Part 13 · Electricity
The Transformer
Two coils on one iron core change alternating current from one voltage to another — up to a high voltage to send power far along thin wires, and down again to a safe voltage for lamps and tools. How it works, how to size one, and how to build and insulate it.
- Difficulty
- ●●●●●
- Time
- One to two weeks for a 100-watt transformer, most of it drawing iron wire and winding
- Steps from zero
- 23 prerequisites →
The full path from nothing — 23 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Pottery
- Hides and Leather
- Fermentation
- The Wheel and Axle
- Bellows
- Gears
- Copper Smelting
- Iron (the Bloomery)
- The Waterwheel
- Blacksmithing
- The Battery
- Magnets
- Copper Wire
- The Electromagnet
- The Generator
- The Transformer
Do them roughly in this order. See it on the tech tree →
Why it matters
A The Generator on a stream gives a few hundred watts at perhaps 100 volts. But the stream is half a kilometre from the village, and copper is precious. Send that power along a wire and a large part of it is lost as heat in the wire. The cure is to send it at a high voltage and a small current, then bring it back down to a safe voltage where it is used. The device that does both, with no moving parts, is the transformer.
It does much more:
- It makes low voltage at high current for Welding, the The Electric Arc Furnace, heating, and Electrolysis (with a rectifier).
- It makes high voltage at low current for Radio transmitters, X-Rays and neon-type glow lamps.
- It isolates a tool or lamp from the supply, so that touching one wire of it cannot shock you to earth (Wiring and Electrical Safety).
- It matches a microphone to a telephone line: the small "induction coil" in every The Telephone is a transformer.
Transformers are the reason the world's power grids run on alternating current (Power Lines and Distribution).
How it works
Two coils, one core
Wind two separate coils of insulated wire on the same closed loop of soft iron. Connect the first — the primary — to an alternating current supply. The current flowing back and forth in it makes magnetism in the iron that also swings back and forth, 50 or so times a second. That changing magnetism passes through the second coil — the secondary — and, exactly as in the The Generator, changing magnetism induces a voltage in it. No wire connects the two coils. Only magnetism passes between them.
The turns ratio
Every turn of wire round the core, on either coil, gets the same voltage — the "volts per turn". So:
secondary voltage ÷ primary voltage = secondary turns ÷ primary turns
- 500 turns primary, 50 turns secondary: 100 V in gives 10 V out (step down).
- 50 turns primary, 500 turns secondary: 100 V in gives 1,000 V out (step up).
Power in = power out
A transformer does not make energy. If the voltage goes down ten times, the current available goes up ten times, and the other way round. 100 V at 1 A in (100 W) gives 10 V at nearly 10 A, or 1,000 V at nearly 0.1 A. A well-made transformer loses only a few percent as heat; a careful home-made one, 5–15%.
Only alternating current
The secondary only gets a voltage while the magnetism is changing. Steady direct current from a The Battery or a dynamo with a commutator makes steady magnetism: nothing comes out of the secondary, and the primary, with nothing to hold back the current except the resistance of its wire, acts almost as a short circuit and overheats. A transformer needs AC — from an alternator with slip rings, or a magneto with no commutator (The Generator). The one exception is the The Induction Coil, which chops DC on and off with a vibrating switch.
Why the core must be cut into thin pieces
The iron core is itself a conductor, and the changing magnetism induces currents in it, swirling round inside the iron like eddies in a stream. These eddy currents waste power and heat the core — a solid iron core in a transformer gets hot quickly. The cure is to build the core from thin wires or thin sheets, each lightly insulated from its neighbours by a film of rust, scale or varnish. The magnetism runs along them freely, but the eddies cannot circle across them. Thin sheets of 0.3–0.5 mm, or iron wire of 0.5–1 mm, are right for 50 cycles a second.
Why the core must be a closed loop
Magnetism flows far more easily through iron than through air. An open, straight core needs a much larger current in the primary just to magnetise it (the magnetising current), and this current flows all the time, even with nothing connected to the secondary. A closed ring or rectangle of iron, with no gaps, keeps this current small.
Sizing a transformer
You need three numbers: the power (watts), the frequency of your supply (cycles per second, hertz, Hz), and the voltages.
1. Find your frequency. For a generator, frequency = (number of north poles that pass a coil per turn) × (turns per second). A machine with 4 magnets set alternately north and south (two north poles) turning 10 times a second gives 2 × 10 = 20 Hz. A machine with 8 alternating poles (four north) at 12.5 turns a second gives 50 Hz. Lower frequencies need bigger transformers; 40–60 Hz is a good aim, and it does not make lamps flicker.
