◆ Rebuild

Part 13 · Electricity

The Induction Coil

A coil of a few hundred turns of thick wire inside one of many thousands of turns of fine wire, with a buzzing switch that makes and breaks the current many times a second. From a few battery cells it gives sparks of tens of thousands of volts — the heart of early radio transmitters, X-ray machines, vacuum testing and engine ignition.

Difficulty
●●●●●
Time
A week or two, most of it winding the secondary
Steps from zero
18 prerequisites →

You need first

The ElectromagnetThe Battery

This unlocks

Arc Lamps, Neon and Fluorescent LightsRadioElectric FencesX-Rays
The full path from nothing — 18 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Charcoal
  9. Pottery
  10. Hides and Leather
  11. Fermentation
  12. Bellows
  13. Copper Smelting
  14. Iron (the Bloomery)
  15. Blacksmithing
  16. The Battery
  17. Copper Wire
  18. The Electromagnet
  19. The Induction Coil

Do them roughly in this order. See it on the tech tree →

Why it matters

A battery gives a few volts. A spark that jumps across a centimetre of air needs tens of thousands. The induction coil (also called a spark coil or Ruhmkorff coil) turns one into the other, with no moving parts except a buzzing spring. It was the high-voltage source of the late 19th century, and it opened several doors at once:

  • Radio. The first transmitters were induction coils driving a spark gap. Heinrich Hertz discovered radio waves with one in 1887, and Guglielmo Marconi sent signals across the Atlantic with spark transmitters in 1901 (Radio).
  • X-rays. Wilhelm Röntgen found X-rays in 1895 by running an induction coil through an evacuated glass tube. Every early X-ray machine was a big induction coil (X-Rays).
  • Vacuum testing. The colour and shape of the glow a coil makes in a sealed tube tell you how good a vacuum your pump has reached (The Vacuum Pump, The Light Bulb, The Vacuum Tube).
  • Ignition. A small induction coil fires the spark plug of a petrol or gas engine (The Internal Combustion Engine). Every petrol car still has one.
  • Science and testing. It tests insulation, charges Leyden jars (Static Electricity and the Leyden Jar), lights gas jets and shows the spectra of gases.

It is also the direct ancestor of the The Transformer — the same idea, used with alternating current.

How it works

Faraday found that a changing magnetism makes a voltage in every turn of wire around it (The Generator). Wind two coils on the same iron core:

  • The primary coil — a few hundred turns of thick wire — is connected to a battery.
  • The secondary coil — many thousands of turns of very fine wire — is wound over it, perfectly insulated from it, and its two ends go to a spark gap.

When current starts flowing in the primary, the core becomes magnetised; when it stops, the magnetism vanishes. Each change pushes a voltage through every turn of the secondary, and because the secondary has thousands of turns, these add up to thousands of volts. A steady current does nothing; only change works. So the primary current must be switched on and off, over and over.

Spark gap: tens of thousands of volts Secondarythousands of turns,fine wire Primarya few hundred turns,thick wire Battery6–12 V switch Spring and iron headpulled to the core, it breaksthe contact, then springs back Contactscrew Condenseracross thecontact iron core
Fig. 1 The induction coil's circuit. The battery drives current through the primary. The iron core then pulls the iron head on the spring, which breaks the contact; the current stops, the magnetism collapses, a high voltage appears across the secondary and a spark jumps the gap. The spring returns, the contact closes, and it all repeats. The condenser across the contact makes the break sudden.

The interrupter

The switching is done by the same trick as an electric bell (The Electromagnet). The primary current passes through a contact on a steel spring with an iron head, close to the end of the core. When current flows, the core pulls the head, the contact opens, the current stops; the core lets go, the spring springs back, the contact closes, and the cycle repeats — 50 to 200 times a second, with a loud buzz. This is the hammer or trembler interrupter.

Why the break matters most

The voltage in the secondary depends on how fast the magnetism changes. When the contact closes, the current rises fairly slowly (the coil resists the change) and the secondary voltage is modest. When the contact opens, the current can stop very suddenly — and that sudden collapse gives a much higher voltage. So the useful spark comes at the break, and the sparks mostly jump the same way.

