◆ Rebuild

Part 4 · Food and Farming

Tea, Coffee and Cocoa

How to grow tea, coffee and cacao, and how to turn their leaves and seeds into drinks and chocolate. It covers picking, withering, rolling and drying tea; picking, fermenting, drying and roasting coffee and cacao; and the tea roller, coffee roaster and chocolate itself.

Difficulty
●●●●●
Time
Three to five years before new bushes and trees bear; a day to make tea; three weeks to dry coffee; a week to ferment cacao and two to dry it
Steps from zero
7 prerequisites →

You need first

Farming from SeedPreserving Food

This unlocks

—
The full path from nothing — 7 steps before this one
  1. Stone Tools
  2. Fire
  3. Finding and Preparing Clay
  4. Pottery
  5. Farming from Seed
  6. Salt
  7. Preserving Food
  8. Tea, Coffee and Cocoa

Do them roughly in this order. See it on the tech tree →

Why it matters

Tea, coffee and cocoa are not needed to stay alive, but they have shaped work and trade for a thousand years. A drink made with boiled water is a safe drink, which saved many lives in towns with dirty wells (Finding and Purifying Water). Their mild stimulants (caffeine in tea and coffee, theobromine in cocoa) keep watchmen, sailors and clerks awake. Dried tea, green coffee and fermented cocoa beans keep a year or more, which made them some of the first goods worth shipping across oceans (Money, Trade and Record-keeping).

All three are made the same way: grow, pick, then control the plant's enzymes (substances in living cells that speed up chemical changes) with heat, air and time. Tea leaf has its enzymes killed at once (green tea) or let work in air (black tea). Coffee and cacao seeds are dried and then roasted to build flavour.

How it works

  • Enzymes and air. A crushed tea leaf goes brown, like a cut apple: enzymes use oxygen to turn colourless polyphenols into brown, strong-tasting ones. Tea makers call this "fermentation", but no microbes are involved; it is oxidation. Heat above about 70 °C stops it.
  • Drying preserves. Below about 5% moisture (tea) or 12% (green coffee), moulds and bacteria cannot grow (Preserving Food).
  • Roasting makes flavour. At 150–230 °C sugars and proteins react into hundreds of brown, fragrant compounds, as in bread crust.
  • Cacao is truly fermented. Wild yeasts and bacteria eat the sweet pulp round the seeds and heat the heap to 45–50 °C, killing the seed and starting the chemistry of chocolate flavour. Unfermented cacao roasts bitter and dull.

What you need

Item For Notes
Young plants or fresh seed Starting a plantation Seed must be fresh; see below
Bamboo or wooden trays, mats Withering, drying Raised off the ground, in shade or sun
Shallow iron pan or wok Firing green tea Pots, Pans and Kettles
Tea roller Rolling large batches Built below
Drying floor, raised beds Coffee and cacao Clean, sloped, covered at night
Wooden boxes or a heap with leaves Fermenting cacao Banana or plantain leaves, or any large safe wrapping leaf
Coffee roaster Roasting Built below
Mortar and pestle or quern Hulling coffee, grinding cocoa Oils and Pressing, Grain, Flour and Bread
Warm grinding stone Making chocolate A metate: flat stone and roller
Sugar Chocolate Sugar

Where to find it

  • Tea (Camellia sinensis): an evergreen shrub with glossy, finely toothed leaves 5–15 cm long and white flowers with yellow centres. It needs acid soil (pH 4.5–5.5; where rhododendrons thrive, tea usually will), 1,500 mm or more of rain, and no hard frost. Look in old gardens and estates in China, India, Sri Lanka, East Africa and Japan. Flowering camellias are relatives, not tea.
  • Coffee: shrubs with shiny, wavy leaves in pairs, white scented flowers and berries (cherries) that ripen green to red, each holding two seeds. Arabica wants tropical highlands at 1,000–2,000 m; robusta grows in hot, wet lowlands and is more bitter.
  • Cacao (Theobroma cacao): an understory tree 4–8 m tall of the hot, wet tropics within about 20° of the equator, liking shade. Ridged pods 15–30 cm long grow straight from the trunk, ripen yellow, orange or red, and hold 20–50 seeds in white, sweet-sour pulp.

