Part 6 · Building
Foundations and Floors
How to read the ground before you build, dig and lay footings that will not sink, heave or crack, keep damp out of walls with drains and damp-proof courses, and make floors of beaten earth, stone flags, timber or lime.
- Difficulty
- ●●●●●
- Time
- A few days to a few weeks of digging and laying for a house; an earth floor takes a month to dry
- Steps from zero
- 9 prerequisites →
You need first
Stone MasonryThis unlocks
—The full path from nothing — 9 steps before this one
- Stone Tools
- Fire
- Finding and Preparing Clay
- Simple Machines
- Quarrying and Cutting Stone
- The Kiln
- Lime
- Mortar and Concrete
- Stone Masonry
- Foundations and Floors
Do them roughly in this order. See it on the tech tree →
Why it matters
A building is only as good as what it stands on. If the ground under one corner gives way, the walls crack, doors jam and arches split. If the ground freezes and swells, it lifts the walls and drops them again every winter. If water soaks up from below, timber rots, earth walls slump (Cob, Adobe and Rammed Earth), and the house is cold and damp for ever. Almost every serious failure of an old building starts below ground or at ground level.
The work is not glamorous — digging, carrying stone, laying gravel — but a day spent on the foundation saves a year of repairs. This chapter covers reading the ground, the footings that suit each kind of ground, keeping the building dry, and the floor you will walk on.
How it works
Spreading the load. A wall presses down on the soil under it. Every soil can carry only so much weight per square metre before it squeezes out sideways and the wall sinks. The answer is to make the base of the wall wider than the wall — a footing — so the same weight is spread over more ground.
| Ground | Safe load, roughly (tonnes per m²) | How to recognise it |
|---|---|---|
| Solid rock | 100 and more | Needs a pick or bar; rings when struck |
| Dense gravel, or dense sand and gravel | 20–60 | Hard to dig even with a pick; does not ooze water |
| Stiff clay | 15–30 | A thumb dents it only with great effort |
| Firm clay | 8–15 | A thumb pushes in with moderate effort |
| Soft clay, loose sand | under 8 | Easily moulded by hand; a boot sinks in |
| Peat, made ground, rubbish, organic mud | Unsuitable | Black or brown, spongy, smells, full of plant remains |
A worked example. A stone wall 50 cm thick and 5 m high weighs about 5.5 tonnes per metre of its length (stone walls weigh about 2.2 tonnes per cubic metre). Add the share of floor and roof — say 1.5 tonnes — and each metre of wall puts 7 tonnes on the ground. On firm clay that safely carries 10 tonnes per m², the footing must be at least 7 ÷ 10 = 0.7 m wide. On dense gravel, the wall's own width is almost enough. On soft clay you need a footing well over a metre wide — or a better site.
Frost heave. Water in the soil swells by about 9% when it freezes, and wet clay or silt can grow ice lenses that lift a footing several centimetres. Each spring it drops back unevenly, and the walls crack. Footings must go below the depth the ground freezes — or the ground under them must be kept free of water.
Shrinking clay. Some clays shrink as they dry and swell when wet; in a dry summer they open cracks you can put your hand in. Go deeper on such clays (1 m or more), where the moisture is steadier, and keep thirsty trees (willow, poplar, oak, eucalyptus) at least their own mature height away from the walls.
Rising damp. Porous stone, brick and earth suck water up from the ground like a lamp wick, often up to a metre. A damp-proof course — a layer that water cannot climb through — stops it.
Reading the ground
Before you choose a site, walk it in wet weather and dry.
- Avoid hollows and flood marks. Look for debris lines on tree trunks and banks, silt on grass, and ask anyone who knows the place. Build above the highest flood you know of.
- Wet-ground plants — rushes, sedges, reeds, horsetail, moss on open ground — mean water near the surface. Springs and seeps on a slope mean water will find your walls.
