Part 6 · Building
Trusses and Frames
Why a triangle cannot change shape, and how to build frames of triangles — king and queen post roof trusses, and Howe, Pratt and Warren bridge trusses — that span far wider than any single beam. With a pencil, a ruler and a little arithmetic you can work out the push or pull in every member before you cut a single timber.
- Difficulty
- ●●●●●
- Time
- An evening to learn to work out the forces; a day to lay out and cut a king post truss; a few weeks for a small truss footbridge
- Steps from zero
- 22 prerequisites →
This unlocks
—The full path from nothing — 22 steps before this one
- Stone Tools
- Fire
- Cordage and Rope
- Finding and Preparing Clay
- Finding and Identifying Ores
- Writing and Numbers
- Measurement from Scratch
- Basic Woodworking
- Hunting and Trapping
- Charcoal
- The Scientific Method
- Arithmetic and Fractions
- Hides and Leather
- Forces, Energy and Heat
- Algebra
- Bellows
- Strength of Materials
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Timber Framing and Log Building
- Trusses and Frames
Do them roughly in this order. See it on the tech tree →
Why it matters
A single beam is a poor way to cross a gap. Its strength grows with its depth, but so does its weight, and no tree gives a sound beam much more than 8–10 m long and 40 cm deep. Past about 5–6 m a solid beam gets so heavy that it spends most of its strength holding up itself (Strength of Materials).
A truss solves this. It is a frame of straight pieces (members) joined at their ends into triangles — a very deep beam with most of the middle taken away. With trusses you can roof a hall or barn 10–20 m wide without posts (Roofs), bridge a ravine 15–50 m wide with timbers no longer than 4–5 m (Roads and Bridges), build towers, cranes and masts that do not sway (Cranes and Lifting, Walls, Palisades and Watchtowers), and later frame railway bridges, aircraft and steel buildings (Railways, Gliders and Aeroplanes, Steel Frames and Tall Buildings).
And because each member only pushes or pulls along its length, you can work out the force in every piece with a ruler and simple arithmetic, then size it from the tables in Strength of Materials. That turns bridge building from guesswork into design.
How it works
Why a triangle holds its shape
Join four sticks at the corners with single pegs and push one corner sideways: the square folds flat into a diamond. This is racking, and it is why barns, gates and scaffolds collapse sideways. A triangle joined the same way cannot change shape unless a stick stretches or shortens. So a frame made entirely of triangles is rigid even with pinned joints — and every brace nailed across a gate turns a square into two triangles.
Push and pull
If loads are put on a truss only at its joints, each member carries a force along its own length and nothing else:
- Compression — the member is being pushed, squashed shorter. Rafters, posts and struts. A compression member fails by crushing or, if long and thin, by buckling (bowing sideways). It must be thick.
- Tension — the member is being pulled. Ties and hangers. A tension member can be thin — even a rope, a chain or an iron rod — but its joints must not pull apart.
The test for which is which: imagine the member removed. If the two joints it joined would fly apart, it was in tension. If they would fall together, it was in compression. You can also feel it on a model of sticks and string: the string members go tight; the stick members press into the joints.
Deeper is stronger
A truss bends like a beam. Its top edge (top chord) is squeezed and its bottom edge (bottom chord) is stretched; the members in between (the web: verticals and diagonals) carry the shear — the load working its way sideways to the supports.
The chords share the bending as a pair of opposite forces separated by the truss depth h:
Chord force ≈ bending moment ÷ depth
A truss twice as deep has half the force in its chords. The bending moment comes from the beam formulas (Strength of Materials): for an evenly spread total load W on span L, it is W × L ÷ 8 at mid-span.
