Part 8 · Chemistry
Chemical Fertilisers
Concentrated plant food made with acid and fire — superphosphate from bones or phosphate rock dissolved in sulfuric acid, ammonium sulfate from ammonia, potash from ash and mineral salts. Used in the right amounts alongside manure, they can double a harvest; used carelessly, they burn crops and poison wells.
- Difficulty
- ●●●●●
- Time
- An afternoon to mix a batch of superphosphate, then 2–6 weeks to cure; a growing season to see results
- Steps from zero
- 33 prerequisites →
The full path from nothing — 33 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Sulfur
- Hunting and Trapping
- Basic Woodworking
- Pottery
- The Kiln
- Charcoal
- Hides and Leather
- Lime
- Salt
- Lye and Potash
- Fermentation
- The Wheel and Axle
- Glass
- Bellows
- Saltpeter
- The Lathe
- Copper Smelting
- Iron (the Bloomery)
- Sulfuric Acid
- Laboratory Glassware
- Blacksmithing
- The Battery
- Steel
- The Steam Engine
- Electrolysis
- Hydrogen, Oxygen and Gases
- Machine Tools
- Ammonia
- Chemical Fertilisers
Do them roughly in this order. See it on the tech tree →
Why it matters
A field that grows grain year after year slowly loses the elements in that grain. Manure, compost, urine, ash and legumes (Compost and Manure) put much of it back — but never all, because some always leaves the farm in the food that feeds towns and in the nitrogen that drifts away as gas. On poor soils, the lack of one element can hold yields down to a third of what they could be no matter how much manure you spread.
Chemical fertilisers are those elements in concentrated, quick-acting form. A sack of superphosphate carries as much phosphorus as several cartloads of manure. Used well, they let a farm feed many more people from the same land, free labour for other work, and rescue soils that have been worn out for generations. Most of the growth in the world's food supply since 1900 came from them.
They are also easy to misuse. Too much burns roots, sours soil, wastes money and labour, and washes into wells and rivers. This chapter shows how to make the main ones — superphosphate, ammonium sulfate and potash — and how much to use.
How it works
The big three
Plants need about seventeen elements. Air and water supply carbon, hydrogen and oxygen; the soil supplies the rest. Three are needed in large amounts and are the ones most often short:
| Nutrient | Plants take it up as | Main sources here |
|---|---|---|
| Nitrogen (N) | Ammonium and nitrate salts | Ammonia, ammonium sulfate, Saltpeter, guano, urine |
| Phosphorus (P) | Phosphate dissolved in soil water | Bones, phosphate rock, guano — made soluble with Sulfuric Acid |
| Potassium (K) | Potassium salts | Wood ash, potash, seaweed, mineral potash |
Sulfur, calcium and magnesium come next; Lime supplies calcium, and ammonium sulfate and superphosphate both carry sulfur. Signs of each shortage are in the table in Compost and Manure.
The label. Fertiliser strength has long been written as three numbers: the percentage of nitrogen (N), of phosphate (written as P₂O₅) and of potash (written as K₂O). Ammonium sulfate is 21–0–0; superphosphate about 0–18–0; saltpeter about 13–0–46. These odd forms of P and K are an old convention, but every table and rate in the world uses them, so this chapter does too.
The law of the minimum
The chemist Justus von Liebig made this famous in the 1840s: yield is limited by whichever nutrient is scarcest. If a soil lacks phosphorus, piling on nitrogen gives almost nothing — and may only make weak, leafy plants that fall over. The art of fertilising is finding the short stave. That is what test strips are for (see "How to tell it worked").
Why bones must be dissolved
Bones and phosphate rock are made mostly of calcium phosphate, which hardly dissolves in water. Ground fine, it feeds plants only slowly, over years, and only on acid soils. Strong sulfuric acid takes most of the calcium away from the phosphate (as gypsum, calcium sulfate) and leaves calcium dihydrogen phosphate (monocalcium phosphate) — "superphosphate" — which dissolves readily. The same weight of phosphorus becomes many times quicker to act.
Why salts burn
All soluble fertilisers are salts. A heap of salt next to a seed or root pulls water out of it, just as salt draws water out of meat. Seedlings yellow and die — fertiliser burn. Spread fertilisers thinly, keep them away from seeds, and water or rain them in.
