Part 6 · Building
Chimneys, Stoves and Heating
How to build a hearth and chimney that draw well and do not set the house alight, then how to heat far better with less wood — the shallow Rumford fireplace, the masonry heater, the rocket stove, the iron stove and heated floors — and how to keep the air in the house safe from smoke and carbon monoxide.
- Difficulty
- ●●●●●
- Time
- A week or two for a fireplace and chimney; a month for a masonry heater; a day for a rocket cooking stove
- Steps from zero
- 18 prerequisites →
This unlocks
Hot Water and Central HeatingVentilation and Air ConditioningCooking Ranges, Iceboxes and Vacuum FlasksThe full path from nothing — 18 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- The Kiln
- Charcoal
- Hides and Leather
- Bricks
- The Wheel and Axle
- Firebrick and Refractories
- Bellows
- Gears
- Iron (the Bloomery)
- The Waterwheel
- The Blast Furnace and Cast Iron
- Chimneys, Stoves and Heating
Do them roughly in this order. See it on the tech tree →
Why it matters
An open fire in the middle of a hut warms the people right beside it, fills the room with smoke, and sends most of its heat out through the roof. Smoke from indoor fires damages the lungs and eyes, and even today it kills millions of people a year. A chimney carries the smoke away. A well-designed stove does better still: it burns the same wood two to five times more effectively and puts the heat into the room instead of the sky.
Heating is also where most of a cold-climate household's labour goes — cutting, splitting and hauling firewood (Firewood and Coppicing). A good stove can halve that work. The same skills give you ovens for bread (Grain, Flour and Bread), kitchen ranges (Cooking Ranges, Iceboxes and Vacuum Flasks), and kilns and furnaces (The Kiln).
How it works
Hot air rises. Air expands as it warms, so a column of hot gas is lighter than the same column of cold air outside. In a chimney, the cold outside air pushes the lighter hot gas upward, and fresh air flows into the fire to take its place. This is the draught (draft) — the stack effect. The draught is stronger when the chimney is taller and the gas inside is hotter.
So a chimney draws badly when it is short, cold, too wide, leaky, or has sharp bends. A cold chimney full of cold air may even push smoke back into the room until it warms up.
Complete burning. Wood burns in two stages. First, heat drives out gases (wood gas) and leaves charcoal. Then the gases burn as flame — but only if they are hot enough (above about 600 °C) and get enough air. A smouldering, starved fire lets the gases escape unburned as thick smoke, which condenses in the chimney as black tar (creosote) and wastes about half the wood. Hot, fast, small fires with plenty of air burn clean.
Mass stores heat. A tonne of brick or stone heated by a fire gives out its warmth slowly for many hours. This is why a masonry heater, fired once or twice a day, keeps a house warm all day and night.
What you need
| Item | Notes |
|---|---|
| Fired bricks or flat stone | Bricks, Stone Masonry. About 1,000–1,500 bricks for a fireplace and a two-storey chimney |
| Firebrick and fireclay | For anything the fire touches directly: Firebrick and Refractories |
| Mortar | Clay and sand mortar for the hot inside (lime crumbles in fierce heat); lime mortar for the outside of the chimney (Lime) |
| Clay flue liners | Optional but good: square or round fired clay pipes (Tiles and Clay Pipes) |
| Iron | A damper plate, lintel bars and stove plates (The Blast Furnace and Cast Iron, Blacksmithing, Sheet Metal and Rolling) |
| Stone or slate slabs | For the hearth |
The hearth and chimney
First: the smoke hood
Before you can build a full chimney, a smoke hood — a funnel of wattle and daub (Cob, Adobe and Rammed Earth) or plastered timber, over a hearth set against a stone or earth wall, leading into a short flue through the roof — clears most of the smoke. Keep all timber in the hood well plastered and at least 1 m above the fire. It is a big improvement on an open hearth but still a fire risk; build a masonry chimney as soon as you can.
