◆ Rebuild

Part 8 · Chemistry

Chlorine and Bleach

Pass electricity through salt water between carbon plates and you get bleach — a liquid that whitens cloth and paper and, a few drops to a litre, makes drinking water safe from cholera and typhoid. Chlorine gas itself, made the same way or from acid, becomes bleaching powder with lime. It is also a deadly poison and must be handled with great care.

Difficulty
●●●●●
Time
An afternoon to build an electrolytic cell; 2–4 hours per litre of bleach; 30 minutes to treat drinking water
Steps from zero
16 prerequisites →

You need first

SaltElectrolysis

This unlocks

Water Treatment for a TownBromine and Bromides
The full path from nothing — 16 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Pottery
  9. Charcoal
  10. Hides and Leather
  11. Salt
  12. Fermentation
  13. Bellows
  14. Copper Smelting
  15. The Battery
  16. Electrolysis
  17. Chlorine and Bleach

Do them roughly in this order. See it on the tech tree →

Why it matters

In 1900 typhoid and cholera, spread by dirty water, killed tens of thousands of people every year in the cities of Europe and America. Once towns began to filter their water and add a few milligrams of chlorine to each litre, typhoid deaths fell steeply, and within a generation the disease had become rare wherever it was done. Few inventions in history have saved more lives for less effort. Chlorine bleach does three jobs:

Chlorine is also a raw material for Hydrochloric Acid, solvents (Ether, Acetone and Solvents), many medicines and plastics, and the purification of metals.

There is a dark side. Chlorine gas is a poison heavy enough to flow along the ground and fill a cellar or a trench, and it was the first poison gas used in war. This chapter gives the safest route first — making liquid bleach directly, with almost no free gas — and treats chlorine gas as a job for a proper, outdoor works.

How it works

Common Salt is sodium chloride. When an electric current flows through salt water (brine) between two plates (electrodes) — see Electrolysis:

  • At the positive plate (the anode), chlorine is released.
  • At the negative plate (the cathode), hydrogen gas bubbles off, and the water around it becomes caustic soda (sodium hydroxide, a strong alkali like Lye and Potash).

What happens next depends on whether the two products are kept apart:

  1. Kept apart (by a porous pot or a cloth wall between the plates), you get chlorine gas from the anode side and caustic soda from the cathode side. This is the industrial chlor-alkali process.
  2. Allowed to mix in a cool, single pot, the chlorine dissolves and immediately reacts with the caustic soda to make sodium hypochlorite — liquid bleach, the same chemical as household bleach. Almost no chlorine gas escapes. This is the method for you.

How bleach works. Hypochlorite is a strong oxidiser: it tears electrons out of other chemicals. It destroys the coloured parts of stains and dyes (bleaching), and it destroys the outer skins and inner machinery of germs (disinfecting). Its power is measured as available chlorine. Household bleach of the modern world is 3–6% available chlorine; what you will make is about 0.3–0.8%.

Hypochlorite is used up by everything it attacks — dirt, plant matter, and the germs themselves. That is why cloudy water needs more of it, and why you check that a little is left over (a faint smell) after half an hour: that leftover proves there was enough.

What you need

For the bleach cell

Item Amount Notes
Container 1–2 litres Glass jar or glazed stoneware (Glazes). Not metal.
Salt 30 g per litre of water About two level tablespoons. Clean, no iodine needed. Or use seawater boiled down to about the same saltiness.
Clean water 1 litre per batch Rain water or boiled water
Anode (positive plate) 1–2 Must be carbon: a rod or plate of graphite, gas-retort carbon or hard dense coke (see below). Any metal anode dissolves.
Cathode (negative plate) 1 Carbon, or a strip of iron or steel
Electricity 4–6 volts, 2–5 amperes, for 2–4 hours Three lead-acid cells in series, or a small dynamo. Ordinary single-use batteries give too little current for long.
Wires and clips Copper (Copper Wire), joints kept out of the liquid
Cooling A larger tub of cold water To stand the jar in
Ammeter Optional Measuring Electricity

For using bleach

A dropper (a hollow reed or straw), a teaspoon (5 ml), clean buckets with lids, and dark bottles or glazed pots with stoppers.

Where to find it

  • Salt: see Salt — from seawater, brine springs or rock salt.
  • Graphite: a soft, black, greasy mineral that marks paper and fingers grey-black, found in metamorphic rocks (marble, schist, gneiss) as flakes and veins. A natural graphite lump can be sawn into plates. See Pencils and Chalk.
  • Carbon from coke: the hard, dense, silvery-grey carbon that builds up on the inside walls of coal-gas retorts or coke ovens (Coal and Coke), or the densest pieces of hard coke, ring when tapped and conduct well. Ordinary soft charcoal falls apart in the cell.
  • Manganese ore (for chlorine gas, Method 3): black, sooty, heavy lumps of pyrolusite that stain the fingers (Finding and Identifying Ores).

