◆ Rebuild

Part 2 · Earth and Fire

Mining and Tunnelling

How to follow ore, flint, coal or clay underground — from open trenches to shafts and tunnels — breaking hard rock with fire, keeping the roof up with timber, and getting air in and water and rock out. Mining is dangerous; this chapter is as much about staying alive as about digging.

Difficulty
●●●●●
Time
Days for a trench; weeks for a first shaft; mines grow over years and generations
Steps from zero
3 prerequisites →

You need first

Quarrying and Cutting StoneSimple Machines

This unlocks

Ore Dressing: Jigs, Tables and FlotationTunnels and Rock DrillingCoal and Coke
The full path from nothing — 3 steps before this one
  1. Stone Tools
  2. Simple Machines
  3. Quarrying and Cutting Stone
  4. Mining and Tunnelling

Do them roughly in this order. See it on the tech tree →

Why it matters

The richest ore, the best flint, the cleanest clay and almost all coal lie below the surface, often in a narrow layer or vein that dips into the hill. Once you have picked up everything lying loose and dug out the easy outcrops, the only way to get more is to follow it down. Mining fed the Bronze Age, the Iron Age and the Industrial Revolution: copper and tin for Bronze, iron ore for Iron (the Bloomery), lead and silver for Lead and Gold and Silver, salt (Salt), Coal and Coke for the The Steam Engine — which itself was first built to pump water out of mines.

The same skills also dig Wells and Cisterns, drains, Canals and Locks and railway tunnels (Railways); long tunnels through hills have their own chapter, Tunnels and Rock Drilling. Rock falls, bad air and flooding have killed miners in every age: read the Dangers section before you dig.

How it works

You have four problems underground, and every mine is a solution to all four at once:

  1. Breaking rock. Soft ground (clay, chalk, soft shale, weathered ore) can be dug with picks and shovels. Hard rock must be broken — with fire, wedges and hammers (see Quarrying and Cutting Stone).
  2. Keeping the roof up. Rock and earth above a hole push down and inward. Hard, unjointed rock may stand on its own; soft or cracked ground must be held up with timber or stone, or with pillars of unmined rock left in place.
  3. Air. Fresh air does not go down a dead-end hole by itself. Breathing, lamps and fires use up oxygen, and some rocks give off poisonous or suffocating gases. Air has to be made to flow.
  4. Water and spoil. Any hole below the water table fills with water. And every cubic metre of rock broken must be carried out — 2.5 tonnes of it.

Kinds of working

Windlasslifts rock and water Shaftlined in soft ground Timber setsevery 1–1.5 m Freshair in Stale air outwarm air rises up the shaft Stopeore removed; propsand pillars hold the roof Ore veinfollowed into the hill Sumpwater collects Aditslopes gently outward:drains water, carries out ore
Fig. 1 A small mine in a hillside, in section. An adit drives in level from the valley, draining water and carrying out ore; a shaft from above meets it and makes a through-draught of air. Ore is followed along the vein in galleries held up with timber sets.
  • Open pit or trench — follow the deposit down from the surface, keeping the sides sloping. The safest and simplest; use it as long as the overburden (barren rock and soil on top) is not too deep.
  • Adit — a near-level tunnel driven into a hillside. It drains itself if it slopes slightly outward, and ore can be wheeled or dragged out without lifting. Always choose an adit over a shaft when the land allows it.
  • Shaft — a vertical or steep hole from the surface. Needed when the deposit lies below the valley floor. Everything — rock, water, people — must be lifted.
  • Gallery — a tunnel along the deposit. Stope — the space left where ore has been removed, with pillars of rock left standing to hold the roof.

