Part 11 · Power and Energy
Petroleum and Refining
Rock oil seeps out of the ground in many places and lies in pools deeper down. Find it, collect it or drill for it, and boil it apart in an iron still into petrol, kerosene, diesel, lubricating oil, wax and asphalt — or, where there is none, make engine fuel from plant oil.
- Difficulty
- ●●●●●
- Time
- Days to collect from a seep; weeks to months to drill a shallow well; a day per distillation run
- Steps from zero
- 16 prerequisites →
The full path from nothing — 16 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Pottery
- Charcoal
- Hides and Leather
- Fermentation
- Bellows
- Distillation
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Petroleum and Refining
Do them roughly in this order. See it on the tech tree →
Why it matters
Petroleum packs more energy into less space than any other natural fuel: about 42–45 MJ per kg, three times seasoned wood and half again as much as good coal — and it is a liquid, so it pours, pipes and sprays. Distilled into its parts, it gives:
- kerosene, the clean, bright lamp oil that lit the world's homes from the 1860s (Lamps and Candles);
- petrol and diesel, the fuels that make the The Internal Combustion Engine engine small enough to carry, giving the The Motor Vehicle, the The Tractor and the Gliders and Aeroplanes;
- lubricating oils and greases for every bearing and gear (Lubricants and Greases, Bearings and Lubrication);
- paraffin wax for candles and waterproofing, and asphalt for roads and roofs (Roads and Bridges);
- later, the raw material of plastics (Petrochemicals and Modern Plastics), Synthetic Rubber Works (Overview) and many medicines.
But oil is found only in certain places, and deep oil needs heavy drilling. This chapter starts with what you can do with your hands — collect oil from seeps and distil it — then drilling, and ends with the alternatives when you have no oil at all.
How it works
What oil is. Petroleum is a mixture of hundreds of different hydrocarbons — molecules made only of carbon and hydrogen — formed from tiny sea plants and animals buried in mud and cooked slowly underground for millions of years. Small molecules (1–4 carbon atoms) are gases; medium ones (5–20) are liquids; big ones are waxes and tar.
Where it collects. Oil is lighter than water, so it creeps upward through porous rock (sandstone, cracked limestone) until it is stopped by a tight layer such as shale. It gathers under the high points of folded rock — domes (anticlines) — like air trapped under an upturned bowl. Where a fault or eroded fold lets it reach the surface, it leaks out as a seep.
How refining works. Each hydrocarbon boils at its own temperature: the smaller the molecule, the lower the boiling point. Heat crude oil in a closed still and the lightest parts boil off first; raise the heat and heavier ones follow. Cool the vapour and collect what condenses in separate containers for each temperature range, and you have split crude into fractions — the same principle as distilling alcohol (Distillation), but at much higher temperatures.
| Fraction | Boils at | Approx. weight per litre | Use |
|---|---|---|---|
| Gas | below 30 °C | — | Burned on the spot as fuel for the still |
| Petrol (gasoline, naphtha) | 30–180 °C | 0.70–0.76 kg | Spark-ignition engines; solvent |
| Kerosene (paraffin oil, lamp oil) | 150–275 °C | 0.78–0.82 kg | Lamps, stoves, hot-bulb engines |
| Diesel (gas oil) | 250–350 °C | 0.82–0.87 kg | Diesel engines, heating |
| Residue | above 350 °C | 0.90–1.0 kg | Lubricating oil, wax, fuel oil, asphalt |
Crudes differ enormously. A light crude from a simple still may give a quarter or more of petrol and a third of kerosene and diesel together; a heavy, tarry crude may give almost nothing but residue.
What you need
| Item | Notes |
|---|---|
| Buckets, absorbent cloth or wool, a skimming ladle | For seeps |
| For drilling: a stout timber tripod or derrick 6–10 m high, a springy pole 8–12 m long (hickory, ash or young oak), rope | See below |
| A drill bit and stem of iron with a hardened Steel edge, 30–80 kg | Forged by a smith (Blacksmithing) |
| A bailer: a pipe 2–3 m long, 7–10 cm wide, with a flap valve at the bottom | Sheet iron rolled and riveted (Sheet Metal and Rolling) |
| Casing pipe | Iron pipe, or bored wooden pipe for shallow holes |
| An iron or steel still pot of 50–200 litres with a bolted, clay-sealed lid | Riveted boiler plate is best; never clay or glass for oil |
| A condenser: 6–10 m of iron or copper pipe, 2–3 cm bore, running through a tank of cold water | See Distillation |
| A dozen covered metal or stoneware receivers | One for each cut |
| Small pellets of tin and lead, a scale, and a measuring vessel | For judging temperature and density without instruments |
Where to find it
- Rainbow films on water. Oil makes a thin, shimmering film on springs, ponds and slow streams. Poke it with a stick: an oil film swirls and flows back together. A film that breaks into flat, cracked plates is iron bacteria, not oil (see Iron (the Bloomery)).