Steepness matters
For the simplest truss — two rafters and a tie, with a load P at the peak — the force depends only on the slope angle θ of the rafters:
| Rafter slope | Push in each rafter | Pull in the tie |
|---|---|---|
| 60° (very steep) | 0.58 × P | 0.29 × P |
| 45° | 0.71 × P | 0.50 × P |
| 30° | 1.0 × P | 0.87 × P |
| 20° | 1.5 × P | 1.4 × P |
| 10° (nearly flat) | 2.9 × P | 2.8 × P |
(The formulas: rafter = P ÷ (2 sin θ); tie = P ÷ (2 tan θ).) A nearly flat triangle multiplies the load. Keep diagonals between 40° and 60° from horizontal wherever you can.
What you need
| Item | Notes |
|---|---|
| Timber | Straight-grained, without large knots. Oak or other durable hardwood for bridges; pine, spruce or fir for roofs. Seasoned if possible (Timber Framing and Log Building). |
| Iron | Rods 16–30 mm for tension members in Howe trusses; straps 5–8 mm thick × 40–60 mm wide for joints; bolts and washers (Blacksmithing, Screws, Nuts and Bolts, Nails, Rivets and Wire Fasteners). |
| Tools | Saws, axe, adze, chisels, auger, mallet (Axes, Chisels, Knives and Planes, Files and Saws, Drills and Boring); string line, plumb bob, try square, a long straightedge. |
| For design | Paper, a ruler marked in mm, a protractor or bevel (Measuring Angles: Theodolite and Sextant, Technical Drawing); a level laying-out floor as big as the truss. |
Working out the forces
Do this before you cut timber. You need three things: the shape of the truss drawn to scale, the loads at each joint, and one of the methods below.
Loads. Add up everything the truss carries, in kilonewtons (1 kN ≈ the weight of 100 kg):
- Its own weight: dry timber about 6–8 kN per cubic metre.
- The roof covering carried by each truss: per square metre of roof, thatch about 0.3–0.5 kN, wooden shingles 0.2, clay tiles 0.6–0.8, slate 0.4–0.6, turf when soaked up to 2 (Roofs).
- Snow: in snowy country 1–2 kN/m² or more; ask the old people how deep it has ever lain. Fresh snow weighs about 1 kN/m² per metre of depth, wet packed snow three to four times that.
- People: a crowded footbridge or floor, 4–5 kN/m².
- Then divide the loads among the joints: each joint takes the load from half the distance to the next joint on each side.
Method 1: Draw the force triangle
This needs no trigonometry, only a ruler. At any joint where only three forces meet, those forces must balance, and three balanced forces drawn nose-to-tail make a closed triangle.
- Draw the known force to scale — for instance the load on the peak, straight down, 1 cm for every kN.
- From the top of that line, draw a line parallel to one unknown member. From the bottom, draw a line parallel to the other.
- Where they cross closes the triangle. Measure each side: that is the force in that member, at your scale.
- Follow the arrows round the triangle in one direction. Copy each arrow back onto its member at the joint. An arrow pointing into the joint means compression; pointing away means tension.
Go joint by joint, always choosing one with no more than two unknown members. Drawn carefully, you will be within 5% — closer than you know your loads. Engineers called this graphical statics and designed iron bridges this way for a century.
Method 2: Joint by joint with arithmetic
The same idea in numbers. At every joint, the up forces equal the down forces, and the left forces equal the right forces. For a member sloping at angle θ, its force F pushes or pulls F × sin θ up or down and F × cos θ sideways. For a slope of rise a over run b, sin θ = a ÷ (length) and cos θ = b ÷ (length), where length = √(a² + b²) — no tables needed.
Worked example: a king post truss. Span 8 m, rise 2 m (a slope of 1 in 2, about 27°). A king post hangs from the peak to the middle of the tie; two struts run from its foot up to the middle of each rafter, where the purlins sit. Each purlin and the ridge put 10 kN on their joint (trusses 3 m apart under a tiled roof, roughly). Total 30 kN, so each wall pushes up 15 kN.
- Heel (the foot of the rafter). The rafter slopes 1 up in 2 along; its length per unit is √5 = 2.24, so sin θ = 0.447, cos θ = 0.894. Only the rafter can resist the 15 kN upward reaction: rafter force × 0.447 = 15, so rafter = 33.5 kN compression. Its sideways push, 33.5 × 0.894 = 30 kN, must be held by the tie: tie = 30 kN tension.
