◆ Rebuild

Part 4 · Food and Farming

Soy Sauce, Miso and Koji

How to grow koji mould on steamed rice and soybeans and use it to make miso and soy sauce, and how to make fish sauce, tempeh and tofu. These turn cheap beans, grain and small fish into foods rich in protein, full of flavour and slow to spoil. The chapter also covers how to tell good moulds from dangerous ones.

Difficulty
●●●●●
Time
Two days to make koji; a day to set up miso, then 3–12 months to age it; soy sauce 6–24 months; tempeh in 2 days; tofu in an afternoon
Steps from zero
19 prerequisites →

You need first

Starter Cultures and Food MicrobiologyThe Great Staple Crops

This unlocks

Spirits, Sake and Liqueurs
The full path from nothing — 19 steps before this one
  1. Fire
  2. Stone Tools
  3. Finding and Preparing Clay
  4. Sanitation and Germs
  5. The Kiln
  6. Pottery
  7. Farming from Seed
  8. Lime
  9. The Great Staple Crops
  10. Lye and Potash
  11. Fermentation
  12. Glass
  13. Distillation
  14. Laboratory Glassware
  15. Sterilising Instruments and Dressings
  16. Lenses
  17. The Microscope
  18. Culturing Microbes
  19. Starter Cultures and Food Microbiology
  20. Soy Sauce, Miso and Koji

Do them roughly in this order. See it on the tech tree →

Why it matters

Soybeans give more protein per hectare than any other common crop. Raw, though, they are hard to digest and taste grassy. Over two thousand years, cooks in East and South-East Asia found ways to turn them into foods that keep for years and make plain rice or grain taste rich: miso (a salty fermented paste), soy sauce, tempeh (a cake of beans bound by mould) and tofu (bean curd). Fish sauce does the same for small fish too bony to eat.

Most of these rest on one mould, koji (Aspergillus oryzae). Grown on steamed grain or beans, koji floods them with enzymes (natural chemical tools) that break starch into sugar and protein into the savoury amino acids that give meat and broth their taste. Salt then stops spoilage while those enzymes keep working for months. The same koji makes sake and rice vinegar (Spirits, Sake and Liqueurs, Vinegar and Pickling). A village with koji, salt and beans has a year-round source of protein and flavour that needs no refrigeration (Preserving Food).

How it works

  • Koji is a tool-maker. In two days on warm, damp rice or beans the mould grows a mat of white threads and pours enzymes into the grain. In a salty mash the mould soon dies, but its enzymes keep working for months.
  • Salt chooses who lives. At 10–13% salt (miso) or 17–18% in the liquid (soy sauce), spoilage and disease bacteria cannot grow, but salt-tolerant yeasts and lactic bacteria can, adding winey, sour notes. Too little salt and the batch rots; too much and nothing works.
  • Fish digest themselves. Packed in salt, small fish dissolve in their own gut enzymes into a clear brown liquid over a year.
  • Tempeh is a fast, unsalted ferment: the mould Rhizopus binds cooked beans into a white cake in a day (Growing Mushrooms).
  • Tofu is not fermented at all. It is made like cheese (Dairy and Cheese): a magnesium or calcium salt curdles the protein in boiled soy milk.

What you need

Item For Notes
Koji spores (tane koji) Koji Must come from an existing culture; see below
Soybeans Everything Round, pale, sound beans
Rice, barley or wheat Koji, soy sauce Polished rice is easiest for koji
Salt Miso, soy sauce, fish sauce Clean sea or rock salt (Salt)
Bittern or gypsum Tofu Salt, Gypsum and Plaster of Paris
Steamer Rice and soybeans A pot with a basket or a wooden steaming box over it
Koji trays and chamber Koji Built below
Crocks or barrels Miso, soy sauce, fish sauce Glazed Stoneware and Porcelain or Barrels and Cooperage
Clean cloth, a press Soy sauce, tofu Linen or cotton; a lever or screw press (Oils and Pressing)
Thermometer Koji, tempeh Very helpful (The Thermometer)

Where to find it

  • Soybeans grow wherever beans grow in warm summers: sow after frost, 5 cm apart in rows 50 cm apart, and harvest when the pods rattle (The Great Staple Crops). Seed is in old farm and food stores in China, Korea, Japan, the American Midwest, Brazil and Argentina.
  • Koji spores do not reliably appear wild, and the wild look-alike is deadly (see Dangers). Look for tane koji (koji seed) or dried koji rice in East Asian food stores, sake breweries, miso works and soy sauce factories. Sealed, cool and dry, spores live a year or more. Once you have koji, never let it die out (Starter Cultures and Food Microbiology).
  • Tempeh mould can be caught: Javanese makers grew it on the undersides of sea hibiscus leaves (Hibiscus tiliaceus, waru) pressed onto cooked soybeans.
  • Bittern, the bitter liquid left after salt crystallises from seawater (Salt), is the tofu-maker's nigari.

