Part 11 · Power and Energy
Firewood and Coppicing
How much wood a household, a forge and a furnace really burn, which woods give the most heat, how to dry it so it burns well — and how to cut trees in a way that makes them grow back, so your fuel never runs out.
- Difficulty
- ●●●●●
- Time
- An afternoon to cut a winter's fuel once the woodlot is running; 7–20 years for a new coppice to come into full rotation
- Steps from zero
- 14 prerequisites →
You need first
Axes, Chisels, Knives and PlanesThis unlocks
Forestry and Tree NurseriesThe full path from nothing — 14 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Blacksmithing
- Steel
- Axes, Chisels, Knives and Planes
- Firewood and Coppicing
Do them roughly in this order. See it on the tech tree →
Why it matters
Until about two hundred years ago, wood was almost the only fuel there was, and even today around two billion people still cook with it. Every chapter about heat in this book — Pottery, Lime, Bricks, Glass, Salt, Iron (the Bloomery), the The Steam Engine — quietly assumes a pile of fuel. That pile is enormous. A single iron furnace can eat a forest, and a cold village can strip every tree within a day's walk in a few winters.
Communities that rebuilt well did not just cut wood; they farmed it. Most broad-leaved trees, cut down to a stump, send up a ring of new shoots that grow into straight poles in a few years. Cut those, and they grow again — for centuries. This is coppicing, and a well-run coppice gives the same harvest every year forever, together with poles for fences, tool handles, baskets, charcoal and building. It is the oldest sustainable energy system on Earth, and with an axe and a plan it is yours.
This chapter covers how much you need, which wood to burn, how to dry it, and how to lay out a woodlot that never runs out. Turning wood into a hotter fuel is in Charcoal; burning it efficiently is in Chimneys, Stoves and Heating; turning it into a gas for engines is in Biogas and Wood Gas and Gas Engines and Producer Gas.
How it works
All dry wood carries about the same energy per kilogram. Oven-dry wood of almost any species gives about 18–20 MJ per kg (other fuels: Materials Data Tables) (a megajoule is the heat needed to warm about 3 litres of water from cold to boiling). What differs between species is density: a log of oak weighs nearly twice as much as the same log of poplar, so it holds nearly twice the heat, burns twice as long and takes up half the space in the woodshed.
Water steals heat. Freshly cut ("green") wood is 40–55% water by weight. Before that wood can burn, the fire has to boil all that water away, which uses up a large part of its heat and cools the fire so it smoulders and smokes. Dried ("seasoned") wood at 15–20% water gives roughly 50–80% more useful heat per kilogram than green wood, lights easily, and burns hot and clean. Seasoning is the cheapest improvement you will ever make to any fire.
| Fuel | Heat per kg | Notes |
|---|---|---|
| Green wood (50% water) | about 8 MJ | Smoky, hard to light, coats chimneys with tar |
| Seasoned wood (20% water) | about 15 MJ | The normal firewood standard |
| Oven-dry wood | 18–20 MJ | What wood gives in a gasifier or kiln after drying |
| Charcoal | 28–31 MJ | Hotter, smokeless, but costs 4–5 kg of wood per kg |
| Coal | 24–32 MJ | See Coal and Coke |
Why coppicing works. A tree keeps most of its food store in its roots. When the trunk is cut in winter, the living root system is untouched, and in spring it pushes up dozens of buds from around the cut stump (the stool). These shoots grow far faster than a seedling — often 1–2 m in the first year — because they draw on a root system built for a whole tree. The stool lives on, and many coppice stools are several hundred years old, far older than the tree would have lived uncut.
How much do you need?
These are rough figures for planning. Measure your own use in the first year and adjust.
