a central strength member, inside armour and a polyethylene jacket. Right: a deep-sea cable, with the fibres in a steel tube, steel strength wires, and a copper layer that carries the power for the amplifiers on the sea bed.

Glass fibre is strong but hates being stretched, crushed, bent sharply or wet. A fibre-optic cable protects it:

  • Loose tubes: up to 12 fibres, each a different colour, lying loosely in a plastic tube 2–3 mm across filled with water-repelling gel, so that when the cable stretches or shrinks with temperature, the fibres do not.
  • Strength member: a steel wire or glass-reinforced rod at the centre takes the pull when the cable is hauled through a duct.
  • Water blocking tape or powder that swells when wet; then steel tape or wire armour against rodents and digging; and a black polyethylene jacket (Petrochemicals and Modern Plastics). A land cable with 48–288 fibres is 10–20 mm across.
  • Undersea cables put the fibres inside a welded steel tube, surrounded by steel wires for strength and a copper sleeve that carries several thousand volts of direct current to power amplifiers on the sea bed every 50–100 km, all inside thick polyethylene. In deep water the cable is about the thickness of a garden hose (17–20 mm); near the shore, where anchors and trawls threaten it, it is armoured to 5 cm.

Bury land cable in a duct at least 60–100 cm down, with a warning tape above it; never bend it tighter than about 20 times its own diameter. Splices sit in sealed boxes every 2–6 km, the length that fits on one cable drum.

Sending light hundreds of kilometres

A practical link is a budget of decibels. Example at 1,550 nm:

  • The laser diode puts about 1 milliwatt into the fibre.
  • The receiver (a fast photodiode and amplifier) needs about 1 microwatt: a ratio of 1,000, or 30 dB to spend.
  • Keep 3–5 dB in reserve for ageing and repairs.
  • Fibre at 0.2 dB per km plus a splice every few km: about 0.22 dB per km.
  • So the link reaches about (30 − 4) ÷ 0.22 ≈ 120 km with no help at all.

Beyond that, the light must be renewed: at first by repeaters that turned light into electricity, cleaned up the pulses and sent them on with a new laser; since about 1990 by optical amplifiers, lengths of fibre doped with the rare metal erbium, which, pumped by their own small laser, amplify the passing light directly, all colours at once. A transatlantic cable has around a hundred of them.

Many colours at once. Because an optical amplifier boosts a whole band, a single fibre can carry 80–100 lasers of slightly different wavelengths side by side, separated again at the far end by fine filters, each carrying 100 billion bits a second or more: tens of trillions of bits a second in one hair of glass.

Why fibre carries the internet

  • Capacity. One fibre pair carries more than every copper and radio link of the mid-twentieth century together, and a cable holds dozens of pairs.
  • Distance. 100 km between amplifiers, against 2–5 km for high-speed copper.
  • Cost. The raw material is sand; the cable is light, and a single cable laid once can be upgraded for decades just by changing the lasers at its ends.
  • Immunity. No electrical noise, no lightning, no crosstalk between fibres, and very hard to tap without being noticed.

The routers and servers of The Internet sit at the ends of these fibres; everything between them is glass.

How to tell it worked

  • Light through: a glass-clad fibre held to a lamp shines at the far end and stays bright when gripped, wetted or gently bent; a bare fibre dims at every touch.
  • Loss by cutting back: measure the light out of a long fibre with a photocell and meter (Measuring Electricity), cut it to 1–2 m near the launch end without disturbing the launch, and measure again. Loss in dB = 10 × log₁₀(short reading ÷ long reading), divided by the length removed.
  • Fibrescope: print is readable through it, the right way round, with no scrambled patches.
  • Splice: no line, bubble or step under the microscope, and no measurable drop on a light meter.
  • Echo testing (industry): a pulse sent into one end is faintly scattered back from every point; timing the echo maps every splice and break from one end.

Note Troubleshooting. Fibre shatters as it cools, or the skin flakes off → core and cladding glasses mismatched; redo the thread test. Dim output, glittering specks along the fibre → bubbles or dust between rod and tube; clean better, draw slower. Fibre breaks on the drum → too thin, uncoated, or touched before coating. High loss in silica fibre → water (dry the oxygen and the chlorides better) or metal contamination (re-distil, keep every part of the gas line glass or clean stainless steel). Splice loss high → bad cleave (chipped or angled end), dirt, or cores offset. A link works for a while and then fails in cold weather → fibre bent too tightly in a splice box or a duct; it leaks light as the cable shrinks.

Dangers

Danger Invisible laser light. Telecom fibres carry infrared light that you cannot see, often strong enough to burn the retina, especially from amplified links. Never look into the end of a fibre or a connector, even one you believe is dark. Check with a meter or an infrared viewing card. See Lasers.

Danger Chlorides and chlorine. Silicon and germanium tetrachloride fume in damp air into hydrochloric acid; the deposition process gives off chlorine. Work in a fume hood or outdoors, with the exhaust through a caustic scrubber. See Pure Silicon and Chlorine and Bleach.

  • Glass splinters. Offcuts of bare fibre are thin, sharp, almost invisible and work deep into skin; in the eye they are serious. Drop every scrap into a marked jar with a lid, work on a black mat so they show, wear safety spectacles, and never eat or rub your eyes at the bench.
  • Heat. Oxy-hydrogen flames and the 2,000 °C draw furnace: Hydrogen, Oxygen and Gases.
  • Fusion splicer arc uses a few thousand volts.

What this unlocks

The Internet at full speed between cities and across oceans. Fibre links inside power stations and substations that carry signals safely across thousands of volts (Power Lines and Distribution). Fibrescopes and endoscopes for medicine and engineering (Medical Instruments). Fibre sensors that measure strain and temperature along a dam or a bridge. And light delivered to where it is needed: to a laser scalpel in Basic Surgery, or into a sample in a laboratory.

How it was first done

Jean-Daniel Colladon in Geneva guided light along a jet of water in 1841, and John Tyndall made the demonstration famous in London in 1854. Alexander Graham Bell sent speech on a beam of sunlight with his photophone in 1880. In the 1920s and 1930s John Logie Baird, Clarence Hansell and Heinrich Lamm tried bundles of glass fibres for carrying pictures, but without cladding they leaked.

In 1954 Abraham van Heel in the Netherlands and Harold Hopkins and Narinder Kapany in London published imaging bundles, van Heel's with cladding. In 1956 Lawrence Curtiss, an undergraduate at the University of Michigan, made glass-clad fibre by the rod-in-tube method, and in 1957 Basil Hirschowitz tested the first fibre-optic gastroscope. In 1966 Charles Kao and George Hockham in England showed that glass losses came from impurities, not from glass itself, and that fibre losing under 20 dB per km could carry telephone calls; Kao received the Nobel Prize in 2009. In 1970 Robert Maurer, Donald Keck and Peter Schultz at Corning beat that target with silica fibre, and John MacChesney's team at Bell Labs developed the inside-the-tube vapour method in 1974. Fibre carried public telephone traffic from 1977, the first transatlantic fibre cable (TAT-8) opened in 1988, and erbium-doped fibre amplifiers, demonstrated at Southampton and Bell Labs in 1987, made today's long, many-coloured links possible.

Source: content/entries/electronics/fibre-optics.md