Part 4 · Food and Farming
The Plough
From digging stick to ard to mouldboard plough — how to build a wooden ard with an iron share, hitch it to a team, plough a straight furrow, and break the soil fine with harrows and rollers.
- Difficulty
- ●●●●●
- Time
- A week to build an ard; a day to plough about 0.4 hectares (one acre) with an ox team
- Steps from zero
- 8 prerequisites →
The full path from nothing — 8 steps before this one
- Stone Tools
- Cordage and Rope
- Basic Woodworking
- Hunting and Trapping
- Farming from Seed
- Hides and Leather
- Keeping Animals
- Draft Animals and Harness
- The Plough
Do them roughly in this order. See it on the tech tree →
Why it matters
Digging by hand with a spade, a fit person turns perhaps 20–40 square metres a day (see Farming from Seed). That is enough for a garden, not for the grain fields that feed a village. With a plough and a pair of oxen, the same person breaks about 0.4 hectares — 4,000 square metres — a day, a hundred times more. The plough is what made fields of wheat and barley large enough to feed towns, armies, craftsmen and scholars who grew no food themselves.
Ploughing does four jobs at once: it loosens the soil so roots and water can get in, buries weeds and old stubble so they rot, mixes in manure (see Compost and Manure), and leaves a surface that harrows can break into a fine seedbed. A ploughed field comes up with far fewer weeds than one sown into grass.
It also has a cost. Bare, ploughed soil washes and blows away. A good ploughman knows when not to plough (see Dangers).
How it works
There are three stages of tool, and you can build all three.
- The digging stick and hoe — a sharpened, fire-hardened stick or a blade on a handle, worked by hand. Still the best tool for small plots and rocky ground.
- The ard (scratch plough) — a pointed wooden spike dragged through the ground by animals. It cuts a groove and stirs the soil to each side but does not turn it over. To break all the ground, you plough a field once lengthways and again crossways. The ard is light, simple, and ideal for light, dry soils in warm climates, where you want to keep moisture in, not bury it.
- The mouldboard plough — adds three parts to the ard. A vertical knife, the coulter, slices the sod in front. A flat blade, the share, cuts it loose underneath. A curved board behind, the mouldboard, lifts the cut strip — the furrow slice — and turns it upside down beside the furrow. This buries weeds completely and handles heavy, wet clay soils that an ard cannot. It also needs more pulling power: two to four oxen or two horses for a single furrow.
Depth and the line of draught
A plough is a wedge pulled along a line. Where you hitch it controls how deep it runs.
- The pull runs in a straight line from the animals' shoulders (the yoke or the hames, see Draft Animals and Harness) through the hitch point at the front of the plough beam, to the point where the soil resists — roughly the share.
- Hitch lower on the beam (or use a shorter chain) and the point lifts — shallower ploughing. Hitch higher (or longer chain) and the point dives — deeper.
- On an ard, you also change depth by changing the angle of the share in the body with wedges.
When the line is right, the plough runs level by itself and the ploughman only steers. When it is wrong, the ploughman fights the handles all day.
What you need
| Item | Material | Size |
|---|---|---|
| Beam (draught pole) | Straight ash, oak, elm or any tough hardwood, 10–12 cm thick | 2.5–3 m for an ox yoke; 1.5–2 m for chain traces |
| Body / sole | Oak or another hard, heavy wood, 10–12 cm square | 60–80 cm long |
| Handle (stilt) | Ash or oak | 1–1.2 m, reaching a ploughman's hip |
| Share | Hardwood spike at first; iron tip as soon as you can | Iron share 15–25 cm long, 5–8 cm wide, 0.5–1 kg |
| Wedges and pegs | Dry oak or ash | Several, for adjusting depth |
| Team | A pair of trained oxen, or one or two horses or mules | See Draft Animals and Harness |
| Hitch | Rope, rawhide (see Hides and Leather) or chain; iron ring or clevis | |
| Tools | Axe, adze, auger or a red-hot iron for boring, chisels, mallet | See Basic Woodworking |
Where to find it
- The body and beam. The oldest ards were made from a single tree: a trunk with a strong side branch growing at the right angle, the trunk becoming the body and share and the branch the beam ("crook ard"). Walk the woods looking for an oak, elm or ash with a straight branch leaving the trunk at 30–45°. Otherwise, join a separate beam and body with a mortise (see below).
- Hard, wear-resistant wood for the share. Oak heartwood, hornbeam, holm oak, olive, or tropical hardwoods. Fire-harden the tip (see Basic Woodworking). A wooden share wears out in a few days of hard ploughing; carry spares.
- Iron for the share comes from your smith (see Iron (the Bloomery) and Blacksmithing). Even a small iron tip lasts a season instead of a few days.