The condenser

Without help, the current does not stop suddenly at the break: the primary's own "kick" (the same kick described in The Electromagnet) makes a fat spark across the opening contact, which keeps the current flowing a little longer, burns the contact, and wastes the coil's energy. A condenser — a capacitor, the flat cousin of the Leyden jar (Static Electricity and the Leyden Jar) — connected across the contact swallows that kick. The current stops almost instantly, the contact barely sparks, and the secondary spark becomes several times longer.

The core: a bundle of wires

A solid iron core would have currents swirling round inside it each time the magnetism changed (eddy currents), heating it and slowing the change. A bundle of thin iron wires, each lightly varnished or rusted so they are insulated from each other, stops those currents. The same idea — thin, separated iron — is used in every The Transformer and AC The Electric Motor.

How high a voltage?

Very roughly, a spark in dry air needs 10,000–30,000 V for each centimetre of gap, the lower figure for long sparks between points. A small coil with 1.5–3 km of fine wire on its secondary gives sparks of 1–3 cm. The great coils of the 1870s, with hundreds of kilometres of wire, threw sparks over a metre long.

What you need

Part Specification Notes
Core Soft iron wire 0.5–1 mm thick, cut to 25 cm, enough to make a bundle 2.5 cm across (about 500–1,000 pieces) Iron (the Bloomery), Copper Wire for drawing; anneal, then varnish or rust lightly
Primary wire 30–40 m of 1.5 mm covered copper wire Copper Wire
Insulating tube 3–5 mm wall, 20 cm long, sliding over the primary Glass tube (Glass), split mica built up in layers, or paper soaked in shellac
Secondary wire 1.5–3 km of the finest covered wire you can draw — 0.15–0.2 mm, silk-covered Copper Wire, Silk — the hard part
Insulating discs 10–15 rings of waxed card, mica or shellacked paper, 1 mm thick Between the secondary sections
Wax 2–3 kg: beeswax with a third its weight of pine resin (rosin) Beekeeping, Tar, Pitch and Glue
Condenser 40–60 sheets of thin tin foil, 10 × 15 cm, and twice as many sheets of thin paper Tin and Pewter, Paper
Interrupter Steel spring strip 1 mm × 1 cm × 8 cm; soft iron head 2 cm across; contact screw Springs, Steel
Contact tips Platinum, or silver Gold and Silver; The Light Bulb on platinum
Battery 6–12 V able to give 3–5 A 3–6 lead-acid cells
Wood Base box, end cheeks Dry hardwood, boiled in wax (Basic Woodworking)

Where to find it

All the metals and materials come from earlier chapters. Mica is worth finding: a mineral that splits into thin, clear, flexible sheets, found as shiny "books" in granite, pegmatite veins and schist (Rocks and Minerals). It is one of the best high-voltage insulators there is, and survives heat. Silk for covering fine wire is far better than cotton: thinner, smoother and a better insulator (Silk).

Step 1: The core and primary

  1. Cut the core wires to 25 cm. Anneal them in a closed iron pipe in the fire (bright red, then cool slowly in ash). Dip them in thin shellac or let them rust lightly in damp air for a day, so each wire has an insulating skin.
  2. Bundle them tightly into a round rod 2.5 cm across. Bind it with thread every few centimetres and soak it in shellac.
  3. Wrap the core in three or four layers of shellacked paper.
  4. Wind the primary: two layers of 1.5 mm covered wire along 20 cm of the core, leaving the core sticking out 2.5 cm at each end. That is about 120–130 turns per layer, 240–260 in all. Put a layer of shellacked paper between the two layers. Bring both ends out at the same end of the coil. Varnish.

Step 2: The insulating tube

The secondary will carry tens of thousands of volts; the primary a few. Between them must be the best insulation you can make — this is where most homemade coils fail.

  1. Slide the primary into a glass tube with walls 3–5 mm thick, or build a tube on it from 30–40 layers of thin paper, each brushed with hot shellac, rolled tight and dried; or interleave thin sheets of mica with shellacked paper. The tube must reach at least 3 cm beyond the secondary at each end — sparks creep along surfaces.

Step 3: The secondary — in sections

Wound as one long coil, the turns at the two ends of each layer would be thousands of volts apart and only a sheet of paper apart. Instead, the secondary is wound as many thin flat sections ("pies"), each holding only a small part of the total voltage.