Tip Seed does not keep. Coffee and cacao seeds die within weeks of leaving the fruit, and dried or roasted beans never sprout. Plant cacao seeds within a few days of opening the pod. Plant coffee from fresh ripe cherries with the pulp washed off. Tea seed keeps a few months if it is kept cool and slightly damp. Cuttings with one leaf and a short stem root well under shade and mist.

Growing

Raise seedlings in a shaded nursery, plant them out at 6–12 months, and keep them weeded, mulched and fed with compost (Compost and Manure). Plant tea 1.2 m apart each way and prune it to a flat "plucking table" about 1 m high; light picking starts in the third year, and a hectare gives 1–3 tonnes of made tea a year. Plant coffee 2–3 m apart; it bears from the third or fourth year, 0.5–2 kg of green coffee per tree, and fruits on new wood, so cut old stems back every few years. Plant cacao 3 m apart under shade trees; from the third to fifth year each tree gives 20–40 pods, or 1–2 kg of dry beans.

Tea

BLACK TEA GREEN TEA Pick two leaves and a bud 1 Wither 12–18 h in shade loses a third 2 Roll 30–60 min, hard breaks the cells 3 Oxidise 1–3 h at 25 °C until copper air 4 Fire 90–120 °C black and crisp 1 Heat at once hot pan 3–5 min or steam 30–60 s 2 Roll 5–10 min into twists 3 Dry low heat until it snaps Heat kills the enzymes, so the leaf stays green.
Fig. 1 Tea from bush to cup. Black tea is withered, rolled, left to oxidise until coppery, then dried. Green tea is heated at once to stop the enzymes, then rolled and dried.

Picking

Pick "two leaves and a bud": the tender tip of each new shoot. Snap it off between thumb and finger; don't tear or crush it. In the growing season new shoots come every 7–14 days. Older, tougher leaves make coarse, bitter tea. A good picker gathers 15–30 kg of fresh leaf a day. About 4.5 kg of fresh leaf makes 1 kg of dry tea.

Green tea

  1. Kill the green within a few hours of picking. Heat an iron pan until a drop of water skitters and vanishes (about 200–250 °C at the metal). Add a double handful of leaf and toss it constantly with your hands or a pair of wooden paddles for 3–5 minutes, until it wilts, turns dull dark green, smells sweet like cooked greens, and stops squeaking. The Japanese way is to steam the leaf for 30–60 seconds over boiling water instead.
  2. Roll the hot, soft leaf on a bamboo mat. Push it away from you with both palms in a ball and draw it back, again and again for 5–10 minutes, until the leaves curl into twists and feel slightly sticky.
  3. Dry in the pan over a low fire, tossing, or spread on trays over warm embers, until the leaf crumbles and snaps (about 4–5% moisture). Done by hand, a batch takes an hour or two.

Black tea

  1. Wither. Spread the leaf 2–3 cm deep on racks in a shaded, airy shed for 12–18 hours, turning it now and then. It loses about a third of its weight. When it is ready, a handful squeezed into a ball stays together without cracking, and the stalk bends without snapping. A withering rack is a frame of shelves 30 cm apart, each with a floor of woven bamboo, slatted wood or coarse cloth so air passes through. One square metre takes about 1–1.5 kg of fresh leaf.
  2. Roll hard for 30–60 minutes by hand or in a tea roller (below). This breaks the cells and lets the juice out over the leaf.
  3. Oxidise. Spread the twisted leaf 5–8 cm deep on a cool, clean surface, cover it with a damp cloth, and keep it at about 25 °C. Over 1–3 hours it changes from green to bright copper, and the smell changes from grassy to fruity and flowery. Stop when the colour is even. Too long and it smells stewed and makes flat, dark tea.
  4. Fire. Dry the leaf quickly over a charcoal fire on trays, or in a hot-air chamber at 90–120 °C, for about 20–30 minutes, until it turns black and crisp.