2. Choose the core size. The net cross-section of iron, A, in square centimetres:
A ≈ √(watts) at 50 Hz
| Power | Net iron area at 50 Hz | At 25 Hz |
|---|---|---|
| 25 W | 5 cm² | 7 cm² |
| 100 W | 10 cm² | 14 cm² |
| 500 W | 22 cm² | 32 cm² |
| 1,000 W | 32 cm² | 45 cm² |
"Net" means the iron itself, not the gaps: a round bundle of wire is only about 75–80% iron, so make it about a quarter bigger.
3. Work out the turns per volt. For home-made soft iron, worked gently:
turns per volt ≈ 2,800 ÷ (frequency in Hz × A in cm²)
Then primary turns = primary voltage × turns per volt. Add 5% to the secondary turns to make up for losses under load.
4. Choose the wire thickness. Allow about 2.5 amps per square millimetre of copper (less if the coil is buried deep and cannot cool):
| Current | Copper cross-section | Wire diameter |
|---|---|---|
| 0.5 A | 0.2 mm² | 0.5 mm |
| 1 A | 0.4 mm² | 0.7 mm |
| 2.5 A | 1 mm² | 1.1 mm |
| 5 A | 2 mm² | 1.6 mm |
| 10 A | 4 mm² | 2.3 mm |
| 20 A | 8 mm² | 3.2 mm (or several thinner wires side by side) |
Worked example: a 120 W transformer from 100 V to 10 V at 50 Hz.
- Iron area: √120 ≈ 11, so make it 12 cm² of iron — a round bundle about 4.4 cm across.
- Turns per volt: 2,800 ÷ (50 × 12) ≈ 4.7.
- Primary: 100 × 4.7 ≈ 470 turns. Current 1.2 A → 0.8 mm wire.
- Secondary: 10 × 4.7 × 1.05 ≈ 50 turns. Current 12 A → 5 mm² → 2.5 mm wire, or four 1.3 mm wires wound together side by side as one.
On a 20 Hz magneto, the same core would need 2½ times as many turns — or a core 2½ times bigger.
What you need
For the 120 W example:
| Item | Amount | Notes |
|---|---|---|
| Soft iron wire 0.6–1 mm | About 5 kg (roughly 800 m of 1 mm wire) | Drawn like copper wire (Copper Wire) from bloomery iron (Iron (the Bloomery)), then annealed |
| Covered copper wire | 90 m of 0.8 mm; 12 m of 2.5 mm (or 50 m of 1.3 mm) | Copper Wire |
| Insulation | Thin paper, cotton or linen tape, shellac varnish, mica if you have it | Paper, Copper Wire, Rocks and Minerals |
| Former | A wooden drum 12 cm across | For winding the iron ring |
| Netting shuttle | A flat wooden needle 25–30 cm long | For threading wire through the ring |
| Hardwood base and terminals | Basic Woodworking |
Where to find it
All of it comes from other chapters. Iron wire is the biggest job: draw it through the same steel draw plate as copper (Copper Wire), annealing often — iron hardens faster than copper. Anneal the finished wire by heating it to bright red (about 900 °C) in coils in a fire, or better packed in a clay pot of charcoal dust, and letting it cool slowly in the ashes. Soft iron is essential (The Electromagnet): steel or hard iron wastes power and heats up. The thin film of black scale left on the wire after annealing is a useful insulator between the strands; a dip in thin shellac or linseed oil varnish, dried, is better.
If you can roll or hammer thin iron sheet (Sheet Metal and Rolling), you can build a rectangular core from strips instead (Method 2).
Method 1: The iron-wire ring transformer
This is the easiest core to make well, because it has no joints or gaps at all. It is the design of the first practical transformers, built in Budapest in 1885.
- Wind the core. Wind the annealed, varnished iron wire round a wooden drum 12 cm across, turn after turn, like winding a hank of yarn, until the bundle is about 4.4 cm thick. Keep the turns neat and pressed together. Tie it tightly every 5 cm with cotton tape and slide it off the drum. You now have an iron ring, 12 cm across inside and about 21 cm outside.
- Shape it round. Bind it all round with cotton or linen tape, overlapping by half, so that the bundle becomes a smooth round "doughnut". Soak it in shellac varnish and let it dry. Then add two more layers of tape and varnish. This is the core insulation: the wire must never touch the iron.
