Part 13 · Electricity
Arc Lamps, Neon and Fluorescent Lights
Light made by electricity passing through a gas rather than a hot wire. The self-feeding carbon arc lamp and the searchlight; neon tubes, signs and glow lamps; the blue-green mercury lamp and the yellow sodium street lamp; and the fluorescent tube, whose phosphor turns invisible ultraviolet into white light at five times the efficiency of a filament bulb. Light-emitting diodes are covered in outline.
- Difficulty
- ●●●●●
- Time
- Two weeks for a self-feeding arc lamp; a month to set up for neon tubes; many months to a first fluorescent tube
- Steps from zero
- 30 prerequisites →
This unlocks
—The full path from nothing — 30 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- The Kiln
- Pottery
- Charcoal
- Hides and Leather
- Lime
- Mercury
- Lye and Potash
- Fermentation
- The Wheel and Axle
- Glass
- Bellows
- The Lathe
- Copper Smelting
- Iron (the Bloomery)
- Laboratory Glassware
- Pumps
- Blacksmithing
- The Battery
- The Vacuum Pump
- The Light Bulb
- Copper Wire
- The Electromagnet
- The Induction Coil
- Arc Lamps, Neon and Fluorescent Lights
Do them roughly in this order. See it on the tech tree →
Why it matters
A filament bulb (The Light Bulb) turns only about 1 % of its electricity into light. The rest is heat. Make the electricity flow through a gas instead and much more of it becomes light. The lamps in this chapter light streets, factories, ships' decks, shop signs and every office of the twentieth century, for a fraction of the power.
| Lamp | Light per watt, compared with a carbon filament bulb |
|---|---|
| Carbon filament bulb | 1 (about 3 lumens per watt) |
| Tungsten filament bulb | 4 |
| Open carbon arc | 3–5 |
| Flame arc | 8–12 |
| Low-pressure mercury tube | 5–8 |
| High-pressure mercury lamp | 13–18 |
| Fluorescent tube | 20–30 |
| Low-pressure sodium lamp | 50–60 |
| White LED | 30–60 |
The easiest route is the arc lamp, which needs no vacuum. Next comes the neon tube, which needs a vacuum pump and high voltage. The fluorescent tube adds special powders and good chemistry. Sodium lamps and LEDs need a full industry.
How it works
A gas at ordinary pressure does not conduct. But if the voltage is high enough, or the gas is thin enough, a few stray electrons get pulled so fast that they knock electrons off gas atoms. Those freed electrons knock off more, in an avalanche. The gas becomes a conductor. Each time a fast electron jolts an atom without breaking it, the atom gives the energy back as a flash of light of its own colour. Neon gives red-orange, mercury gives blue-green plus a great deal of invisible ultraviolet, and sodium gives yellow.
Two facts govern every lamp here:
- A discharge has "negative resistance". The more current flows, the more the gas is broken up and the easier it conducts. On its own it runs away until a fuse blows. Every gas lamp needs a ballast in series to hold the current down: a resistor, or with alternating current a choke (a coil on an iron core), which wastes much less power.
- Starting needs more voltage than running. A neon tube may need 3,000 V to strike and 1,500 V to run. An arc lamp starts with its rods touching, and a fluorescent tube is kicked into life by a brief high-voltage pulse.
The self-feeding arc lamp
The Light Bulb shows how to make carbon rods and a hand-fed arc. For lasting light you need a lamp that feeds its own carbons.
The clutch lamp (Charles Brush, 1878) is the easiest to build.
- The carbon holder. The upper carbon is clamped in a brass rod 6–8 mm thick, 30–40 cm long, that slides freely down through a guide tube. The lower carbon is fixed.
- The clutch. A flat iron washer with a hole 1 mm bigger than the rod surrounds the rod. When one side of it is lifted, it tilts and grips the rod. A stop below the washer levels it again when it drops, and then the rod slides through.
- The lifting magnet. A coil of 30–60 turns of thick wire (3 mm, see Copper Wire) round an iron plunger, connected in series with the arc. The plunger lifts one side of the washer (The Electromagnet).
