How to build the things a household lives on — a three-legged stool that never wobbles, a trestle table, a green-wood chair with a woven seat, a chest and a rope bed — using joints that tighten as the wood dries, hide glue, and mattresses stuffed with straw and wool.
- Difficulty
- ●●●●●
- Time
- A day for a stool; a week for a chair or a bed; a winter to furnish a house
- Steps from zero
- 14 prerequisites →
The full path from nothing — 14 steps before this one
- Stone Tools
- Fire
- Cordage and Rope
- Finding and Preparing Clay
- Finding and Identifying Ores
- Basic Woodworking
- Hunting and Trapping
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Furniture
Do them roughly in this order. See it on the tech tree →
Why it matters
People who sit and sleep on the floor spend their lives in its cold, its damp, its draughts, its dust, and among the fleas, mites and mice that live in floor rushes and bedding. A bed raised half a metre off the ground is warmer and healthier; a chair saves the backs and knees of the old; a table gives a clean surface to eat, write, sew and prepare food on; and a lidded chest keeps cloth, papers, seed and tools dry and away from vermin.
Furniture is also where woodworking skill grows. The joints you learn here — mortise and tenon, wedged tenons, dovetails, frame and panel — are the joints of houses, wheels, looms, spinning wheels, carts and clocks.
How it works
Wood moves. As wood dries, it shrinks — but not evenly:
- Along the grain (the length of the tree): almost nothing, about 0.1–0.2 %.
- Across the grain: a lot — about 4 % from the centre outwards (radially), and about 8 % around the growth rings (tangentially), from green to dry. A green board 30 cm wide may end up 2 cm narrower.
It goes on swelling and shrinking a little with every damp and dry season. This explains almost every furniture failure, and suggests three rules:
- Never fix two pieces with their grain crossing at right angles over a wide area, such as gluing a cleat solidly across a tabletop. One piece wants to shrink, the other doesn't — something cracks. Fix wide boards only at one point, or let them slide in a groove or a slotted hole.
- Use the shrinkage to lock joints. A dry tenon pushed into a hole in green wood gets gripped harder and harder as the green wood dries and shrinks around it. Then the dry tenon absorbs a little moisture and swells. Traditional chairs were made this way with no glue at all.
- Rive, don't saw, for strength. Wood split along its fibres (riven) follows the grain, so no fibres run out of the side of a leg or rung. A riven chair leg 3 cm thick is as strong as a sawn one 4 cm thick.
Triangles do not rack. A rectangle of four rails and four legs can fold sideways like a parallelogram unless its corners are rigid. Make the joints deep and tight, add stretchers low between legs, or brace with a diagonal.
Three legs never wobble. Any three points always lie on one plane, so a three-legged stool sits firm on the roughest floor. Four legs are steadier against tipping but must be trimmed to the floor.
What you need
| Tool | What for | Chapter |
|---|---|---|
| Axe and froe (a blunt splitting blade on a handle), mallet, wedges | Splitting logs into blanks | Axes, Chisels, Knives and Planes, Basic Woodworking |
| Drawknife — a blade with a handle at each end, pulled towards you | Shaping legs, rungs, posts | Axes, Chisels, Knives and Planes |
| Shaving horse — a bench with a foot-operated clamp | Holding work for the drawknife | Below |
| Spokeshave (a small plane for curves) and a knife | Finishing round parts | Axes, Chisels, Knives and Planes |
| Auger or brace and bits, 12–25 mm | Boring holes for rungs and pegs | Drills and Boring |
| Chisels 6–25 mm, a saw, a plane | Mortises, dovetails, flat boards | Files and Saws |
| Square, straightedge, marking gauge, measuring stick | Laying out | Measurement from Scratch |
Woods: ash (the best: straight, springy, splits and bends well), oak (strong, durable, splits well), hickory, maple, beech (turns and carves well), elm (refuses to split, so ideal for seats), hazel and willow (rods for weaving), chestnut, walnut, cherry. Pine and other softwoods are fine for chests, tables and shelves.
Glue: hide glue (below) or none. Seat weaving: soft rush, cattail leaves, inner bark of hickory, elm or lime, or cord. Bedding: straw, wool, linen or hemp cloth (Flax, Hemp and Linen).