- Load the shuttle. Measure 90 m of 0.8 mm covered wire and wind it onto a netting shuttle (or a long, thin wooden stick with notched ends) that will pass through the ring's hole.
- Wind the primary. Pass the shuttle through the hole and round the outside of the ring, again and again, laying each turn close beside the last. Spread the 470 turns evenly all the way round the ring — about two layers. Count turns in groups of ten with a knotted cord. Keep the direction the same throughout. Bring both ends out to the same point, leaving 20 cm tails, and label them.
- Insulate between the windings. This is the most important layer in the transformer. Wrap the whole ring, over the primary, with at least three layers of varnished cotton tape or varnished paper, overlapping each time by half, letting each layer dry. If you have mica, lay thin flakes under the tape.
- Wind the secondary (50 turns of 2.5 mm, or four 1.3 mm wires together) evenly over the insulation all round the ring. Thick wire is stiff: bend each turn round the ring with your fingers or a wooden lever. Bring the ends out on the opposite side of the ring from the primary's ends.
- Finish. Bake the whole transformer gently in a warm oven (about 80–100 °C) for several hours to drive out moisture. Then soak it in hot shellac varnish, or for a transformer that will run cool, in melted beeswax, and let it drain and set. Mount it on a hardwood base with the four terminals well apart, and mark them clearly: "100 V" and "10 V".
Method 2: The rectangular laminated core
If you can make thin iron sheet, a rectangular core is quicker to wind, because the coils are wound on a simple bobbin and slipped over the core.
- Cut strips of soft iron sheet 0.3–0.5 mm thick. For a 12 cm² core, make the strips 3.5 cm wide; you need enough of them to stack 4 cm thick (so with a little paper and varnish, about 12 cm² of iron).
- Insulate the strips: anneal them, then paint one side of each with thin shellac or glue on thin paper.
- Shape: the core is a rectangle with two long sides (the limbs) about 12 cm long and two short sides (the yokes), leaving a window inside about 6 × 9 cm for the coils.
- Wind the coils on wooden or card bobbins that slide over a limb: half the primary and half the secondary on each limb, the secondary over the primary with insulation between, all wound in the same direction. Or both coils on one limb, the secondary over the primary.
- Build up the core through the bobbins in layers, overlapping the corners like bricks: in one layer the limb strips run the full height and the yoke strips butt against them; in the next layer, the other way round. This overlap keeps the magnetic gaps at the corners tiny. Clamp the stack tightly between hardwood bars bolted together, or it will hum and buzz.
Method 3: Sending power a long way
The heat lost in a wire goes with the square of the current. Example: 1,000 W sent along a line whose two wires together have a resistance of 2 Ω:
| Sent at | Current | Lost as heat in the line | Share lost |
|---|---|---|---|
| 100 V | 10 A | 10 × 10 × 2 = 200 W | 20% |
| 1,000 V | 1 A | 1 × 1 × 2 = 2 W | 0.2% |
So: a step-up transformer at the generator (wound 1:10), a line of thin copper or even iron wire on poles and insulators, and a step-down transformer (10:1) at the far end, close to where the power is used. Both transformers are built as above. The 1,000 V winding needs far better insulation — see below — and the 1,000 V line must be treated as deadly (Power Lines and Distribution).
Insulating for high voltage
- Between layers. The voltage between the end of one layer and the start of the next can be twice the voltage of a whole layer. Put two layers of varnished paper between every layer of a high-voltage winding. Better, divide the winding into several short sections (pies) side by side, each only a few hundred volts.
- Between windings and to the core. For 1,000 V, at least 3 mm of varnished paper, cloth and mica, and the winding should stop 2–3 cm short of any edge or of the core, so sparks cannot creep along the surface.
- Under oil. Large high-voltage transformers stand in a tank of thin, dry mineral oil (Petroleum and Refining), which insulates and carries heat away. Dry the transformer in a warm oven first and heat the oil to drive out water. Water in the oil ruins it.
- Test every high-voltage transformer at low voltage first, then at full voltage with nobody near it, for an hour.
How to tell it worked
- The lamp test (no load). Connect a lamp rated for the supply voltage in series with the primary, and connect them to the AC supply, with nothing on the secondary. The lamp should glow only dimly or not at all: the transformer takes little current with no load. A brightly lit lamp means a shorted turn, too few turns, or a gap in the core.
- The ratio test. With the lamp removed, connect a lamp of the secondary's rating to the secondary. It should glow at its normal brightness. Compare against the same lamp run straight from a known supply.