| Use | Wood needed (seasoned) | Notes |
|---|---|---|
| Cooking on an open three-stone fire | 1.5–2.5 kg per person per day | A family of five: about 3–4 tonnes a year |
| Cooking on a closed clay or rocket stove | 0.7–1.2 kg per person per day | Halves the wood and the smoke |
| Heating a small house through a cold winter | 4–10 tonnes a year | Open fireplace at the high end; a good masonry stove at the low end |
| A blacksmith's forge (on Charcoal) | 10–20 kg charcoal a working day = 50–100 kg of wood | About 15–25 tonnes of wood a year for a full-time smith |
| One Iron (the Bloomery) bloomery smelt | 40–60 kg charcoal = 200–300 kg of wood | Per bloom of a few kilograms |
| One firing of a The Kiln or Lime kiln | 0.5–3 tonnes of wood | Depends on size; lime takes the most |
| A small charcoal blast furnace | 8–15 tonnes of wood per tonne of iron | Needs hundreds of hectares of coppice |
Measuring wood. Firewood is measured stacked. A stere is a stack 1 m × 1 m × 1 m; because of the air gaps it holds only about 0.65 m³ of solid wood — roughly 450–500 kg of seasoned hardwood or 300–350 kg of light wood like willow or poplar. The old English and American cord is a stack 4 ft × 4 ft × 8 ft (1.2 × 1.2 × 2.4 m), about 3.6 steres, or 1.5–1.8 tonnes of seasoned hardwood.
How much land. A well-tended temperate coppice of hazel, oak, ash, chestnut or alder grows about 3–6 tonnes of dry wood per hectare per year. Willow and poplar on good wet ground grow 8–12 tonnes. Tropical trees such as eucalyptus, leucaena or acacia can do more again. So:
- A household needing 6 tonnes a year needs roughly 1.5 hectares (two football pitches) of ordinary coppice, or under one hectare of good willow.
- A village of 30 households needs 30–50 hectares, plus more for its smith, potter and lime-burner.
Plan the woodlot before you need it. A new coppice takes 5–15 years to give its first full crop.
What you need
| Item | Purpose |
|---|---|
| A good felling axe, 1.5–2 kg head | Cutting stools and poles. See Axes, Chisels, Knives and Planes |
| A billhook or light hatchet | Trimming side branches, cutting small shoots cleanly |
| A bow saw or crosscut saw | Cutting logs to length with less waste (Files and Saws) |
| A splitting maul (3–4 kg) and 2–3 iron or hardwood wedges | Splitting rounds |
| A chopping block | A wide round of tough wood, knee height |
| Cord or chain, and a sledge or cart | Hauling (Wagons and Carriages) |
| A woodshed or stacking place | Off the ground, roofed, open-sided |
Without iron, stone axes will cut coppice poles up to about 10 cm across — Neolithic farmers managed whole coppiced landscapes with nothing else — but iron makes the work several times faster. See Stone Tools and Basic Woodworking for felling and splitting technique.
Where to find it
Good coppice trees are the broad-leaved trees that sprout strongly from the stump:
- Hazel — many-stemmed shrub of woodland edges; soft, round, toothed leaves; nuts in autumn. Rotation 6–10 years. Poles for hurdles, beanpoles, thatching spars and fuel.
- Willow — wet ground, river banks; long narrow leaves, silvery underneath; the fastest of all. Rotation 1–4 years for basket rods and fuel. Cuttings as thick as a thumb and as long as a forearm, pushed into wet soil in winter, root by themselves — the easiest way to start a new coppice.
- Ash — compound leaves, black buds in winter. Rotation 12–25 years. Excellent firewood; tool handles (The Lathe).
- Oak — lobed leaves, acorns. Rotation 15–30 years. Dense, hot firewood, the best charcoal, and tan bark for Hides and Leather.
- Sweet chestnut — long saw-toothed leaves, spiny husks. Rotation 12–20 years. Rot-proof fence posts; good charcoal (spits sparks on an open fire).
- Alder — wet ground; small woody "cones". Rotation 15–20 years. Light firewood but excellent charcoal; regrows in bogs where nothing else will.
- Hornbeam, lime (linden), maple, sycamore, birch, eucalyptus, acacia — all coppice. Hornbeam is among the hottest-burning woods there is.
Poor coppice trees: almost all conifers (pine, spruce, fir, larch) die when cut — they must be replanted. Beech coppices weakly and is better grown as tall trees.
Heat by species. Since heat follows weight, a rough ranking by density (seasoned wood):
| Heat per stacked cubic metre | Woods |
|---|---|
| Highest | Hornbeam, oak, hickory, beech, ash, apple, holly, eucalyptus, acacia |
| Good | Birch, maple, cherry, elm, sweet chestnut, hawthorn |
| Moderate | Pine, larch, alder, sycamore, hazel |
| Low | Willow, poplar, aspen, lime, spruce, fir |
Light woods are not useless: they catch quickly and are perfect kindling, bread-oven fuel and charcoal stock. They just burn fast, so you need more of them. Conifers spit sparks and make more soot; burn them dry and in a stove, not on an open floor. Ash is unusual in holding little water even when green (about 30–35%), which is why old sayings praise it as the one wood that "burns wet".