- Mid-rafter joint (purlin load 10 kN). Balancing up/down and left/right gives upper rafter = 22.4 kN compression and strut = 11.2 kN compression.
- Peak (ridge load 10 kN). Each upper rafter pushes up 22.4 × 0.447 = 10 kN; two of them give 20 kN up; the ridge load is 10 kN down. The difference, 10 kN, pulls down on the king post: king post = 10 kN tension.
- Check at the foot of the king post. It pulls up 10 kN; the two struts push down 11.2 × 0.447 = 5 kN each. Balanced — the sums are right.
Note what the arithmetic showed: the "king post" is not a post at all. It hangs, in tension, holding up the middle of the tie. Its foot must be strapped or tenoned so it cannot pull out.
Sizing. With the safe working stresses in Strength of Materials (oak about 8 MPa in tension and bending, about 6–7 in compression; pine about 6 and 5):
- Tie: 30,000 N ÷ 8 N/mm² = 3,750 mm² of sound wood left after the joints are cut. Joints cut away a third to a half, so use about 15 × 10 cm.
- Rafter: 33,500 ÷ 6 ≈ 5,600 mm², and it spans 2.24 m between joints while also carrying the battens — use about 15 × 10 cm, deep side vertical.
- Struts: 11 kN is small; 10 × 10 cm keeps them from buckling.
Method 3: Cut through it
For a long bridge truss, a quicker way to the biggest forces: imagine sawing through the truss, cutting three members, and look at one half. It must stay in balance.
Worked example: a Pratt truss footbridge. Span 12 m, four panels of 3 m, depth 2 m (span ÷ 6). Two trusses, one each side, a deck 1.5 m wide. Crowd plus deck and self-weight: about 4 kN per metre along each truss, 48 kN in all, so each end pushes up 24 kN.
- Chords. Mid-span moment = 48 × 12 ÷ 8 = 72 kN·m. Chord force ≈ 72 ÷ 2 = 36 kN: top chord compression, bottom chord tension. No chord carries more.
- Diagonals. The end panel passes on the end reaction less the load on the end joint: 24 − 6 = 18 kN of shear. The diagonal is 3.61 m long for 2 m of height, so its force is 18 × 3.61 ÷ 2 = 32.5 kN. In the next panel the shear is only 6 kN, giving 10.8 kN.
- Sizes. Bottom chord in oak, 36,000 ÷ 8 = 4,500 mm² net: 15 × 10 cm with the joints allowed for, or two wrought-iron bars of 20 mm square. Top chord, 36 kN over 3 m: 15 × 15 cm keeps the length under 20 times the thickness. End diagonal in tension: wrought iron at 80 MPa needs 32,500 ÷ 80 = 400 mm², a 25 mm rod — with its threaded end thickened (upset) on the forge so the thread does not weaken it.
Under even load the middle diagonals do almost nothing, but a loaded cart on one half reverses the shear there. Either make middle diagonals that can take both push and pull, or add a crossing counter-diagonal in the middle panels.
Roof trusses
The roof frames themselves — collar roofs, close couples, king post and queen post trusses, purlins and spacing — are in Roofs. What this chapter adds:
- King post truss: spans 5–9 m. Rise usually span ÷ 4 to span ÷ 3. The king post is a hanger (above).
- Queen post truss: spans 8–12 m. Two hangers (queen posts) and a horizontal straining beam between their heads. Its centre panel is a rectangle, not a triangle, so it relies on stiff joints or a light diagonal to stop it racking under uneven snow or wind.
- Scissors truss: ties cross from each heel to the opposite rafter for a raised ceiling; strap the heels, which push outward harder.
- Many-panel iron or steel trusses (the Fink or "W" truss and others) roof factories and stations of 20–60 m (Steel Frames and Tall Buildings).
Bridge trusses
All three common patterns use parallel top and bottom chords divided into equal panels, with diagonals between. They differ in which way the diagonals lean, and so in which members push and which pull.