Where to find it
Pick a straight, branch-free length of trunk 20–40 cm thick, with bark that runs straight up rather than twisting round. Cut it fresh. Split it in halves, quarters and then eighths with wedges and a froe, always splitting through the centre of each piece so the two halves are the same thickness and the split runs true. A 1.5 m ash log 30 cm thick gives enough pieces for two chairs. Keep riven blanks you are not using yet in the shade with their ends sealed (see Basic Woodworking), or under water, so they stay green.
The shaving horse
Make this first: it turns the drawknife into a fast, safe tool.
- A bench: a split log or plank 150 cm long on three or four splayed legs, 50 cm high.
- A sloping work table on top, 60 cm long, raised 20 cm at the far end on a block.
- A swinging arm (the dumbhead) through a slot in the bench, pivoting on a peg, with a heavy jaw on top and a foot bar at the bottom. Push with your feet, and the jaw clamps the work against the table. Release your feet, turn the work, clamp again.
Method 1: A three-legged stool
The quickest piece of furniture, and the base of all chairmaking.
- Seat. Split or saw a slab of elm, ash or oak 5 cm thick and 30–35 cm across. Flatten the top with an adze or axe and round the edge.
- Legs. Rive three legs from ash or oak, 45 cm long for a low stool. Shave them to about 3.5 cm thick, tapering at both ends, with a tenon at the top end — a round peg 2.5 cm across and 6 cm long. Let the legs dry for a few weeks by the fire (not on it), then shave the tenons to their final size: they should be drier than the seat.
- Bore the holes. Mark three points on an equilateral triangle, each 10 cm from the centre. Bore right through the seat with a 2.5 cm auger, tilted outward at 15–20° from vertical, so the legs splay. Line the auger up by eye with a stick stood at the right angle.
- Saw a slot 5 cm deep in the top of each tenon.
- Drive the legs in with a mallet. Turn each so the slot runs across the grain of the seat (if it ran along the grain, the wedge would split the seat).
- Wedge. Dip a dry hardwood wedge in glue (or not) and drive it into each slot from above. Saw off the protruding tenon and wedge flush.
- Level the legs by standing the stool on a flat floor and trimming each one until the seat is level. A three-legged stool will never rock.
Method 2: A green-wood chair
The ladderback chair — two tall back posts, two short front posts, and many round rungs — can be made from one ash log with a drawknife and an auger, and needs no glue.
| Part | Count | Size (finished) |
|---|---|---|
| Back posts | 2 | 100 cm long, 4 cm thick |
| Front posts | 2 | 45 cm long, 4 cm thick |
| Seat rungs | 4 | Front 47 cm, sides and back 38 cm (plus tenons), 2.5 cm thick |
| Lower rungs | 6–8 | Same lengths, 2.2 cm thick |
| Back slats | 2–3 | 38 cm long, 6–7 cm wide, 1 cm thick |
| Tenons on all rungs | 16 mm across, 2.5–3 cm long |
- Rive and shave the posts from green wood. Keep them green.
- Bend the back posts (optional but comfortable; see Steam-Bending Wood). Steam them for about one hour per 2.5 cm of thickness in a box over a boiling pot, then bend them over a wooden form so the top 40 cm leans back by about 10 cm. Leave them strapped to the form for a week.
- Make the rungs and slats and dry them hard — two to three weeks in a warm, dry place, or a few days near (never on) a stove. Shave the tenons to 16 mm with a test hole bored in a scrap board; it should push in only with firm blows.
- Bore the posts while they are still green. Seat rungs go 43–45 cm above the floor; lower rungs at about 15 and 25 cm. Holes on adjacent sides must be at slightly different heights so they do not meet inside the post. Bore 2.5–3 cm deep. Chop narrow mortises for the back slats.
- Assemble. Join the front frame (two front posts and their rungs) and the back frame, then join the two with the side rungs. Drive all together with a mallet. Check that the chair stands square by measuring the diagonals of the seat — equal diagonals mean square.
- Peg the slats with a thin dry peg through post and slat.
- Leave it a month. The green posts shrink onto the dry tenons and lock the chair.
- Weave the seat. Wrap a seat of twisted rush, cattail leaves, cord or 1 cm strips of inner bark round the four seat rungs, working from the corners towards the middle. Bark strips are woven in a simple over-two, under-two pattern while wet; they shrink tight as they dry.