- Oil in pits and hollows. Brown, green or black oil oozing from the ground, often with gas bubbles, a strong kerosene smell and sometimes a rotten-egg smell.
- Tar and asphalt. Black, sticky pools or hard, glossy black lumps (bitumen) along faults and hillsides — the residue of a seep whose light oil has evaporated. Famous examples are the Pitch Lake of Trinidad and the tar pits of Los Angeles. See Tar, Pitch and Glue.
- Burning springs and "eternal flames". Natural gas leaking from the ground can be lit and burns for centuries. Where there is gas there is often oil.
- Oil sands and oil-soaked rock. Dark, sticky sandstone that smells of kerosene and smokes in a fire.
- Oil shale. Dark, tough, finely layered shale that burns with an oily flame. It holds no liquid oil, but heating it gives some (see below).
- The shape of the land. In layered rocks, look for places where the beds dip away in both directions from a ridge or a dome. Seeps along the crest or flanks of such a fold are the classic sign.
Method 1: Collecting from seeps
- Dig a pit beside the seep, 1–2 m across and as deep as you can safely go (no more than 1.5 m without shoring — see Dangers). Oil and water seep in together; the oil floats.
- Skim daily. Lay a woollen blanket or bundle of rags on the surface, lift and wring it into a bucket — the method the Seneca people used in Pennsylvania. Or skim with a flat ladle.
- Settle it. Let the oil stand for a few days in a covered vessel. Water and mud sink; draw the oil off the top. Water left in crude oil makes it foam violently in the still.
A good seep may give a few litres a day — enough for lamps, lubrication and experiments, not for engines in quantity.
Method 2: Drilling a shallow well with a spring pole
For more oil you must go down to it. Cable-tool drilling — lifting and dropping a heavy chisel on a rope — was used in China for salt and gas wells two thousand years ago, and drilled the first oil wells. It needs no rotating machinery.
- Site. Close to a seep, or on the crest of a fold, on firm ground with water nearby.
- Derrick. Raise a tripod of three straight poles 6–10 m long, lashed at the top, with a pulley for pulling the tools out.
- Spring pole. Anchor the thick end of a springy pole 8–12 m long under a heavy log or stakes, rest it on a forked post about a third of the way along, and let the thin end overhang the hole by about 1 m. Hang two rope stirrups from the end.
- Tools. Hang the drill string from the end of the pole: rope, then a heavy iron stem (1–2 m long), then the bit — an iron chisel 5–10 cm wide with its cutting edge steel-faced and hardened (see Axes, Chisels, Knives and Planes). Total weight 30–80 kg.
- Start the hole by digging a pit 2–3 m deep, and drive a wooden or iron pipe (the conductor) into it to stop loose soil caving in.
- Drill. Two or three people stand in the stirrups and kick the pole down together, then let it spring up; each stroke lifts the bit 30–60 cm and drops it. Aim for 30–40 strokes a minute. The driller holds the rope and turns it a quarter turn every stroke so the bit hits a new place each time and the hole stays round.
- Keep it wet. Pour in water if the hole is dry: the chips must make a mud.
- Bail. Every 30–60 cm, pull out the tools (through the pulley) and lower the bailer. As it drops into the mud its flap valve opens; as it is lifted, the valve closes and brings up a pipe-full of slurry. Two or three bails clear the hole.
- Dress the bit. Every day or two, the bit goes back to the forge to be drawn out, sharpened and re-hardened. The width of the bit sets the width of the hole; a worn bit makes a tapering hole that jams the tools.
- Case the hole. Once through loose ground and fresh-water layers, lower or drive casing pipe down the hole to stop it collapsing and keep water out of the oil.
- Progress. Expect up to a metre a day in soft shale, a few centimetres in hard sandstone. A 60 m well takes weeks to months; spring poles have reached 300 m.