Method 1: Liquid bleach by electrolysis

+− Battery or dynamo4–6 volts, 2–5 amperes Split wooden lidgap lets gas escape Anode (+)must be carbon:graphite or retort carbon Chlorinedissolves and becomeshypochlorite (bleach) Cold water tubkeep the cellbelow 30 °C Joints abovethe liquid Cathode (−)iron or carbon Hydrogen bubblesburns explosively —no flames near the cell Brine30 g salt per litre 2–3 cm gapplates must not touch
Fig. 1 A single-pot bleach cell. Current flows through salt water between a carbon anode and a cathode. Chlorine made at the anode mixes with caustic soda made at the cathode and turns into hypochlorite bleach. Hydrogen bubbles away from the cathode. The jar stands in cold water to keep it cool.
  1. Make the brine. Dissolve 30 g of salt in 1 litre of clean water. Let any dirt settle and pour the clear brine into your jar.
  2. Set the electrodes. Fix the carbon anode and the cathode 2–3 cm apart, upright, held by a split wooden lid that leaves a gap for gas to escape (never seal the jar — hydrogen builds up). The plates must not touch, and their tops and all wire joints must stay out of the brine. Let the plates reach nearly to the bottom, so the chlorine from the anode has to rise through plenty of liquid and dissolves before it can escape.
  3. Cool it. Stand the jar in a tub of cold water. The cell must stay below about 30 °C — no warmer than the hand. Hot cells waste current and turn the bleach into useless and dangerous chlorate.
  4. Connect the carbon to the positive terminal and the other plate to the negative. If you are not sure which is which, switch on for a moment: fine hydrogen bubbles stream off the negative plate, and the positive one bubbles less. If it is reversed and the anode is iron, it will rust and the liquid will go brown — swap the wires.
  5. Run it outdoors or by an open window, with no flame or spark nearby: the hydrogen given off can burn or pop. Hold the current at about 2–5 amperes. The liquid smells faintly of swimming pools.
  6. Time it. Every ampere flowing for one hour can make, at best, about 1.3 g of chlorine; a simple cell turns roughly a third to a half of that into bleach. Run about 10 ampere-hours per litre — for example 4 amperes for 2½ hours. That gives roughly 4–6 g of available chlorine per litre, about 0.5%.
  7. Stop, settle and bottle. Let any black carbon dust settle, then pour the clear, pale or colourless liquid into a clean dark bottle or glazed pot, stopper it, and label it clearly: BLEACH — POISON.

Without an ammeter, run it two to four hours per litre with the cell steadily bubbling, then strength-test it as below. The test is what matters.

Tip Seawater shortcut. Clean seawater is about 3.5% salt — almost exactly right. Filter it through sand and cloth and electrolyse it as it is.

Storing bleach

Hypochlorite slowly breaks down, faster in light and heat. Keep it stoppered, cool and dark, and make fresh every 2–4 weeks. Before each use, check that it still smells clearly of chlorine.

Method 2: Treating drinking water

First make the water clear. Chlorine cannot reach germs hidden inside mud particles, and mud uses it up. Let cloudy water settle overnight in a covered pot, pour off the clear top, and strain it through clean cloth or a sand filter (Finding and Purifying Water). Only then disinfect.

The jar test (finding your dose)

Homemade bleach varies, so measure its strength against your water:

Four jars, 1 litre of the same clear water in eachadd drops of bleach, stir, cover, wait 30 minutes, then smell 4drops No smelltoo little 8drops No smelltoo little 12drops Faint smellUSE THIS DOSE 16drops Strong smellmore than needed
Fig. 2 The jar test. Four one-litre jars of the same water get 4, 8, 12 and 16 drops of your bleach. After 30 minutes, the right dose is the lowest one that leaves a faint smell of chlorine.
  1. Fill four clean jars with exactly 1 litre each of the clear water you plan to treat.
  2. Add 4, 8, 12 and 16 drops of your bleach (a drop from a reed or straw is about 0.05 ml). Stir each with a clean stick and cover.
  3. Wait 30 minutes.
  4. Smell each jar. Choose the lowest dose that has a faint but definite smell of chlorine — like a swimming pool from a distance. No smell means too little: the bleach was used up. A strong, harsh smell means too much (safe, but unpleasant).
  5. Your dose for that water is that number of drops per litre: a 20-litre bucket needs 20 times as much. Using a teaspoon (5 ml, about 100 drops) is easier for big amounts.