Koji

The koji tray

Koji makes its own heat and needs air. In a deep heap it smothers and cooks itself above 40 °C, so it is grown spread thin on trays.

KOJI CHAMBER, CUT AWAY ONE TRAY TEMPERATURE OF THE GRAIN Damp cloth Thermometer in the grain Trays stacked crosswise, with 2–3 cm air gaps Hot water pan or lamp; air 28–35 °C straw-packed walls 45 cm 30 cm 5 cm Rice 2–3 cm deep, furrowed bare cedar or pine, pegged, no nails; battens underneath keep the gap 30 °C 40 °C 0 h 18 h 48 h Too hot: bacteria win wrapped, warm, quiet spread on trays stir to cool harvest 40–48 h
Fig. 1 The koji tray and chamber. Shallow wooden trays are stacked crosswise so air passes over each one. A cloth keeps in the moisture, and a pan of hot water or a lamp warms the box. At the bottom, how a batch's temperature rises as the mould grows, and when to stir and spread.
  1. Wood. Use unpainted softwood with no resin smell. Japanese makers use cedar or cypress. Pine works if it is well aired. Bare wood soaks up surplus moisture and gives it back as the koji dries.
  2. Size. A good tray is about 45 × 30 cm with sides 5 cm high, of boards 1.2–1.5 cm thick, joined with wooden pegs rather than iron nails, which rust. One tray holds about 1–1.5 kg of steamed rice spread 2–3 cm deep. For bigger batches, use more trays rather than deeper ones.
  3. Feet or cross-stacking. Nail two battens under each tray, or stack the trays crosswise, so there is a 2–3 cm gap between each tray and the one above.
  4. Scald trays with boiling water before use and dry them in the sun afterwards. Never use soap. A good tray smells only of wood and faintly of koji.

The koji chamber

Any insulated box that holds 28–35 °C with damp air will do.

  • Simplest: a wooden chest lined with straw or Insulation and Keeping Buildings Warm or Cool, with a pan of hot water on the floor that you top up every few hours, and a damp cloth over the trays.
  • Better: a small room or cupboard (a muro) with thick walls of earth or timber, a charcoal brazier or a small stove outside with a flue running through, and a door you can open a crack to cool it. With electricity, a lamp of 40–60 W controlled by a thermostat works well.
  • Keep a thermometer pushed into the grain, not just hanging in the air. The grain will run several degrees warmer than the air.

Making rice koji

  1. Wash and soak 2 kg of polished rice for 8–12 hours; drain for an hour.
  2. Steam (do not boil) for 45–60 minutes, until a grain pressed between the fingers is soft and clear right through but the grains stay separate. Boiled rice is too wet and rots instead.
  3. Cool on a clean cloth to 35–38 °C, about blood warm, breaking up lumps.
  4. Inoculate with 1–2 g of tane koji per kg of rice, first mixed with a spoonful of flour so it spreads evenly. Mix well.
  5. Incubate heaped and wrapped in a cloth at 30–32 °C for about 18 hours, until it smells faintly of chestnuts and shows faint white fuzz.
  6. Spread it 3 cm deep on the trays, breaking clumps, and draw furrows in it with your fingers to let heat out. From now on the koji heats itself.
  7. Hold it under 40 °C. Check every 3–4 hours. Above 38 °C, stir, spread thinner, swap top and bottom trays, or open the chamber. Above 40–42 °C bacteria take over.
  8. Harvest at 40–48 hours from inoculation: every grain covered in short white fuzz, loosely bound into a mat, smelling sweet, of chestnuts or mushrooms. Stop just before a yellow-green tinge appears, which means it is starting to make spores.
  9. Use within a day, or dry it below 45 °C and keep it sealed for months.

Barley or soybean koji is made the same way. Soybeans for koji are soaked, steamed (not boiled) for 3–4 hours until soft, and usually mixed with roasted cracked wheat (see soy sauce below), because koji grows poorly on wet whole beans alone.

Keeping your own spores

Spread part of a batch on its own tray and let it grow on for 4–5 days, until it is thick with yellow-green powder. Traditional makers mix a little clean wood ash into the rice first (about 2% of its weight). Koji tolerates the ash, but most other microbes are slowed by it. Dry it below 45 °C, sieve off the powdery spores, and keep them sealed in glass in a cool, dark place. A teaspoon seeds many kilograms. Only do this from koji you know is pure. Spores bred from a contaminated batch carry the contamination forward.