Oolong sits in between: wither, toss in baskets to bruise only the leaf edges, oxidise partly for an hour or two, then fire. To brew, use 2–3 g of leaf per cup: black tea in boiling water for 3–5 minutes, green tea in water cooled to 70–80 °C for 1–3 minutes.

The tea roller

Rolling by hand tires the arms after a few kilograms. The machine roller was invented in Assam in the 1870s and does the same pushing and pulling on 20–50 kg at a time.

SIDE VIEW, BOX CUT AWAY TOP VIEW Screw and handwheel press, release, press Pressure lid Box 50–60 cm Leaf 20–50 kg Centre door Ribbed table 90 cm across, ribs 1.5 cm high crank or belt drive two cranks turn together The box moves round in a 20–25 cm circle but never spins. The leaf rolls over the curved ribs and twists. 40–50 circles a minute
Fig. 2 A hand-cranked tea roller. The box of leaf is moved round in a small circle over a table with raised ribs, and a pressure lid squeezes the leaf from above. The leaf rolls over the ribs and twists.
  1. Table. Build a round hardwood table about 90 cm across, standing on heavy legs so it doesn't walk about. Fix curved wooden battens (ribs) on it, each 1.5 cm high, running out from the centre in a gentle spiral. Leave a small door in the centre to let the rolled leaf drop out.
  2. Box. Make a bottomless cylinder 50–60 cm across and 40 cm deep from staves or sheet metal (Barrels and Cooperage, Sheet Metal and Rolling). Mount it on a frame so it can move over the table.
  3. Drive. The box must travel in a circle about 20–25 cm across without turning round itself. Carry it on two cranks of equal throw at opposite sides, linked so both turn together (Cranks, Cams and Linkages). One person turns a handle, or a belt from a water wheel or animal gear drives it at about 40–50 turns a minute (Belts, Chains and Power Transmission).
  4. Pressure lid. A wooden disc slides inside the box on a screw or a weighted lever. Roll the first 10 minutes with no pressure, then press down for 10 minutes, release, and press again. Too much pressure early turns young leaf into mush.

A good roller gives leaf twisted tightly along its length, with juice on its surface but not dripping. If the leaf comes out flat and dry, it needed more withering time or more pressure. If it comes out pulpy, it was over-pressed or under-withered.

Coffee

Picking and processing

  1. Pick only ripe red cherries. Pick each tree several times through the season. Green cherries make sour, grassy coffee. About 5–6 kg of cherries make 1 kg of green coffee.
  2. Then use one of two ways:
    • Dry (natural) way: spread whole cherries 3–4 cm deep on a clean, sloped stone floor or on raised mesh beds. Rake them several times a day and cover them at night and in rain. In 2–4 weeks they turn dark brown and the beans rattle inside. This way gives fruity, heavy coffee and needs little water.
    • Wet (washed) way: squeeze the beans out of the skins within a day of picking, in a hand pulper or by treading. Leave them in a tank of water for 12–48 hours until the slimy coat rubs off and the beans feel gritty, not slippery. Wash them, then dry them in the sun for 1–2 weeks. The bean is still in a papery shell called parchment. This way gives clean, bright coffee.
  3. Judge dryness: bite a bean. It should be hard enough to dent only with effort and should not be soft or chewy. That is about 11–12% moisture. Drier beans crack; wetter ones go mouldy in store.
  4. Hull in a wooden mortar with a light pestle, or in a millstone set wide apart (Grain, Flour and Bread), and winnow away the husks. The beans are now green coffee. Kept dry in sacks, off the floor, they last a year or more (Granaries and Food Storage).

Roasting

Roast in small batches, a few days before use. Ground coffee goes stale in days; whole roasted beans keep about a month.

