◆ Rebuild

Part 10 · Machines

The Lathe

A machine that spins a piece of wood while you hold a sharp tool against it, making it perfectly round. Build a bow lathe or a spring-pole lathe from wood and cord, and turn handles, bowls, axles and spindles — the first step to accurate machines.

Difficulty
●●●●●
Time
Two or three days to build a pole lathe; a few weeks of practice to turn well
Steps from zero
4 prerequisites →

You need first

The Wheel and AxleCordage and Rope

This unlocks

Recording SoundWood Turning and TreenBearings and LubricationDrills and BoringMachine ToolsScrews, Nuts and BoltsThe Steam EnginePumpsMetal Spinning and Raising
The full path from nothing — 4 steps before this one
  1. Stone Tools
  2. Cordage and Rope
  3. Basic Woodworking
  4. The Wheel and Axle
  5. The Lathe

Do them roughly in this order. See it on the tech tree →

Why it matters

Many of the things a working community needs must be round and true: tool handles, wheel hubs and axles (The Wheel and Axle), lantern staves and pins for Gears, bearings, pulley sheaves, spindles and whorls for Spinning and Weaving Cloth, bowls, cups, chair legs, pegs, pump barrels and pistons. Carving them round by hand is slow and never quite accurate. On a lathe, a person who has practised for a few weeks can turn a straight, round chair leg in ten minutes.

The lathe is also the mother of machine tools. Every accurate machine of the modern world — engines, pumps, screws, clocks — was made on lathes that were first made on lathes. The chain starts here, with a few poles, a cord and a springy sapling.

How it works

The work is held between two pointed centres so it can spin on a fixed line, its axis. A cutting tool is rested on a bar (the tool rest) close to the work and pressed against it. Because the work turns while the tool stays still, the tool cuts away everything outside a perfect circle around the axis. Move the tool along the rest and you shape the profile — thick here, thin there — while every cross-section stays round.

The simplest lathes spin the work back and forth, by a cord wrapped round the work:

  • Bow lathe — a bow, like the one used for fire-making, saws back and forth with its cord wrapped once round the work. One hand bows, the other holds the tool. Good for small things up to about 3 cm thick: pegs, beads, small handles.
  • Spring-pole lathe — the cord runs from a springy pole overhead, two or three turns round the work, down to a foot pedal (treadle). Pressing the treadle spins the work towards you: that is the cutting stroke. Letting the treadle up, the pole pulls the cord back and spins the work the other way; you ease the tool off. Both hands are free for the tool. This is the lathe to build.

On the cutting stroke, the side of the work facing you moves downwards, past the tool's edge. A treadle stroke of 45 cm turns a 5 cm thick spindle about three times (45 ÷ (3.14 × 5) ≈ 2.9). A thick piece turns fewer times per stroke, a thin one more.

What you need

Part Size Wood
Bed rails (2) 1.8 m long, 12–15 cm thick Any straight, sound wood; split logs or poles
Legs (4) To bring the centres to elbow height, about 1 m Any
Poppets (2) 50 cm tall, 10 × 10 cm, with a tenon to fit between the rails Oak or other hardwood
Wedges (2) 25 cm long Hardwood
Centres (2) Pointed iron pins 1.5 cm thick, 12 cm long — or hardwood cones Blacksmithing, or hornbeam, box
Tool rest A straight bar 60–80 cm long, 5 × 5 cm Hardwood
Spring pole 3–4 m long, 6–8 cm at the thick end Ash, hazel, larch, willow or birch sapling
Cord 4 m, 5–6 mm thick, strong and smooth Leather thong, hemp or nettle cord (Cordage and Rope)
Treadle Board 1–1.2 m long, 15 cm wide Any

Turning tools need hard, sharp edges of steel (Steel) or, failing that, iron or Bronze. Flint flakes (Stone Tools) can scrape soft green wood round slowly, but they chip at once against a spinning edge; treat stone as a stop-gap only. You need:

Tool Shape Use
Roughing gouge A U-shaped chisel, 2–3 cm wide, bevel ground on the outside Taking a square or split billet down to round; hollows and coves
Skew chisel A flat chisel, bevelled on both sides, its edge slanted at about 20° Smoothing (a planing cut that leaves a shine), beads, V-cuts
Parting tool Narrow, deep, 3–6 mm wide Cutting grooves to a set depth; cutting the finished piece free
Hook tool A flat bar bent into a hook, sharpened on the inside Hollowing bowls and cups

Where to find it

  • The spring pole. A young, straight ash, hazel, larch or birch, cut green. Test: clamp the thick end and pull the tip down 60 cm; it should spring back smartly and not stay bent. A pole loses its spring after a few months; cut a new one. Instead of a pole, a long bow of springy wood fixed above the lathe, or a bundle of thin rods, does the same job and takes less room.
  • Wood for turning — turn it green (freshly cut). Green wood cuts like cheese; dry wood is hard and dulls tools fast. Good turning woods: birch, beech, ash, sycamore and maple, alder, cherry and other fruitwoods, lime (basswood). Avoid knotty or twisted pieces. Split billets out of a log with wedges; a split piece follows the grain and turns more cleanly than a sawn one.
  • Cord. Leather thong is ideal — grippy and long-lasting. A plant-fibre cord works but wears through in a few days of heavy use; carry spares.