Step by step: starting a coppice
- Choose the ground. Use land near home (fuel is heavy to carry), on a slope or poorer soil that is not your best farmland. A woodlot within 1 km saves months of hauling over the years.
- Use what is there. If there is existing broad-leaved woodland, you already have a coppice — just start cutting it on rotation (below). Leave the best straight oaks or ash as standards: about 30–50 tall timber trees per hectare, spaced 15–20 m apart, to grow on for building beams. This "coppice with standards" gives both fuel and timber.
- Planting new. In winter, plant rooted saplings or willow and poplar cuttings 1.5–2.5 m apart (about 2,000 per hectare). Keep the grass and weeds cleared from around them for the first two summers — they choke young trees.
- First cut. When the young trees are wrist-thick (3–6 years for most, 1–2 for willow), cut them all down to a stump about 10 cm above the ground. This "stools" them and starts the cycle.
Step by step: cutting a coupe
- Divide the woodlot. Split it into as many equal blocks (coupes) as the rotation has years. With a 10-year rotation, make 10 coupes and cut one each winter. In year 11 you are back at the first one, which has regrown. Mark corners with stones or posts and write down the plan.
- Cut in the dormant season, after the leaves fall and before the buds burst — roughly late autumn to early spring. Wood cut then holds less sap and the stool regrows strongly. Cutting in summer weakens and can kill the stool.
- Cut low and clean. Cut each stem 5–15 cm above the stool, with a slanting cut that faces outwards so rain runs off. Work from the outside of the stool inwards. Never leave a torn, split stump: rot gets into ragged wood and kills the stool. Use a sharp axe or billhook in one or two clean strokes, or a saw.
- Sort as you go. Straight poles for building and tools in one pile; firewood lengths in another; brushwood (twigs and tops) in a third.
- Protect the regrowth. This is where most coppices fail. Deer, goats, cattle, sheep and rabbits love the tender young shoots and will kill the stools in one summer. Pile the brushwood into a dead hedge around the coupe — two rows of stakes a pace apart with the brush packed between them, chest high — or fence it, and keep animals out for 3–5 years until the shoots are out of reach.
- Fill gaps. Where a stool has died, peg a long shoot from a neighbouring stool down into the soil (this is layering); it roots and becomes a new stool in two years.
Pollarding is coppicing at a height of 2–3 m (above the reach of grazing animals), so that cattle or sheep can graze under the trees while the crop grows above them. Climb or use a ladder and cut every branch back to the trunk-top, on the same rotation as coppice. Willow, ash, oak, hornbeam and lime pollard well, and their leafy branches cut in summer make leaf hay for winter fodder (Keeping Animals). Pollards are slower and more dangerous to cut — falls from ladders are common — so coppice wherever you can keep animals out.
Step by step: seasoning firewood
- Cut to length. Saw or chop into lengths that fit your hearth or stove — usually 25–50 cm.
- Split. Split everything thicker than about 10 cm (a wrist). Water leaves wood mainly through the cut ends and split faces; bark is nearly waterproof. A split log dries in half the time of a round one. Split green wood — it splits far more easily than dry. Stand on the far side of the block, aim at the far edge of the round, and let the maul's weight do the work.
- Stack it off the ground on two poles or a row of stones, bark side up on the top layer to shed rain.
- Roof the top, open the sides. Wind does more drying than sun. Build stacks in a sunny, breezy place with the long side facing the usual wind. A roof of bark, boards or thatch keeps the rain off; never wrap the sides.
- Wait. Most hardwoods need 6–12 months in a dry, windy summer; oak needs 18–24 months. Light woods (willow, poplar, birch) dry in 3–6 months. Cut this winter, burn next winter — or the one after for oak.
- Bring in a week's supply to a covered place near the fire. Never store wood touching a stove or hearth.
How to tell it worked
Seasoned wood:
- Has cracks (checks) radiating from the centre on the cut ends.
- Is noticeably lighter — it has lost a third or more of its green weight.
- Gives a sharp hollow clack when two pieces are knocked together. Green wood gives a dull thud.
- Bark is loose or falls away easily.
- Burns cleanly: lights from kindling in a minute or two, gives bright yellow flames and little smoke, and does not hiss, bubble or ooze water and froth from the cut ends.