- When you strike oil, it may rise part way up the hole, flow out on its own, or arrive with a rush of gas. Pump it out with a long-stroke Pumps worked by a rocking beam (a walking beam), driven by hand, animal or engine.
Method 3: Refining in a batch still
- Build it safe. Set the iron still over a brick firebox. Lead the vapour pipe from the top of the still through a brick or earth wall to the condenser tank and receivers on the far side, at least 5 m from the fire. Vapour and drips must never be able to reach a flame.
- Charge it. Fill the still to no more than two-thirds with settled, water-free crude. Seal the lid joint with clay mixed with flour or with fireclay.
- Temperature without a thermometer. Fit a short closed iron tube into the vapour pipe at the top of the still (a pocket the vapour flows around). Drop small pellets in it: tin melts at 232 °C, lead at 327 °C. Water dripped onto the outside of the pocket sizzles from 100 °C. Check the pellets with a wire. Better still, use a proper The Thermometer.
- Heat slowly through the first hour. Light, colourless liquid soon runs: petrol. Collect it in a closed receiver and keep it well away from any flame.
- Change receivers as the heat rises. The distillate gets slightly yellow, oilier and heavier: kerosene starts at about 150 °C and runs until the tin pellet has long melted. Then diesel until the lead pellet is close to melting (~330–350 °C).
- Stop at about 350 °C. Above this, heavy oil starts to crack (break apart) — gas and strong smells increase and the distillate darkens. Let the still cool completely, overnight, before opening. The thick black residue is left in the pot.
- Weigh every cut. Weigh a litre of each: use the table above to tell petrol from kerosene from diesel.
Cleaning kerosene. Raw kerosene smells and smokes. Stir it for 30 minutes with about 1–2% of its volume of concentrated Sulfuric Acid in an iron or stoneware vessel, let the black sludge settle and draw it off, then wash the oil with a weak lye solution (Lye and Potash) and then with water, and let it settle clear. Water-white kerosene burns without smell or smoke.
Lubricating oil and wax. The residue boils too high to distil without breaking down. Blow steam into the still through a perforated pipe in the bottom (see steam distillation in Distillation); the steam carries the heavy oil over below its own boiling point. Chill the heavy oil in winter or in an ice house (Ice and Refrigeration); paraffin wax crystallises out and can be pressed out through canvas. The thin oil that passes is lubricating oil. What will not distil is asphalt, for roads, roofs and waterproofing.
Shale oil. Heat crushed oil shale in a closed iron or clay retort to a dull red (about 450–500 °C), exactly like making charcoal in a retort (Charcoal), and lead the vapours through a condenser. Good shale gives roughly 50–150 litres of oil per tonne; refine it like crude.
Method 4: No oil? Plant oil and alcohol
Most places have no oil. You can still fuel engines:
- Straight plant oil from rapeseed, sunflower, groundnut, palm, olive or linseed (Oils and Pressing) burns in hot-bulb engines and in slow diesel engines if heated to 70–80 °C first (The Internal Combustion Engine).
- Biodiesel: stir 1 litre of dry, warm (55 °C) plant oil for an hour with 200 ml of methanol in which 3.5 g of caustic soda has been dissolved; let it settle overnight, draw off the glycerine at the bottom, wash and dry the oil on top. The full method and its dangers are in The Tractor. A hectare of rapeseed or sunflower gives about 800–1,200 litres of oil a year.
- Alcohol at 95% or stronger, from fermented grain, potatoes, sugar or fruit (Fermentation, Distillation), runs spark-ignition engines.
- Wood gas from a gasifier runs both kinds of engine (Biogas and Wood Gas).
- Coal-tar oils from a gasworks (Coal and Coke) give lamp oil and engine fuel.
How to tell it worked
- Petrol evaporates from the back of your hand in seconds, leaving it cold and dry. Kerosene takes minutes and leaves a slight greasy feel. Diesel stays oily.
- Flash test for lamp oil. Outdoors, warm a spoonful of kerosene in a small cup standing in warm water at about 35 °C — warm to the hand, a little cooler than your body. Pass a small flame just over the surface. Safe kerosene does not flash. If a blue flash runs across it, it still contains petrol: redistil it. Petrol flashes even on ice.
- A good lamp oil burns in a wick lamp with a steady bright flame and no smoke when the wick is set right.
- Lubricating oil stays slippery between two warm metal surfaces, does not gum up when left a week in the open, and does not smoke at the temperature of a running bearing.