Repeat the jar test with each new batch of bleach and each new water source, and after heavy rain.

Everyday use

  1. Add the dose to a clean container of clear water, stir, and cover.
  2. Wait at least 30 minutes (an hour if the water is cold, below 10 °C).
  3. Smell it. A faint chlorine smell means it is safe. If there is none, add the same dose again and wait another 15 minutes.
  4. Store treated water covered, and draw it out with a clean dipper or a tap so hands never enter it. Use it within a day or two.

Rough guide for clear water, when you know the strength:

Bleach strength Per litre Per 20-litre bucket
0.5% (homemade, Method 1) 8–16 drops (0.4–0.8 ml) 8–16 ml — about 2–3 teaspoons
1% 4–8 drops 4–8 ml — 1–1½ teaspoons
5% (old household bleach) 1–2 drops ¾–1½ ml — about 15–30 drops
Bleaching powder stock (below) 8–16 drops of the clear liquid as for 0.5%

These give about 2–4 milligrams of chlorine per litre, which leaves the faint leftover smell in clear water.

Warning What chlorine does not do. It kills bacteria and viruses well, but some parasites (for example Cryptosporidium) and worm eggs survive normal doses, and it does nothing about poisons, metals or salt. If people still fall sick, boil the water instead: a rolling boil for one minute kills everything living. See Finding and Purifying Water.

Disinfecting and bleaching

Disinfecting (during outbreaks of cholera, dysentery and similar):

  • 0.05% solution — 1 part 0.5% bleach to 9 parts water: for washing hands when soap is scarce, rinsing dishes and soaking clothes of the sick.
  • 0.2% solution — 2 parts 0.5% bleach to 3 parts water: for floors, beds, latrine seats, buckets and tools. Leave it wet for 10 minutes, then rinse.
  • Full-strength bleach poured onto vomit and diarrhoea before cleaning it up.

Clean off dirt before disinfecting; bleach does little under a layer of filth. Never use it on wounds or skin repeatedly at full strength; for wounds, see Wound Care and Antiseptics.

Bleaching linen, cotton and paper:

  1. Wash the cloth well first, ideally boiled in weak lye (Lye and Potash).
  2. Soak it in bleach diluted to about 0.1–0.2% (1 part 0.5% bleach to 3 parts water) for 2–6 hours, turning now and then.
  3. Rinse, then soak 30 minutes in water with a cupful of vinegar per bucket (this sours out the last of the bleach — do it only after a thorough rinse, never in the bleach bath itself).
  4. Rinse again thoroughly. Repeat for whiter cloth.

Never bleach wool or silk with chlorine — it dissolves animal fibres. Whiten them with sunlight, or with the fumes of burning Sulfur in a closed box, as was done for centuries.

Note Without chlorine. Before 1800, linen was whitened by crofting: boiling in lye, then spreading it on grass in the sun and keeping it wet for weeks, then souring it in buttermilk, over and over for up to six months. It works; it just takes a summer. See Flax, Hemp and Linen.

Method 3: Bleaching powder (for a works)

Liquid bleach is weak and does not keep long. Bleaching powder (chloride of lime) is dry, about 30–35% available chlorine, and keeps for months in a sealed pot — so a central works can make it and send it to villages. It is made by passing chlorine gas over slaked Lime.

Making chlorine gas is a works job, never a household one. It is made either in a divided electrolytic cell (a porous, unglazed clay pot around the anode keeps the chlorine from mixing with the caustic soda), or by warming Hydrochloric Acid with crushed manganese ore, as described in that chapter. Either way it must be done outdoors, in a closed system of glazed or glass vessels joined with acid-proof clay lutes, upwind of everyone, with the last outlet led through a pot of lye or lime water to catch any gas that is not absorbed.

In outline:

  1. Spread dry, freshly slaked lime powder, very slightly damp to the touch, 5–10 cm deep on shelves or the floor of a small, tightly sealed chamber of stone, glazed brick or tarred wood.
  2. Lead the chlorine in slowly at the top over 12–24 hours. The lime warms as it absorbs it; keep the chamber cool (below about 25 °C), or the product loses strength.
  3. When no more is absorbed (the gas above stays yellow-green), drive the remaining chlorine out through the lime-water trap with fresh air before anyone opens the chamber.
  4. Rake the powder out, wearing a wet cloth over nose and mouth, and pack it in sealed pots.

To use it, stir 15 g (one heaped tablespoon) into 1 litre of water, let it settle, and use the clear liquid — about 0.5% — as you would homemade bleach. Stirring in a little Soda Ash and Baking Soda makes the chalky sludge settle out, leaving clear sodium hypochlorite.