- How it runs. At switch-on the carbons touch, a large current flows, the coil pulls, and the clutch grips and lifts the rod 2–3 mm. That strikes the arc. As the carbons burn, the gap widens, the current falls, and the coil weakens. The washer settles onto its stop, and the rod slips down a fraction of a millimetre until the current rises again. The lamp feeds itself in tiny steps for as long as the carbons last.
- Adjust the coil's pull with a spring or a counterweight on the plunger, so it holds a gap of 2–4 mm at your chosen current.
A dashpot (a small piston in a cylinder of oil or air) on the plunger stops the lamp hunting up and down. The differential lamp (Hefner-Alteneck at Siemens, 1879) adds a second coil of thin wire across the arc. The voltage coil pulls the carbons together as the gap grows, while the current coil pulls them apart. Because the balance does not depend on the current, many lamps can run on one circuit.
Running them. An open arc runs at about 45–50 V on direct current, or 30–35 V on alternating current, at 5–10 A.
- On a 100–110 V supply, run two lamps in series with a small resistance of iron wire, or one lamp with a resistance that drops the other 55–60 V.
- Series street lighting. One dynamo built to give a constant current of about 10 A runs dozens of lamps in a chain, at 50 V each. Each lamp needs an automatic switch that shorts it out if its carbons break, or the whole street goes dark. Forty lamps make about 2,000 V. That is deadly, and needs the insulation of The Transformer and Wiring and Electrical Safety.
Better arcs.
- Enclosed arc. A small, nearly airtight inner globe round the arc soon uses up its oxygen. Then the carbons burn slowly, about 100–150 hours instead of 8–16. It runs at about 80 V and 5 A.
- Cored carbons. A rod with a 2–3 mm core of softer carbon keeps the arc centred and steady.
- Flame arc. Carbons cored with fluorite (calcium fluoride) or other salts fill the arc with glowing vapour. It gives a yellow-orange light two to three times brighter for the power, but it makes white fumes and needs a chimney.
Good or bad? A good lamp burns silently or with a soft hum, steady, with no hissing. Hissing and a flickering violet edge mean too much current for the carbon size. Use thicker carbons or more ballast.
The searchlight
A searchlight puts an arc at the focus of a large curved mirror (Mirrors). The tiny white-hot crater of the positive carbon is the brightest light you can make. A mirror 60 cm across gathers it into a beam that is narrow and very long.
- Carbons. The positive carbon lies along the axis with its crater facing the mirror, exactly at the focus. The negative carbon comes in at an angle from below. Use direct current, which forms a deep crater, at 30–100 A for a mirror of 60–90 cm. Feed the carbons with a screw, or with a regulator as above.
- Mirror. A glass or speculum mirror ground to a parabola (The Telescope shows how), silvered on its back or front. The Mangin mirror (1874) is easier: a thick glass dish whose two faces are ground as plain spherical curves of different radii, silvered on the back. The glass bends the light just enough to give a parallel beam. The focal length is about 0.4 times the diameter.
- Drum. A sheet-iron drum with a chimney for the hot gas, a front door of thin glass strips (a single big sheet cracks with the heat), and a cradle that turns and tilts on bearings.
- Shutter. A set of louvres in front lets you flash the beam for signalling (Signal Fires, Flags, Semaphore and Heliographs).
The beam's brightness depends on the crater's brightness times the mirror area. A bigger mirror, not a bigger arc, throws farther. A good searchlight throws a crisp disc onto a cloud base and lights a ship several kilometres away on a clear night.
Neon lamps and signs
Liquid Air, Nitrogen and the Noble Gases explains how to get neon and how a simple neon tube is filled. Here is how a sign maker works.
- Glass. Soft soda or lead glass tubing, 8–15 mm across, with walls about 1 mm thick (Laboratory Glassware, Glass).