Method 3: Tables
The simplest strong table is a trestle table: a loose top on two stands, which comes apart to clear the room.
- Height: 72–76 cm. Width: 70–90 cm. Length: about 60 cm per person along each side.
- Top: planks 3–4 cm thick, split and hewn flat, or sawn. Join them edge to edge with dowels and glue, or simply lay them on the trestles and join them underneath with two or three battens. Fix each batten with pegs through slotted holes (holes made long in the direction across the top) so the top can shrink and swell.
- Trestles: two slab ends with feet, joined by a long stretcher passing through a mortise in each and locked by a tapered wedge driven through a hole in the stretcher's end. Knock out the wedges and the table falls flat.
For a fixed table, make a frame of four legs joined by four aprons with pegged mortise and tenon joints (see Basic Woodworking and Timber Framing and Log Building), and fasten the top to the aprons with wooden buttons that hook into a groove, so it can move.
Method 4: A chest
The six-board chest — front, back, two ends, bottom and lid — is the quickest. The ends run with their grain upright and are notched at the bottom to make feet. Nail or peg the front and back into rebates in the ends. It works, but the grain of front and ends cross at the corners, and many old six-board chests have split there.
The dovetailed chest is the lasting answer: dovetails are interlocking fan-shaped "tails" and "pins" cut on the corners of the boards, so the joint cannot pull apart and all the grain runs the same way round the box.
- Make boards of equal thickness, planed flat and square-ended.
- Mark the tails on one board: fans with sides sloping about 1 in 8 for hardwood (1 in 6 for softwood), 5–8 cm apart.
- Saw down the sloping lines with a fine saw to the depth line, and chop out the waste between with a chisel, working half-way from each side.
- Lay the cut tails on the end of the other board and scratch round them with a knife; saw and chop the pins.
- Tap together. Glue if you have glue.
Put the bottom in a groove, not nailed solid, so it can move. Hang the lid on iron strap hinges or on two wooden pins at the back. A lock is in Locks and Keys.
Method 5: A bed
A bed raised 40–60 cm keeps sleepers out of the coldest, dampest air and away from crawling pests.
- Size: inside the frame, 195 × 90 cm for one person, 195 × 140 cm for two.
- Frame: four posts 8–10 cm square, two long side rails and two end rails about 8 × 5 cm, joined with deep mortise and tenon joints. For a bed that comes apart, use long tenons held with a wedge or a bed bolt.
- Rope bed: bore 2 cm holes through all four rails, every 15–20 cm. Lace a strong rope (see Cordage and Rope) through them lengthways, then crossways, weaving over and under. Tighten it by working round with a bed key — a stick with a notch — or by pulling hand over hand, starting at one corner and taking up the slack row by row. Ropes stretch; retighten every few weeks. (People often say "sleep tight" comes from this, though that is probably a myth.)
- Slats are simpler: boards 10 × 2 cm across the frame, resting on ledges on the inside of the side rails, 5 cm apart.
Mattresses and bedding
A mattress is a tick — a strong, tightly woven cloth bag — filled with something springy.
- Ticking: a dense linen or hemp twill (Spinning and Weaving Cloth, The Loom) that straw and feathers cannot poke through. Sew a bag the size of the bed frame and 15–20 cm deep, with an opening along one side (Sewing, Needles and Thread).
- Filling, from cheapest to best:
| Filling | Amount for a single bed | Notes |
|---|---|---|
| Straw (oat straw is softest), maize husks, dried bracken, beech leaves, heather | 8–12 kg | Cheap, but packs flat. Shake up daily; replace every year after the harvest |
| Wool — washed and carded (Wool) | 8–12 kg | Warm, springy, lasts decades; re-card every few years |
| Horsehair (tail and mane), curled by twisting into a rope, boiling and drying | 8–12 kg | Very springy, lasts generations |
| Feathers and down | 4–6 kg | A soft upper mattress (featherbed) on top of a straw one |
- Tufting keeps the filling from drifting to the edges: with a long needle and strong twine, stitch right through the mattress every 20–25 cm in a grid, tying each stitch over a small pad of cloth on both faces.
- Pillows: smaller ticks of feathers, wool, chaff or buckwheat husks.