- Howe truss (1840): diagonals slope up toward the middle of the span, like pairs of rafters, and are in compression; verticals are in tension. Ideal for timber with iron rods: the diagonals are short timber struts pressed into cast or carved angle blocks, and the verticals are iron rods with nuts. Tighten the nuts and the whole truss is drawn together and cambered; re-tighten them as the timber shrinks. Spans 15–50 m in timber.
- Pratt truss (1844): diagonals slope down toward the middle, making a V, and are in tension; verticals are in compression. The long members pull and the short members push, so it uses metal most efficiently — the standard for iron and steel spans of 15–75 m.
- Warren truss (1848): equilateral or isosceles triangles with no verticals. Diagonals alternate push and pull. Few joints, all alike — good for riveted or bolted iron and steel. Verticals are sometimes added to carry a deck between joints.
- Lattice truss: many crossing planks pinned at every crossing with wooden pegs. Weak per kilogram but needs only boards, pegs and labour — a fine first bridge for a village with a sawmill (Sawmills and Lumber).
Proportions. Depth span ÷ 6 to span ÷ 10 (timber trusses deeper, steel ones shallower). Panels about as wide as the truss is deep, so diagonals lie near 45°. Two trusses side by side, tied together at top and bottom by cross-bracing (an X between them in plan) so the pair cannot fold sideways in wind. A truss deep enough to walk through can have the deck along its bottom chord (through truss); otherwise put the deck on top (deck truss).
Joints: where trusses fail
Trusses almost never break in the middle of a member. They fail at the joints, and almost always at the joints of tension members, because wood is easy to push together and hard to hold apart.
- Heel joint (rafter into tie). Cut a notch (step) into the top of the tie 3–5 cm deep, at right angles to the rafter, so the rafter bears squarely. The rafter's sideways push tries to shear off the block of tie beyond the notch along the grain. Wood is weak in that direction — allow only about 1 MPa (1 N/mm²) in oak, 0.7 in pine. For the king post example: 30,000 N ÷ (1 N/mm² × 100 mm width) = 300 mm. Leave at least 30 cm of tie beyond the notch, and add an iron strap or a bolt through rafter and tie.
- King post foot. A tenon into the tie with a pegged or iron stirrup strap round the underside of the tie and bolted or gib-and-cottered through the post. A wedge in the strap lets you take up shrinkage.
- Gusset plates. In iron and steel trusses, and in modern timber ones, the members meet on a flat plate (gusset) and are riveted or bolted to it (Screws, Nuts and Bolts, Welding). Draw the centre lines of all members meeting at a joint so they cross at one point; if they miss each other, the joint bends.
- Compression joints need only a square, tight bearing: a shallow notch, a cast-iron shoe, or a hardwood block. Gaps here let the truss sag.
- Pegs and nails are fine for holding parts in place, but never trust pegs alone in a tension joint that carries the main load. Use a long timber overlap with several pegs, a bolted iron strap, or iron rods.
Step by step: a king post truss
- Draw it at 1:20; work out the forces and sizes.
- Lay out full size on the floor with a chalked string. The two rafter centre lines must be exactly equal, and the diagonals from each heel to the opposite rafter's mid-point must match.
- Camber: raise the middle of the tie line by span ÷ 300 (about 3 cm on 8 m), so that when the joints bed down it comes level instead of sagging.
- Lay the timbers on blocks over the drawing and mark every joint straight from the lines.
- Cut the joints — steps in the tie, mortises for king post and struts (Timber Framing and Log Building). Cut compression joints tight: better to pare three times than cut loose once.
- Assemble, peg or bolt, fit the strap, mark each piece. Use this truss as the pattern for all the others.
- Raise each truss onto the wall plates, brace it temporarily, and set the next 3–4 m along (Cranes and Lifting, Scaffolding and Ladders). Fix purlins and wind braces before removing props.