- Hum. A transformer hums softly at twice the supply frequency. A loud buzz or rattle means loose strips or turns: clamp tighter, varnish again.
- Warmth. Run it at full load for an hour. It should be warm but comfortable to hold (under about 60 °C). Too hot to hold means too small a core, too few turns or too thin wire.
- Insulation. With a battery and galvanometer (The Electromagnet), check there is no connection between primary and secondary, or between either winding and the core.
Note Troubleshooting. Gets hot with nothing connected → too few primary turns for your frequency, a short between turns, or a solid or badly insulated core (eddy currents). Add turns, check the core. Output voltage much lower than expected → turns miscounted, or the supply frequency lower than you thought. Count again; measure the generator's speed. Output fine with no load but drops badly under load → secondary wire too thin, or the two windings too far apart (on separate limbs). Thicker wire; wind secondary over primary. Buzzes loudly → loose core strips or turns. Clamp and varnish. Smells of hot varnish, wax runs → overloaded. Reduce the load or build bigger. Supply fuse blows when switched on → it was connected to DC, or a winding is shorted. Never use DC.
Dangers
Danger A transformer makes deadly voltage from safe voltage. A step-up transformer on a 100 V supply can deliver 1,000 V or more — enough to kill instantly. And any transformer works backwards: a step-down transformer fed by mistake from its low-voltage side puts a high voltage on its "input" terminals. Label every winding with its voltage, cover all high-voltage terminals, switch off before touching, and never work on high-voltage gear alone.
Danger Insulation failure. If the insulation between windings breaks down, the high voltage appears on the low-voltage side, on tools and lamp sockets that people touch. Connect the iron core, and one end of the low-voltage winding, firmly to earth (Wiring and Electrical Safety), so that a breakdown blows a fuse instead of electrifying the low side.
- Never connect a transformer to DC. It draws a huge current, overheats and may burn; when the DC is disconnected, the primary gives a violent spark and a high-voltage kick.
- The kick on switching off. Even on AC, opening the primary circuit by hand can draw a spark. Use a proper switch (Wiring and Electrical Safety).
- Fire. Overloaded transformers char their varnish and set fire to wax, wood and oil. Fuse the primary (Wiring and Electrical Safety); mount transformers on stone or brick, not on wooden shelves near straw or cloth. An oil-filled transformer that fails can boil and burst into flame: keep it outdoors or in a stone room, with sand to smother a fire.
- Weight. A 1 kW transformer weighs 15–25 kg. Lift with care.
Going further
- Better iron. Iron with 3–4% silicon, made by Robert Hadfield around 1900, cuts core losses by more than half, and became the standard transformer iron (Alloy and Stainless Steels, Transformer Steel, Ferrite and Magnetic Shielding).
- Three-phase power. Three alternating currents, each a third of a cycle behind the next, sent on three wires, carry more power with less copper and turn simple induction motors. Three-phase transformers have three limbs.
- Rectifiers. A transformer and a rectifier (Rectifiers: Turning AC into DC: copper oxide, a The Vacuum Tube or a semiconductor diode) give low-voltage direct current from AC mains — for charging the The Rechargeable Battery, plating and electrolysis.
- The grid. Chains of transformers, stepping up to tens or hundreds of thousands of volts and down again, carry power across whole countries: Power Lines and Distribution.
How it was first done
Michael Faraday built the first transformer without knowing it: on 29 August 1831 he wound two coils on an iron ring and saw a galvanometer on one coil kick when he connected or disconnected a battery to the other. Through the mid-1800s, induction coils of Nicholas Callan (1836) and Heinrich Ruhmkorff (1851) used the same principle, with an interrupter, to make high-voltage sparks.
In 1881–83 Lucien Gaulard and John Dixon Gibbs built "secondary generators" with open, straight iron-wire cores, and in 1884, at an exhibition in Turin, Italy, used them to light lamps along a line tens of kilometres long. In Budapest in 1884–85, three engineers at the Ganz works — Károly Zipernowsky, Ottó Bláthy and Miksa Déri — saw that a closed core of iron wire worked far better and that transformers should be connected side by side (in parallel); they gave the transformer its name. In 1886 William Stanley, working for George Westinghouse, lit the shops and offices of Great Barrington, Massachusetts, through transformers with E-shaped laminated iron cores — the basic design still used today. In 1891 a 175 km line at about 15,000 volts carried power from a waterfall at Lauffen to an exhibition at Frankfurt in Germany, and the argument about whether to supply cities with AC or DC was effectively settled.
Source: content/entries/electricity/transformer.md