Part 7 · Home and Daily Life
Kitchen Utensils and Gadgets
The hand tools of a working kitchen and how to make each — rolling pins, pastry and cutting boards, wooden spoons and spatulas, ladles, whisks and the geared egg beater, colanders, sieves, tea strainers and funnels, cleavers, pepper mills and coffee grinders, nutcrackers, can openers and corkscrews, kitchen scales, oven mitts and aprons.
- Difficulty
- ●●●●●
- Time
- An hour for a whisk or a funnel; an evening for a rolling pin, spatula or cutting board; a day for a pepper mill; several days for a geared egg beater or coffee mill
- Steps from zero
- 18 prerequisites →
This unlocks
—The full path from nothing — 18 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Pottery
- Charcoal
- Hides and Leather
- The Wheel and Axle
- Bellows
- Gears
- Iron (the Bloomery)
- The Waterwheel
- Blacksmithing
- Sheet Metal and Rolling
- Kitchen and Cooking
- Kitchen Utensils and Gadgets
Do them roughly in this order. See it on the tech tree →
Why it matters
A cook with a knife and a pot can feed people; with the right small tools the work goes faster, more safely and with less waste. A sieve takes grit and bran out of flour; a colander drains a pot without scalding hands; a funnel fills bottles for pickling and brewing; a scale makes a recipe come out the same every time; an oven mitt prevents the commonest kitchen burn. Each is also a good first product for a new workshop, teaching turning, wire bending, punching and seaming sheet, cutting gears or hardening a small blade on something cheap that every household wants.
What you need
| Utensils | Workshop and materials | Chapters |
|---|---|---|
| Rolling pins, boards, spoons, spatulas, mill bodies | Close-grained hardwood, lathe, plane, knife | Basic Woodworking, The Lathe, Doors, Windows and Joinery |
| Ladles, colanders, funnels, strainers | Tinplate, copper or sheet iron 0.4–1 mm; snips, punches, pure-tin solder | Sheet Metal and Rolling, Soldering and Brazing |
| Whisks, sieves, corkscrews | Iron, steel or brass wire 0.3–4 mm | Iron and Brass Wire |
| Cleavers, openers, mill burrs | Tool steel, forge, files | Axes, Chisels, Knives and Planes, Steel, Files and Saws |
| Egg beater, coffee mill | Small gears in brass or cast iron | Gears, Metal Casting |
| Mitts, aprons | Linen, cotton or canvas; wool wadding | Sewing, Needles and Thread, Quilting, Down and Warm Clothing |
Where to find it
Use tasteless, close-grained hardwoods — maple, beech, birch, cherry, pear, hornbeam, and boxwood for small parts that must wear — never oak (tannin), resinous pine, or poisonous yew and oleander. Horsehair from manes and tails weaves into fine, rot-proof sieve cloth. Dried, split bottle gourds make ladles and funnels in an afternoon. Wool wadding for mitts chars instead of flaring and stays insulating when slightly damp (Wool).
Wooden utensils
Rolling pin
A plain pin is a cylinder 45–50 cm long and 5–6 cm across; a handled pin has a barrel 25–30 cm long and 7–8 cm across that turns on a central rod between two handles. Turn a dry blank of beech or maple on the The Lathe and check it with a straightedge against the light: no gap anywhere. For handles, bore the barrel through 1–1.5 cm, pass a rod through, and peg a 10 cm turned handle on each end. Good pin: rolls across a flat table with no wobble; no end checks. A cold pin of glazed stoneware, glass or stone keeps rich pastry firm.
Pastry board and cutting board
A pastry board is 60 × 45 cm, 2–2.5 cm thick, of two or three boards glued edge to edge (Glues and Adhesives), with a cross-batten under each end screwed through slotted holes so the wood can move, or a lip underneath that hooks over the table edge. A slab of marble or slate stays cooler.
A cutting board is hardwood 3–4 cm thick, about 40 × 30 cm. An end-grain board is kinder to knives: rip a thick plank into 4 cm strips, turn them on edge and glue them into a slab; crosscut that into 4 cm strips, turn them end-grain up, glue again and plane flat. A shallow groove near the edge catches juices. Keep a separate, marked board for raw meat and fish (Butchery and Meat). Scrub with hot water, Soap and salt, dry on edge, and re-plane when deeply scored: deep cuts hold germs.
Wooden spoon and spatula
A cooking spoon is longer and stouter than an eating spoon: 30–35 cm, a shallow bowl 6 × 5 cm with walls 5–6 mm, and one side of the bowl cut flat to scrape the pan's corner. A spurtle — a round stick 30 cm long swelling to 2.5 cm — stirs porridge without lumps. Carve both from green wood as in Cutlery and Tableware.