- Bend the letters. Draw the design full size and mirror-reversed on a heat-proof sheet, since you work from the back. Heat 5–10 cm of tube over a ribbon burner, a pipe with a row of small gas flames 20–30 cm long (Lanterns, Gas Lamps and Lighters). Bend it to the pattern while blowing very gently through a rubber hose on one end. The blowing keeps the bend round, not flattened. Join lengths by melting their ends together.
- Electrodes. At each end, seal on a glass sleeve holding a cup of iron or nickel, 10 mm across and 30–40 mm long, welded to a lead-in wire through the glass (The Light Bulb covers the glass-to-metal seal).
- Pump and bombard. Connect the tube to the pump (The Vacuum Pump). With the air thin, pass a heavy current (about 0.5 A) through the tube for a minute or two. This heats the glass until a scrap of paper laid on it scorches (about 250 °C), and makes the electrodes glow red. It drives out the gas that is hidden in the glass and metal. Pump hard while it cools.
- Fill and seal. Let in pure neon to about 5–15 mbar, less for wide tubes and more for narrow ones. Melt the filling tube shut.
- Age it by running it for a few hours, until the colour is even.
Colours. Neon gives red-orange. Argon with a drop of Mercury gives blue, and through yellow glass, green. Helium gives a pinkish white. Other colours come from coloured glass, or from phosphors inside the tube (see the fluorescent lamp below).
Power. A 12 mm neon tube needs about 1,000 V for each metre of length, plus a few hundred volts more for the electrodes, at 20–30 mA. A neon sign transformer does this: a The Transformer with iron shunts between its coils that leak away magnetism, so its current cannot rise past the limit. An The Induction Coil lights short test tubes.
The neon glow lamp. A tiny bulb with two wires 1–2 mm apart, filled with neon at a higher pressure. It lights at 70–90 V with a soft orange glow, and needs only about 1 milliamp through a series resistor of 100,000–220,000 ohms on a 230 V supply (Resistors, Capacitors and Coils). It makes a pilot light, a mains tester (Measuring Electricity) and a simple oscillator.
Good or bad? A good tube lights instantly and evenly, with no flicker, and stays the same colour for years. A pink or white glow means air got in. Dark ends or blackened glass by the electrodes mean poor bombarding.
Mercury and sodium street lamps
The low-pressure mercury tube
Peter Cooper Hewitt's lamp (1901) is the mercury lamp you can build with a mercury pump. Use a glass tube 25 mm across and 1 m long, sloping slightly. It has an iron anode at the upper end and a pool of mercury as the cathode in a bulb at the lower end. Pump it hard and seal it, with mercury vapour and nothing else. Run it on direct current through a resistance and a choke, at about 3 A and 70–80 V across the tube. To start it, tilt it so that a thread of mercury briefly runs from end to end, then tip it back. The breaking thread strikes the discharge.
Its blue-green light has almost no red, which makes faces look ghastly. But it gives five or more times the light of a carbon-filament bulb for the power, and it is steady and shadowless. It was ideal for factories and for blue-sensitive photographic plates (Photography).
The high-pressure mercury lamp
This is the bluish-white street lamp of the 1930s–1990s. Its arc runs inside a small tube of fused quartz (1–2 cm across, 3–10 cm long), with a few milligrams of mercury and a little argon. Once the lamp warms up, the mercury pressure rises to several atmospheres. That makes the light whiter and the lamp two to three times as efficient as the low-pressure tube. It needs electrodes coated to give off electrons, a small starting electrode, a choke, and an outer glass bulb to block ultraviolet. It takes 4–5 minutes to warm up, and cannot restart while hot. Quartz softens only at about 1,700 °C and must be worked in an oxygen–hydrogen flame (Hydrogen, Oxygen and Gases, Fused Quartz and Halogen Lamps). Treat this lamp as a goal for a well-equipped glassworks.
The sodium lamp
The low-pressure sodium lamp (Philips, 1932) is the most efficient lamp ever made for seeing at night, but its pure yellow light makes every colour look the same. It needs sodium metal, made by electrolysis of molten salt or caustic soda (Electrolysis), and special glass, because sodium vapour eats ordinary glass brown within hours. The tube is lined with a borate glass that resists it. The U-shaped discharge tube sits inside an evacuated outer jacket (The Vacuum Pump) that keeps it at about 260 °C. It starts in neon with a red glow, and over about 10 minutes the yellow takes over. Build it only after you have mastered fluorescent tubes.