What you need

Item Details
Picks Iron picks with a long pointed end; before iron, antler picks (red deer antler, the brow tine left as a point) work in chalk and soft rock
Hammers and wedges (gads) 1–4 kg hammers; short iron wedges 15–20 cm long; hardwood wedges; see Quarrying and Cutting Stone
Shovels and baskets Wooden or iron shovels; baskets, leather bags or wooden buckets for spoil
Timber Straight poles 15–25 cm thick, peeled, of oak, larch, pine or chestnut, for props and caps; split poles or planks for lagging
Windlass See below and Simple Machines; rope of hemp or hide (Cordage and Rope)
Ladders Strong pole ladders, pegged and lashed, fixed to the shaft wall every few metres
Lamps Clay or stone lamps burning animal fat or plant oil (Lamps and Candles); a candle for testing air
Water buckets or pump Leather or wooden buckets; later pumps (Pumps)
Firewood For fire-setting — a lot of it, dry and split
Measuring Plumb line, level, compass if you have one (The Compass), to keep tunnels straight (Surveying and Levelling)

Where to find it

You mine what you have already found at the surface: an outcrop of ore (Finding and Identifying Ores), a flint band in chalk, a coal seam showing black in a stream bank (Coal and Coke), or a fine clay under the topsoil (Finding and Preparing Clay). Before you dig:

  • Trace the deposit along the surface with test pits every 10–20 m. Note its direction and the angle it dips into the ground.
  • Judge the ground. Hard, unbroken rock stands well but is slow to break; soft, wet or crumbly ground is easy to dig but must be supported everywhere.
  • Find the water table from springs, wet hollows and wells. Below it, you will have to drain.
  • Choose the entrance. If the deposit runs into a hillside, drive an adit from the lowest practical point, sloping gently up into the hill so water drains out. If it dips under flat ground, you need a shaft.

Step by step: opening a working

1. Start in the open

Dig a trench along the outcrop and follow the deposit down. Keep the sides sloping back at least 45° in soft ground (one step out for every step down), or step them in benches about 1–1.5 m high. Pile spoil at least 2 m back from the edge so its weight does not push the wall in. Many ancient mines never went deeper than this.

2. Sinking a shaft

  1. Mark the collar — the top of the shaft — on firm, dry ground, out of the way of floods, at least 3 m from the outcrop edge so the opening is in solid ground.
  2. Size. A one-person shaft is about 1.2 × 1.5 m (rectangular) or 1.5 m across (round).
  3. Line the collar. Build a ring of stone or a square frame of logs round the top, sitting on firm ground, and raise it 30–50 cm above the surface so rainwater and loose stones cannot run in. Cover the shaft with a lid of poles or a fence whenever no one is working.
  4. Dig down, sending spoil up in buckets. In soft ground, line the shaft as you go: square frames of logs (cribs) laid one on another, notched at the corners like a log cabin, or a dry-stone lining (see Wells and Cisterns — wells are dug exactly like this). Never leave more than about 1 m of unsupported wall below the last frame in soft ground.
  5. Fix ladders as you go, each one resting on a platform or cross-timber every 4–6 m, so a fall is never longer than one ladder.

3. Driving a tunnel

  1. Size. A working tunnel is about 1.8 m high and 1.0–1.2 m wide.
  2. Keep it straight and graded. Hang two plumb lines from the roof a few metres apart along the tunnel's centre line and sight along them to keep direction. Give an adit a gentle outward slope for drainage, about 1 in 200 to 1 in 100 (1 cm per 1–2 m) — enough for water to flow, not enough to make hauling hard. Check with a water level (Surveying and Levelling).
  3. Work the face (the end of the tunnel) with picks in soft ground. In hard rock, use fire-setting (below) and wedges. Cut the top part (the heading) first, then take up the floor.
  4. Support it. Set timber as you go (below).

Breaking hard rock: fire-setting

Before modern explosives, hard rock was broken by fire-setting, used for at least 5,000 years and right into the 1800s. Heat makes the surface of the rock expand while the cold rock behind does not; the surface layer cracks and spalls (flakes) off, and rock that was too hard for any pick becomes a mass of loose, cracked slabs.