Building a fireplace and chimney
- Foundation. A chimney is very heavy — several tonnes. Give it its own footing (Foundations and Floors).
- The hearth. A slab of stone, slate or fired brick on the footing, extending at least 50 cm in front of the fireplace opening and 20–30 cm beyond each side. Nothing that burns may be under it or within reach of a rolling log.
- The firebox (the Rumford pattern, the best simple design):
- Shallow: the depth from front to back about a third of the opening's width, so the fire sits close to the room.
- Splayed sides angled outward at about 45° to the back, and a back that leans forward in its upper part, so the hot surfaces reflect heat into the room.
- Opening: about as high as it is wide — for example 75 cm wide and 75 cm high for an ordinary room.
- Firebrick or hard stone lining where the fire touches, set in clay mortar.
- The throat. Above the fireplace opening, bring the front wall (breast) back in a smooth curve to meet the leaning back wall, leaving a narrow slot — the throat — only about 10 cm from front to back and as wide as the firebox, about 30 cm above the top of the opening. The narrow throat speeds the gas and stops cold air tumbling down. Above it, the chimney widens into a smoke chamber with a flat smoke shelf behind the throat, which turns back cold down-draughts.
- A damper — an iron plate that can close the throat when no fire is burning — saves heat. Never close it while anything is still glowing (see Dangers).
- The flue — the passage up the chimney. Its cross-section should be about one-tenth of the area of the fireplace opening: a 75 × 75 cm opening (5,600 cm²) needs a flue of about 560 cm², roughly 24 × 24 cm. Too big and the gas cools and dawdles; too small and it smokes. Keep it straight; if it must bend, no more than 30° from vertical, with smooth sides.
- Walls of the chimney. At least one brick (10–11 cm) thick around the flue, with every joint full. Line the flue with clay pipes, or plaster it smooth inside (parging) with clay-lime mortar as you build. Leave a gap of at least 5 cm between the chimney's outer face and any timber, and never build a beam end into a chimney.
- Height. A chimney needs a total height of at least 4.5–5 m from hearth to top to draw well. Its top must be at least 1 m above where it comes out of the roof, and at least 60 cm higher than any part of the roof, wall or tree within 3 m. Above thatch, go higher still (Roofs).
- The top. A flat stone or a pair of tiles on small piers above the opening keeps rain out without blocking the smoke. A cap of wire mesh stops sparks and birds.
- Flashing where the chimney passes through the roof: see Roofs.
- Cure it. Let the mortar dry for two weeks, then light only small fires for the first few days.
Masonry heaters
A masonry heater (Russian stove, Finnish contraflow, the tiled stove of Central Europe) is the most efficient wood heater you can build without modern materials. You burn a big, hot, fast fire for 1–3 hours once or twice a day; the hot gases snake through long channels in a heavy mass of brick, which soaks up the heat and gives it out gently for the next 12–24 hours.
- Mass: 1–3 tonnes of brick or stone (soapstone, which holds heat superbly, was prized in Finland), on its own footing.
- Firebox: lined with firebrick, about 40–50 cm wide and deep and 60–80 cm high for a house heater, with a tight-fitting iron door and an air inlet below or in the door.
- Channels: 4–8 m of passages of roughly the same cross-section as the flue, leading up from the firebox to the top and then down the sides before reaching the chimney at the bottom. Leave cleanout openings, closed with bricks or iron plates, at every turn.
- Build with thin joints of clay-sand mortar. Leave a 1–2 cm gap between the firebox and the outer shell where possible, so the inner core can expand without cracking the outside.
- Use: load 10–20 kg of dry split wood, light it from the top, and let it roar with the air wide open. When nothing but ash and grey charcoal is left and no flame or glow remains, close the door and the damper.
The outside never gets dangerously hot — warm to the hand, 40–70 °C — and people in Russia traditionally slept on top of the stove.