Iron corebundle of varnishedsoft iron wires Iron headon a steel spring Contactscrew with aplatinum orsilver tip Primary2 layers of thick wire, 1.5–2 mm Secondarymany thousands of turnsof fine wire, wound inthin sections Insulating tubeglass, mica or waxedpaper, 3–5 mm wall all soaked inwax and resin Spark gapknobs on glass pillars Condenserfoil and waxedpaper, in the base
Fig. 2 The induction coil in cross-section. The core is a bundle of iron wires. The primary lies directly on it, inside a thick insulating tube. The secondary is wound in thin sections separated by insulating discs, and everything is soaked in wax. The interrupter's iron head sits just off the end of the core; the condenser lies in the base.
  1. Make a winding jig: a wooden spindle the size of the insulating tube, with two removable cheeks clamped about 6 mm apart. Turn it with a crank or on a The Lathe, with the wire running from its bobbin through a pad of felt soaked in melted wax.
  2. Wind each section full to an outside diameter of about 7 cm. Count turns and wind every section the same way round. Each section holds roughly 1,000–1,500 turns of 0.2 mm wire, about 200 m. Make 10–15 sections.
  3. Soak each section in melted wax (beeswax with a third its weight of rosin) at about 100 °C until it stops bubbling — the bubbles are air and moisture coming out. Lift it out, let it set, and slide it off the jig.
  4. Test each section for a break with a cell and galvanometer (Measuring Electricity) before going on. A break inside a finished coil cannot be mended.
  5. Stack the sections on the insulating tube with an insulating disc between each pair. Join them so that the current goes round all of them the same way: the inside end of one to the inside end of the next, then outside to outside, alternately — because each section is turned over relative to its neighbour. Solder each joint, tuck it into the disc gap, and cover it with wax.
  6. Bring the two free ends out to the secondary terminals at the top — brass knobs on glass or waxed wooden pillars, as far from everything else as possible.
  7. Seal it all. Pour melted wax over and around the whole secondary until it is buried, or set the coil in a box and fill it with wax. Let it cool slowly so the wax does not crack.

Step 4: The condenser

  1. Stack sheets of thin tin foil 10 × 15 cm with two sheets of thin waxed paper between each pair. Let each foil stick out 2 cm beyond the paper — odd-numbered sheets to the left, even-numbered sheets to the right. Clamp the stack and press the protruding foils at each side together into a terminal strip.
  2. Soak the whole stack in melted wax, press it flat while warm, and fit it in the base box.
  3. Begin with about 40 foil sheets. When the coil is running, try more and fewer: the right condenser gives the longest spark and the least sparking at the contact.

Step 5: The interrupter

  1. Fix the steel spring upright on the base at the primary end, so that its iron head sits 2–3 mm from the end of the core.
  2. Rivet a small piece of platinum (or silver) onto the back of the spring, about halfway up.
  3. Mount a brass pillar behind the spring with an adjusting screw tipped with platinum or silver, which touches the spring's contact when the spring is at rest. Fit a lock nut.
  4. Wire it (see the circuit drawing): battery → switch → contact screw → spring → primary → back to the battery. Connect the condenser across the contact — one side to the screw pillar, the other to the spring.

Step 6: Running it

  1. Set the spark gap to about 5 mm. Close the switch. The interrupter should buzz and sparks jump the gap.
  2. Adjust the screw: turn it until the buzz is crisp and steady and the spark strongest. Tighter = slower, heavier current; looser = faster, lighter.
  3. Widen the gap a millimetre at a time to find the coil's longest spark. Do not keep it running at its longest spark: if the spark cannot jump outside, it will find a path inside through the insulation. Work at about two-thirds of the maximum.

Tip Big coils. For coils larger than about 5 cm of spark, the hammer interrupter is too slow and burns its contacts. 19th-century workers used a motor-driven mercury interrupter (a rotating jet of mercury striking metal vanes) or the electrolytic interrupter (a platinum point in dilute sulfuric acid, which makes and breaks hundreds of times a second by itself). Both are dangerous — mercury vapour and acid — and best left until you have the experience.

