Part 8 · Chemistry
Coal Tar Chemicals
The black, stinking tar left from making coke and coal gas distils into oils that float, oils that sink, white crystals and pitch. From them come carbolic acid, the disinfectant that made surgery safe; creosote, which keeps fence posts and railway sleepers sound for decades; mothballs; solvents; and the raw materials of synthetic dyes, drugs and plastics. Nearly all of them are poisons, and several cause cancer.
- Difficulty
- ●●●●●
- Time
- A day to distil a still-charge of tar; a day to extract crude carbolic; a day per batch of creosoted posts
- Steps from zero
- 10 prerequisites →
The full path from nothing — 10 steps before this one
- Stone Tools
- Fire
- Finding and Preparing Clay
- Simple Machines
- Quarrying and Cutting Stone
- Pottery
- Mining and Tunnelling
- Fermentation
- Distillation
- Coal and Coke
- Coal Tar Chemicals
Do them roughly in this order. See it on the tech tree →
Why it matters
Every coke oven and gasworks (Coal and Coke) produces, along with its coke and gas, about 40–50 kg of thick black tar from each tonne of coal. For decades it was a nuisance dumped in rivers. Then chemists found that this one waste held hundreds of useful substances:
- Carbolic acid (phenol) and its cousins the cresols — strong, cheap disinfectants for latrines, drains, floors, bedpans, instruments and sick-room linen. In the hands of Joseph Lister, carbolic cut deaths after surgery by more than half (Basic Surgery, Sterilising Instruments and Dressings, Sanitation and Germs).
- Creosote — the oil that, soaked deep into a fence post, telegraph pole or railway sleeper, keeps rot and insects out for 20–40 years instead of 5 (Railways, The Telegraph, Power Lines and Distribution, Fences and Hedges, Rot, Woodworm and Termites).
- Naphthalene — white mothballs to protect wool (Wool, Household Pests).
- Pitch — for roads, roofs, waterproofing and carbon electrodes (Tar, Pitch and Glue, Roads and Bridges, The Electric Arc Furnace).
- Benzene and its relatives — solvents and motor fuel, and the starting point of the synthetic dyes, many drugs (Sulfa Drugs, Making Medicines) and plastics such as Bakelite (Early Plastics).
This chapter covers the practical, achievable products — disinfectant and wood preservative — in full, and the dye and benzene chemistry in outline, because that is a job for a trained chemical works.
How it works
Tar is a mixture of hundreds of substances, each with its own boiling point. Heat it in a closed still and they come off roughly in order, lightest first — fractional distillation (Distillation). You collect the distillate in a new receiver each time the temperature, colour or weight of the oil changes. Each fraction is still a mixture, but one rich in a few useful things.
| Fraction | Comes over at | Share of the tar | Looks like | Main contents |
|---|---|---|---|---|
| Water and ammonia liquor | up to about 110 °C | a few % | Brown water | Ammonia (for fertiliser — Ammonia) |
| Light oil | up to 170 °C | 2–5% | Pale yellow, floats on water | Benzene, toluene, xylene |
| Middle or carbolic oil | 170–230 °C | 10–12% | Yellow-brown; white crystals on cooling | Phenol, cresols, naphthalene |
| Heavy or creosote oil | 230–270 °C | about 10% | Brown-green, sinks in water | Creosote |
| Anthracene or green oil | 270–350 °C | 15–20% | Greenish, sets to a mush when cold | Anthracene, heavy creosote |
| Pitch | stays in the still | 50–60% | Black, glossy, hard when cold | Pitch |
Why carbolic disinfects. Phenol and the cresols are mild acids that also dissolve in fats. They soak through the fatty skin of bacteria, wreck the proteins inside and kill them. They do the same to your skin, which is why they are used on things, not people.
Why creosote preserves. Wood rots because fungi and insects eat it. Creosote is poisonous to both, does not wash out in rain, and fills the cells of the sapwood. A post soaked to a depth of 2–3 cm has a poisoned shell that nothing can eat through.
