Insulation and Keeping Buildings Warm or Cool

How heat leaks out of a house and how to stop it — sealing draughts, packing roofs, walls and floors with straw, wool, cork, sawdust or moss, banking earth against walls, and using thick masonry to store heat — plus how to stay cool in hot climates with shade, thick walls, breezes, wind towers and evaporation, while keeping the air fresh and the walls dry.

Difficulty
●●●●●
Time
A day to draught-proof a house; a week or two to insulate a roof and floor; a season for a straw-bale or earth-sheltered house
Steps from zero
7 prerequisites →

You need first

Cob, Adobe and Rammed EarthFelt

This unlocks

Cooking Ranges, Iceboxes and Vacuum Flasks
The full path from nothing — 7 steps before this one
  1. Stone Tools
  2. Finding and Preparing Clay
  3. Farming from Seed
  4. Cob, Adobe and Rammed Earth
  5. Keeping Animals
  6. Wool
  7. Felt
  8. Insulation and Keeping Buildings Warm or Cool

Do them roughly in this order. See it on the tech tree →

Why it matters

In a cold climate, a poorly built house eats firewood: a family with an open fire in a draughty cottage can burn 10 tonnes or more in a long winter, and spend months cutting it (Firewood and Coppicing). The same house, sealed and insulated, can be kept warmer on a third or a quarter of that. That is land, labour and forest freed for everything else. Warm, dry houses also mean fewer deaths of the old and the very young from cold and lung disease (Surviving Cold and Heat).

In a hot climate the same knowledge works in reverse. A house that keeps the sun's heat out can be 5–10 °C cooler inside than the air at midday, without any machine.

Insulation is cheap. Most of it is waste: straw, chaff, sawdust, wool too coarse to spin, moss, earth. The skill is knowing where to put it and how to keep it dry.

How it works

Heat always flows from warm to cold. It leaves a house in four ways:

  1. Conduction — heat passing through solid material, molecule to molecule. Stone and metal conduct heat fast; wood slowly; still air very slowly.
  2. Convection — warm air moving. Air touching a cold window cools, sinks and flows across the floor; air touching a stove warms and rises. Inside a hollow wall, circling air carries heat across the gap.
  3. Radiation — heat shining from a warm surface to a cold one, the way you feel a fire on your face or a cold window chilling your cheek from a metre away.
  4. Air leakage (draughts) — warm air escaping through cracks and cold air flooding in. In an old, unsealed house this is often the biggest loss of all.

Insulation works by trapping still air. Wool, straw, feathers, felt and moss are good not because of the fibres themselves but because they hold millions of tiny pockets of air that cannot move, so neither conduction nor convection gets far. Two rules follow: insulation must be fluffy (crushing it pushes out the air) and dry (water conducts heat about 25 times better than air, so wet wool or damp straw insulates very badly).

Thermal mass is a different thing. A thick stone or earth wall is a poor insulator but a good store of heat: it takes hours to warm and hours to cool. Mass evens out temperature swings — it soaks up the day's heat and gives it back at night. Insulation slows heat flow; mass delays it. A good house uses both: mass inside, insulation outside.

Chimney10 cm clear of any fill Loft fill20–30 cm of straw,wool, or sawdustand lime Shutterclosed at night Insulationoutside the mass Gravel, 15 cmstops rising damp Roofloses the most heat:insulate it first Draughtsseal every crack first Earth bermwindward side Masonry stovestores the heat for hours
Fig. 1 Where heat leaves a cold-climate house, and what stops it. The roof and the draughts lose most; insulation goes on the cold side of the thick inner walls, which store the stove's heat.

How good is each material?

The figure compares materials by how thick a layer you need to keep out as much heat as 10 cm of sheep's wool. Thin is good.