Method 1: Build a sole ard
The sole ard has a horizontal wooden body (the sole) that slides along the bottom of the furrow, with the share fitted at its front and the handle rising from its back. It is stable, easy to steer and easy to build.
- Shape the sole. Hew a block of oak 60–80 cm long and 10–12 cm square. Taper the front 25 cm to a point, flat on the bottom and sloping on top, like a chisel lying on its back.
- Cut the beam mortise. About 30 cm from the front, cut a rectangular hole through the sole, sloping forward and upward at about 35° from the horizontal, just big enough for the end of the beam. Burn it out with a red-hot iron bar or chop it with a chisel.
- Fit the beam. Shape the thick end of a 2.5–3 m pole to fit the mortise. Drive it through so 5 cm sticks out underneath, then trim flush. Cut a slot for a hardwood wedge in front of and behind the beam inside the mortise; moving these wedges changes the angle between beam and sole.
- Fit the handle. Bore a hole at the back of the sole and peg in a handle of ash rising at about 60° backward, ending at the ploughman's hip height, with a short cross-grip at the top.
- Make the share. For a wooden share, the pointed front of the sole is the share — fire-harden it. Better: forge an iron share. Hammer a bar into a flat blade 15–25 cm long and 5–8 cm wide, then fold the back half around a mandrel the shape of the sole's point to form a socket. Draw the point out thick (1–1.5 cm) so you can sharpen it again and again. Harden the tip by quenching (see Steel). It slides onto the sole's point and is held by friction or a nail.
- Hitch. At the far end of the beam, bore a hole and drive in an iron or wooden peg. For an ox yoke, the beam end passes through a loop of rawhide or rope tied to the yoke's centre ring, held by the peg. Several holes let you change length. For horses, fit a ring or clevis to the beam end and hook on the whippletree (see Draft Animals and Harness).
Finished, it weighs 15–25 kg — light enough for one person to carry to the field.
Method 2: The mouldboard plough
When you have iron, a good smith and heavy soil, build a mouldboard plough. It has the same beam, handles and hitch as the ard, plus:
- The coulter — a heavy iron knife, 50–60 cm long, wedged through a mortise in the beam, its edge pointing forward and down so its tip runs just ahead of and 2–3 cm above the point of the share, and a little to the land side. It slices the edge of the sod.
- The share — a flat, triangular iron blade, its point and cutting edge sloping back toward the mouldboard side. It cuts the slice free underneath. Width about 20–25 cm.
- The landside — a flat, smooth board or iron plate on the side away from the mouldboard. It presses against the unploughed wall of the furrow and keeps the plough running straight.
- The mouldboard — a curved board, carved from a single block of tough wood or built from planks, set on the other side. It starts nearly level with the share at the front and twists up and over to near-vertical at the back, like a slice of a screw. Cover its working face with iron strips nailed on, or it wears through in a season. The shape matters: a long, gently twisting board turns the soil with least effort; a short, steep one breaks it up more.
- Wheels (optional) — a small wheel under the front of the beam, or a two-wheeled fore-carriage, holds the depth steady and makes the plough far easier to handle on heavy land.
A medieval wheeled heavy plough needed six to eight oxen. A well-shaped light plough with an iron mouldboard turns a 23 cm × 15 cm slice in medium soil behind two horses or two to four oxen.
Step by step: ploughing a field
- Pick the day. Squeeze a handful of soil from plough depth. It should crumble when you poke it. If it smears, makes a ribbon or sticks to the share, it is too wet: ploughing now makes hard clods and spoils the soil's structure for the whole year. If it is dust and the share skids, it is too dry; wait for rain.
- Mark out. Ploughing goes in long straight runs, turning as rarely as possible. Divide the field into strips called lands, 10–20 m wide. Leave a strip about 5 m wide at each end — the headland — for turning the team. Set two tall sticks in a line at the far end of the first land to aim at.
- Open the first furrow. Line up the team on the sticks. Fix your eye on the far stick, lined up with the near one, and walk the team straight toward it. Do not look down at the plough. Lift or lower the handles slightly to keep an even depth: press down to lift the point, lift up to make it dive.
- Turn and come back. At the headland, tip the plough onto its side or lift it out, turn the team, and plough back beside the first furrow. With a mouldboard plough, which always throws soil to one side (usually the right), coming back beside the first furrow throws the second slice against the first, forming a ridge. This is gathering: working round and round outward from the centre ridge of each land.
- Keep it even. Each new furrow slice should lie at the same angle against the last, like books leaning on a shelf, with no grass showing. With an ard, plough the whole field one way, then again crossways.
- Finish the headlands last, ploughing round the field along them.
- Pace. Oxen walk about 3 km/h. To plough 0.4 ha with furrows 23 cm wide you must walk about 17 km of furrow — six hours of work. That is why the old English acre was a day's ploughing for an ox team, and the furlong ("furrow long", about 200 m) was the length a team could pull before resting.