What you need
| Item | Notes |
|---|---|
| Coal tar | From a gasworks retort or a closed coke oven (Coal and Coke). 100–200 litres per still-charge. Tar from open coke heaps is mostly burned and unusable. |
| Iron still | A cast- or wrought-iron pot with a bolted lid, a swan-neck outlet, a drain valve at the bottom for the pitch, and a well holding a thermometer near the top (Metal Casting, Sheet Metal and Rolling, The Thermometer). Never glass or clay for tar: they crack, and a tar fire follows. |
| Condenser | An iron coil or straight pipe through a tank of running water |
| Receivers | 5–6 iron or stoneware pots, numbered, each with a lid |
| Firebox | Brick, built so flames cannot reach the top of the still or the outlet |
| Caustic soda and sulfuric acid | For carbolic (Soda Ash and Baking Soda, Lye and Potash, Sulfuric Acid) |
| Soft potash soap | For cresol soap (Soap) |
| Creosoting tank | An iron tank big enough to stand posts in, over its own firebox, with a lid; and a second, unheated tank if you can (Sheet Metal and Rolling) |
| Protective gear | Long leather or oiled-cloth gloves and apron, goggles, a hat with a brim, barrier cream of fat or lanolin |
Where to find it
Coal tar exists only where coal is baked in closed ovens or retorts — see Coal and Coke for gasworks and coke ovens. Tar from baking wood in a retort (Charcoal, Tar, Pitch and Glue) is a different mixture: it gives wood creosote (a good wood preservative and the original medical creosote), wood spirit and acetic acid (Ether, Acetone and Solvents), but little phenol for disinfectant and none of the benzene family. Use it as a stand-in for preserving wood if you have no coal.
Bituminous (soft, smoky, sticky-burning) coal gives the most tar; anthracite and lignite give little.
Method 1: Distilling the tar
- Settle the tar for a week in a warm place. Draw off the watery ammonia liquor that rises to the top (save it for Ammonia).
- Charge the still no more than two-thirds full. Bolt on the lid with a gasket of clay mixed with flax fibre.
- Heat very slowly at first. Wet tar froths violently as its water boils, and can foam over through the condenser into the receivers — or onto the fire. For the first hour or two, keep a small fire and watch the outlet. Water and a little light oil come over; when the frothing ends and the running water stops, change to receiver 2.
- Light oil (to about 170 °C). Pale yellow oil that floats on water. Change receivers when the thermometer reaches 170 °C — or, without one, when a drop of the distillate let fall into a glass of water no longer floats but hangs or sinks.
- Middle oil (170–230 °C). Darker; set a drop on a cold stone and it soon shows white crystals of naphthalene.
- Heavy oil — creosote (230–270 °C). Sinks clearly in water. Change receivers when the oil coming over turns greenish and thickens on cooling.
- Anthracene oil (270–350 °C). Greenish-yellow, sets to a buttery mush when cold. Keep the condenser water warm now (turn the flow down), or the oil sets solid inside the coil and blocks it.
- Stop when the oil slows to a trickle. What is left is pitch. Stopping earlier leaves soft pitch (good for roads and roofing); going further leaves hard pitch (for electrodes and briquettes) — but past about 350 °C the pitch cokes onto the bottom and the still can burn through.
- Let it cool sealed until the still top is cool enough to touch for a moment (about 150 °C inside). Then open the bottom valve and run the pitch into shallow iron pans or a clay-lined pit well away from any fire. Never open the lid of a hot still: air rushing in can ignite the vapour.
Method 2: Carbolic acid and cresol disinfectant
- Freeze out the naphthalene. Let the middle oil stand in a cold place for a few days. Strain off the oil from the crystals through sacking; press the crystals (keep them, Method 4).
- Wash out the carbolic. In a stoneware pot or iron drum, mix the oil with an equal volume of 10% caustic soda solution (1 kg in 10 litres of water). Stir hard for 15 minutes, then let it settle for some hours. The phenol and cresols dissolve in the lye as their sodium salts and sink in the lower, watery layer. Draw it off. Wash the oil once more with half as much fresh lye and add that to the first. The washed oil can go to creosote.
- Free the carbolic. Pour dilute sulfuric acid (1 part acid into 4 parts water) slowly into the lye layer, stirring, until a drop turns red-cabbage juice pink (Acids, Bases and Testing). It warms up. A brown oil separates and floats: crude carbolic, a mixture of phenol and cresols. (The old works used carbon dioxide from a lime kiln instead of acid — Lime.)
- Wash and use, or distil. Wash it once with a little salty water. This crude carbolic is already a strong disinfectant. Distilled in an iron or glass still, the part coming over at 181–185 °C is fairly pure phenol, which sets on cooling to long colourless needles (they turn pink in light and air); the part at 190–205 °C is cresols.
Using it
| Product | How to make it | Use at |
|---|---|---|
| Carbolic solution | Crystal phenol or crude carbolic stirred into hot water | 5% (1 part in 20): soaking instruments 30 minutes or more, then rinse in boiled water; latrines, bedpans, spittoons, infected linen soaked before washing. 2% for wiping floors, walls and tables in sick rooms. |
| Cresol soap ("lysol") | Warm equal weights of crude cresols (or crude carbolic) and soft potash soap together, stirring, to a clear brown syrup | 1 tablespoon per litre of water (about 1.5%) for floors, drains, latrines, stables and sheep dips (Animal Health); it turns milky in water. |
| Carbolic soap | A few per cent of crude carbolic stirred into soap just before it sets | Scrubbing floors and laundering (Laundry and Bleaching Cloth) |
Warning Not for wounds or skin. Lister poured carbolic into wounds and washed hands in it, because nothing better existed. It also burns and numbs living tissue, is absorbed through the skin, and poisoned some of his patients and surgeons. Use plain soap and boiled water for wounds and hands; alcohol or iodine for skin (Wound Care and Antiseptics, Iodine). Use carbolic for things: instruments, floors, linen, latrines.