A layer of dried fragrant herbs in straw ticks — lady's bedstraw, lavender, tansy, wormwood — was long used to discourage fleas. Better is to air and beat all bedding in the sun weekly and to change the straw yearly. See Personal Hygiene and Household Pests for lice and bed bugs; Mattresses and Upholstery goes further with sprung and stuffed mattresses.
Glue and finish
Hide glue is the furniture glue of history (see Glues and Adhesives):
- Collect scraps of rawhide, hide trimmings from Hides and Leather making, sinew and rabbit skins. Soak them in water for a day, then simmer gently — never boil hard — for 4–6 hours, until they dissolve into a thick liquid.
- Strain through cloth into a shallow tray and let it set into a jelly. Cut it into slabs and dry it on a net.
- To use, soak dry glue overnight in about twice its weight in water, then warm it in a water bath to about 60 °C (too hot to keep a finger in for more than a moment). It should run off a brush like thin honey.
- Spread it on both faces of a warm joint, clamp or tie tight, and leave 24 hours.
Hide glue is strong and can be undone with heat and steam for repair. Keep it dry: damp unsets it.
Finishes: scrub tables and benches with sand and water and leave them bare; or rub in linseed oil (Oils and Pressing) — one thin coat a day for a week, wiping off the excess (linseed oil dries hard in air). A polish of beeswax melted into a little turpentine (Distillation) or oil gives a soft shine to chairs and chests.
How to tell it worked
- Rack test: push a chair or table sideways at the top. A good one does not move or creak.
- Rock test: a four-legged piece does not rock on a flat floor.
- Sit test: lean back hard in a chair; no joints should open.
- Six months later: no cracks across wide boards, no rungs working loose.
Note Troubleshooting. Rungs work loose → the rungs were not dry enough, or the posts were too dry when bored; or the tenons were too small. Re-make the rung dry and slightly oversize, or glue and wedge it. A wide board or tabletop splits → it was fixed across its width; let it move. A leg breaks at a knot or across the grain → it was sawn, not riven; split legs along the grain. Steamed wood cracks on the outside of the bend → not steamed long enough, or the wood was too dry or had run-out grain. Use fresh, straight wood and support the outside of the bend with a steel strap. Glue joint fails → glue too thin, joint too cold, or the faces did not touch. Warm the wood and clamp it.
Dangers
Danger Drawknives, axes and froes cut deep. Always work with the edge moving away from your body or across it, never towards your legs; clamp the work, not your hand. Keep blades sharp and in a sheath. See Wound Care and Antiseptics.
- Steam scalds faster than boiling water. Open steam boxes with a long stick, away from your face, and wear gloves.
- Heavy lifting: logs and finished beds are heavy; lift with your legs, and get help.
- Fire: straw mattresses and shavings burn fast. No naked candles near beds — use a lantern or a candle in a dish of water (Lamps and Candles).
- Mould: damp straw ticks grow mould that harms lungs. Keep them dry and change the filling.
What this unlocks
The joints and the shaving horse lead straight to Barrels and Cooperage, wheelwrighting, looms, spinning wheels and wooden machinery. Turned legs and spindles come from the The Lathe (Wood Turning and Treen). Cupboards, shelves and desks are in Cupboards, Drawers, Shelves and Desks; cradles, hammocks and sofas in Cradles, Hammocks, Sofas and Folding Chairs. Upholstery (Mattresses and Upholstery) leads to coiled iron Springs. Glued, laminated wood leads to strong, light structures for boats and Gliders and Aeroplanes.
How it was first done
Furniture is older than writing. Stone beds, shelves and dressers survive in the 5,000-year-old houses of Skara Brae in Orkney. Egyptian furniture makers had mastered mortise and tenon, dovetails and veneer by 2500 BC; the gilded chairs, beds and chests of Tutankhamun's tomb (about 1325 BC) still stand. Hide glue was used in Egypt and probably long before. Through most of history, though, ordinary people owned only a chest, a stool, a board table on trestles and a straw-filled bed. Green-wood chairmaking with a pole lathe and drawknife was a village craft across Europe for centuries; English Windsor chairs, with legs and spindles wedged into a solid elm seat, became common in the 1700s. In the 1850s Michael Thonet in Vienna perfected steam-bending solid beech, and his chair No. 14 (1859) was sold by the tens of millions.