1. Burn against the faceSeveral hours of dry split wood.Light it at the end of the shift,then everyone leaves the mine. 2. Wait for the smoke to clearThe hot surface layer expands andcracks away from the cold rock.Hours to a day or more. 3. Bar down and break outLever off loose slabs, wedge thecracks, clear the spoil. Thenrepeat. 5–30 cm smoke
Fig. 2 Fire-setting at the face of a tunnel. A stack of split wood burns against the rock for several hours; the heated surface cracks and spalls. After the fire is out and the smoke has cleared, the broken rock is levered and wedged away.
  1. Build the fire against the face. Stack dry split wood upright and crosswise against the rock, from the floor to as high as you want to break. A sloping rack of poles leaning against the face holds the fuel close to the rock. Leave an air gap at the bottom.
  2. Light it at the end of the shift and leave the mine. Burn it for several hours, adding wood from a distance if needed. The rock should glow dull red in places or be too hot to touch with a wetted finger long after.
  3. Wait for the smoke to clear. This can take many hours — overnight or longer, depending on ventilation. Old mines lit fires on Saturday and returned on Monday. Never go back in while there is smoke — see Dangers.
  4. Quench (optional). Some miners threw water on the hot rock to crack it more. Modern experiments suggest the heat does most of the work; water helps a little but makes a blast of scalding steam. If you quench, do it from a distance with a long-handled bucket and stand clear.
  5. Break out the rock. Lever off loose slabs with a bar, then use hammers and iron wedges in the cracks. Clear the spoil away.
  6. Repeat. Each firing typically advances the face by 5–30 cm, depending on the rock and how much wood you burn. It works best in hard, brittle rock such as quartz, granite and hard ore; it works poorly in soft, crumbly or clayey rock, and limestone can partly burn to quicklime.

Fire-setting eats wood — whole forests were cut for it around old mining districts — so plan your fuel (Firewood and Coppicing).

Black powder was first used in mining in the 1600s (see Black Powder (history) for the history), and later explosives replaced fire-setting. Explosives are extremely dangerous and are not covered in this book.

Supporting the roof

Wherever the roof or walls are soft, cracked or "drummy" (they sound hollow when tapped with a bar), support them. The standard is the timber set:

LOOKING ALONG THE TUNNEL SIDE VIEW Laggingpoles or slabs Cap20–25 cm thick Wedgeslock it tight Leg15–25 cm thick,leaning in 1 in 6 Foot stoneor sill log 1.8 m 1.0–1.2 m 1–1.5 m Faceset timber right up to it
Fig. 3 A timber set, seen from along the tunnel. Two legs lean slightly inward to a cap; lagging boards behind the timbers hold up loose rock between sets; wedges lock everything tight against the ground.
  1. Legs — two posts 15–25 cm thick, standing on firm rock or on a flat stone or sill-log, set leaning slightly inward toward the top (about 1 in 6). The lean helps them resist the walls pushing in.
  2. Cap — a beam across the top, 20–25 cm thick, resting in a shallow notch cut in the top of each leg.
  3. Lagging — split poles, slabs or planks laid behind the legs and above the cap, between one set and the next, to hold up the loose rock.
  4. Wedging — drive wooden wedges between the lagging and the rock so the set bears firmly on the ground all round. A set that is loose does nothing until the rock has already fallen onto it.
  5. Spacing — sets every 1–1.5 m in fair ground, closer (down to 0.5 m) in bad ground. Always set timber right up to the face. The most dangerous place in a mine is the unsupported few metres just dug.

Use sound, peeled timber (bark holds damp and rot). Oak, chestnut and larch last longest underground. Timber "talks": it creaks, cracks and groans as the load comes on. Listen. New cracking, splitting caps, legs bending, or dust and small stones dribbling from the roof are warnings — get out and add more support from a safe place.

Pillars. In a wide working, leave pillars of untouched rock or ore — at least 3 × 3 m, and more as you go deeper — spaced so no open span is more than about 4–5 m. Robbing pillars for their ore has caused many collapses.

Barring down. At the start of each shift, before anyone works under a roof, one person taps the roof and walls with a long bar from a safe position. A clear ring means sound rock; a dull drum means a loose slab. Lever it down deliberately, standing back under supported roof.

Air

Look again at the section drawing above: fresh air enters by one opening and leaves by another that is higher or warmer.