What you need
| Fertiliser | Roughly N–P₂O₅–K₂O (%) | Made from |
|---|---|---|
| Ammonium sulfate | 21–0–0 (+24% sulfur) | Ammonia + sulfuric acid (Ammonia) |
| Saltpeter (potassium nitrate) | 13–0–46 | Nitre beds (Saltpeter) |
| Chile saltpeter (sodium nitrate) | 16–0–0 | Desert deposits |
| Seabird guano | 8–16 N, 8–12 P₂O₅, 2–3 K₂O | Islands and coasts in dry climates |
| Bone meal, steamed | 3–4 N, 20–24 P₂O₅ | Bones, boiled and ground |
| Bone ash | 0–35–0 | Bones burnt white |
| Phosphate rock | 0–25–0 to 0–35–0 | Mined |
| Superphosphate | 0–16–0 to 0–20–0 | Bone or rock + sulfuric acid |
| Hardwood ash | 0–2–5, plus lime | Fires (Lye and Potash) |
| Potash (potassium carbonate) | 0–0–50 to 0–0–65 | Leached and boiled-down ash (Lye and Potash) |
| Potassium sulfate | 0–0–50 | Potash + sulfuric acid |
| Lime nitrogen (calcium cyanamide) | about 20–0–0 | Carbide + nitrogen (Ammonia) |
For making superphosphate you also need: concentrated sulfuric acid (Sulfuric Acid), a mixing trough of stone, hard-fired glazed stoneware, or wood lined thickly with pitch (Tar, Pitch and Glue) — never metal; a wooden paddle; a stone or brick floor under a roof for the curing heap; a sieve; and the protective gear listed in Sulfuric Acid.
Where to find it
- Bones — the phosphorus source you will always have. Collect every bone from kitchens and butchering (Keeping Animals). Old battlefields, middens and bone pits have been mined for fertiliser in the past.
- Phosphate rock (phosphorite) — a sedimentary rock that is usually grey, brown or black, dull, often in nodules or pebbly beds within marine shale, chalk, limestone or greensand, and often full of fossil teeth, bones and shells. It is noticeably heavier than limestone of the same size, fizzes only a little in acid. Be ready to test many dull pebbles: phosphate rock looks unremarkable, and the surest proof is a strip trial with superphosphate made from it. In 19th-century England, "coprolite" nodules dug from the Cambridgeshire greensand were the first mined phosphate. Big deposits occur in North Africa, Florida, Russia and many other places.
- Guano — layers of dried dung on seabird islands and rocky coasts in rainless climates (Peru, Chile, Namibia, some Pacific islands) and in bat caves everywhere. Fresh guano smells strongly of ammonia; old, rain-leached guano has lost its nitrogen but keeps its phosphate. Take only from abandoned or seasonal colonies, not from nesting birds.
- Potash — wood ash and plant ash (Lye and Potash); kelp and seaweed ash on coasts; and in some dried-up salt lakes and salt mines, layers of sylvite and carnallite: pinkish or reddish salt crystals with a bitter, sharper taste than common salt (taste only a grain and spit it out). Carnallite gets damp and runny in moist air.
- Nitrates — Saltpeter beds, nitrous earth from old stables and caves, and in a few extremely dry deserts (northern Chile above all) crusts of caliche, a cemented layer rich in sodium nitrate. A pinch thrown on glowing charcoal makes it flare and sparkle.
Method 1: Superphosphate
Prepare the phosphate
- Bones: boil them to remove fat and glue (keep both — Soap, Glues and Adhesives). Then either burn them in a hot fire until they are white and crumbly (bone ash), or dry them and pound them as fine as possible. Bone ash is easier to grind and reacts more cleanly; raw bone meal keeps its nitrogen but froths and reacts more slowly.
- Rock: crush, then grind in a quern or edge-runner mill (The Watermill) to a powder that passes a fine cloth sieve — like flour.
Fineness is everything. Coarse grains get a skin of gypsum and stop reacting inside.
Amounts
For each 10 kg of bone ash or ground phosphate rock: about 6 kg of concentrated sulfuric acid (about 3.3 litres; strong acid is nearly twice as heavy as water), diluted into about 3 litres of water.
For each 10 kg of raw bone meal: about 4 kg of concentrated acid (about 2.2 litres) diluted into about 2 litres of water.
If your acid is weaker (see Sulfuric Acid for judging strength by weight), use correspondingly more acid and less water: what matters is the amount of real acid and ending up with a damp, stiff mass, not a soup.
Steps
- Work outdoors, upwind, with water, wood ash or crushed chalk at hand to neutralise spills, and your eyes and hands protected.
- Dilute the acid: pour the measured water into a glazed pot or stone trough, then pour the acid slowly into the water, stirring. Never pour water into acid. It gets very hot. Let it cool a little.
- Spread the powder in the mixing trough.
- Pour in the diluted acid a little at a time, stirring and turning with the paddle. It foams, steams and gives off choking fumes. Keep your face back. Mix for 5–10 minutes until every bit of powder is wet and the mass looks even.