  1. Heat the beans steadily while keeping them moving. They go from green to yellow (smelling of hay) to light brown (smelling of bread).
  2. At about 8–10 minutes comes the first crack: a sound like popcorn. The beans swell and the papery chaff flakes off. From here on, watch closely.
  3. Light roast: stop 1–2 minutes after first crack ends. The beans are cinnamon brown and dry, and the coffee tastes bright and sharp.
  4. Medium roast: stop just before the second crack, at chocolate brown.
  5. Dark roast: when a quieter, faster crackle begins (second crack), the beans go nearly black and oily. Stop within a minute or the beans turn to charcoal.
  6. Cool at once. Tip the beans into a sieve and toss them in a breeze, or spread them on a stone, so they are hand-warm within 4 minutes. Beans left hot keep roasting.

Roasted beans weigh 15–20% less than green beans. Grind just before brewing (Kitchen Utensils and Gadgets) and use about 60 g to a litre of water just off the boil (Pots, Pans and Kettles).

The coffee roaster

The simplest roaster is an iron pan over a steady fire, stirred without stopping with a wooden spoon. Roasting this way is uneven, but it works. The drum roaster is far better: it turns the beans over and over, so every bean gets the same heat.

SIDE VIEW END SECTION OF DRUM 15–20 cm across, 25–30 cm long Sliding door load, sniff, listen, empty Drum sheet iron, 3 mm holes Charcoal glowing, no flame Spit square rod Crank 1 turn a second 10–15 cm above coals Fins lift and tip Beans no more than one third full
Fig. 3 A drum coffee roaster over a charcoal fire. The perforated iron drum turns on a spit. Fins inside tumble the beans; a sliding door lets you load, sample and empty.
  1. Drum. Roll a cylinder 15–20 cm across and 25–30 cm long from 0.8–1 mm sheet iron (Sheet Metal and Rolling). Punch it full of 3 mm holes about 1.5 cm apart so heat and smoke can pass. Rivet three strips 2 cm wide along the inside as fins to tumble the beans.
  2. Ends and spit. Close both ends with discs. Run a square iron rod through the middle as a spit, ending in a wooden crank handle. Cut a door 6 × 8 cm in the side with a sliding cover.
  3. Firebox. Build a brick or sheet-iron box with two notches for the spit, so the drum sits 10–15 cm above a bed of glowing charcoal (Charcoal). Steady embers beat flame.
  4. Use. Fill the drum no more than one third full (300–500 g for this size). Turn it at about one turn a second. Open the door now and then to look at and smell the beans and to hear the cracks.

Big roasters are the same thing with a larger drum turned by a belt, and a fan to cool the beans. A good roaster gives beans that are all one colour with no black tips or scorched faces. Black tips mean the fire is too hot. A spread of colours means the drum is too full or turning too slowly.

Cocoa and chocolate

48 °C 1 Open ripe pods 20–50 beans in white pulp covered with banana leaves 2 Ferment 5–7 days turn every 2 days; pulp drains 3 Dry 1–2 weeks down to about 7% water; beans rattle, shells crack shells blow away 4 Roast, crack, winnow 120–150 °C; nibs fall stone roller 5 Grind on warm stone 40–50 °C 6 Add sugar, temper 45 → 27 → 31 °C, mould, cool, snap
Fig. 4 From cacao pod to chocolate. The beans are fermented under leaves, dried, roasted, cracked and winnowed to nibs. The nibs are ground on a warm stone to liquid cocoa mass, then mixed and ground with sugar.

Fermenting and drying

  1. Harvest pods when they are fully coloured and sound hollow when you tap them. Cut them off with a knife, without tearing the cushion on the trunk where next year's flowers grow. Split them open with a wooden club within a week. A steel blade can cut the beans.
  2. Ferment. Scoop the beans and their pulp into a heap on banana leaves, or into a wooden box with drain holes. Each box should be about 60 cm on each side and hold at least 50 kg, because small heaps don't heat. Cover with more leaves. The pulp drains away as a sweet liquid, and the heap heats to 45–50 °C in 2–3 days. Turn it every 2 days so air reaches it. After 5–7 days (2–3 days for the pale "criollo" kind), cut a bean in half. It should be brown inside, cracked into ridges, and smell of vinegar and fruit. Slate-grey, solid beans are unfermented. Purple ones are underdone.
  3. Dry in the sun on mats or raised trays, 5 cm deep, raking often, for 1–2 weeks, down to about 7% moisture. Beans that are ready rattle, and the shell cracks away cleanly when you press it. Cover them against rain and dew. Damp beans grow mould in days, and mouldy beans must be thrown away.
  4. Store dried beans in sacks in a dry, airy place. They keep a year.