Thickness that keeps in as much heat as 10 cm of wool Wool, felt Cork Straw, hay, reed Sawdust, chaff Softwood Light straw-clay Cob, brick Stone 10 cm 11–12 cm 13–16 cm 15–20 cm 30 cm 25–40 cm ≈ 2 m ≈ 3–6 m 010 cm20 cm30 cm Bars to scale up to 40 cm; the last two are broken — they would run off the page.
Fig. 2 How thick a layer of each material insulates as well as 10 cm of wool. A wall of solid stone would have to be several metres thick.
Material Same as 10 cm of wool Notes
Wool, felt (loose or batts) 10 cm Best natural insulation; resists fire and damp better than plant fibres. Protect from moths.
Cork (bark granules or slabs) 11–12 cm Does not rot, mice dislike it, almost waterproof. Only where cork oak grows.
Straw, hay, reed, loose or baled 13–16 cm Cheap and plentiful. Must be kept dry; burns easily unless plastered.
Sawdust, wood shavings, chaff 15–20 cm Mix with lime against mice and insects. Settles: top it up.
Dry moss (sphagnum) 12–15 cm Traditional for chinking logs and stuffing roofs.
Softwood (logs, boards) 30 cm Thick logs insulate fairly well (Timber Framing and Log Building).
Light straw-clay (straw dipped in clay slip) 25–40 cm Strong enough to fill a frame; fireproof once plastered.
Turf, dry earth 1–2 m Mostly mass, not insulation. Earth berms work because they are very thick.
Cob, rammed earth, brick 1.5–2.5 m Good mass, poor insulation.
Stone 3–6 m Cold to live behind unless lined.

What you need

Item Amount, roughly, for a 5 × 8 m one-storey house From
Straw, hay or reed 30–50 big armfuls for the loft; 250–300 small bales for straw-bale walls Grain harvest (The Great Staple Crops), reed beds
Sawdust or shavings 4–6 m³ for a loft Saw pits (Files and Saws)
Coarse wool, felt Any amount; felt strips for doors Wool, Felt
Clay Several tonnes for slip and plaster Finding and Preparing Clay
Lime A few sacks: to mix with sawdust, and for plaster Lime
Moss Sacks of it for chinking Bogs and wet woods
Gravel or broken stone 15 cm under a floor Riverbanks
Boards For a ceiling and to hold loose fill Timber Framing and Log Building
Leather, felt or rope Draught strips Hides and Leather, Felt

Where to find it

  • Straw — the stems left after threshing grain; keep it under cover. Hay (dried grass) is wanted for animals, so use the poor stuff.
  • Wool — the short, coarse, dirty wool from bellies and legs that is no good for Spinning and Weaving Cloth is fine for insulation. Wash it first; grease and dirt attract insects (Wool).
  • Cork — the thick, spongy outer bark of the cork oak, which grows around the western Mediterranean. It can be stripped every 9–10 years without killing the tree.
  • Sawdust and shavings — from any saw pit or carpenter's shop; dry before use.
  • Moss — sphagnum and other mosses grow in thick cushions in bogs and wet forest. Pull it, squeeze it out and dry it in the sun.
  • Reed and cattail from marshes, and turf from matted grassland — see Roofs.

Method 1: Stop the draughts first

This is the cheapest and quickest saving. Do it before anything else.

  1. Find the leaks. On a cold, windy day, hold a candle flame or a smoking stick near door and window edges, where walls meet roof and floor, around beams and chimneys. Wherever the flame bends or the smoke streams, air is moving.
  2. Seal gaps in walls with clay plaster or lime mortar. Stuff gaps in log walls with moss or tarred fibre, then cover them with clay or lime (chinking; see Timber Framing and Log Building).
  3. Seal around doors and windows. Nail strips of felt or soft leather around the frame so the door closes against them. Fit a hinged board or a sausage of sand in cloth along the bottom of the door. Hang a thick curtain inside the door and close shutters at night.
  4. Add a porch. A small entry room with a second door (an airlock) means the warm air does not rush out every time someone comes in.
  5. Fit double windows for the winter — a second sash with a still air gap between (Window Glass).
  6. Close the chimney when the fire is out, with a damper or a plate (Chimneys, Stoves and Heating). An open chimney is a hole in the roof.