Method 3: Creosoting wood
The wood must be ready first. Peel off all the bark, cut and shape the posts (points, notches, bolt holes) before treating them — a cut made afterwards exposes untreated wood. Season them until they are dry: a split end shows cracks, and the wood feels light. Wet wood takes in almost nothing. Pine, larch, spruce and beech take creosote well; oak heartwood takes very little (but oak heartwood lasts anyway).
The hot-and-cold (open-tank) method:
- Stand the posts butt down in the tank and fill it with creosote to 30 cm above the ground line of the posts — or cover them entirely for sleepers and poles.
- Heat to 85–95 °C, below the boil of water, and hold it there for 2–4 hours. A stream of fine bubbles comes out of the wood as the air and water in it expand and escape. The oil must not smoke: smoking means too hot. Use a thermometer if you have one (The Thermometer).
- Let it cool in the oil overnight, or lift the posts with a hoist into a second tank of cold creosote for several hours. As the wood cools, the air left inside contracts and sucks the oil in.
- Drain the posts over the tank and stack them to dry for a week or two in the open before use.
A pine post 10 cm thick and 2 m long should take up about 2–3 litres. Cut a test post in half: the sapwood should be dark brown to a depth of 2–3 cm, and the oil should have run up through the end grain.
Brushing on two or three hot coats of creosote gives only a thin skin. It helps above ground (fences, barn timbers, boats) but does not protect a post in the earth.
Fire, and food. Never heat a tank of creosote over flames that can lick its sides or top. Keep a tight lid beside it to drop on a fire, and sand, not water. Do not use creosoted wood indoors, for beehives, animal mangers, food stores, water tanks or children's play; and never burn it on a cooking or house fire.
Method 4: Naphthalene
Melt the pressed crystals from Method 2 with a little hot water, let them set, and press again. For whiter flakes, distil them: naphthalene boils at about 218 °C and sets at 80 °C, so the condenser must be kept warm or the crystals block it. It is the white, strong-smelling "mothball". Hang a little in a cloth bag in closed chests of wool and furs against moths (Wool, Household Pests).
Keep naphthalene away from babies and young children: a single mothball can poison a toddler, and babies wrapped in mothballed blankets have died. Some people inherit a blood weakness that makes even its vapour dangerous to them.
Benzene, aromatics and dyes (outline)
These are the most valuable coal-tar products — and the most dangerous to make. They are described here so you know what is possible and what it takes.
- Benzol. Light oil washed with a little strong sulfuric acid (which takes out tars and sulfur compounds), then with lye, and then distilled through a fractionating column (Distillation) separates into benzene (boils at 80 °C), toluene (111 °C) and xylenes (about 140 °C). They are excellent solvents for rubber, fats, waxes and resins (Rubber, Ether, Acetone and Solvents), and "benzole" was used as motor fuel (The Internal Combustion Engine). Prefer toluene as a solvent: benzene causes leukaemia.
- The road to dyes and drugs. Benzene treated with Nitric Acid and Sulfuric Acid gives nitrobenzene; nitrobenzene with iron and acid gives aniline. Every step is hazardous, and is described honestly in Sulfa Drugs. In 1856 the 18-year-old William Henry Perkin oxidised impure aniline and got mauveine, a brilliant purple that dyed silk — the first synthetic dye. Within twenty years came magenta, aniline blacks and blues, then alizarin (madder red) made from the anthracene of the green oil (1868–1869), and finally synthetic indigo (1897). Natural madder and indigo farming collapsed (Dyes and Mordants).
- Medicines and more. Coal-tar dyes stain bacteria for the microscope (Biological Stains, Culturing Microbes); one of them, Prontosil, became the first sulfa drug. Phenol is the raw material of salicylic acid and so of aspirin (until then, willow bark — Medicinal Plants) and, with formaldehyde, of Bakelite (Methanol and Formaldehyde, Early Plastics).
All of this needs a chemical works with acid-proof vessels, cooling, ventilation, precise temperature control, trained chemists and a lot of failed batches. The bench skills such a works is built on are in Organic Synthesis and Fine Chemicals. Until then, use natural dyes (Dyes and Mordants) and willow bark.
How to tell it worked
- Fractions: light oil floats on water; creosote sinks; middle oil grows white crystals when cold; pitch is hard and glossy when cold and softens in hot water.