  • Two openings. Air flows naturally through a mine with two openings at different heights, or where the air in one is warmer. An adit plus a shaft, or two shafts, give a through-draught. No working should be more than a few tens of metres from a through-draught.
  • Help the draught. A fire kept burning in a basket at the bottom of one shaft (the upcast) heats the air, making it rise, and draws fresh air down the other. This old trick (furnace ventilation) works well, but never in coal mines — it can ignite gas.
  • Force air to a dead end. For a single tunnel or shaft being driven, push air to the face through a duct: a square wooden trunk of planks sealed with clay, or a tube of oiled leather, from a large Bellows worked at the surface or at the tunnel mouth. A wind sail — a cloth funnel facing the wind on top of the shaft — can feed a duct with no work.
  • Brattice. In a single shaft, a wall of planks or oiled cloth down the middle divides it into two passages, one for air going down and one for air coming up.

Testing the air with a flame

Carry a lit candle or fat lamp, held low and in front of you, into any working that has been left closed:

Flame Means What to do
Burns normally Air fit to breathe — for now Continue, and keep watching it
Shrinks, dims, burns low and blue at the base, goes out Blackdamp (chokedamp): not enough oxygen, too much carbon dioxide — common in old workings, wells and low places Leave at once. You will be unconscious in minutes if the flame dies. Ventilate before re-entry.
Flame grows taller with a pale blue cap or halo Firedamp (methane), in coal mines and some shales Lower the flame gently and leave. It can explode. See Coal and Coke.
Smell of rotten eggs Stinkdamp (hydrogen sulfide) — poisonous; at high levels it kills the sense of smell Leave and ventilate
(no sign) Headache, dizziness, confusion after a fire Afterdamp (carbon monoxide) Leave; it gives no warning to the flame

A flame goes out when oxygen falls to about 15–16% of the air (normal is 21%); people begin to lose judgment about there, and collapse at about 10%. So a dying flame means you have very little time. Never go deeper to relight a lamp.

Water

  • Drain by gravity first. An adit driven in from a lower valley drains everything above its level for free.
  • Bail. Below that level, lift water in buckets with the windlass. Dig a sump (a pit at the lowest point) for it to collect in.
  • Pump. For more water, use a chain of buckets or discs on an endless rope, an Archimedes screw, or piston pumps (see Pumps), worked by people, animals (Draft Animals and Harness) or a The Waterwheel.
  • Know when to stop. Water coming in faster than you can lift it will win. Don't dig toward old flooded workings — see Dangers.

Hauling: the windlass

A windlass is a drum (a log 20–30 cm thick) turned by a crank on a frame over the shaft. A crank of 40–50 cm radius on a 25 cm drum gives a mechanical advantage of about 3–4 (see Simple Machines), so two people at the cranks can raise 50–100 kg of rock or water steadily.

  • Fit a ratchet and pawl (a toothed wheel and a hinged catch) or at least a brake (a lever pressing a pad on the drum), so a slipping hand does not let the load fall.
  • Use a hook with a latch, or tie on with a knot you trust.
  • Shout before lifting and lowering. Anyone in the shaft bottom stands clear, under a shelter of planks to one side.
  • For deeper shafts or heavier loads, a horse whim — a large horizontal drum turned by a horse or ox walking in a circle — does the work of several people (Draft Animals and Harness, Cranes and Lifting, Lifts, Hoists and Mine Winding).

How to tell it worked

  • You are advancing steadily, and every metre of tunnel behind you is supported, dry enough and has moving air (a candle flame leans gently with the draught).
  • Timber stays tight and quiet; new cracking is rare and noticed.
  • Water is under control: the sump level holds or falls.
  • The ore or material you bring out matches what you were following (check it with Finding and Identifying Ores or Rocks and Minerals).

Note Troubleshooting. Air goes stale at the face → the working is too far from a through-draught; drive a connection or fit a duct and bellows. Fire-setting smoke takes days to clear → ventilation too weak; make a second opening before going further, and burn less wood per firing. Fire-setting hardly breaks the rock → the rock is soft or wet, or the fire too small; build the fire tighter against the face and higher, or switch to picks and wedges. Timber sets keep getting crushed → ground is heavier than expected; use thicker timbers, closer spacing, and leave bigger pillars. Water keeps rising → stop sinking; drive a drainage adit from lower ground or build a stronger pump before going deeper.