Roasting and winnowing

  1. Roast at 120–150 °C for 15–35 minutes, more gently than coffee. You can use a coffee roaster with less fire, or an oven. Stop when the shells crackle and loosen and the beans smell strongly of chocolate. A burnt smell means you went too far.
  2. Crack the cooled beans by rolling a bottle or rolling pin over them, or pass them through a millstone set wide.
  3. Winnow away the papery shells to leave the nibs. You can toss them in a flat basket in a breeze. A cocoa winnower makes this quicker: a hopper drops the cracked beans through a box while a hand-cranked fan blows across the stream, so the light shell blows out of a side opening and the heavy nibs fall into a tray below. It is a smaller version of the grain winnowing fan in Grain, Flour and Bread. Adjust the fan speed until shell comes out of the side but no nibs do.

Grinding: from nibs to chocolate

Nibs are more than half fat (cocoa butter), so they grind into a thick liquid: cocoa mass (also called cocoa liquor).

  1. The metate. Grind the nibs a handful at a time on a flat stone slab about 40 × 30 cm, tilted towards you, with a stone roller 30–40 cm long. Mesoamerican cooks warmed the slab over a small fire to 40–50 °C: warm to the hand, never too hot to touch. The nibs turn to paste, then to a glossy, runny mass in 20–40 minutes.
  2. Add sugar. Grind in one part sugar to two or three parts cocoa mass by weight, until the grit is barely felt between tongue and palate. Hand-ground chocolate always stays a little gritty. Machines grinding with granite rollers in a heated pan for 24–72 hours make it smooth, and a conche (a heated trough in which a roller works the chocolate back and forth for a day or more) also drives off sour flavours.
  3. Milk chocolate has dried milk powder ground in (Dairy and Cheese): roughly 30% cocoa mass, 20% cocoa butter, 25% milk powder and 25% sugar. Even a drop of water makes chocolate seize into a stiff, grainy lump, so the milk must be fully dry.
  4. Cocoa butter and cocoa powder. Press warm cocoa mass in a cloth bag in a screw press (Oils and Pressing). Pale yellow cocoa butter runs out; the cake left behind is ground and sieved to cocoa powder. Cocoa butter added back makes chocolate flow and snap cleanly, and on its own makes a skin salve that keeps for years.

Tempering and moulding

Chocolate that simply melts and sets turns dull, soft and streaked with grey ("bloom"). Tempering makes the fat set in its one good crystal form.

  1. Melt dark chocolate to 45–50 °C over warm water. Keep steam and water away from it.
  2. Cool it to 27–28 °C while stirring constantly, ideally by working it on a cool stone slab with a scraper. It thickens slightly.
  3. Rewarm it gently to 31–32 °C (milk chocolate 29–30 °C) and use it at once.
  4. Test: smear a little on a knife blade at room temperature. Tempered chocolate sets in 5 minutes, glossy and firm. Untempered chocolate is still tacky and later goes streaky.
  5. Pour it into wooden, tin or carved stone moulds. Tap them to free bubbles, and cool them at 12–18 °C.

Drinking chocolate needs no tempering. The Mesoamerican way is to dissolve a tablet of ground cocoa, sugar and spices in hot water and whip it to a froth by pouring it from a height between two vessels.