Warning Do not seal a house completely. Every fire needs air, and people need fresh air. See Ventilation below before you seal the last crack.

Method 2: Insulate the roof

Warm air rises, so the roof or ceiling loses the most heat — insulate it next.

  1. Make a ceiling. Lay boards or close-set poles across the tie beams or joists above the room. Cover them with a 2–3 cm layer of clay plaster or a sheet of birch bark so loose fill does not fall through and dust cannot sift down.
  2. Lay 20–30 cm of loose insulation on top: straw, hay, reed, wool, moss, or sawdust mixed with about one part slaked lime to ten parts sawdust by volume against vermin and mould. Spread it evenly, fluffed, not trodden.
  3. Cover straw or sawdust with a thin crust of clay slip (clay stirred in water to a thick cream) or clay plaster. This slows fire and keeps the fill from blowing about.
  4. Keep it dry. Check under the roof after the first heavy rain. Wet patches must be found and the roof mended at once (Roofs).
  5. Keep it away from the chimney. Leave at least 10 cm of bare clay or masonry round any chimney or flue, and never let straw touch a stove pipe.

Thick thatch and turf on birch bark are themselves good insulation; slate, tile and sheet roofs are not and need the ceiling fill.

Method 3: Insulate the walls

Pick the method that fits your walls:

  • Light straw-clay. Stir clay into water to a thin cream. Toss loose straw in it until every stem is coated but not dripping. Pack it into removable boards set between the posts of a timber frame, tamping it firm but not hard, about 30 cm thick, and move the boards up as you go. Dry for 4–8 weeks in good weather, then plaster.
  • Straw-bale walls. Tight bales about 35 × 45 × 90 cm, stacked like big bricks on a stone plinth at least 30 cm high, staggered, pinned with hazel stakes through two courses, a timber plate on top tied down to the foundation, and lime or clay plaster 3–5 cm thick on both faces. A 45 cm bale wall insulates many times better than a metre of stone. Bales must be dry and tightly tied when laid; protect walls with a wide roof overhang (at least 50 cm).
  • Filled double walls. Build an inner wall (wattle, boards or brick) 15–20 cm inside the outer one and fill the gap with dry sawdust and lime, straw or moss. Leave hatches near the top to top up the fill as it settles.
  • Line an existing stone or earth wall. Fix a frame of poles 10 cm away from the inside face, pack the gap with straw-clay or wool, and plaster over. Or hang felt or woven mats on the inside of a cold wall, as the nomads line their tents (Felt).
  • Earth berms. Pile earth against the outside of a wall on the windward and shady sides, up to the eaves, or dig the house into a south-facing slope (north-facing in the southern hemisphere). The ground a metre down stays near the year's average temperature — far above the winter air in cold places. Only berm a wall that is built to take the pressure and is waterproofed — stone or brick with a good lime render, a layer of birch bark or clay against it, and a drain at the foot (Foundations and Floors). An earth wall buried in damp soil will slump.

Method 4: The floor

Cold rises from the ground, and damp with it.

  1. Lift the floor. A timber floor on joists over a ventilated space of 30–45 cm stays dry.
  2. Or break the damp. Under a beaten-earth or flag floor, lay 15 cm of gravel or broken stone; water cannot climb through it. Then a layer of clay, then the floor (Foundations and Floors).
  3. Insulate it. Under a timber floor, fill between the joists with dry straw-clay, sawdust and lime, or cork. On an earth floor, lay rush mats, felts or rugs; a thick felt underfoot makes a cold room bearable.