- Let it set. Within 30 minutes to a few hours it thickens and becomes a warm, damp, crumbly solid. Shovel it into a heap on a stone floor under a roof.
- Cure it for 2–6 weeks in the heap (the "den"), turning it once a week. The reaction continues slowly; the heap dries and becomes porous.
- Dry and crush. Spread it out to dry, then break it up and sieve it. Store it in a dry place, in sacks or covered baskets.
Made with phosphoric acid instead of sulfuric acid, the same rock gives triple superphosphate, more than twice as strong and with no gypsum to carry (Phosphoric Acid and Phosphates).
Tip No acid yet? Bone ash or very fine bone meal still works — slowly. Dig 100–200 g per square metre into acid soils, or mix it into the compost heap, where the acids made by rotting help to dissolve it. Bone ash heated with potash or soda in a kiln, or the slag from steelmaking by the basic process (Steel in Quantity), also gives a slow-acting phosphate fertiliser.
Method 2: Ammonium sulfate
This is ammonia caught in sulfuric acid; the method is in Ammonia. Sources, from easiest:
- Stale urine distilled with lime into a receiver of dilute acid.
- Bone, horn and hoof heated in an iron retort.
- Coke ovens and gas works (Coal and Coke): their ammonia liquor, distilled with lime into acid, was the world's main nitrogen fertiliser before Haber–Bosch.
- Haber–Bosch ammonia bubbled into acid, or combined with carbon dioxide into Urea, the richest solid nitrogen fertiliser (46% N).
Boil the solution down until crystals form on a drop cooled on a stone, cool it, and drain the white or greyish crystals. They keep indefinitely if dry.
Urine itself is a liquid ammonium fertiliser, ready made — see Compost and Manure for how to use it directly. Making ammonium sulfate is worth it when you need to store nitrogen or carry it to distant fields.
Method 3: Potash
- From ash: leach wood or plant ash and boil the lye down to dry, brown black salts, then bake them to white potash (Lye and Potash). About 1 kg of potash comes from 10–20 kg of hardwood ash.
- From seaweed: dry kelp and wrack, burn them slowly in a pit into a hard, glassy cake ("kelp"), crush and leach it like ash. It is rich in potassium (and iodine).
- From mineral salts: dissolve sylvite or carnallite rock in hot water, let mud and common salt settle (common salt is less soluble when the water is hot and full), pour off and cool: potassium chloride crystallises first.
- Potassium sulfate: stir sulfuric acid into a potash solution until it no longer fizzes, then boil down. This form contains no chloride, which is better for potatoes and fruit.
Potash draws water from the air and becomes runny. Store it in sealed pots.
Mixing your own fertiliser
A useful general garden mixture is roughly 2 parts ammonium sulfate, 2 parts superphosphate and 1 part potash by weight (about 8–7–10).
Rules for mixing:
- Never mix ammonium fertilisers with lime, wood ash or potash and store them. The alkali drives off ammonia. Mix just before spreading, or spread them separately, a week apart.
- Never mix superphosphate with lime — the lime turns it back into insoluble phosphate.
- Keep it dry. Damp mixtures cake into hard lumps.
How much to use
The amounts below are per square metre per season. A square metre is a stride by a stride. Weighing is best (Measurement from Scratch); without scales, a level tablespoon holds about 15 g of most fertiliser salts and a cupped handful about 40–50 g.
| Fertiliser | Grain, beans | Potatoes, cabbages, maize | Grass, hay |
|---|---|---|---|
| Ammonium sulfate | 20–30 g | 30–50 g, in two doses | 20–40 g, in spring |
| Superphosphate | 20–40 g | 40–60 g | 20–30 g every 2–3 years |
| Potash (carbonate or sulfate) | 10–15 g | 15–25 g | 10 g |
These are moderate rates, for soil that also receives manure or compost. Legumes (beans, peas, clover) make their own nitrogen; give them phosphate and potash only.
How to apply:
- Phosphate and potash move little in soil. Spread them before sowing and rake or dig them into the top 10 cm.
- Nitrogen washes down quickly. Give it in two or three smaller doses — at sowing and again when the crop is growing fast — not all at once.
- For crops in rows, sprinkle fertiliser in a band about 5 cm to the side of and 5 cm below the seed, never touching it.
- On a growing crop, scatter it between the rows, on dry leaves (so it falls off them), just before rain or followed by watering.
- Lime regularly. Ammonium sulfate makes soil more acid; about 1 kg of ground limestone for every 1 kg of ammonium sulfate used, applied in a different season, keeps it balanced (Compost and Manure has liming rates).
How to tell it worked
The strip trial — the only way to know what your soil lacks:
- Mark out a row of plots, each 2 × 2 m, in an even part of the field, with a 50 cm path between them.