A simple moisture test. Weigh a split piece (a balance, see Measurement from Scratch), then dry it beside the fire for several days until its weight stops falling. If it lost less than a fifth of its starting weight, it was well seasoned. If it lost a third or more, the rest of the stack needs more time.
A coppice is healthy when cut stools put up 10–30 vigorous shoots within a year, few stools die, and each coupe yields about the same amount of wood each time it comes round.
Note Troubleshooting. Wood still hisses after a summer → stack too tight, in shade, or the sides were covered; restack in the open, split smaller. Fire smoulders and chimney drips black tar → wet wood; see Dangers. Stack rotting at the bottom → it is touching the ground; raise it on poles or stones. Cut stools not regrowing → cut in summer, cut too high and torn, or shoots eaten. Fence better; cut only in winter. Shoots grow but then thin out and die → shaded by standards or by an overgrown neighbouring coupe; thin the standards. Running short every winter → you are burning faster than the woodlot grows. Fit better stoves before you cut more; a good stove halves consumption.
Dangers
Danger Felling kills. Most woodland deaths come from falling trees and branches. Before felling anything larger than a pole, look up for dead branches ("widow-makers") that can drop on you. Plan the fall line and two escape routes at 45° behind you; never stand directly behind a falling trunk, which can kick back off its stump. Never work alone at felling, never fell in strong wind, and never try to free a tree hung up in another by cutting the one it rests on. See Basic Woodworking, and Forestry and Tree Nurseries for felling big trees.
Danger Wet wood sets chimneys on fire. Smoky fires from green wood coat the inside of a chimney with creosote — black, sticky, flaky tar. It can ignite in a roaring chimney fire that cracks masonry and sets roofs alight. Burn only seasoned wood, run a hot fire for a while each day, and sweep chimneys at least once a year. See Chimneys, Stoves and Heating.
- Axe and maul injuries. Keep blades sharp (a blunt axe glances off). Chop with feet apart and the log on a block, so a miss hits the block or the ground, not your shin. Wear stout boots. Nobody else within two axe-lengths.
- Carbon monoxide. Any fire indoors without a good draught makes this odourless poison — see Fire.
- Ladders and pollards. Tie ladders to the trunk. Never cut above your head with an axe.
- Toxic wood smoke. Do not burn poison ivy, poison oak, oleander, or painted, tarred or salvaged treated timber. Yew is poisonous to livestock — keep its brash away from animals.
- Stack collapse. Tall stacks fall on children. Keep stacks below chest height, or brace the ends with crossed "cribs".
- Back injuries. Wood is heavy. Use carts, sledges and rollers; split where it falls.
What this unlocks
A steady supply of fuel underpins every fire-based craft: Charcoal for Iron (the Bloomery), Steel and the forge; firing for Pottery, Bricks and Lime; boiling for Salt, Sugar and Soap; and steam for the The Steam Engine. Coppice poles give hurdles and wattle for Cob, Adobe and Rammed Earth, rods for Baskets and Containers, handles and turning wood for the The Lathe, and fuel for wood-gas engines (Biogas and Wood Gas, Gas Engines and Producer Gas).
When the demand outgrows the woodlot — as it did in 17th-century England — the answer is Coal and Coke. But keep the coppice: it is the one fuel that grows back by itself, without mines, wells or machines.
How it was first done
Coppicing is at least six thousand years old. The Sweet Track, a wooden walkway across the Somerset Levels in England, was built from poles felled in the winter of 3807–3806 BC; many of them are long, straight, even-aged rods of hazel, ash, oak and lime that could only have come from coppiced stools. Roman writers describe chestnut and willow coppices for vine stakes, and medieval European woods were run as coppice-with-standards on fixed rotations, recorded in estate books for centuries — some English woods have been cut on the same rotation since the Middle Ages, and stools of ash and lime there are many centuries old.
Coppices fed the charcoal iron industries of the Weald of England, the Forest of Dean and Sweden, and ironmasters managed whole districts of woodland on rotation to keep their furnaces in charcoal. Pollarded trees, many over 500 years old, still stand in the wood-pastures of England, France and Spain. In the tropics, people have coppiced and pollarded trees for fuel and fodder for just as long, and fast-growing coppice of eucalyptus and acacia still fuels much of the world's cooking.
Source: content/entries/energy/firewood-and-coppicing.md