- Crude carbolic has the sharp hospital smell, dissolves partly in water (about 1 part in 12) and wholly in lye, and turns a drop of iron chloride solution violet (iron dissolved in Hydrochloric Acid and left open to the air until it turns yellow-brown).
- Disinfectant strength: lay two pieces of fresh meat in jars — one in water, one in 2% carbolic. In warm weather the first stinks within two or three days; the second should stay sweet for a week or more.
- Creosoted posts: a cut through a test post shows dark oil 2–3 cm into the sapwood; after ten years in the ground the post is still sound when you strike it with a hammer and push a knife into it at the ground line.
Note Troubleshooting. Tar foams over at the start → it was wet; settle and draw off water first, and heat more slowly. Condenser blocks solid → naphthalene or anthracene setting in a cold coil; let the cooling water run warm for the later fractions. Pitch cokes in the still, still glows red at the bottom → over-heated; stop sooner, at a lower temperature. No oil separates when acid is added to the lye layer → too little acid; add more until red-cabbage juice goes pink. Creosote barely enters the wood → wood wet or unpeeled, oil not hot enough or not long enough; dry the wood and hold the heat longer. Posts weep oil for months → too much taken up, or not drained; let them stand longer in the sun before use.
Dangers
Danger Phenol (carbolic acid) passes straight through skin. Strong carbolic splashed over a large area, such as a whole arm, has killed people within hours, and children are at greater risk. It numbs as it burns, so you may feel little while the skin turns white. Pull off contaminated clothing and wash with large amounts of water (or wipe with vegetable oil, then wash) for at least 15 minutes. Swallowed carbolic killed many people in the 1800s; keep it in ridged or marked "poison" bottles, never in drinking bottles, and out of children's reach.
Danger Tar, creosote, pitch fumes and benzene cause cancer. Chimney sweeps covered in soot, tar distillers and creosote workers got skin and other cancers after years of exposure. Benzene causes leukaemia. Wear gloves, apron and goggles; wash skin at once with soap; work outdoors and upwind; do not eat, drink or smoke at the works. Tar and creosote on skin in sunlight also cause painful burns ("tar smarts").
Danger Fire. Light oil and benzene vapour is heavier than air: it flows along the ground to a distant flame and flashes back. Keep all flames away from receivers. A cracked still or a boil-over onto the fire makes a tar fire that water cannot put out — use sand and lids. Build the still in the open, away from other buildings (Firefighting).
- Naphthalene poisons small children and damages blood (see Method 4).
- Hydrogen sulfide and ammonia come off with the first fraction. Stay upwind.
- Pollution. Tar and its oils poison soil and groundwater for generations. Never dump them in streams, pits or wells; burn waste oils as fuel in a furnace, or turn residues into pitch.
What this unlocks
Clean hospitals and latrines (Sanitation and Germs, Basic Surgery); fence posts, poles, piers and sleepers that last a working lifetime (Railways, The Telegraph, Power Lines and Distribution); paved roads and roofs (Roads and Bridges, Roofs); electrodes for arc furnaces (The Electric Arc Furnace); and, with a trained chemical industry, the whole family of synthetic dyes, coal-tar medicines such as aspirin and the sulfa drugs, saccharin, plastics and the styrene of synthetic rubber (Sulfa Drugs, Early Plastics, Rayon and Nylon, Synthetic Rubber Works (Overview)).
How it was first done
People had distilled tar from coal in small amounts since the 1600s. In 1781 Archibald Cochrane, Earl of Dundonald, built kilns in Scotland to make coal tar for coating ships' bottoms. When gas lighting spread from the 1810s (London had gas streetlights from 1812), gasworks produced tar in great quantities. Michael Faraday discovered benzene in 1825 in the oily residue of gas made from whale oil; in 1834 Friedlieb Ferdinand Runge in Germany found phenol and aniline in coal tar. In 1838 John Bethell patented forcing creosote into timber under pressure, and creosoted sleepers carried the world's railways.
In the 1860s the city of Carlisle treated its sewage with carbolic acid to stop the smell. Joseph Lister, a surgeon in Glasgow, read Louis Pasteur's work on germs and in 1865 began using carbolic on wounds, dressings, instruments and hands. Death after amputation in his wards fell from about 45% to 15%. His 1867 papers launched antiseptic surgery. Perkin's mauve (1856) began the synthetic dye industry, which grew above all in Germany. In 1775 the London surgeon Percivall Pott had noticed cancer in chimney sweeps; in 1915 Katsusaburo Yamagiwa in Tokyo produced cancers by painting coal tar on rabbits' ears — the first proof that a chemical can cause cancer.
Source: content/entries/chemistry/coal-tar-chemicals.md