What to do with it

  • Vacuum testing. Seal a wire into each end of a glass tube, connect it to your pump (The Vacuum Pump) and to the coil. At ordinary air pressure, nothing. As the pump works: thin purple threads; then the whole tube fills with pink-violet glow; then the glow breaks into bands; then the tube goes dark and the glass at the positive end glows green — the vacuum is now good enough for a The Light Bulb filament and for X-rays. Beyond that, the coil can no longer push current through at all.
  • Radio. A spark gap between two metal rods or plates, fed by the coil, sends out radio waves. A simple receiver can detect them across a room — and with tall aerials, much further (Radio).
  • Ignition. A small coil (1 cm spark is plenty) with a spark plug — two wires a millimetre apart, sealed through a ceramic plug — fires the fuel–air mixture in a gas or petrol engine (The Internal Combustion Engine, Gas Engines and Producer Gas).
  • Lighting gas lamps and testing insulators, cables and glassware for hidden cracks: a crack lights up when the spark finds it.

How to tell it worked

  • The interrupter buzzes steadily and the contact makes only a small spark. A large, fat spark at the contact means the condenser is missing, too small, or broken down.
  • The secondary gives a thin, crackling, blue-white spark of 1–3 cm between points. Between a point and a plate the spark is longer from the point when it is positive; this tells you which terminal is which.
  • The coil stays cool and silent inside — no hissing, crackling or smell of burning wax from within.

Note Troubleshooting. No buzz → the contact is not closing, the battery is flat, or the head is too far from the core. Adjust the screw; check the battery. Buzzes, no spark at the gap → a break in the secondary (test each half with the galvanometer), or the gap is too wide. Spark weak, contact sparks heavily → condenser faulty or disconnected. Check it with a cell and galvanometer: a good condenser gives a single kick, then nothing; a leaking one passes current steadily. Spark gets shorter over minutes, crackling inside → the insulation is breaking down between sections or between secondary and primary. Usually it must be rewound. Make the tube thicker and the sections thinner. Contacts weld or blacken → too much primary current, or silver/copper tips instead of platinum. File them clean and flat; reduce the battery.

Dangers

Danger High voltage. The secondary gives tens of thousands of volts. From a small coil the shock is violent and painful but the current is small; from a large coil, or any coil connected to Leyden jars or a condenser on the secondary side, it can burn deeply and stop the heart. Never touch the secondary terminals or anything connected to them while the coil runs. Switch off and touch the terminals together with an insulated wire before handling. Never give shocks to people or animals. Keep one hand behind your back when adjusting a running coil.

Danger X-rays are invisible and destroy flesh. A vacuum tube driven by a coil can give off X-rays once the vacuum is good — even when you are only testing a pump. Early X-ray workers suffered burns, lost fingers and hands, and died of cancer. Stand at least 2–3 m away from any glowing tube when the glass fluoresces green, keep the tube behind a sheet of lead, run it only for seconds, and never put your hand between a tube and a screen. See X-Rays.

  • Fire. Sparks ignite hydrogen, solvent vapour, gas and dust. Keep the coil away from charging batteries (The Rechargeable Battery) and flammable liquids.
  • Bad air. Long running in a closed room fills it with ozone and nitrogen oxides — a sharp, "electric" smell that irritates the lungs. Air the room.
  • The primary kick. Opening the primary circuit by hand gives a sharp shock across your fingers (The Electromagnet). Always use the switch.
  • Radio interference. A spark coil sends out radio noise over a wide band. Once others use Radio, run spark coils only shielded, or briefly (Interference, Screening and Earthing).
  • Hot wax causes deep burns, and wax heated too far catches fire. Melt it in a pot standing in hot water, never over an open flame.

What this unlocks

How it was first done

In 1836 Nicholas Callan, a priest and professor at Maynooth College in Ireland, wound a long secondary of fine wire over a primary on an iron core, interrupted the primary with a rocking wire dipping in mercury, and got shocks strong enough to be dangerous. In the same year Charles Grafton Page in the United States built a similar coil. Heinrich Ruhmkorff, a German instrument maker in Paris, made carefully insulated coils for sale from 1851 and gave the instrument its common name; Armand Fizeau added the condenser across the contact in 1853. In 1876–77 the London instrument maker Alfred Apps built a giant coil with about 450 km of secondary wire that threw sparks 107 cm long. Étienne Lenoir used a Ruhmkorff coil to fire his gas engine in 1860, and trembler coils were still firing the Ford Model T's engine in the 1920s. Heinrich Hertz used an induction coil to make and detect radio waves in 1886–88; Wilhelm Röntgen discovered X-rays with one in November 1895; and Guglielmo Marconi's first radio transmitters of 1895–1901 were induction coils and spark gaps.

Source: content/entries/electricity/induction-coil.md