◆ Rebuild

Part 8 · Chemistry

Fluorspar and Fluorine Compounds

Fluorspar is a glassy, often purple mineral that makes slags and enamels flow. Its acid, hydrofluoric acid, is the only common substance that eats glass, and it is so treacherous that this chapter gives only its outline and its first aid. The safe ways to frost and mark glass, the role of cryolite in making aluminium, and the double edge of fluoride in drinking water are covered in full.

Difficulty
●●●●●
Time
An hour to frost a pane by hand; a day to build a sandblaster; a week to set up a bone-char filter
Steps from zero
11 prerequisites →

You need first

Sulfuric AcidLaboratory Glassware

This unlocks

—
The full path from nothing — 11 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Sulfur
  4. Pottery
  5. The Kiln
  6. Lime
  7. Lye and Potash
  8. Glass
  9. Saltpeter
  10. Sulfuric Acid
  11. Laboratory Glassware
  12. Fluorspar and Fluorine Compounds

Do them roughly in this order. See it on the tech tree →

Why it matters

Fluorspar (the mineral fluorite, calcium fluoride) is the gentlest of fluorine compounds and one of the most useful. Its name comes from the Latin fluere, "to flow", because a handful thrown into a furnace makes thick slag run like water. It is used in steelmaking, welding rods, enamels and aluminium smelting.

From fluorspar comes hydrofluoric acid. It is the only common acid that dissolves glass. That makes it valuable for marking burettes and thermometers, frosting lamp globes and cleaning castings. It also makes it one of the most dangerous substances in this book. It soaks through skin without pain and kills from the inside. This chapter explains what it does and how to treat a burn, but not how to make it. For almost every job, there is a safer way, and this chapter teaches those.

Fluorine also matters to everyone who drinks water. A trace of fluoride in water hardens children's teeth against decay. A little more mottles them brown, and a lot cripples the skeleton. Knowing which you have, and how to remove it, protects whole towns (Water Treatment for a Town).

How it works

As a flux. A flux is a substance that helps something melt at a lower temperature or flow more easily. Fluorspar melts at about 1,400 °C by itself, but in a slag full of lime it breaks up the stiff, tangled structure of the molten rock, so the slag runs thin without becoming acid. Steelmakers can then use plenty of lime to pull sulfur and phosphorus out of the metal and still tap a runny slag (Steel in Quantity, The Electric Arc Furnace). In glass and enamel, a few percent of fluorspar helps the batch melt. More of it makes tiny crystals form as the glass cools, which turns it milky white, as in opal glass and white enamel (Enamel on Metal).

As an acid. Strong sulfuric acid drives hydrogen fluoride out of fluorspar. Glass is a network of silicon and oxygen, and fluorine grips silicon more tightly than oxygen does. So hydrogen fluoride pulls glass apart into a gas (silicon fluoride), and the surface it touches becomes rough and frosted.

In the body. This is what makes hydrofluoric acid different from every other acid:

  1. It does not burn on contact. Dilute acid feels like nothing for minutes or hours. Stronger acid stings a little. Meanwhile it passes straight through the skin.
  2. It poisons the deep tissues. Underneath, fluoride grabs the calcium and magnesium that nerves, muscle and bone need. The tissue dies, slowly and with terrible pain, down to and into the bone.
  3. It poisons the whole body. Enough fluoride in the blood strips calcium from it, and the heart stops. A splash of concentrated acid the size of a palm can kill.
Ordinary acidHydrofluoric acid burns the surface and hurts at once,so you wash it off skindermisfatmusclebone No pain at firstsoaks through the skinDying tissuedeep, hours later, agonyFluoride grabscalciumfrom cells and boneheart stops fluoride calcium Antidote: wash 5 min, then rub in calcium gel
Fig. 1 Why hydrofluoric acid is uniquely dangerous. An ordinary acid burns the surface at once and hurts, so you wash it off. Hydrofluoric acid passes through the skin without pain, then fluoride pulls calcium out of the tissues and blood, killing deep tissue and, if the burn is large, stopping the heart. The antidote is calcium, rubbed in as a gel.

In teeth. Tooth enamel is a calcium phosphate mineral. A trace of fluoride swapped into it makes it more resistant to the acid that mouth bacteria make from sugar. Too much fluoride while teeth are forming disrupts the enamel itself.