Thermal mass and the sun

  • Put mass inside, where the heat is. A big masonry stove in the middle of the house (Chimneys, Stoves and Heating) stores the heat of a short, hot fire and gives it out for 12–24 hours.
  • Catch the winter sun. Put most windows on the sunny side (south in the northern hemisphere) and few on the shady side. Sun through glass falling on a dark stone or earth floor warms it; it gives the heat back in the evening. Shutter the windows at night. Use a roof overhang sized so the high summer sun is shaded and the low winter sun gets in — about a third to half the height of the window below it, at middle latitudes.
  • Plant evergreens on the windward side as a windbreak; it can cut the wind on the house by half.

Damp, condensation and keeping it dry

Warm indoor air carries water from breathing, cooking and washing. When it meets a cold surface it turns to drops (condensation), as on a cold cup. If that happens inside a wall or roof, the insulation gets wet, stops working and rots.

  • The warm side tight, the cold side open. Make the inside face of an insulated wall or ceiling the most airtight layer (a good clay or lime plaster, sealed at the edges). Let the outside face breathe — lime render, not tar or paint — so any damp that gets in can dry out.
  • Lime and clay plasters soak up moisture and let it pass slowly, protecting straw and timber. Never seal straw in a waterproof skin.
  • Straw and sawdust rot when damp. Push your hand into the fill. It should feel dry and springy and smell of hay. If it is warm, damp or smells musty, find the water and fix it.

Ventilation

A house sealed tight against draughts still needs controlled fresh air — roughly half the air in the house changed every hour.

  • Give every fire its own air supply from outside (Chimneys, Stoves and Heating).
  • Leave small vents high up in each room, and open windows wide for 5–10 minutes a day, even in winter.
  • If windows stream with water every morning, mould grows in corners, or people wake with headaches, the house is too tight. Ventilate more. For fans, ducts and machine cooling, see Ventilation and Air Conditioning.

Keeping cool in hot climates

Here the enemy is the sun, mostly falling on the roof.

  1. Shade first. Wide eaves, verandahs and trees; shade the roof, the walls facing the afternoon sun, and the ground around the house. Vines on a frame over a courtyard cool the whole space.
  2. Light colours. A fresh coat of lime whitewash on the roof and walls reflects most of the sunlight; a dark roof can be 30–40 °C hotter than a white one in full sun.
  3. Insulate the roof. A thick thatch or a ventilated double roof (an outer roof that takes the sun, an air gap open at both ends, and an inner ceiling) keeps the sun's heat out of the room below.
HOT AND DRY HOT AND WET Wind towercatches the breezeand sends it down Whitewashreflects the sun Thick earth wallsheat takes 8–12 hoursto soak through Courtyard, poolholds the night'scool air Ridge venthot air rises out High thatchwide eaves Open wallscross breeze Raised floorlight timber, bamboo, palm;dry and in the breeze
Fig. 3 Keeping cool without machines. In a hot, dry climate thick walls store the night's coolness; a wind tower brings in the breeze; a courtyard holds cool air and water evaporates. In a hot, wet climate the house is light, raised and open to every breeze.

Hot and dry (deserts, with cold nights):

  • Thick walls and roof of earth or stone, 40–60 cm or more (Cob, Adobe and Rammed Earth). Heat takes 8–12 hours to soak through, arriving in the night when it can be let out. Few, small windows.
  • Night flushing. Open everything at night to let cool air in and cool the walls; close up at dawn.
  • Courtyards surrounded by rooms, shaded, with a pool or fountain. The cool night air settles in the court and stays there into the day.
  • Wind towers (the badgir of Iran): a tall shaft rising above the roof, open at the top toward the wind, which catches the breeze and sends it down into the house. Air passing over water or wet pots at the bottom cools further.
  • Evaporation. Hang wet mats of reed or straw in windows and doors; water evaporating takes heat with it (Ice and Refrigeration).

Hot and wet (tropics, warm nights, where mass does not help):

  • Build light, of timber, bamboo, palm and thatch, which cool quickly at night.
  • Raise the floor on stilts to catch the breeze and stay dry.
  • Open walls — screens, shutters and louvres on opposite sides for cross-ventilation.
  • High roofs with vents at the ridge: hot air rises and escapes through the top, drawing cooler air in low down (the stack effect).