- Wooden spatula: a paddle 30 cm long with a blade 6–7 cm wide, thinned to a 2 mm bevel, for turning food without scratching seasoning.
- Metal turner (fish slice): a blade of steel or tinned iron 0.8–1 mm, about 8 × 12 cm, slotted so fat drains, with a cranked neck so the handle clears the pan's rim, on a wooden handle; file its front edge thin. A palette knife — a flexible, blunt, round-ended blade 15–20 cm long — spreads icing and lifts biscuits.
Ladles, whisks and the egg beater
Ladle
A ladle's bowl is 8–10 cm across and holds 100–150 ml; its handle is 28–32 cm, hooked at the end.
- Gourd ladle: halve a dried bottle gourd lengthwise through its neck; scrape and oil.
- Wooden ladle: a deep spoon with the handle at about 110° to the rim, so it scoops and hangs upright.
- Metal ladle: sink a disc of 1 mm copper or iron in a hollowed stump as for a wok (Pots, Pans and Kettles), planish, add a pouring lip, and rivet on a forged handle. Tin copper inside.
Good ladle: rivets tight and smooth inside; the handle does not bend under a full bowl; the hook holds it on the pot's side.
Whisk
The simplest whisk is 20–30 peeled birch or willow twigs 25 cm long, tied tightly at one end. For a balloon whisk, bend 8–12 lengths of springy wire 1–1.5 mm thick (tinned steel or brass), each 55–60 cm, into long loops over a pear-shaped wooden former about 7 cm wide; cross them evenly at the tip; bind the ends tightly with soft wire for 8 cm, slide on a handle, and fill it with hot pine resin or pure tin so no food gets in. Good whisk: loops evenly spaced that spring back after a squeeze.
The geared egg beater
The rotary beater does in two minutes what takes ten with a whisk. A crank turns a large drive wheel with teeth on its face (a crown wheel). Near the bottom of the wheel, a little to the left and right of its centre line, these teeth mesh with two small pinions on two upright shafts. Each shaft carries a dasher — four thin metal strips bent into an open egg shape — and the two dashers overlap, their blades passing between one another to shear the liquid.
- Ratio: a drive wheel of 40–50 teeth and pinions of 10 teeth give 4–5 beater turns per crank turn — about 500–600 turns a minute at a brisk crank (Gears).
- Making it: cast the drive wheel in brass or iron, or saw and file it from 2–3 mm brass plate; turn the pinions from brass rod and file their teeth. Bend the frame from 3 × 15 mm iron strip, drilled for the crank axle and the two shaft bearings. Rivet dashers of 1 × 6 mm tinned steel strip to a hub on each shaft, staggered so the blades interleave by about a third of their width without touching.
- Good beater: turns smoothly with one finger; no tooth catches; the blades never touch.
Colanders, sieves, strainers and funnels
Colander
A bowl 22–28 cm across (2–4 litres) with holes 3–5 mm across, 1–1.5 cm apart, on a ring foot or three feet, with two handles. In metal, punch the holes from the inside outward so the burrs are outside and the inside stays smooth — the opposite of a grater (Kitchen and Cooking) — then form the bowl and solder on foot and handles. In clay, push the holes through the leather-hard bowl with a pointed stick before glazing (Pottery). A tightly woven basket drains rice and curd well (Baskets and Containers).
Sieve
A kitchen sieve is a wire-mesh bowl 15–20 cm across on a handle; a drum sieve (tamis) is mesh stretched across a wooden hoop 25–30 cm across and 8–10 cm deep, for sifting and pressing purées.
- Hoop: steam or boil a strip of ash, oak or beech 8–10 cm wide and 3–4 mm thick, bend it round a former (Steam-Bending Wood) and nail the overlap. Make a second hoop slightly larger.
- Mesh: weave horsehair, silk or linen (Spinning and Weaving Cloth), or brass or tinned iron wire (Iron and Brass Wire). Stretch it over the inner hoop and push the outer hoop down over it.
| Use | Mesh opening |
|---|---|
| Riddle for grain and gravel | 3–5 mm |
| Purées, straining stock | about 1 mm |
| Flour | 0.2–0.4 mm |
| Icing sugar, fine starch | about 0.15 mm |
To measure, count threads per centimetre: 20 wires of 0.2 mm to the centimetre leave openings of 0.3 mm.
Tea strainer: a tiny sieve 5–6 cm across of fine mesh or tinplate punched with 1 mm holes, with a handle and a ledge opposite to rest across a cup. A tea ball is two hinged, perforated hemispheres hung in the pot on a chain.
Funnel
For bottles: a mouth 12–15 cm across and a spout 1–1.5 cm across and 5–8 cm long. For filling jars in Canning and Bottling: a spout 5–6 cm wide.