Harrows and rollers
Ploughing leaves the soil in slices and clods. Before sowing, break it into a tilth — fine, crumbly soil.
- Brush harrow. The simplest: a big thorny bush or a bundle of branches weighed down with a log, dragged over the field. Good for covering broadcast seed.
- Tine harrow. A square or triangular wooden frame about 1.2–1.5 m across, with 20–30 pegs (tines) of hardwood or iron, 15–20 cm long, sticking down. Set the tines so that each one makes its own track, about 8–12 cm apart, by staggering them on the cross-bars. Pull it from one corner so it runs at a slant and the tines don't follow each other. Go over the field two or three times, crossways and diagonally.
- Roller. A smooth log 25–40 cm thick and 1.5–2 m long, with iron pins or wooden pegs in each end turning in a simple frame. Rolling crushes clods and firms the soil around seeds so they stay moist. Roll after sowing on light soils; never roll wet clay.
How to tell it worked
- Straight, even furrows of the same depth, with every slice turned and no green showing between them.
- Depth: push a stick into the ploughed soil. An ard should loosen 10–15 cm; a mouldboard plough 15–25 cm.
- The team walks steadily without being driven hard, and the ploughman isn't wrestling the handles.
- After harrowing, the surface is crumbly, with clods no bigger than a walnut, and your heel sinks in a little but leaves a firm print.
Note Troubleshooting. Plough keeps jumping out of the ground → point too blunt or angled too flat, or hitched too low. Sharpen or replace the share, drive the wedge to tip the point down, or hitch higher. Plough dives deep and stalls the team → hitched too high or the point tipped down too much. Hitch lower or re-wedge. Plough pulls constantly to one side → hitch is off-centre; move the hitch toward the side the plough runs away from. On a mouldboard plough, check that the landside is flat and sitting against the furrow wall. Slices don't turn over and fall back → going too slowly, slice too narrow for its depth (a slice should be about one and a half times as wide as it is deep), or the mouldboard is too short. Huge hard clods → ploughed when too wet or too dry. Wait for rain, then harrow at once while they are soft. Share wears away in days → wooden share; fit iron, or carry several spares and fire-harden each.
Dangers
Danger The handles strike back. When the share hits a buried root or rock, the plough stops dead or leaps, and the handles can smash into your ribs, chin or groin. Hold the handles firmly but not rigidly, stand slightly to one side, and plough slowly on new ground until you know where the stones are. Clear big stones before you start.
- The team. Everything in Draft Animals and Harness applies: kicks, runaways, crushed fingers in hitches. Never step between the plough and the team while it is moving.
- The share is sharp. Carry it covered and keep feet away from the front of the plough.
- Erosion destroys land. Bare ploughed soil on a slope washes away in heavy rain; on dry plains, it blows away (the American "Dust Bowl" of the 1930s). Plough across the slope, along the contour, never up and down it. Leave strips of grass or hedges between fields on slopes, build terraces and contour banks (see Field Drains, Terraces and Erosion Control), and do not leave soil bare over winter if you can sow a cover crop. See Understanding Soil.
- Over-ploughing. Ploughing every year at the same depth can form a hard "plough pan" beneath. Vary the depth, and grow deep-rooted crops (clover, lucerne) in your rotation.
What this unlocks
The plough turns small gardens into fields of The Great Staple Crops. Rows of ploughed soil invite the Seed Drill and Reaper, which sows and harvests at the plough's scale, and the sickle gives way to the scythe. Steel ploughs, multi-furrow "gang" ploughs and finally engines to pull them lead to the The Tractor. The same idea — a wedge pulled through earth — is behind road-building and canal-digging tools (see Roads and Bridges and Canals and Locks).
How it was first done
The first ards were probably dragged by people before animals were harnessed to them. Ard ploughing with oxen was established in Mesopotamia and Egypt by about 4000–3000 BC; Mesopotamian seals of the 2nd millennium BC even show ards with a seed funnel attached. Criss-cross ard marks preserved under an earthen burial mound at South Street, Wiltshire, England, date to about 3500 BC, and a ploughed field at Kalibangan in India to about 2800 BC. Wooden ards themselves survive from the Iron Age in Danish bogs.
The Chinese were using iron ploughs with curved cast-iron mouldboards by the Han dynasty (around the 1st century BC or earlier), more than a thousand years before Europe. In Europe, heavy wheeled ploughs with coulter and mouldboard spread across the wet clay lands of the north between about AD 600 and 1000, making them into the great grain fields of the Middle Ages. Lighter, better-shaped ploughs came from the Netherlands to England in the 17th century (the "Rotherham" plough, about 1730), and in 1837 the American blacksmith John Deere made a polished steel plough that cut the sticky prairie soils of the Midwest without clogging.