The fluorescent lamp
A fluorescent tube is a low-pressure mercury discharge whose ultraviolet strikes a phosphor: a white powder on the inside of the glass that glows when ultraviolet hits it. Most of the mercury's energy comes out as invisible ultraviolet. The phosphor turns it into visible light.
The tube. A common size is 1.2 m long and 26–38 mm across, rated 36–40 W. It holds a few milligrams of mercury and argon at about 3 mbar. The tube works best when its wall is about 40 °C.
Phosphors
| Phosphor | Glows | Made from |
|---|---|---|
| Calcium tungstate | Blue | Wolframite ore turned into sodium tungstate, then precipitated with a calcium salt |
| Zinc silicate with about 1 % manganese (artificial willemite) | Green | Zinc oxide, pure silica, a little manganese |
| Calcium halophosphate with antimony and manganese | Warm white, all in one | Calcium phosphate (bone ash or rock phosphate, see Chemical Fertilisers), fluorite, a little calcium chloride, about 1 % antimony oxide and 1 % manganese |
- Purity is everything. A few parts per million of iron, copper or nickel kill the glow. Use the purest chemicals you can make (Identifying Substances). Grind them with flint or porcelain balls, never iron, and fire in clean silica or porcelain crucibles.
- Fire the mixed powders in a covered crucible at 1,000–1,200 °C for one to two hours (The Kiln). Cool, crush gently and sieve.
- Test each batch in the dark under the light of a bare low-pressure mercury tube. A good phosphor glows brightly. A dull or blotchy glow means impurity or wrong firing.
- Coat the tube. Grind the phosphor in a ball mill until it is finer than flour. Stir it into a thin varnish of nitrocellulose in solvent (Early Plastics, Ether, Acetone and Solvents). Pour it through the upright tube and let it drain, leaving an even white film. Dry it with warm air, then bake the tube at about 550 °C to burn off the varnish.
Electrodes, filling and sealing
Each end has a filament of coiled tungsten wire (Alloy and Stainless Steels covers tungsten ore). It is coated with a paste of barium, strontium and calcium carbonates, which turn into oxides when heated in the vacuum and then give off electrons easily. Seal the electrode stems into the tube ends. Pump the tube while baking it at about 400 °C. Heat the filaments with current to activate them. Add the mercury, fill with argon, and seal. Cement on end caps with two pins at each end.
Without tungsten, make a cold-cathode tube instead. It is a neon-sign tube filled with argon and mercury, coated with phosphor and driven by a sign transformer. It is less efficient, but it lasts very long and needs no filaments. This is the most realistic first fluorescent lamp.
The choke and starter
- The choke is a coil of insulated wire on a laminated iron core with a small air gap (The Transformer). For a 40 W tube on 230 V at 50 Hz it needs about 1.5 henry and must pass 0.43 A without overheating. Adjust the gap until a test tube draws the right current, measured with an ammeter (Measuring Electricity).
- The glow starter is a small glass bulb of neon or argon with two electrodes, one of them a U-shaped bimetal strip (two metals rolled together that bend when warmed). At switch-on, a glow forms in the bulb and heats the strip. The strip bends and touches the other electrode, so current flows through both tube filaments and heats them. With the glow gone, the strip cools in a second or two and springs open. Breaking the current through the choke gives a kick of 800–1,000 V, which strikes the tube. Once the tube is lit, the voltage across it, about 100 V, is too low to restart the glow, so the starter stays idle.
- Without a starter, use a push button in its place. Hold it for 2 seconds, then let go.
- A small capacitor (about 0.005 µF) across the starter quietens radio interference. A larger one (about 4.5 µF) across the supply saves current in the wires (Wiring and Electrical Safety).