For a bridge, assemble each truss flat on the bank on blocks, check its camber, then raise or slide it into place across temporary trestles, and tie the pair together with cross-bracing before any load goes on (Roads and Bridges).
How to tell it worked
- A model first. Build a 1:10 model of sticks and string pinned at the joints and hang weights on it. The strings that go tight must be your tension members. Load it to breaking: the weakest joint shows itself.
- The sight line. Stretch a string from end to end of the bottom chord. After loading, the chord should still be at or above level — no visible sag. Under its full load a good truss sags no more than span ÷ 300 (4 cm on 12 m).
- Proof load. Before a bridge opens, load it with sandbags or stones to 1.5 times the heaviest load it will carry, spread evenly, for a day. Measure the sag at mid-span before, during and after. It must spring back almost entirely; any sag that stays means joints are slipping.
- The joints. Look and listen under load: no opening gaps, no cracking sounds, no crushed fibres at bearings, no bent bolts.
Note Troubleshooting. The truss sags more each year → tension joints creeping or shrinking. Tighten the Howe rods or the wedges in the straps every autumn for the first few years; add iron straps to pegged tension joints. The tie split along its length from the heel → too little timber beyond the notch. Add a bolted strap round tie and rafter; make the next ones longer. A top chord bowed sideways → buckling. Add cross-bracing between the two trusses at every panel point, or make the chord thicker. Walls pushed outward → the tie is not really tying (loose joint, or a collar too high). The rafters' feet must be held to each other, not just to the walls. The forces from your drawing disagree with the sums → a line drawn not quite parallel. Draw bigger, use a sharp pencil, and check that every joint's force triangle closes exactly.
Dangers
Danger A truss can fail all at once. If one joint gives, the frame becomes a mechanism and folds — there is often no slow sagging to warn you. Never let a crowd onto a new bridge before a proof load, keep people off any bridge that has started to creak or lean, and post a load limit at both ends.
Danger Raising trusses. A truss stood upright is tall, top-heavy and easily blown over until it is braced to its neighbours. Raise on still days, with guy ropes held on both sides, and never stand on the side it could fall toward. Trusses swung by cranes must have tag lines (Cranes and Lifting).
- Rot in hidden joints destroys trusses from inside: water collects in notches and under bearing plates. Roof bridges over, shape joints to shed water, and inspect every few years (Rot, Woodworm and Termites).
- Fire: iron rods and steel members lose half their strength by dull red heat, and a burning roof truss drops its load suddenly. Firefighters should never stand under a burning truss roof (Firefighting).
Going further
Iron and steel trusses, riveted or bolted on gussets, lead to factory roofs, railway bridges and the skeletons of tall buildings (Steel Frames and Tall Buildings, Steel in Quantity). The same triangles make crane jibs, radio masts, wind-turbine towers and the lattice of airship and aircraft frames (Cranes and Lifting, Radio, Airships, Gliders and Aeroplanes). Space frames — triangles in three directions — roof whole stadiums. Today engineers compute forces in thousands of members at once, but every program still does what you did here: balance each joint.
How it was first done
Builders used tie-beam roofs, where a horizontal beam stops the rafters spreading, in Greek and Roman times; the great basilicas of Rome, such as Old St Peter's (4th century AD), were roofed with timber trusses spanning more than 20 m. Medieval carpenters developed crown posts, king posts and queen posts by experience. Andrea Palladio published drawings of timber truss bridges in 1570, including one he built over the Cismone river. American carpenters, with vast forests and wide rivers, built thousands of covered truss bridges: Theodore Burr's arch-truss (1804), Ithiel Town's lattice (1820), William Howe's truss with iron rods (patented 1840), and the iron-diagonal truss of Thomas and Caleb Pratt (1844). In Britain James Warren and Willoughby Monzani patented the Warren truss in 1848. Squire Whipple, an American engineer, published the first correct method for calculating the force in each truss member in 1847; the German engineers Karl Culmann (graphical statics, 1866) and August Ritter (the method of sections, 1862) made it the everyday tool of bridge designers.
Source: content/entries/building/trusses.md