- Unstable slopes. Trees with curved, J-shaped trunks, cracks in the turf, bulges at the foot of a slope, or terraces that look slumped mean the hillside is creeping. Do not build on it or just below it.
- Made ground. Old pits, ditches, rubbish dumps and ruins filled with loose material settle for decades. Dig through them to natural ground.
- Dig trial pits. At each corner of the planned building dig a pit about 1.2–1.5 m deep. Look at the layers, feel each with your thumb (table above), and note where it changes. Leave the pits open for a day: water seeping in and standing in the bottom tells you the water table — the level of ground water. Footings below it are hard to build and to keep dry.
- The probe. A pointed iron bar (or a fire-hardened stake) driven with a heavy mallet goes in easily through soft ground and stops on firm ground or rock. Probe across the site to find soft patches between your pits.
What you need
| Item | Notes |
|---|---|
| Picks, mattocks, spades, baskets or barrows | Most of the work is digging and carrying |
| Large flat stones | For the footing: the biggest you can handle, at least as thick as a hand |
| Clean gravel and rubble | For drains, rubble trenches and floor bases; washed, no soil |
| Lime mortar or lime concrete | Lime, Mortar and Concrete |
| Damp-proof material | Slate, dense stone, tar or bitumen, birch bark |
| Rammer, string lines, pegs, levels | Cob, Adobe and Rammed Earth, Measurement from Scratch |
Footings
Strip footings in a trench
This is the standard foundation for stone, brick and earth walls.
- Lay out the building with pegs and string, squaring the corners with a 3–4–5 rope and checking the diagonals are equal (Measurement from Scratch).
- Dig the trench down through topsoil to firm natural subsoil — at least 50–60 cm, and below frost depth: 45–60 cm where winters are mild, 1–1.5 m or more where the ground freezes hard. Local graves, wells and old cellars show how deep frost reaches; or dig in late winter to see. The trench is at least the footing width (from the table and example above) — usually about twice the wall thickness.
- Level the bottom. Cut it flat and level, removing any loose soil. On a slope, step it: each step level, no higher than the thickness of a footing course, with the course above overlapping the step by at least its own height.
- Lay the footing. Bed the largest, flattest stones in lime mortar across the full width of the trench, long sides across the trench, with joints broken as in Stone Masonry. Build up in two or three spread courses, each a little narrower than the one below, until you reach the wall width just below ground.
- Lime concrete works well instead of stone in the trench: 1 part lime putty to 2 parts sand to 4–5 parts broken stone or gravel, with crushed brick or volcanic ash added as a pozzolan (Mortar and Concrete). Lay it in layers 15–20 cm thick and ram each layer hard. Let it harden for a week or two before building on it.
- Carry up the plinth. Continue in stone or fired brick at least 30 cm above ground for timber and brick walls, 45 cm for earth walls.
- Damp-proof course on top of the plinth (below).
Rubble trench footing
Where frost is deep and stone is scarce, a trench filled with clean stone works because it drains: no water stays in it, so there is nothing to freeze.
- Dig the trench below frost depth, 40–60 cm wide, with its bottom sloping about 1 cm per metre toward a low outlet: open daylight on a slope, a ditch, or a soakaway.
- Lay a drain along the bottom — clay pipes (Tiles and Clay Pipes) with small gaps between them, or a channel of flat stones — and fill the trench with clean, washed stone 2–5 cm in size, rammed in layers.
- Build a footing course of large stones or lime concrete on top, at ground level, and the plinth on that.
Pads and piers for timber buildings
A timber frame or log house stands on its posts or sill corners. Dig a pit 60 cm square to firm subsoil (and below frost), ram 15 cm of gravel in the bottom, and set a big flat stone or a built pier of stones in lime mortar, its top at least 30 cm above ground. Put a damp-proof layer of slate or birch bark between stone and wood. Granaries stand on staddle stones — mushroom-shaped piers that rats cannot climb (Granaries and Food Storage).