Miso

Miso is mashed cooked soybeans mixed with koji and salt and left to age. Less salt and more koji make sweet white miso in weeks. More salt and less koji make dark red miso over a year or more.

Kind Soybeans (dry) Rice koji Salt Ageing
Sweet white 1 kg 2 kg 0.3 kg 3–8 weeks, warm
Everyday 1 kg 1 kg 0.45 kg 6–12 months
Dark red 1 kg 0.6 kg 0.5 kg 1–3 years
  1. Soak the soybeans in three times their volume of water for 12–18 hours, until a split bean is one colour right through.
  2. Cook in fresh water for 3–5 hours, skimming the foam, until a bean crushes easily between thumb and little finger. Undercooked beans make gritty miso. Save a litre of the cooking water.
  3. Mash the warm beans by pounding, mincing or treading in a clean tub, and cool to below 35 °C.
  4. Mix the koji with all but a handful of the salt, then into the mash, adding cooking water until the paste is as soft as modelling clay.
  5. Pack it into a crock or wooden tub by throwing it in as hard balls, to drive out the air pockets where mould grows, and press flat.
  6. Seal. Sprinkle on the last salt, lay a cloth directly on the surface, put on a wooden lid that fits inside, and weight it with stones at about a quarter of the miso's weight. Cover against dust and insects.
  7. Age in a cool, dark place; summer warmth speeds it. A dark liquid (tamari) rises round the edges: stir it back in or ladle it off as sauce.

Meju and doenjang: if you have no koji. The Korean method uses wild microbes instead. Shape mashed cooked soybeans into bricks about 20 × 15 × 10 cm (meju), dry them a few days, then hang them in loops of rice straw in a warm, airy room for 1–2 months while bacteria and moulds from the straw grow through them. Soak the bricks in brine for 1–2 months to make soup sauce (ganjang), then mash them with salt into paste (doenjang) and age it like miso. Because the moulds are wild it carries more risk: throw out any brick with bright yellow-green powder deep inside, pink or black growth, or a smell of rot rather than a strong, cheesy, earthy one.

Soy sauce

soybeans, soaked, steamed wheat, roasted and cracked 1 Beans + wheat, 1 : 1 inoculate, spread on trays, 25–30 °C 2 Koji, 2–3 days white, just turning pale green cloth 3 Moromi in 23% brine stir daily, then weekly JFMAMJJASON darker 4 Age 6–24 months through at least one summer; mash darkens to near black 5 Press in cloth bags slowly, over days 6 Heat to 70–80 °C, settle, bottle
Fig. 2 Soy sauce from start to finish. Steamed soybeans and roasted cracked wheat are grown into koji, then stirred into strong brine as moromi. After 6–24 months the mash is pressed in cloth bags, and the raw sauce is heated and settled.
  1. Beans. Soak 1 kg of soybeans for 12 hours and steam them for 3–4 hours until soft.
  2. Wheat. Roast 1 kg of wheat in a dry pan, stirring, until deep golden brown and smelling of toast, then crack it coarsely in a quern (Grain, Flour and Bread). The roasting gives much of the colour and aroma.
  3. Koji. Mix the warm beans with the wheat, which soaks up their surface water. At 35 °C inoculate with 2 g of tane koji and grow on trays as for rice koji, at 25–30 °C for 2–3 days, until the mass is bound with white mould just turning pale green.
  4. Brine. Dissolve 1.2 kg of salt in 4 litres of water (about 23% salt). A fresh egg floats high in it, showing a patch of shell the size of a large coin.
  5. Moromi. Stir the koji into the brine in a crock or barrel. Cover with cloth against flies.
  6. Stir daily for the first month, pushing the floating cap down, then weekly. The mash darkens to almost black and smells first of beer, then of soy sauce.
  7. Age at least 6 months, better 1–2 years, through at least one summer.
  8. Press slowly in strong cloth bags in a lever or screw press over several days (Oils and Pressing); fast pressing bursts the bags.
  9. Heat the raw sauce to 70–80 °C for 20 minutes to stop fermentation and deepen the flavour, let it settle a few days, and bottle the clear sauce. It keeps for years.

Tamari is the old style: the dark liquid that pools in a miso made of mostly soybeans and little or no wheat.