The rocket stove
The rocket stove is a modern design that burns small sticks very cleanly, ideal for Cooking and Recipes where firewood is scarce.
- Make an L-shaped passage of one constant size — about 12 × 12 cm inside — with a short horizontal burn tunnel (25–30 cm) and a vertical heat riser 40–60 cm tall. The fuel goes in the open end of the tunnel, or in a separate vertical feed tube; a shelf of iron or stone halfway up the opening lets air flow under the sticks.
- Insulate the riser. This is the secret: the riser must get very hot, very fast. Surround it with 5–10 cm of light insulation — wood ash, crushed pumice, or a mix of clay with lots of sawdust or chopped straw fired so the organic matter burns out and leaves it full of air pockets. Use firebrick or fired clay for the inner surfaces (Firebrick and Refractories).
- Set the pot on three supports about 3 cm above the top of the riser, and surround it with a skirt of clay or sheet metal leaving a gap of only about 1–1.5 cm, so the hot gas is forced along the pot's sides.
- Feed only the ends of small dry sticks — finger-thick — pushing them in as they burn. The fire roars, burns almost smokelessly, and boils water with a fraction of the wood of an open fire.
A rocket mass heater uses the same burner inside a closed steel drum (the hot drum heats the room), then leads the exhaust through a long duct buried in a bench of cob or stone, which stores the heat. It needs sheet steel (Sheet Metal and Rolling) and careful building to draw well.
Iron stoves
A closed iron box with a door, an air inlet and a pipe is easy to install, heats the room fast and can cook on its top.
- Cast iron: cast flat plates 6–10 mm thick in sand moulds (Metal Casting, The Blast Furnace and Cast Iron) with flanges around the edges, and bolt them together, sealing the joints with a paste of fireclay. Six-plate box stoves of this kind warmed Northern European houses from the 1600s.
- Sheet iron: quicker to make but burns through in a few years unless lined with firebrick.
- Stove pipe: sheet iron, 12–15 cm across. Run it upward all the way, rising at least 2 cm in every metre of horizontal run, with as few bends as possible, into a proper masonry chimney. Fit each joint with the narrower end pointing down toward the stove, so tar runs back into the stove rather than out of the joints. Put a damper in the pipe.
- Clearances: an iron stove must stand on a non-burning hearth that extends 45 cm in front of the door, at least 90 cm from any wooden wall or furniture, and the pipe at least 45 cm from wood — unless shielded by a brick or tile wall with an air gap.
- A mica window in the door lets you see the fire (Window Glass).
Heated floors and beds
- The hypocaust (Roman). The floor is raised on short pillars of stacked tiles about 60 cm high and 40–60 cm apart, carrying large tiles and a layer of lime concrete. A furnace outside one wall sends its hot gas under the whole floor and up flues in the walls to the roof. Warm, but it uses a lot of fuel; best for bath-houses.
- The ondol (Korea) and kang (northern China) are simpler and thriftier: the kitchen fire's smoke passes through stone-slab flues under the floor of the living room (ondol) or through a brick sleeping platform (kang) before reaching the chimney. The cooking fire heats the house at the same time.
Air and ventilation
Every fire uses air — an open fireplace can pull the whole air of a room up the chimney every few minutes. If the house is tight, the fire starves, smokes and spills carbon monoxide into the room.
- Give every fire its own fresh air supply: a vent or pipe from outside to near the hearth.
- Keep a small opening high in each sleeping room.
- Never burn charcoal, coal or wood in a brazier, pot or oven without a chimney inside a closed room.
For ventilating a whole house, see Ventilation and Air Conditioning.
How to tell it worked
- The smoke test. Hold a smouldering stick at the fireplace opening: the smoke should be drawn firmly in and up. Light a twist of dry grass in the firebox: the flame should lean toward the back and up.
- A good fire burns with yellow flames and little visible smoke from the chimney top — just a shimmer of heat once it is going well.