Step by step: building a spring-pole lathe

Spring polespringy sapling, 3–4 m, lashed to a post Poppetslides and wedges Centrespoints exactly in line work: green wood Tool restin front, 1–2 cm off Wedgelocks the poppet Cord2–3 turnsround the work Treadle press springs back END VIEW to pole to treadle tool rests just above the centre turns towards you YOU ← press = cutting stroke
Fig. 1 A spring-pole lathe. Pressing the treadle pulls the cord down and spins the work towards the turner for the cut; the pole springs back and spins it the other way.
  1. Make the bed. Set two rails side by side with a gap of 4–5 cm between them, on four legs, so the top of the bed is about 15 cm below your elbow. Peg or lash the rails to cross-pieces on the legs. The bed must be rigid: if it rocks or flexes, every cut will chatter. Outdoors, stakes driven into the ground make good legs.
  2. Make the poppets. Each is an upright block of hardwood with a tenon at its foot that slides down into the gap between the rails, coming out underneath. Cut a slot through the tenon below the rails for a wedge. Tapping the wedge in pulls the poppet down tight; knocking it out lets you slide the poppet along to suit the length of the work.
  3. Fit the centres. Bore a hole through each poppet about 15 cm above the bed. Drive in the centres — pointed iron pins, or hardwood pins whittled to a 60° cone point and greased. Bring the poppets together: the two points must meet exactly. If not, re-bore.
  4. Fit the tool rest. Fix a straight hardwood bar parallel to the bed on two arms, or on pegs in the poppets, at about the height of the centres and adjustable in and out so it can sit 1–2 cm from the work.
  5. Rig the pole. Lash the thick end of the pole firmly to a post, wall or roof beam behind the lathe, and prop it on a crossbar so its tip lies above the work. At rest, the tip should be bent slightly — under a little tension.
  6. Fit the treadle. Hinge the back end of the treadle board to the floor or ground with a rope loop or a peg, and let its front end lie under your foot, about 30 cm off the ground at rest.
  7. Hang the cord. Tie the cord to the pole tip, take it two or three turns round the work, and tie it to the treadle. The cord must run down to the treadle from the near side of the work (your side), so that pressing the treadle turns the side facing you downwards and the top of the work towards you. Adjust the length so the treadle rises nearly to its full height at rest.

Step by step: turning a tool handle

  1. Prepare a billet. Split a piece of green ash or beech about 30 × 6 × 6 cm. Chop or shave the corners off to make it roughly eight-sided.
  2. Mark the centres. Find the centre of each end (draw lines corner to corner, or by eye) and punch a small dimple there with an awl.
  3. Mount it. Put one end on the fixed centre, slide the other poppet up until its centre seats in the other dimple, and wedge it. The work should spin freely but not rattle. A drop of fat on each centre helps; if it squeaks or smokes, grease it.
  4. Wrap the cord. Two turns, near the middle of the billet, running down to the treadle on your side. Bring the tool rest close.
  5. Rough it round. Hold the gouge firmly on the rest, handle low, with its bevel rubbing the wood just above the centre line. On each down-stroke of the treadle, raise the handle gently until the edge starts to cut; on the up-stroke, ease off. Work from the high ends towards the middle. Shift the cord along as you go.
  6. Shape and smooth. Mark the shape with charcoal while it spins. Cut to size with the parting tool and gouge; smooth with the skew, cutting with the lower half of its edge, bevel rubbing.
  7. Finish. Burnish with a handful of your own shavings pressed against the spinning work. Part off the ends with the parting tool, or saw them off.

For bowls, the cord wraps instead round a mandrel — a short wooden cylinder with three iron spikes in one end, driven into the back of the bowl blank. Hollow the inside with hook tools. A green bowl will warp oval as it dries: rough-turn it with walls about 2 cm thick, dry it slowly for a few weeks wrapped in its own shavings, then turn it again to finish. Forging a fuller set of tools, faceplates and treen work are taught in Wood Turning and Treen.