Note Troubleshooting. Still foams and spits oil into the condenser → water in the crude, or overfilled. Settle and drain the crude; heat more slowly through 100 °C; fill only two-thirds. Kerosene dark or smoky → collected too hot (diesel mixed in) or not acid-washed. Redistil more slowly; wash. Kerosene flashes in the test → petrol left in it. Redistil, discarding the first tenth. Drill bit stuck → the bit wore narrow and the hole tapered, or the hole caved. Ream with a fresh full-width bit; case sooner. Hole fills with water → you have hit a water layer; case past it before going deeper.
Dangers
Danger Petrol vapour explodes. Petrol gives off vapour even in freezing weather. Mixed with air at only 1–8%, it explodes. The vapour is heavier than air and flows along the ground and into pits and cellars, where it finds a fire, a lamp or a spark metres away.
- Keep the still's fire behind a wall, and the receivers and stores far from any flame.
- Never open a still, receiver or storage tank while hot or near a flame. Never pour petrol near a fire.
- Store fuel in closed metal containers, outside, in the shade, away from houses.
- Keep a pile of dry sand and spades by every still and store. Never throw water on burning oil — it spreads the fire. Smother it.
- Never put petrol or a light spirit in a lamp (Lamps and Candles).
Danger Wells kill. Oil and gas seeps and wells give off hydrogen sulfide (rotten-egg gas), which at high levels kills the sense of smell and then kills within minutes; and methane and other gases that suffocate and explode. Never climb into a hand-dug oil pit or well; never lean over a well head; work upwind. A drilled well can suddenly blow out, throwing tools, mud, oil and gas high into the air — keep fire, lamps and smoking far away from any drilling.
- Burns and fires at the still. Leaking joints drip oil near the firebox. Check every joint before lighting, and clean up spills with sand.
- Poison. Petroleum fuels damage the lungs if swallowed and vomited — never siphon with your mouth. The light fraction contains benzene, which causes cancer; do not wash with petrol or breathe its fumes for long.
- Skin. Oils, tar and residues cause rashes and, with years of contact, skin cancer. Wear gloves or wash off quickly.
- Concentrated sulfuric acid for washing kerosene causes deep burns; always add acid slowly to the oil, wear eye protection. See Sulfuric Acid.
- Pollution. Spilled oil poisons wells, streams and soil for years. Keep stills and stores away from water sources and dig a bund (an earth bank) around tanks to catch leaks.
What this unlocks
Kerosene gives cheap, bright light (Lamps and Candles). Petrol and diesel run The Internal Combustion Engine engines — the The Tractor, The Motor Vehicle, motor boats and Gliders and Aeroplanes. Lubricating oil (Lubricants and Greases) keeps Bearings and Lubrication, gears and Machine Tools running. Asphalt surfaces Roads and Bridges and waterproofs roofs (Roofs). Later, the light fractions are the raw material for Early Plastics, Rayon and Nylon and much of modern chemistry.
How it was first done
Bitumen from seeps is one of humanity's oldest materials: Neanderthals in Syria used it to glue stone tools to handles some 70,000 years ago, and the cities of Mesopotamia used it as mortar, to waterproof boats and baskets, and to pave roads. In China, drillers in Sichuan were probably sinking wells for salt brine and natural gas by percussion two thousand years ago, using bamboo cables and iron bits; the Shenhai well, finished in 1835, reached 1,001 m. In the 9th century the Persian physician al-Razi described distilling petroleum into a clear "white naphtha" for lamps. Oil was collected from hand-dug pits around Baku on the Caspian Sea for centuries; Marco Polo heard of it in the 1270s.
The modern industry began in the 1850s. In Lviv (in today's Ukraine), Ignacy Łukasiewicz distilled kerosene from local seep oil and in 1853 designed a lamp to burn it; a hospital operation was carried out by its light. In Scotland, James Young distilled paraffin oil and wax from coal and then from oil shale. Wells were dug or drilled near Baku in 1846–48 and in Ontario in 1858, and on 27 August 1859 Edwin Drake, using a steam-driven cable-tool rig and iron casing driven through the gravel, struck oil at 21 m near Titusville, Pennsylvania, starting an oil rush. Thermal cracking — breaking heavy oil into more petrol with heat and pressure — followed in 1913, as the motor car made petrol, not kerosene, the most valuable fraction.
Source: content/entries/energy/petroleum.md