Good or bad? A good lamp lights within 1–3 seconds, without blinking, gives an even white light, and has no dark ends. Blackened ends mean the filaments are wearing out or the starter is faulty.
LEDs in outline
A light-emitting diode is a junction between two kinds of semiconductor (Semiconductors and the Transistor). When electrons cross it and drop into "holes", each gives out a flash of light. The colour depends on the crystal. You can see the effect yourself. A carborundum (silicon carbide) crystal, touched by a fine wire as in a crystal detector, glows faintly yellow-green in a dark room with 10–30 V across it through a resistor. H. J. Round saw this in 1907. Practical LEDs need near-perfect layered crystals of gallium compounds. A blue LED coated with a yellow phosphor gives white. An LED lamp runs each diode at about 3 V and a carefully limited current. It needs the semiconductor industry of Integrated Circuits, so it is a target, not a first project; Light-Emitting Diodes covers how they are made and driven.
How to tell it worked
Each lamp above has its own test. In general, a good gas lamp starts by itself, burns steadily for hours unattended, and its ballast or transformer stays only warm.
Note Troubleshooting. Arc lamp pumps up and down → no damping; add a dashpot or a heavier counterweight. Arc goes out with a snap → carbons stuck in the guide or burned out; clean the guide and check the clutch. Neon tube flickers at one end → electrode poorly bombarded or gas impure. Re-pump. Fluorescent tube glows at the ends but will not strike → choke too weak, starter stuck closed, or the tube too cold. Tube blinks on and off → starter worn out; or the supply voltage is low. Phosphor glows dull and patchy → iron contamination, or the binder was not fully burned off.
Dangers
Danger High voltage kills. Neon transformers (up to 15,000 V), series arc circuits (thousands of volts) and fluorescent kicks can all kill or burn. Switch off and discharge before touching. Mount sign transformers in earthed metal boxes, and keep high-voltage wiring on glass or porcelain insulators, far from wood (Wiring and Electrical Safety).
Danger Ultraviolet burns the eyes. Arcs, bare mercury tubes and quartz lamps give off ultraviolet that causes painful "arc eye" within minutes and can burn skin. Look at them only through dark welding glass (Welding). Always enclose them in ordinary glass, which blocks most of it.
- Mercury vapour is a cumulative poison (Mercury). Work with it in a well-aired place, keep it off hot surfaces, and gather spills; do not sweep them.
- Sodium metal burns fiercely and reacts violently with water. Keep it under oil.
- Glass. Tubes under vacuum burst inward and throw slivers. Wear eye protection when handling them.
What this unlocks
Arc lamps light streets, harbours and film projectors (Photography), and searchlights guide ships (Harbours and Lighthouses). The gas discharge leads straight to rectifier valves (The Vacuum Tube, Rectifiers: Turning AC into DC), to the The Spectroscope and to X-ray tubes (X-Rays). Phosphor-making leads to the screens of Cathode Rays and Television and radar. The diode light leads into the Semiconductors and the Transistor industry.
How it was first done
Humphry Davy showed a carbon arc from a huge battery at the Royal Institution in about 1808. Pavel Yablochkov's electric candles lit the Avenue de l'Opéra in Paris in 1878, and Charles Brush's clutch lamps and constant-current dynamos lit the public square of Cleveland, Ohio, in 1879. Heinrich Geissler made glowing gas tubes from 1857. Peter Cooper Hewitt sold his mercury lamp from 1901. Georges Claude in France showed neon tubes in 1910 and sold the first neon signs in 1912. Low-pressure sodium lamps were first used to light a road in the Netherlands in 1932, and high-pressure mercury lamps in Britain the same year. Fluorescent tubes went on sale in 1938, and the halophosphate phosphor (A. H. McKeag, 1942) made them cheap and white. H. J. Round saw light from carborundum in 1907. Oleg Losev studied it in the 1920s. Nick Holonyak made the first practical red LED in 1962. Shuji Nakamura and others made the bright blue LED in the early 1990s, and that made white LED lighting possible.
Source: content/entries/electricity/arc-and-discharge-lamps.md