- Lay out the cone, which unrolls into a sector of a circle. Its radius R is the cone's slant length; its angle is 180 × mouth diameter ÷ R degrees. For a 14 cm mouth and 12 cm slant: 180 × 14 ÷ 12 = 210°. Swing it with nail and string on tinplate, cut off the tip where the spout begins, and add 6 mm on one edge for the seam.
- Roll it round a former, solder or lock-seam the joint (Sheet Metal and Rolling), solder in a rolled spout, and wire the rim.
- Air rib: solder a thin wire along the outside of the spout. Without it the spout seals in the bottle neck and the funnel stops.
The narrow end of a gourd or a cow horn, cut off across, makes a ready funnel (Horn and Bone Working).
Cleaver
A meat cleaver has a rectangular blade 18–20 cm long and 8–10 cm deep, 4–6 mm thick at the spine, weighing 0.6–1 kg; the Chinese vegetable cleaver is the same shape but 2–3 mm thick and much keener. Forge it from steel or with a forge-welded steel edge (Axes, Chisels, Knives and Planes), with a full tang. Harden in brine and temper to purple or blue (280–300 °C) — softer than a knife, so it bends a hair on bone instead of chipping. Grind 25–30° each side for meat, 15–20° for vegetables. Rivet on hardwood scales and drill a hanging hole in the top front corner. Good cleaver: the weight sits forward so it falls through a joint; the handle does not sting on impact. See Butchery and Meat for its use.
Pepper mills and coffee grinders
A mortar crushes (Kitchen and Cooking); a burr mill grinds evenly at whatever fineness you choose. Its heart is a grooved cone (the rotor) turning inside a grooved ring (the stator). The gap is wide at the top, where coarse teeth crack whole peppercorns or beans, and narrow at the bottom, where fine grooves grind them. Drawing the cone up into the ring makes the grind finer.
- Cone: turn it from steel bar, 2.5 cm across at the base for pepper or 4 cm for coffee, tapering about 15° a side. File 8–12 coarse teeth in its upper part and 20–30 fine grooves in its lower part, all spiralling the same way.
- Ring: the same inside a short steel tube, grooves spiralling the opposite way.
- Harden both and temper to straw (about 220 °C) (Steel). Chilled cast iron makes good coffee burrs straight from the mould (The Blast Furnace and Cast Iron).
Pepper mill: a turned maple or beech body 15–20 cm tall and 5–6 cm across, bored through with a long auger, with the ring fitted tight in its foot. A steel shaft runs from the cone up through the body to a turned cap, held by a knurled nut: turning the cap turns the cone; tightening the nut draws the cone up for a finer grind.
Coffee grinder: a box mill — a hardwood box 12–15 cm square, an iron hopper on top, a vertical shaft carrying the cone, a crank 12–15 cm long, and a drawer underneath. A nut on the shaft under the cone sets the grind: coarse for boiled coffee, medium for drip pots (Pots, Pans and Kettles), very fine for Turkish coffee.
Good mill: no shaft wobble; no whole corns get through; the grind stays where it is set.
Nutcrackers, can openers and corkscrews
Nutcracker
Two arms hinged at one end, with the nut squeezed close to the hinge. Your squeeze is multiplied by the ratio of the distances: arms 15 cm long with the nut 3 cm from the hinge give 5 times the grip. Forge it from two 6 × 15 mm iron bars riveted at the hinge, with shallow notches filed in the jaws, or carve it from hardwood with a wooden peg hinge. A screw nutcracker — a cup with a screw through its side — cracks the hardest nuts slowly and leaves the kernel whole. A stone anvil and hammerstone work too (Foraging Wild Food).
Can opener
Tin cans (Tins, Cans, Drums and Tanks, Canning and Bottling) were opened with hammer and chisel for decades before a proper opener existed.
- Lever opener (easiest to make): a flat steel blade with a short, sharp, hooked point and a blunt guard 1 cm behind it, in a handle 12–15 cm long. Push the point through the lid beside the rim, rest the guard on the rim, and rock the handle so the point saws its way round. Harden the point and temper it straw.
- Wheel opener: a hardened cutting wheel 15–20 mm across presses through the lid inside the rim while a toothed feed wheel grips the rim from below; turning a key drives the can round past the cutter. It leaves a smoother edge but needs accurately turned, hardened wheels.
Good opener: cuts cleanly in one pass with no metal slivers. Wash and dry it after each use.
Corkscrew
The worm must be an open spiral: it pushes the cork aside and grips it along its length, where a solid screw like a wood screw splits the cork and tears out.
- Wind 3–4 mm steel wire, red-hot, round a smooth mandrel 6–7 mm across at a pitch of 8–10 mm (one turn to the next), for 5–6 turns — a worm 5–6 cm long. A guide pin or helical groove on the mandrel keeps the pitch even.
- Sharpen the end to a point that follows the spiral's circle, not bent in to the centre.