Fluorspar

Where to find it

  • Veins in limestone and around granite, with lead ore (galena), zinc blende, white calcite, heavy white barite and quartz (Lead, Finding and Identifying Ores). Old lead-mining districts often have heaps of discarded fluorspar.
  • Look: glassy, transparent to translucent crystals, often cubes, coloured purple, green, yellow, blue, pink or colourless, often in bands. The banded purple-and-yellow kind from Derbyshire in England is called Blue John.
  • Test: it breaks along neat flat faces into eight-sided pieces. An iron nail scratches it, but a fingernail does not (hardness 4). It is heavier than quartz or calcite and does not fizz in acid. Many pieces glow violet-blue under ultraviolet light. The word fluorescence was coined from this mineral. Some glow faintly when heated on a hot iron plate in the dark.

Using it as a flux

Use How much Notes
Basic steel slag (Steel in Quantity, The Electric Arc Furnace) 2–5 kg per tonne of steel Thins a lime slag; add in small lumps
Welding rod coating (Welding) About 15 % of the coating Low-hydrogen rods for tough welds
Opal glass, white enamel (Glass, Enamel on Metal) 5–10 % of the batch Makes the glass milky; melt outdoors
Aluminium cell bath (Aluminium) 4–6 % with the cryolite Lowers the melting point
Magnesium refining (Magnesium) A little in the salt flux Helps metal droplets join
Smelting stubborn ores (Finding and Identifying Ores) A handful per charge Old miners' trick for sticky slags

Fluorspar fluxes give off some fluoride fumes. Melt outdoors or under a hood with a strong draught, and keep grazing animals away from the smoke.

Optical fluorite. Rare, perfectly clear pieces bend light with very little colour fringing. Ground into lenses, they make the finest microscope objectives, called apochromats (Optical Glass and Achromatic Lenses, The Microscope).

Hydrofluoric acid: outline and safety only

Danger Do not make or use hydrofluoric acid unless you have no alternative, are trained, and have the antidote ready. Use the abrasive methods below to mark and frost glass. This section exists so that people who meet the acid, in old stores, in an aluminium or phosphate works, or in someone else's workshop, know what it is and how to treat a burn.

In outline: fluorspar heated with strong sulfuric acid in a closed iron or lead vessel gives off hydrogen fluoride gas, which dissolves in water to make the acid. Glass cannot hold it. It was kept in bottles of lead, gutta-percha or wax, and today in polythene (Petrochemicals and Modern Plastics). The same fumes come off when phosphate rock is treated with acid (Chemical Fertilisers, Phosphorus), and that is why those jobs are done outdoors. The Aluminium chapter describes its industrial use for cryolite.

What it was used for: etching scales on burettes, thermometers and measuring glasses; frosting light bulbs and lamp globes; decorative "acid-etched" glass; cleaning sand from iron castings; making cryolite and other fluorides.

Signs of exposure

  • Skin: often nothing at first. Then, within minutes to a day, deep throbbing pain out of proportion to the small white or grey patch on the skin. Under the fingernails, pain is severe and the nail may need to come off.
  • Eyes: pain and clouding; blindness if not washed at once.
  • Breathing fumes: cough, choking and a burning chest. The lungs can fill with fluid hours later, even after the person felt better.
  • Whole body: muscle twitching and cramps, an irregular pulse, collapse.

First aid

  1. Wash at once with large amounts of running water for 5 minutes while you strip off contaminated clothes, rings and watches. Whoever helps must wear gloves.
  2. Then rub in calcium gel, over and beyond the burn, and keep rubbing it in for at least 15 minutes, adding more gel each time the pain returns. Hospitals use 2.5 % calcium gluconate in a water-based jelly. Calcium is the antidote, because it gives the fluoride something to bind with other than the body.
  3. Eyes: wash with clean water for at least 15 minutes, holding the lids open. Do not put gel in the eye.
  4. Fumes: take the person into fresh air, keep them resting and warm, and watch their breathing for 24 hours.
  5. Swallowed: give milk or water to drink. Do not make them vomit.
  6. Get the best medical help you can for any burn larger than a coin, any burn from concentrated acid, any fume exposure, and anything swallowed (Emergencies). Doctors inject calcium under and around the burn and into the blood.