Very soft or wet ground
Avoid it if you can. If you cannot: drive piles — straight logs of oak, elm, alder or larch, sharpened and driven with a heavy drop weight (Cranes and Lifting) until they stop sinking — close together under the wall, then lay a timber grillage or stone footing across their heads. Wood that is always underwater does not rot; wood that is wet and dry by turns rots in a few years, so cut the piles off below the lowest water level.
Keeping out damp
The damp-proof course goes on top of the plinth, above splash height and below the floor timbers and the wall proper.
- Slate: two layers of slates bedded in mortar, the second layer covering the joints of the first. The best low-tech damp-proof course.
- Dense stone: a course of granite, basalt or other non-porous stone, tested by soaking (it should gain almost no weight).
- Tar or bitumen: a thick coat of hot tar or natural bitumen (Tar, Pitch and Glue) on the levelled plinth, sanded while warm so the mortar above can grip. Builders in Mesopotamia used bitumen this way 4,000 years ago.
- Birch bark: several overlapping layers. Birch bark is full of oils that resist rot, and old log houses in Scandinavia and Russia used it under the first logs.
Drainage around the house:
- Slope the ground away from the walls, at least 1 in 20 (5 cm per metre) for the first 2–3 m.
- French drain on the uphill side and anywhere water collects: a trench 30 cm wide and 45–60 cm deep, its bottom falling at least 1 cm in 2 m to an outlet, with a pipe or stone channel at the bottom and filled with clean gravel. Cover the gravel with turf laid grass-down, then soil, so silt cannot clog it.
- Soakaway where there is no lower ground: a pit of about a cubic metre filled with rubble, at least 5 m from any building, and downhill of and well away from any well (Wells and Cisterns).
- Gutters and downpipes (Roofs) lead roof water to the drain, not to the foot of the wall.
Floors
Beaten earth
The oldest floor, and still a good one: warm underfoot, quiet, and cheap.
- Dig out the topsoil and level the floor area. Ram 10–15 cm of clean gravel as a capillary break — a layer of open stones that ground moisture cannot wick up through.
- Lay damp, rammed-earth-type soil (see Cob, Adobe and Rammed Earth) in layers 5–7 cm deep, ramming each until the rammer rings, to a total of 10–15 cm.
- Finish layer: 2–3 cm of sieved clayey soil mixed with 2–3 parts fine sand and finely chopped straw, wet enough to trowel. Smooth it, then as it stiffens polish it hard with a flat stone or a wooden float.
- Dry slowly for 2–4 weeks with doors open; fill the shrinkage cracks.
- Seal it. Traditionally, earth floors were rubbed with fresh cow dung and water (still done across South Asia and Africa; it dries hard and odourless), or with ox blood. Several coats of warm linseed oil (Oils and Pressing), each soaking in and dried for a few days, make a hard, washable, leather-like floor.
Stone flags
Flagstones of slate, sandstone or limestone 3–8 cm thick, laid on 5 cm of sand or weak lime mortar over 10–15 cm of rammed gravel. Tap each level with a mallet, and point the joints with lime mortar. Cobbles set on edge in sand make a hard-wearing floor for barns and yards.
Timber floors
Never lay boards straight on earth: they rot within a few years. Instead, build a suspended floor:
- Low sleeper walls of stone or brick, or a stone pier every 1.5–2 m, carry beams called joists. Leave at least 15–30 cm of air space between the ground and the timber, and make vents (small openings or gratings) in the outside walls, at least one every 2 m on two opposite sides, so air flows through.
- Joist size: a rough rule is depth in cm ≈ 4 × span in metres + 5, at 40–60 cm apart. A 4 m span needs joists about 21 cm deep and 5–7.5 cm thick, set on edge.
- Boards 2–3 cm thick of well-seasoned wood (Basic Woodworking), nailed or pegged across the joists, tight together. Green boards shrink and leave gaps. Tongued-and-grooved and parquet floors, and stopping squeaks, are in Stairs, Floors and Interior Finishes.