How to tell it worked

  • Tea: dry leaf snaps and is evenly dark (black) or evenly olive (green), with no burnt or green-raw bits. Infused, black tea is clear, bright red-brown, and brisk on the tongue. Green tea is pale yellow-green and sweet-grassy. Wet leaf should look whole and twisted, not crumbled.
  • Coffee: green beans are uniform in size and grey-green or blue-green. Throw out any that are black, sour-smelling or bored by insects. Roasted beans are evenly coloured and smell sweet, and the coffee is not sour (too light or under-ripe beans) or burnt (too dark).
  • Cocoa: cut beans are brown and ridged inside, and taste bitter and chocolatey, not purple and astringent.
  • Chocolate: snaps cleanly, shines, melts in the mouth but not in the hand, and is free of grey streaks.

Note Troubleshooting.

  • Tea tastes grassy and harsh → it was not withered or oxidised enough.
  • Tea is flat and dull → it was over-oxidised, or fired too slowly.
  • Coffee is sour → unripe cherries, or a roast stopped too early.
  • Coffee has a musty, earthy taste → it went mouldy while drying. Dry thinner and faster, and cover it at night.
  • Cacao heap didn't heat → the heap was too small, or the pods were opened too late. Make it at least 50 kg.
  • Chocolate seized into a stiff lump → water or steam got in. It can still be used for drinking chocolate or baking.
  • Grey bloom → it was not tempered, or it was stored too warm or in a fridge.

Dangers

Warning Roasting fires and poisoned animals. Chaff and oily dark beans catch fire: never leave a roaster turning unwatched, keep a lid or sand at hand, and clear out the chaff after each batch. Theobromine in chocolate is harmless to people in normal amounts but poisons dogs, cats and horses; a block of dark chocolate can kill a dog. Never feed cocoa shells as bedding or fodder.

  • Caffeine is a real drug. More than about 400 mg a day for an adult causes shaking, a racing heart, poor sleep and anxiety. A strong cup of coffee holds about 100 mg, tea 30–50 mg. Pregnant women should keep to 200 mg a day or less. Children should take little. Stopping suddenly causes headaches for a few days.
  • Mould. Coffee and cacao that went mouldy while drying can carry ochratoxin, a mould poison that harms the kidneys and is not destroyed by roasting. Throw out mouldy, musty-smelling beans; don't blend them in.
  • Pulp water from wet coffee processing and cacao sweatings is strongly acid and rich in sugar. Poured into a stream it kills fish. Let it soak into a pit or onto a compost heap far from water (Sanitation and Germs).
  • Burns from hot pans, steam and chocolate at 50 °C, which sticks to skin.

What this unlocks

Tea, coffee and cocoa trade well over long distances (Money, Trade and Record-keeping, Steamships). Cocoa butter is a base for salves (Toothpaste, Shampoo, Perfume and Cosmetics). The same drum roasts barley, chicory root and nuts. Where none of the three will grow, roasted barley or chicory and herb teas of mint, lime flowers or rose hips (Foraging Wild Food, Medicinal Plants) give a hot drink without caffeine.

How it was first done

Tea drinking began in south-west China, probably first as a medicine. Around AD 760 Lu Yu described growing, steaming and brewing it in his Classic of Tea, and in 1191 the monk Eisai brought powdered green tea to Japan. Dutch traders shipped tea to Europe from the early 1600s. In 1848–51 the botanist Robert Fortune smuggled tea plants and workers out of China for British India, where planters in Assam built rolling and drying machines; William Jackson's roller of the 1870s was the most successful.

Coffee comes from the highlands of Ethiopia. By the 1400s Sufi monks in Yemen brewed it to stay awake through night prayers; coffeehouses spread through Cairo and Istanbul in the 1500s and London, Paris and Vienna in the 1600s, and plants carried to Java and the Caribbean founded the great plantations.

Cacao was first used more than 5,000 years ago in the upper Amazon of what is now Ecuador. The Olmec, Maya and Aztecs drank it frothy and bitter and used the beans as money. Spaniards brought it to Europe in the 1500s and added sugar. Coenraad van Houten patented his cocoa press in 1828, Fry's moulded the first eating chocolate bar in 1847, Daniel Peter made milk chocolate in 1875, and Rodolphe Lindt invented the conche in 1879.

Source: content/entries/food/tea-and-coffee.md