Warning No calcium gel ready, no hydrofluoric acid. Anyone who handles it must have the gel within reach before the bottle is opened. If you cannot get calcium gluconate, keep a gel made from a soluble calcium salt in a starch or gum jelly. Soluble calcium salts include calcium lactate, which forms when chalk is stirred into soured whey, and calcium chloride, made from limestone and Hydrochloric Acid. These are poorer substitutes, so get the person to medical help even faster. Chalk paste is useless, because chalk does not dissolve.

Etched glass: the safe ways

Etched glass is glass whose surface has been roughened in a pattern so it scatters light. The roughened parts look white and frosted against the clear glass. Uses include measuring marks on Laboratory Glassware, frosted panes for bathroom and office windows (Window Glass), lamp shades that soften glare (Lamps and Candles), ground-glass focusing screens for cameras (Photography), signs, and decoration. All of it can be done with abrasives instead of acid.

Ground glass by hand

The simplest frosting. It is also how a camera's focusing screen and a ground glass stopper are made (Laboratory Glassware).

  1. Lay the glass flat on a folded cloth on a level table.
  2. Sprinkle a teaspoon of fine emery or carborundum grit (about 100–200 mesh, flour-fine to the touch; see Abrasives and Grinding Stones) on it, with a few drops of water.
  3. Rub it with a second piece of glass or a flat iron or stone block, in small overlapping circles with light, even pressure.
  4. Wash the grit off every few minutes and look through the glass at a window. Keep going until there are no clear spots. For a 10 × 12 cm focusing screen this takes 20–40 minutes.
  5. For a finer, silkier frost, finish with a finer grit, about 400 mesh, for 10 more minutes.

Two plates ground together come out frosted at the same time. Good ground glass shows an even, fine grey that sharply catches a projected image. Scratches or clear patches mean grit that was too coarse, or uneven pressure.

Frosting with a stencil by hand. Cover the glass with a resist: something the grit cannot get through. Use a thick layer of hide glue, paper glued down, or a sheet of rubber or thick tape (Glues and Adhesives, Rubber). Cut away the resist where you want frost, and rub only there, using a small felt or leather pad charged with grit.

Marking measuring glasses

Laboratory Glassware shows how to scratch marks through a wax coat. To make them permanent and easy to read:

  1. Coat the glass with a thin film of beeswax with a little pine resin, melted and brushed on warm.
  2. Scratch the lines through the wax with a steel point. Use a ruler or dividing jig for the scale (Measurement from Scratch).
  3. Rub a paste of fine emery and oil into each line with a sharpened stick or a fine wire, back and forth, for a minute. This grinds a shallow frosted groove.
  4. Clean off the wax with hot water and a cloth. Rub black or red pigment in oil into the grooves and wipe the surface clean (Pigments, Paints and Varnish).

A diamond, corundum or hardened steel point (Industrial Diamond and Hard Abrasives, Synthetic Gems) cuts a mark directly. A small copper wheel turning in a lathe with emery and oil cuts clean lines and lettering. This is glass engraving (Engraving, Seals and Etching, The Lathe).

The sandblaster

A jet of air carrying hard grit wears glass away wherever it strikes, and does it fast and evenly. A rubber stencil protects the rest. Benjamin Tilghman invented it in 1870.

Compressed air3–6 bar, withwater trap Grit hopperalumina, emery or garnetnever quartz sand Mixing Trushing air sucksgrit up from below Windowclosed cabinetGlassrubber stencilFrostedwhere cut awayNozzle3–6 mm boreglove holes with long leather gloves; dust outlet to a cloth bag 10–20 cm
Fig. 2 The sandblaster. Air from a compressor rushes through a nozzle and sucks grit up from a hopper; the jet of grit frosts the glass where the rubber stencil has been cut away. Work inside a closed cabinet with a window and glove holes; never use quartz sand, whose dust causes silicosis.