Sharpening

Edges for green wood need a bevel of 25–35°. Sharpen on a flat sandstone with water, keeping the bevel flat on the stone, until a fine burr (a feather-edge you can feel with a fingernail) forms along the whole edge. Then work on a finer stone — slate or a fine-grained whetstone — and finally strop on leather glued to a board, rubbed with a very fine grit such as powdered pumice or the finest silt you can wash from clay. A sharp edge, held edge-on to a light, shows no line of light at all. Sharpen often; a dull tool tears the wood and makes you push, and pushing causes accidents. Stones, strops and gouge sharpening are covered fully in Sharpening and Honing.

Roughing gougeU-shaped; billet to round Skew chiseledge slanted 20°; smoothing Parting toolnarrow; grooves, cutting off Hook toolhollows bowls and cups THE FOUR TOOLS Handles at least 25 cm long, of ash or beech. HOW THE TOOL CUTS (END VIEW) Edge cuts; the bevel (25–35°) rubs just behind it Tool rest1–2 cm from the work raise the handleslowly to cut work turns towards you
Fig. 2 Turning tools and how to hold them. The bevel rubs the wood just behind the cutting edge; raise the handle slowly until the edge begins to cut. The tool rest is close to the work.

How to tell it worked

  • True centres. Spin the mounted work by hand and hold a stick against it on the rest: the gap should stay the same all round.
  • Round. Measure the finished piece across in several directions with calipers — two sticks pinned together at one end — set to the size you want (Rules, Squares, Callipers and Gauges). A good piece differs by less than 1 mm.
  • Clean surface. A sharp tool cutting with the bevel rubbing leaves a smooth, even shine with only fine spiral marks. Torn, fuzzy patches mean a dull tool or a scraping cut.

Note Troubleshooting. The tool grabs and digs in → the edge is not supported by the bevel; keep the bevel rubbing and cut above the centre line. With the skew, never let the upper point touch the wood. Chatter (a rippled surface) → tool rest too far from the work, bed or poppets loose, or the work too thin and whippy; support long thin work with your hand behind it. The work stops on every stroke → cord slipping: add a turn, tighten the pole, or roughen the work where the cord wraps. Work burns or squeaks on the centres → grease the centres; loosen the poppet a little. The pole is lazy → it has lost its spring, or is too thin. Replace it.

Dangers

Warning Work flying out of the centres. If a poppet works loose, the spinning piece can leap out at your face. Tighten the poppet wedge before every session, check the work is seated, and keep your face out of the line of the work. Protect your eyes from flying chips — a hat brim and squinting is not enough for heavy roughing.

  • Sharp tools slip off the rest and cut hands. Keep the hand that steadies the tool behind the edge, never in front of it.
  • Catches can wrench a tool out of your hands. Hold tools firmly, with long handles (at least 25 cm) braced against your body.
  • A breaking pole or cord whips. Check them for cracks and fraying.
  • Powered lathes are a different danger. A lathe driven by water, animals or an engine does not stop when the work jams. It catches loose sleeves, hair and rags and wraps you into the machine. Never wear loose clothing at a powered lathe, and always have a way to stop the drive instantly (see Planers, Thicknessers and Woodworking Machines for guards and stops on powered machines).

Going further

  • Continuous rotation. A crank on a heavy wheel, worked by a treadle and joined to the work by a belt (Belts, Chains and Power Transmission), turns the work steadily in one direction — twice as much cutting time, and faster. The work must then be held in a headstock with a spindle running in bearings (Bearings and Lubrication). A large "great wheel" turned by an assistant does the same for heavy work, and a The Waterwheel can drive a lathe by a belt.
  • Metal turning. Iron and brass can be turned with hardened Steel tools, cutting slowly and with very rigid tool support. The great step is the slide rest: the tool held in a clamp moved by screws, instead of by hand. Combined with a lead screw geared to the spindle, it lets a lathe cut accurate threads — and so Screws, Nuts and Bolts, the The Steam Engine cylinder, and all Machine Tools.
  • Pumps and pipes. Long bored and turned wooden parts make pumps.

How it was first done

Turned wooden bowls are known from at least 3,000 years ago; a turned wooden bowl from an Etruscan tomb in Italy dates to about 700 BC. The oldest picture of a lathe is in the Egyptian tomb of Petosiris, from about 300 BC: one man pulls a strap back and forth around the work while another holds the cutting tool. The bow lathe spread across the Middle East and Asia, where craftsmen still use it, often steadying the tool with their toes.

The spring-pole lathe appears in European pictures from the 13th century and was used for centuries to make furniture, bowls and tool handles. In the beech woods of the Chiltern Hills in England, woodland turners called bodgers worked pole lathes in the forest, turning chair legs by the thousand, until the mid-20th century. Leonardo da Vinci sketched a treadle lathe with a crank and flywheel around 1500, and by about 1800 the English engineer Henry Maudslay had built an all-metal lathe with a slide rest and lead screw that could cut accurate screw threads — the machine from which modern industry grew.

Source: content/entries/mechanics/lathe.md