How to tell it worked

  • Smell: good bleach smells clearly of chlorine.
  • Colour test: a drop on a piece of dyed cloth, a flower petal or a smear of ink fades it within minutes.
  • Strength comparison: dissolve a pinch of indigo in water (or use any dark plant juice) and count how many drops of each batch of bleach it takes to fade a spoonful of it. The fewer drops, the stronger the bleach. This is how chlorine bleach was first graded in the early 1800s.
  • Water: faint chlorine smell after 30 minutes, and fewer cases of diarrhoea in the weeks that follow. A surer check of the leftover chlorine than your nose is the starch–iodide test in Water Treatment for a Town.

Note Troubleshooting. No bubbles → no current: a loose joint, a flat battery, or wires corroded. Clean the contacts; keep joints out of the brine. Liquid goes brown or orange → a metal anode is dissolving, or the wires are reversed. Use carbon as the positive plate. Carbon plate crumbles, liquid goes black → soft, porous carbon. Use graphite or dense retort carbon; let the dust settle and pour off. Weak bleach after hours → too little current, too hot, too weak or too strong brine, plates too far apart. Keep it cool, 30 g/litre salt, plates 2–3 cm apart. Water has no chlorine smell even with lots of bleach → the water is dirty and is using it up, or the bleach has gone off. Settle and filter the water; make fresh bleach.

Dangers

Danger Chlorine gas kills. It is yellow-green, smells sharp and choking, and is 2½ times heavier than air, so it pools in cellars, pits, ditches and low rooms. A few breaths of strong gas burn the lungs; fluid can fill them up to 24–48 hours later in someone who seemed to recover. If gas escapes: go uphill and upwind at once, never down into a hollow. Do not go back in to rescue someone without a supply of fresh air. Keep a poisoned person still, warm and sitting up, and watch them for two days. Rinse the eyes with water for 20 minutes.

Danger Never mix bleach with acids — or with ammonia or urine. Bleach plus any acid (vinegar, Hydrochloric Acid, Sulfuric Acid, even some cleaning mixtures) releases chlorine gas. Bleach plus Ammonia, stale urine or a dirty latrine releases chloramine gas, which is just as poisonous. People die every year cleaning small rooms this way. Use bleach alone, in fresh air, and rinse surfaces before using anything else.

  • Hydrogen from the cell burns explosively in air. No flames, sparks or lamps near a running cell; run it in the open.
  • Bleach and caustic burn eyes and skin. Rinse splashes with plenty of water for 15–20 minutes. Bleach drunk by a child is an emergency: give water or milk to drink, do not make them vomit, and see Emergencies.
  • Keep the cell cool. A hot cell makes chlorate, which is useless for water treatment and is a fire hazard when it dries on cloth, wood or sawdust.
  • Overdosed water tastes bad but is not dangerous at these levels; leave it uncovered for a few hours and the smell fades.
  • Label and lock away all bleach and powder. Never store it in drinking bottles.

What this unlocks

Safe water for a whole settlement (Finding and Purifying Water, Water Treatment for a Town, Sanitation and Germs, Sewers and Wastewater), clean hospitals and instruments (Sterilising Instruments and Dressings, Basic Surgery), white Paper and cloth. The caustic soda from a divided cell makes hard Soap and helps make Aluminium. Chlorine is the starting point for Hydrochloric Acid by burning it with hydrogen, for dry-cleaning Ether, Acetone and Solvents, disinfectants and the chemistry of many medicines and plastics such as PVC (Petrochemicals and Modern Plastics).

How it was first done

The Swedish apothecary Carl Wilhelm Scheele discovered chlorine in 1774 by warming hydrochloric acid with manganese ore; he noticed it bleached plant colours. Humphry Davy showed in 1810 that it was an element and named it from the Greek chloros, pale green. In 1785 the French chemist Claude Louis Berthollet used it to bleach cloth, and in 1789 a works at Javel near Paris began selling chlorine dissolved in potash lye as eau de Javel. In 1799 Charles Tennant of Glasgow patented bleaching powder; his St Rollox works became the largest chemical works in the world. Antoine Labarraque promoted hypochlorite as a disinfectant in the 1820s, and Ignaz Semmelweis cut deaths among new mothers in a Vienna hospital in 1847 by making doctors wash their hands in chlorinated lime. Chlorine was first used to disinfect a town's water during a typhoid outbreak at Maidstone, England, in 1897, and continuous chlorination began at Jersey City, USA, in 1908. Industrial electrolysis of brine began in the 1890s. On 22 April 1915, near Ypres in Belgium, chlorine released from cylinders became the first large-scale poison gas attack — a reminder of why this chapter's warnings are not exaggerated.

Source: content/entries/chemistry/chlorine-bleach.md