Lime floors
- Lime concrete: 10 cm of lime concrete (as in the footings) over 15 cm of rammed gravel, finished with a smooth topping of 1 lime : 2 sand, polished with a stone as it stiffens.
- Opus signinum: the Roman waterproof floor of lime mixed with crushed fired brick or pottery (Bricks), rammed and polished. Excellent for kitchens, dairies, bathhouses and cisterns.
- Keep lime floors damp for a week or two and do not walk on them until they are hard.
How to tell it worked
- After the first year the walls show no new cracks, especially at corners and over openings.
- A long, straight board laid on the floor rocks nowhere; a marble or round pebble does not roll far.
- The bottom of the walls inside is dry, with no tide-mark of damp, no salt crust and no mould.
- In heavy rain, water flows away from the house and the drains run clear at their outlets.
- The space under a timber floor smells of nothing; a mouldy, musty smell means it needs more vents.
Tip The tell-tale. If a crack appears, smear a thin bridge of lime plaster across it and scratch the date on it. If the plaster cracks again in the following months, the building is still moving and the cause must be found. If it stays whole, the crack is old and harmless.
Note Troubleshooting. A corner sinks and cracks open diagonally → a soft spot or made ground under it. Underpin: dig out short lengths (no more than 1 m at a time) under the footing down to firm ground and fill with stone and mortar, one length at a time. Walls lift and crack in winter → footing above frost depth in wet soil. Drain the ground or deepen the footing. Damp tide-mark low on walls → no damp-proof course, ground piled up above it, or a hard render bridging it. Lower the ground, clear the base, use breathable lime. An earth floor cracks and dusts → too much clay, dried too fast, or not rammed enough. Patch with fresh finish layer; seal it. Timber floor springy → joists too small or too far apart. Add a sleeper wall under the middle.
Dangers
Danger Trench collapse kills. A metre-deep trench wall can fall without warning, and a cubic metre of soil weighs well over a tonne — enough to crush and suffocate someone kneeling in the bottom. Never work in a trench deeper than about 1.2 m (chest height) unless its sides are sloped back at least 45° or held up by planks and cross-struts. Collapse is most likely in sand, in wet soil, after rain, next to the pile of dug soil, and next to old walls. Keep spoil heaps at least a metre back from the edge.
- Undermining old walls. Digging beside or under an existing wall can bring it down. Underpin only in short lengths.
- Open pits and trenches at night or full of water are traps for children and animals. Fence or cover them.
- Heavy stones and rammers — see Stone Masonry.
- Lime burns skin and eyes — see Lime. Hot tar burns deeply; heat it outdoors, away from anything that burns, and never over an open flame in a closed space.
What this unlocks
Sound footings carry everything else in this part: walls of earth, timber, stone and brick (Cob, Adobe and Rammed Earth, Timber Framing and Log Building, Stone Masonry), heavy roofs (Roofs), vaults (Arches, Vaults and Domes), chimneys (Chimneys, Stoves and Heating) and towers. The same drainage skills protect roads (Roads and Bridges), fields (Field Drains, Terraces and Erosion Control, Irrigation) and wells (Wells and Cisterns); deep foundations for heavy buildings lead on to Reinforced Concrete.
How it was first done
The first houses had posts dug straight into the ground and floors of trodden earth. Builders in Mesopotamia set mud-brick walls on stone footings and sealed them with bitumen before 2000 BC. The Romans dug foundation trenches to firm ground and filled them with lime concrete, and they invented waterproof floors of lime and crushed brick. Venice was built from the 800s AD onward on hundreds of thousands of wooden piles driven into the lagoon mud, many still sound after a thousand years because they have never dried out. The Leaning Tower of Pisa shows what happens when the ground is misread: begun in 1173 on a foundation only about 3 m deep in soft clay, it began to lean when only two storeys had been built, and was finally stabilised between 1990 and 2001 by carefully removing soil from under its high side.
Source: content/entries/building/foundations.md