Dangers

Danger Roof falls kill more miners than anything else. Support the roof right up to the face. Bar down loose rock at the start of every shift and after every fire-setting. Never walk or work under unsupported ground in soft or cracked rock. If timber starts cracking loudly or dust and pebbles fall, get out first and investigate later.

Danger Bad air kills silently and fast. Never enter an old shaft, well, cellar or closed working without first lowering a flame ahead of you: if it dims or goes out, nobody enters. A flame that keeps burning does not prove the air is safe — carbon dioxide can knock you out at levels a flame survives, and a flame does not detect carbon monoxide or hydrogen sulfide (rotten-egg smell). If a person collapses at the bottom of a shaft, do not climb down after them — rescuers die the same way. Ventilate first — blow or pump fresh air down for a long time, well after a lowered flame burns normally — and only then go down, on a rope with others ready to haul you straight out. Never go down into bad air on a held breath: a single gasp can drop you. Smoke from fire-setting contains carbon monoxide; stay out until it has fully cleared.

Danger Flooding. Breaking into old flooded workings, an underground stream or a water-filled cave can release a torrent that fills a tunnel in seconds. When you are near old workings or the water inside a hill, drill a small probe hole 2–3 m ahead of the face with a long iron rod before advancing. If water spurts from the probe, plug it and retreat.

  • Falls. Fence and cover every shaft. Fix ladders firmly, with platforms. Never ride the bucket.
  • Falling objects. A pebble falling 20 m down a shaft can crack a skull. Wear a thick leather or felt cap, keep the shaft collar clear of loose stones, and shelter at the bottom when loads are moving.
  • Dust. Silica dust from drilling and breaking hard rock causes silicosis, a slow, incurable lung disease. Keep rock wet while working, ventilate, and cover your nose and mouth.
  • Poisonous ores. Lead, arsenic and mercury minerals poison through dust and skin. Wash before eating (Finding and Identifying Ores, Mercury).
  • Getting lost or trapped. Never work alone. Keep a tally at the entrance of everyone underground, agree signals, and mark every junction.
  • Exhaustion and cold. Work short shifts, drink water, and get out of wet clothes afterwards. Never send children underground.

What this unlocks

Ore brought to the surface is crushed and sorted (Ore Dressing: Jigs, Tables and Flotation) and then feeds Copper Smelting, Bronze, Iron (the Bloomery), Lead, Tin and Pewter, Zinc and Brass and Gold and Silver. Mining gives you Coal and Coke, which leads to coke, The Blast Furnace and Cast Iron and the The Steam Engine — invented to pump mines. Tunnelling skills dig Wells and Cisterns, drains (Sewers and Wastewater) and Canals and Locks, and the problems of mine drainage pushed the development of Pumpss and Hydraulic Presses and Rams.

How it was first done

The oldest known mine is at Lion Cavern in the Ngwenya hills of Eswatini, where people dug red hematite for pigment perhaps 40,000 years ago or more. Neolithic farmers sank shafts up to 15 m deep into chalk for the best flint — at Grimes Graves in England (about 2600 BC) hundreds of shafts were dug with red deer antler picks, many still lying where they were dropped. Bronze Age miners at the Great Orme in Wales followed copper ore through kilometres of tunnels around 1700 BC with bone tools, stone hammers and fire-setting. The silver mines at Laurion near Athens had shafts over 100 m deep with ventilation shafts, worked largely by enslaved people. Roman mines in Spain used water wheels and Archimedes screws to drain them. In 1556, Georgius Agricola's De re metallica described and illustrated almost everything in this chapter — windlasses, timbering, ventilation bellows, pumps and fire-setting — and remained the standard mining book for two centuries. The first steam engines (Savery 1698, Newcomen 1712) were built to pump water from mines.

Source: content/entries/earth/mining.md