- No smoke smell in the room, no soot stains on the breast of the fireplace.
- A masonry heater is warm all over the next morning.
Note Troubleshooting. Smoke spills into the room → flue too small, too big or too short; throat too wide; chimney top below the ridge; or the house too airtight. Raise the chimney, narrow the throat, open a window slightly to test. Smokes only when first lit → cold chimney. Burn a handful of dry grass or shavings high in the firebox to warm the flue first. Smokes in certain winds → a hill, tree or higher roof nearby. Raise the chimney or add a cap. Thick black tar in the flue → wet wood or a starved, smouldering fire. Burn dry wood hot. Cracks in the firebox → lime mortar used in the hot zone, or no room for expansion. Rebuild with clay-sand mortar and firebrick.
Dangers
Danger Carbon monoxide kills silently. It has no smell or colour. It is made whenever fuel burns without enough air — a smouldering fire, a closed damper over glowing embers, a blocked or cracked flue, a charcoal brazier in a closed room. Early signs are headache, dizziness, nausea, tiredness and confusion, often in several people at once, that get better outdoors. Sleep can turn into death. If you suspect it: open doors and windows, get everyone into fresh air at once, and put out the fire. An unconscious person who is breathing should be laid on their side in fresh air (Emergencies, Emergency Cards). Never close a damper until the fire is completely dead — no glow at all.
Danger Chimney fires. Creosote and soot in the flue can catch fire, roaring like a train, throwing sparks and flames from the top and heating the chimney red-hot — which can ignite roof timbers and thatch. Prevent them: burn dry wood hot, and sweep the chimney at least once a year (more with heavy use), with a stiff brush on jointed rods, or a bundle of holly or brushwood pulled up and down on a rope. Never send a child up a chimney. If a chimney fire starts: shut the air supply to the fire, get everyone out, wet the roof around the chimney, and keep watch until it is cold. Do not throw water into a red-hot flue: the steam can burst it.
- Burns. Iron stoves and stove pipes burn skin instantly; guard them from children.
- Collapsing chimneys. Tall chimneys are heavy and catch the wind. Tie them to the building at each floor with iron straps, and keep the top in good repair.
- Cracked flues leak smoke and fire into walls and roof spaces. Inspect the chimney from top and bottom each year with a lamp and mirror.
Going further
- Bake and cook with the same fire: Kitchen and Cooking, Grain, Flour and Bread.
- Hot water: a copper or iron tank beside the firebox or a coil in it heats bath water (Hot Water and Central Heating, Pipes, Plumbing and Aqueducts).
- Smoke-free fuel: charcoal (Charcoal), coke (Coal and Coke), and gas (Biogas and Wood Gas).
- Steam heating and central heating lead on from Boilers and Pressure Vessels (Hot Water and Central Heating).
- Insulation and sun: thick walls (Cob, Adobe and Rammed Earth), Insulation and Keeping Buildings Warm or Cool, shutters and double windows (Window Glass), and Solar Heat heat.
How it was first done
For most of history people heated with open hearths, the smoke finding its way out through the roof. The Romans heated bath-houses and villas with hypocausts; the invention is credited to Sergius Orata around 100 BC. In Korea, floors heated by flues (ondol) go back at least 2,000 years. Chimneys appear in European castles and manor houses in the 1100s, but most ordinary houses did without them until the 1500s and 1600s. Tiled masonry stoves spread across Central and Northern Europe from the late Middle Ages. Benjamin Franklin designed an iron fireplace that threw more heat into the room in 1742, and the scientist Benjamin Thompson, Count Rumford, published his shallow, smoke-free fireplace design in 1796; thousands of smoky London fireplaces were rebuilt to it within a few years. The rocket stove was designed in the 1980s by the American engineer Larry Winiarski for families cooking with scarce firewood.
Source: content/entries/building/chimneys-and-stoves.md