Parts:

Part Size Made from
Air supply 3–6 bar (3–6 times air pressure), 100–300 litres of air a minute Bellows to Air Compressors, with a tank and a water trap
Grit hopper 2–5 litres, a cone with its tip at the bottom Sheet iron or a tin (Sheet Metal and Rolling)
Mixing T The air pipe runs straight through; the grit tube joins from below Brass or iron fittings
Nozzle Bore 3–6 mm, 5–8 cm long Hardened steel or fired alumina (Alum and Alumina); cast iron wears out in hours
Cabinet About 60 × 50 × 50 cm Wood or sheet iron, with a glass window, two glove holes with long leather gloves, and an outlet to a dust bag
Grit 60–120 mesh Alumina, emery, garnet or crushed iron slag. Never quartz sand.

How it works. Air rushing through the T sucks grit up from the hopper, like a perfume spray. Some builders put the grit in a closed pressure pot instead. That cuts faster but needs a stronger tank (Pressure Vessels and Valves).

Using it:

  1. Glue a sheet of rubber 1–2 mm thick over the glass. Draw the design and cut away the parts to frost with a sharp knife.
  2. Inside the closed cabinet, hold the nozzle 10–20 cm from the glass and move it steadily, as if spray-painting. A light frost takes seconds. A deep carved letter takes minutes.
  3. Peel off the stencil and wash the glass.

Good or bad: an even, white frost with crisp edges is good. A blotchy or streaky frost means the nozzle moved unevenly or the grit was damp. Chipped edges mean the pressure was too high or the stencil was too thin.

Acid etching (outline only)

Factories once dipped waxed and scratched glass in hydrofluoric acid, or hung it over the acid's fumes, to etch scales and patterns. Frosting baths of acid with fluoride salts give a smooth satin finish that abrasives cannot quite match. This is skilled, dangerous work for a trained chemist with a fume cabinet, a full face shield, long gloves of rubber, and calcium gel at hand. For everything in this book, use the abrasive methods.

Cryolite and aluminium

Cryolite is sodium aluminium fluoride. Alumina will not melt below 2,050 °C, but it dissolves in molten cryolite at about 960 °C, like sugar in tea. An electric current then pulls aluminium metal out of the solution (Aluminium, Electrolysis). The cryolite is not used up, so a smelter needs it only once, plus small top-ups.

  • Natural cryolite came from one place only: Ivittuut in Greenland, mined from 1854 until it ran out in 1987. It is white and glassy, and almost disappears in water, because it bends light nearly as water does.
  • Synthetic cryolite is made from hydrofluoric acid, alumina and soda ash. This is the most dangerous step in aluminium making; the Aluminium chapter covers its precautions.
  • Cryolite also makes white opal glass and enamel, and was once used as an insecticide.

The cells give off fluoride fumes. Cattle grazing downwind of early smelters went lame with fluorosis, and trees died. Keep the bath crusted over, draw the fumes through lime or alumina, and put the smelter away from farms.

Fluoride in teeth and water

How much is right?

Fluoride in drinking water Effect
Below 0.3 mg per litre No protection; more tooth decay
About 0.7 mg per litre Fewer cavities, no visible harm
Above 1.5 mg per litre (the WHO limit) Children's teeth develop chalky white flecks, then brown stains and pits (dental fluorosis)
Above 4–10 mg per litre, for years Stiff, painful joints, bent and brittle bones, crippling (skeletal fluorosis)

High-fluoride water occurs naturally in the East African Rift, much of India, northern China, parts of the Middle East and the Americas. It is common in deep wells in granite and volcanic rock.

Finding out without instruments

Look at the teeth of children aged 8–15 who were born locally and drank only this water (Dentistry):

  • Few cavities and white, glossy teeth suggest roughly the right amount.
  • Opaque, paper-white flecks or streaks in many children suggest more than about 1.5 mg per litre.
  • Brown stains and pitted enamel in most children suggest well over 2–4 mg per litre. Treat the water, especially for children and pregnant women.

This is how fluoride was discovered: by a dentist puzzling over "Colorado brown stain". For a measured test, laboratories use the fact that fluoride bleaches the red lake that alizarin from madder makes with zirconium salts (Dyes and Mordants, Identifying Substances).

Removing excess fluoride

Bone char filter. This is the simplest and very effective.