- Give each plot something different: nothing; N only; P only; K only; N + P; N + P + K; manure only. Label them with stakes.
- Sow and tend them all the same. Weigh or count the harvest of each plot.
- The plot that jumps ahead shows the stave that was short. Repeat for two or three years before trusting the result; weather varies.
Testing what you made:
- Superphosphate: stir a spoonful into a cup of water. The water turns acid — red cabbage juice goes pink-red (Acids, Bases and Testing) — and a good part dissolves; plain bone ash makes no change.
- Ammonium sulfate: crystals mixed with a little slaked lime and a drop of water smell strongly of ammonia.
- In the field: deeper green leaves (N), earlier flowering and ripening and stronger roots (P), stiffer stems and fewer scorched leaf edges (K).
Note Troubleshooting. Seedlings yellow and die after fertilising → fertiliser burn: too much, or too close to the seed. Water heavily; next time use less and keep it 5 cm away. Lush leaves, little grain, crop falls over → too much nitrogen, or nitrogen without phosphate and potash. No response at all → wrong nutrient (do a strip trial), very sour soil (lime it), or too dry for roots to take it up. Superphosphate stays wet and sticky → too much water or acid; mix in more bone ash or rock powder and cure longer. Superphosphate is dry and dusty, little dissolves → too little acid, or powder too coarse. Grind finer; check acid strength. Mixture caked into rock → stored damp. Keep dry; break up with a mallet.
Dangers
Danger Acid and fumes. Mixing superphosphate uses concentrated Sulfuric Acid — read its dangers first. Phosphate rock gives off fluorine-containing fumes (hydrogen fluoride) when attacked by acid, which damage the lungs and can kill, and which etch glass. Mix rock superphosphate only in the open air, upwind, and never breathe the steam. Bone ash gives far less of this — prefer bones if you have them.
Danger Nitrate in wells poisons babies. Nitrogen fertiliser, like manure, washes down into groundwater as nitrate. Water with too much nitrate given to infants (in bottle feeds) stops their blood carrying oxygen — "blue baby" sickness, which can kill. Never spread fertiliser within 30 m of a well or spring, never wash fertiliser buckets in streams, and use the smallest dose that works.
Warning Store nitrate fertilisers safely. Nitrates feed fire. Store saltpeter, sodium nitrate and any nitrate fertiliser in small lots, dry, away from fuel, oil, sulfur, sawdust and straw, and away from flames or heat. Big stores of nitrate fertilisers have caught fire and exploded, destroying whole harbours.
- Ammonium sulfate and potash irritate eyes and cuts. Wash hands after spreading; do not eat with fertiliser on your hands.
- Runoff. Fertiliser washed into ponds and rivers makes them choke with green slime; when it rots, the fish suffocate. Don't spread before heavy rain, on frozen ground, or on steep bare slopes.
- Some phosphate rocks contain cadmium or uranium. Bones contain neither — another reason to favour bones for gardens.
What this unlocks
More food from less land, so more people can be fed while others build, teach and heal (The Great Staple Crops, Farming from Seed). Fertilised pasture carries more animals (Keeping Animals); fertilised flax, cotton and hemp yield more fibre (Flax, Hemp and Linen, Cotton). The same chemistry — acids, phosphates, ammonium salts — feeds Making Medicines, baking powder (Soda Ash and Baking Soda), fire-proofing and the Matches industry. Together with improved seed (Saving Seed and Breeding Plants), irrigation (Irrigation) and machinery (The Tractor), chemical fertiliser was the core of the great rise in harvests of the 20th century. Dissolved in water in the right balance, the same salts feed plants grown with no soil at all (Hydroponics and Nutrient Solutions).
How it was first done
Farmers had long spread bones, and in the 1820s Britain imported shiploads of bones from European battlefields to grind for its fields. In 1840 Justus von Liebig argued that plants live on mineral salts taken from the soil, and suggested dissolving bones in acid. John Bennet Lawes patented superphosphate in 1842, opened a factory at Deptford near London in 1843, and with Joseph Henry Gilbert began the field experiments at Rothamsted that still run today — among the longest-running scientific experiments in the world. From the 1840s, ships carried millions of tonnes of guano from Peru's islands, until it was exhausted in the 1870s; then Chilean saltpeter took over. In 1861 potash salts began to be mined at Stassfurt in Germany. In the 1880s the "basic" steelmaking process gave a phosphate-rich slag that farmers bought eagerly. The Haber–Bosch process (1913) finally made nitrogen fertiliser from the air (Ammonia), and by the end of the 20th century half the world's food depended on it.
Source: content/entries/chemistry/chemical-fertilizers.md