Fish sauce

  1. Use small, very fresh, whole fish (anchovies, sardines, sprats, herring), not gutted: the gut enzymes do the work.
  2. Layer 3 parts fish to 1 part salt by weight in a crock or wooden vat, with a thick layer of salt on top, and weight it with a board and stones so the liquid covers the fish. Cover it against flies but let gas out.
  3. Leave it somewhere warm, in the sun if possible, for 9–18 months, ladling the liquid back over the top now and then for the first months.
  4. Drain the clear liquid off through a tap near the bottom or a cloth, filtered through clean sand or fresh salt, and bottle it. Fresh brine poured over the remains gives a weaker second grade.

Good fish sauce is clear, reddish-amber and very salty, and smells strongly of fish but not of rot or ammonia.

Tempeh

  1. Dehull. Soak 1 kg of soybeans overnight, rub them hard between your hands under water so the skins float off, and pour the skins away.
  2. Boil for 30–45 minutes until just tender, with a tablespoon of vinegar in the water; the acid holds back spoilage bacteria.
  3. Dry and cool the beans on a cloth until their surfaces look dry and they are at 35 °C. Wet beans rot.
  4. Inoculate with a teaspoon of dry tempeh starter per kg, or crumbled fresh tempeh from a good batch. From nothing, press beans between the undersides of fresh sea-hibiscus leaves, incubate as below, and keep only a batch that grows evenly white and smells clean to seed the next.
  5. Pack the beans 2–3 cm thick in banana leaves, or in waxed cloth pricked with holes every 2 cm.
  6. Incubate at 30–32 °C. After about 12 hours the beans warm themselves and white threads appear. By 24–36 hours they are a firm, white cake you can slice, smelling of mushrooms and fresh bread.
  7. Use within 2–3 days, always cooked.

Grey or black spots near the air holes are harmless spores. A slimy surface, a smell of ammonia or rot, or pink, yellow or green colours mean the wrong microbes won: throw it out.

Tofu and the tofu press

THE PARTS, PULLED APART IN USE Weight 1–2 kg Follower 3 mm smaller all round Damp cloth Box 15 × 10 cm inside, 8–10 cm deep; 5 mm holes every 3 cm; no nails Grooved board tilted to drain Ladle in the curd soy milk at 70–80 °C, curdled with nigari or gypsum Press 15–20 min soft, 30–60 min firm whey then lift into cold water
Fig. 3 The tofu press. Hot soy milk is curdled with nigari, and the curd is ladled into a cloth-lined box with drain holes. A loose-fitting lid and weight squeeze out the whey.

Making soy milk and curd

  1. Soak 500 g of soybeans for 10–14 hours.
  2. Grind them with 3 litres of water to a fine white slurry in a quern fed with beans and water together (Grain, Flour and Bread).
  3. Boil in a pot four times the slurry's volume, because it foams hugely, and simmer 10 minutes, stirring the bottom. Boiling destroys the substances in raw soy that block digestion.
  4. Strain through a cloth bag, squeezing with a paddle. The liquid is soy milk; the pulp (okara) goes into bread and fritters or to the animals.
  5. Coagulate. At 70–80 °C, add the coagulant dissolved in a cup of warm water:
    • Nigari (bittern): about 10 g (1.5–2% of the dry bean weight).
    • Gypsum (finely ground, burnt gypsum): 10–15 g (2–3%). It gives softer, smoother tofu.
    • Strong vinegar works in a pinch, but the tofu is crumbly and sour.
  6. Stir briskly, pour in a third of the coagulant, stop the swirl, and sprinkle the rest over the top. Cover for 5–10 minutes. Soft white curds separate from clear, pale yellow whey. If the whey is still milky, add a little more coagulant.

Building and using the press

  1. Box. Make a box of hardwood, about 15 × 10 cm inside and 8–10 cm deep for this batch, with 5 mm drain holes about 3 cm apart in the bottom and sides. Use pegged or dovetailed joints, because iron nails stain tofu (Doors, Windows and Joinery). Leave the wood unfinished.
  2. Follower. Make a lid that slides inside the box with about 3 mm clearance all round.
  3. Use. Line the box with damp cheesecloth, ladle in the curds, fold the cloth over, and put the follower on top with 1–2 kg of weight. Press 15–20 minutes for soft tofu, 30–60 minutes for firm.
  4. Lower the press into cold water, lift off the box, and let the tofu firm for 10 minutes before unwrapping it.

Keep tofu under cold water, changed daily, and eat it within 3–4 days, or freeze, dry or smoke it (Preserving Food). A good press gives a square-edged, smooth block that holds together when lifted. Too few drain holes make wet tofu that breaks; too much weight makes it rubbery.