How to tell it worked

  • Firewood. Count the loads of wood per week before and after. A good job saves a third or more.
  • The morning test. Bank the fire at night and note the room in the morning: can you see your breath? Is the water bucket frozen? A well-insulated house stays comfortable overnight on the heat stored in the stove.
  • The hand test. On a cold day, lay your palm on the inside of an outside wall. A well-insulated wall feels nearly as warm as the room. A cold, clammy wall is losing heat.
  • Snow and frost. After a snowfall, look at roofs. Snow that melts fast off one roof while it lies on its neighbour means that roof is leaking heat.
  • In heat: at midday, the room should feel clearly cooler than the shade outside.

Note Troubleshooting. Still cold despite insulation → look for draughts first; then gaps in the insulation, especially at the eaves and around beams. Ceiling fill compacted to a few centimetres → it got wet or was trodden down. Dry it or replace it and fluff it. Mould on walls and in corners → too little ventilation, or a cold spot where there is no insulation. Ventilate more and fill the gap. Mice and rats in the fill → mix in lime, or use wool, cork or straw-clay instead of loose straw; block holes with wire or broken glass in mortar. Hot house in summer → shade the roof and the west wall, whitewash, ventilate at night. Plaster cracking off straw-clay → it was plastered before it was dry. Wait longer, and key the surface by scratching it.

Dangers

Danger Fire. Straw, hay, sawdust and moss are excellent insulation and excellent kindling. Never let them touch a chimney, stove pipe or hearth: keep at least 10 cm of masonry or clay between them and anything hot, and check the chimney every year for cracks (Chimneys, Stoves and Heating). Cover loose fill with clay slip or plaster. In a straw house, a spark landing in a loose bale can smoulder unseen for hours.

Danger Carbon monoxide in a tight house. A sealed house with a smoky fire or a brazier can kill the sleepers. Every fire must have its own air supply and a sound chimney. Headache, dizziness and drowsiness that ease when you go outside mean poison gas — get everyone out and ventilate (Chimneys, Stoves and Heating).

  • Dust. Handling dry straw, hay, sawdust and old insulation fills the air with dust and mould spores that damage lungs. Wet it slightly and wear a cloth over the mouth and nose.
  • Rot. Wet insulation rots hidden timber, and lime burns skin and eyes (Lime). Look under the roof and at wall bases every spring.
  • Heat. In hot climates, the very young and old can die of heat in an airless room. See Surviving Cold and Heat.

Going further

Once you have a glass furnace, glass can be spun into glass wool (Glass Fibre and Glass Wool), and molten slag from iron furnaces (Iron (the Bloomery), The Blast Furnace and Cast Iron) blown with a jet of steam into mineral wool — both fireproof, rot-proof and as good as sheep's wool. Cork can be baked into rigid boards bound by its own resin. With insulated walls, a house heated by the sun (Solar Heat) becomes practical, and the same knowledge builds ice houses and cold stores (Ice and Refrigeration) and keeps kilns and stoves hot (Firebrick and Refractories).

How it was first done

People have dug houses into the ground and roofed them with earth for at least 20,000 years — Ice Age pit houses, turf houses in Iceland from the Viking settlement (about AD 870) into the 20th century, sod houses on the American prairies in the 1800s. Central Asian nomads have insulated their round tents with layers of felt for at least 2,500 years. The windcatchers of Iran and the Persian Gulf, and courtyard houses across the Middle East and Mediterranean, go back well over a thousand years. Builders in many parts of Europe filled timber frames with straw and clay in the Middle Ages, and straw-bale houses were first built in Nebraska in the 1890s, after machines began to bale hay. Mineral wool was probably first made from slag in Wales in the 1840s and was sold for insulation from the 1870s; double windows were in use in northern Europe and Russia by the 1700s.

Source: content/entries/building/insulation.md