  1. Char clean, defatted bones (boiled, then sun-dried) in a closed iron drum or clay kiln at about 400–600 °C, a dull red, for 4–6 hours, with little air. Good bone char is grey-black to dark brown, not white. White means it was overburned. It must not smell of burnt meat; underburned char spoils the taste of the water.
  2. Crush it to grains of 0.5–2 mm and wash out the dust.
  3. Fill a column, such as a clay pot, bucket or drum with a tap at the bottom, with 10–20 kg of char over a layer of gravel. Pour water through slowly, about 5–10 litres per hour for a household unit.
  4. A household unit of 10 kg treats very roughly 1,500–4,000 litres of water with 5–10 mg per litre of fluoride before it is spent; the richer the water, the sooner. Change the char when children's new teeth start to show flecks again, or on a fixed schedule.

Alum and lime (the Nalgonda method, India). For a 200-litre drum of water, add lime and then alum, in roughly the doses a jar test shows, stir hard for 10 minutes, let it settle for an hour, and draw off the clear water (Water Treatment for a Town). Removing fluoride takes far more alum than clearing mud, often 0.2–1 g per litre. That leaves aluminium in the water, so this method is second best.

Activated alumina (Alum and Alumina) in a column works like bone char and can be refreshed with lye and acid.

Adding fluoride

Towns add about 0.7 mg per litre of fluoride as sodium fluoride or fluorosilicic acid, the latter a by-product of fertiliser works. Do not do this without accurate measurement and a steady water flow. In 1992 a faulty feeder in an Alaskan village put many times the dose into the water, and one person died. The Toothpaste, Shampoo, Perfume and Cosmetics chapter likewise leaves fluoride out of homemade toothpaste: brushing and less sugar do most of the work.

Going further

Elemental fluorine is a yellowish gas that sets fire to almost everything, including water and glass. It is made only by electrolysis of molten fluorides in nickel or copper cells. Its compounds are the basis of non-stick PTFE coatings and of the uranium hexafluoride used to enrich uranium (Nuclear Energy (Overview)). The old CFC refrigerants (Ice and Refrigeration) were safe to handle but destroyed the ozone layer high in the sky, and are banned; do not make them. Calcium fluoride and fluoride salts also appear in fluorescent lamp phosphors (Arc Lamps, Neon and Fluorescent Lights).

Dangers

Danger Hydrofluoric acid and hydrogen fluoride kill through the skin, often without pain at first. See the first-aid section above. Do not make them.

Danger Silica dust from quartz sand used for blasting causes silicosis, an incurable scarring of the lungs that killed thousands of sandblasters. Use alumina, emery, garnet or slag grit, work in a closed cabinet, and wear a mask of many layers of damp cloth even so.

  • Fluoride salts (sodium fluoride, cryolite) are poisons if swallowed: 5–10 g of sodium fluoride can kill an adult, and much less a child. Never store them near flour or baking powder; deaths have happened that way.
  • Fluorspar fumes from furnaces and enamel melts: work outdoors, upwind.
  • Compressed air at 6 bar can blow grit into eyes and skin. Never point the nozzle at anyone.

Note Troubleshooting. Hand-ground glass has clear spots → the glass is not flat, or the pressure was uneven. Rub longer with a soft pad, in small circles. Sandblaster spits or stops → grit is damp or lumpy. Dry the grit and sieve it, and fit a water trap on the air line. Stencil lifts or burns through → glue too weak or rubber too thin. Use thicker rubber and keep the nozzle moving. Bone char makes water taste foul → underburned. Fire it again, hotter and longer. Bone char stops removing fluoride → it is spent; replace it. Spent char makes good phosphate fertiliser (Chemical Fertilisers).

How it was first done

Georgius Agricola described fluorspar as a smelting flux in 1546 and named it fluores. Around 1670 the Nuremberg glass cutter Heinrich Schwanhardt found that a mixture of fluorspar and acid etched his spectacles. Carl Wilhelm Scheele studied hydrofluoric acid in 1771. Many chemists were poisoned or killed trying to free fluorine itself, until Henri Moissan succeeded by electrolysis in 1886 and won a Nobel Prize. Benjamin Tilghman patented sandblasting in 1870. In 1901 the young dentist Frederick McKay arrived in Colorado Springs and began a thirty-year hunt for the cause of local brown-stained teeth. It was traced to fluoride in 1931, and H. Trendley Dean's surveys showed that a little fluoride prevents decay. Grand Rapids, Michigan, became the first city to fluoridate its water in 1945.

Source: content/entries/chemistry/fluorine-compounds.md