How to tell it worked

  • Koji: white, evenly furred grains, sweet chestnut smell, no slime, no colours other than white and a hint of yellow-green. Chew a grain: it tastes faintly sweet.
  • Miso: smells sweet, winey and savoury, tastes deeply salty-savoury, and is the even colour of its kind. A thin film of white yeast on top is normal: scrape it off.
  • Soy sauce: clear, dark red-brown when you hold it up to the light, with a rich smell and a long, savoury taste. A thin white film of yeast on the moromi is common and harmless; skim it.
  • Fish sauce: clear amber, fishy but not rotten.
  • Tempeh: a firm, white, sliceable cake.
  • Tofu: smooth, holds its shape, tastes clean and slightly sweet.

Note Troubleshooting.

  • Koji slimy and smelling sour or of old socks → rice too wet, or it ran too hot. Steam rather than boil; keep it under 40 °C.
  • Koji will not grow → spores dead, or the chamber was too cold. Test spores on a small batch.
  • Miso has mould on top → air pockets or too little salt on the surface. Scrape off white or pale mould with 1–2 cm of miso under it. Throw out the batch if mould is black, pink or deep inside.
  • Moromi smells putrid → too little salt. Check the brine with the egg test.
  • Tofu will not curdle → milk too cool or too little coagulant.
  • Tofu crumbles → stirred too hard after adding the coagulant.

Dangers

Danger Wild "koji" can poison you. Aspergillus flavus looks almost the same as koji, yellow-green and powdery, and makes aflatoxin, which damages the liver and causes liver cancer. Cooking does not destroy it. Never grow koji from wild mould or from mouldy grain, beans or nuts. Only use spores from a known food culture, and throw out any batch that grows the wrong colour or smells wrong.

Danger Tempeh and other unsalted mould ferments can carry dangerous bacteria if the beans were not cooked well, were too wet, or sat warm too long. Cook tempeh before eating it. Throw out slimy or ammonia-smelling batches. A rare but deadly poison (bongkrekic acid) has come from tempeh made with coconut, so only make tempeh from soybeans and other legumes.

  • Too little salt in long ferments lets rot set in. Weigh it; never cut it.
  • Fish sauce from fish that were not fresh can carry histamine, causing flushing, headache and vomiting. Salt fish the day they are caught.
  • Salt and health. A tablespoon of soy sauce holds about 1 g of sodium, nearly half a day's healthy amount (Chronic Diseases).
  • Soy allergy is real. Raw soybeans upset the stomach; always cook beans and boil soy milk.
  • Boiling soy slurry foams over violently and scalds. Use a tall pot and never leave it.

What this unlocks

Koji opens the door to sake, rice vinegar (Vinegar and Pickling), Chinese grain spirits and other mould-saccharified drinks (Spirits, Sake and Liqueurs). It also gives a way to make sugars from starch without malting, using a grain or climate where barley won't grow. Tofu, tempeh and soy milk give protein where meat and dairy are scarce (Nutrition and Deficiency Diseases). Okara and press cakes feed animals (Fodder Crops and Winter Feed). Soybeans' oil can be pressed (Oils and Pressing) and the meal left over feeds pigs and chickens. The same skills of controlling temperature, moisture and salt carry over to Culturing Microbes and, much later, to growing penicillin (Penicillin).

How it was first done

Salted, fermented pastes called jiang were made in China by the time of the Zhou dynasty, nearly 3,000 years ago, first from meat and fish and later from soybeans and grain. Mould cultures for brewing, called qu, are described in Chinese texts from about 2,000 years ago, and the 6th-century farming book Qimin Yaoshu gives detailed recipes for jiang and fermented beans. Soy sauce grew out of the liquid that pooled in jiang. Buddhist monks, who ate no meat, carried these foods to Korea and Japan. By the 13th century, legend says through the monk Kakushin, Japanese miso and the tamari that seeped from it were made at Yuasa, which became a centre of Japanese soy sauce. By the 1400s, guilds in Kyoto held the right to make and sell koji, and specialist spore makers came to sell dried koji spores as a trade product. They were among the first people anywhere to keep a microbial culture pure on purpose.

Fish sauce was made around the Mediterranean as garum by Greeks and Romans, in huge salting tanks along the coasts of Spain and North Africa, and independently in South-East Asia, where it is still the main seasoning. Tempeh comes from Java; it is first mentioned in writing in the early 1800s but is probably older. Tofu is credited by legend to the Han prince Liu An in the 2nd century BC, but the first sure written mention is from the 10th century AD, under the Song dynasty.

Source: content/entries/food/soy-sauce-and-miso.md