- Harden and temper blue, so it springs rather than straightens.
- Fit the straight end through a 10 cm hardwood cross-handle and rivet it over.
Good corkscrew: seen end-on, the point lies on the spiral's circle and the centre is open. A lever corkscrew adds an arm that rests on the bottle's lip, so the cork is levered out, not pulled.
Kitchen scales
Weighing is far more reliable than measuring by volume (Kitchen and Cooking). The simplest scale is an equal-arm balance: a beam about 30 cm long on a steel knife-edge, with a pan 15–18 cm across at each end. Make the weights with water — 1 litre weighs 1 kg (Measurement from Scratch): 1 kg, 500 g, 200 g, 100 g, 100 g, 50 g, 20 g, 10 g, 10 g and 5 g, cast in iron or brass and filed until each balances its water. The Roberval scale puts both pans on top of the beam, held level by a hidden parallel linkage, so a bowl can stand on it; a spring balance reads straight from a scale. Building and checking these is in Balances, Steelyards and Weighing Machines. Good scale: returns to level when empty; swap load and weights between the pans and the reading does not change.
Oven mitts and aprons
Pot holder and mitt. A pot holder is a pad about 20 × 20 cm. A mitt is traced round the hand (fingers together, thumb out) plus 3 cm, reaching 10–15 cm past the wrist. Cut two outer layers of close-woven cotton drill, linen or canvas, put 3–4 layers of wool felt or 1 cm of carded wool or cotton between them (Felt), and quilt them with rows of stitching 3–4 cm apart so the filling cannot slide; seam the halves, bind the cuff and add a hanging loop.
Warning A damp mitt burns. Water carries heat into the hand many times faster than dry cloth, and a wet pad on a hot pan makes scalding steam. Use mitts and pot holders dry.
Apron. A bib apron is linen, cotton or canvas about 90 cm long and 70 cm wide, narrowing to 25–30 cm at the chest, with a neck loop of tape, two 75 cm waist ties and a pocket, all edges double-hemmed (Sewing, Needles and Thread). A half apron ties at the waist. Use leather for the forge (Hides and Leather). Wash cooking aprons often and keep loose strings away from flames.
How to tell it worked
Dough rolls out the same thickness at middle and edge; sifted flour is free of bran specks; egg whites stand in stiff peaks after two or three minutes with the beater; a funnel fills a narrow bottle without backing up; the mill grinds as set; the corkscrew pulls a cork whole; weighed recipes come out the same every time.
Note Troubleshooting. Pin or board warps → wood not dry, or left wet; dry slowly and re-plane. Whisk wires loosen and trap food → bind tighter; seal the handle. Egg beater jams → uneven teeth or shafts not square to the wheel; file high teeth, check bearings. Beaters clash → stagger the hubs more. Funnel gurgles and stops → add an air rib. Mill grind uneven → shaft wobbles; bush the top of the body. Burrs blunt fast → reharden. Corkscrew pulls through → spiral closed or point bent in; open it out. Straightens → temper less or use thicker wire.
Dangers
Danger Cleavers and can lids cut deep. Chop on a heavy board on a firm table, holding hand well back with fingertips curled under. Never try to catch a falling blade. An opened can's edge is as sharp as a knife: press the lid down into the can before throwing it away. For deep cuts see Wound Care and Antiseptics.
- Lead: never solder anything that touches food with lead-bearing solder; use pure tin (Lead).
- Scored wood harbours germs: plane it smooth or burn it.
- Burns: dry mitts only; keep aprons and sleeves from flames.
- Gears and burrs catch small fingers: keep children away from the beater and the mill.
What this unlocks
The egg beater's crown wheel and pinions lead to clockwork (Clockwork, Music Boxes and Counting Machines) and the The Sewing Machine; the burr mill is a small mill; the balance leads to every weighing machine. Motor-driven mixers are in Fans, Vacuum Cleaners and Washing Machines. Pots and pans are in Pots, Pans and Kettles; the stove is in Cooking Ranges, Iceboxes and Vacuum Flasks.
How it was first done
Wooden spoons, spatulas, sieves and rolling pins are older than writing; the Romans used bronze ladles, colanders and balances much like ours. Sieves of horsehair, silk and linen were standard for flour in Europe until woven wire became cheap in the 1800s. The open-spiral corkscrew is mentioned in England in the late 1600s; the Reverend Samuel Henshall patented an improved one in 1795. Peter Durand patented the tin can in England in 1810, but lever openers only appeared in the 1850s, and William Lyman of Connecticut patented a rotating-wheel opener in 1870. Rotary egg beaters were patented in the United States from the 1850s, and the Dover beater of the 1870s made the type famous. The French firm Peugeot made coffee mills from 1840 and its first pepper mill in 1874.