◆ Rebuild

Part 12 · Transport

Snowshoes, Skis and Sledges

In deep snow a person on foot sinks to the thigh and covers a kilometre an hour; on snowshoes or skis they float and travel ten times as far in a day. How to bend and lace snowshoes, carve and bend skis, build hand and dog sledges — and how to travel on snow and ice without falling through or being buried.

Difficulty
●●●●●
Time
Two to three days for a pair of snowshoes (plus a week of drying); about a week for a pair of skis; two days for a toboggan
Steps from zero
5 prerequisites →

You need first

Basic WoodworkingHides and Leather

This unlocks

—
The full path from nothing — 5 steps before this one
  1. Stone Tools
  2. Cordage and Rope
  3. Basic Woodworking
  4. Hunting and Trapping
  5. Hides and Leather
  6. Snowshoes, Skis and Sledges

Do them roughly in this order. See it on the tech tree →

Why it matters

Deep snow can shut people in for months. Each step sinks to the thigh; a strong adult covers a kilometre or two an hour and is soon soaked with sweat — dangerous in the cold (Surviving Cold and Heat). Hunting stops, firewood can't be hauled, and settlements are cut off.

On snowshoes or skis the same person floats on the surface and covers 15–30 km in a day, more on skis over good snow. A sledge lets one person drag a load heavier than themselves; a dog team can haul several hundred kilograms. Frozen lakes and rivers become open roads. For thousands of years these tools made life in the far north possible.

How it works

Spreading the weight. Snow holds up only so much weight on each square centimetre. A boot sole of about 300 cm² pushes hard into it; a snowshoe of 1,000–1,500 cm² spreads the same weight over four or five times the area and sinks only a little. A rule of thumb for soft powder: 10–15 cm² of snowshoe for every kilogram of you plus your pack, on each shoe. On packed or wet snow you need less.

Gliding. Skis also spread the weight, but their gift is gliding: friction melts a microscopically thin film of water under a moving ski. A smooth, waxed, waterproofed base glides; a wet or rough one grabs. To climb you need grip — fur under the ski with the hairs pointing back slides forward but catches when pushed back.

Sledges work the same way: narrow, hard runners glide on packed snow and ice; wide, flat bottoms float on soft snow.

Ice holds weight by bending like a plank; the force it can bear grows with the square of its thickness. Doubling the thickness makes it about four times as strong.

What you need

Item For Source
Straight-grained ash (or birch, hickory, willow, spruce) Snowshoe frames, ski blanks, sledge runners Basic Woodworking
Rawhide from deer, moose, caribou, goat or cattle Snowshoe lacing ("babiche"), lashings Hides and Leather
Tanned leather and sinew Bindings, harness, sewing Hides and Leather
A steam box Bending wood A wooden box or hollow log over a pot of boiling water (Furniture)
Bending forms Shaping frames and ski tips Planks with pegs or blocks
Pine tar, beeswax, tallow Waterproofing and waxing Tar, Pitch and Glue, Beekeeping
Fur strips (elk, reindeer, seal, goat) Climbing grip on skis Hunting and Trapping
Drawknife, axe, knife, auger Shaping and drilling Axes, Chisels, Knives and Planes, Drills and Boring

Where to find it

  • Ash (leaves of 7–13 leaflets, black winter buds) grows in damp lowland woods; birch was the classic Scandinavian ski wood; hickory (North America) is the toughest of all. Pick a straight, knot-free trunk 15–25 cm thick and split it with wedges so the grain runs unbroken end to end; sawn wood with grain running out of the side snaps when bent.
  • Rawhide: any large animal skin, cleaned of hair and flesh and dried, not tanned (Hides and Leather). Moose and caribou hide make the best snowshoe lacing; cattle and horse hide serve well.
  • Willow and birch roots: long, flexible withies and roots for lashing, toe straps and ski-pole baskets.

Method 1: Snowshoes

Cutting babicheone spiral strip froma soaked rawhide Framesplit ash 2.5 × 2 cm,steamed and bent Front crossbar38 cm from the toe Back crossbar33 cm further back Tail sectionfine babiche 2–3 mm Taillashed or riveted Bindingtoe strap + heel strap;heel lifts freely Toe: fine babiche,six-sided weave Middle: heavybabiche 5–6 mm Toe cordball of the foot rests here Toe hole10 × 10 cm; the toes dip into it on each step
Fig. 1 Making a snowshoe. A split ash strip is steamed and bent around a form, the two tails brought together and lashed, and two crossbars fitted. The middle section, where the foot presses, is laced with heavy rawhide; the toe and tail with fine rawhide. The ball of the foot sits on the toe cord, with the toes dipping into the toe hole on each step.

Choose the shape:

Shape Size Best for
Bearpaw (round, no tail) 35 × 75 cm Thick forest, brush, steep ground; easy to turn
Michigan or Huron (teardrop with a tail) 30 × 100 cm All-round use; the best first pair
Alaskan or trail (long and narrow, toe turned up) 25 × 140 cm Open country and deep powder; fast in a straight line

Step by step (a Michigan pair):

  1. Split the frame stock. For each shoe, split and shave a strip of green ash 2.4 m long, 2.5 cm wide and 2 cm thick, the grain running straight along it. Taper the last 40 cm of each end to about 1.5 cm thick, where the tails will join.
  2. Make the form. On a plank, draw the outline of the shoe and fix stout pegs or blocks just inside the line all round, and a centre block where the crossbars go.
  3. Steam. Steam the strip in the steam box for about 1 hour per 2.5 cm of thickness — here about an hour. The wood should bend without cracking. (Without a steam box, soak it in a stream for a week, then pour boiling water over the bend area just before bending.)
  4. Bend. Working quickly while hot, bend the middle of the strip around the toe of the form first, then work both sides around the pegs and bring the two ends together at the tail. Wedge or tie everything to the form. Bend a little further than you need — the wood springs back slightly.
  5. Dry on the form for one to two weeks in a cool, dry place out of the sun.
  6. Fit the crossbars. Shave two crossbars about 2 × 3 cm, each slightly longer than the frame is wide at its place. Cut shallow mortises (slots) into the inside of the frame and spring the bars in: the front crossbar about 38 cm from the toe, the back crossbar about 33 cm behind it. Lash or peg the tail ends together with rawhide or two small iron rivets.
  7. Drill the lacing holes. In the toe and tail sections, drill small holes (4–5 mm) through the frame from inside to outside every 2.5 cm, set back about 6 mm from the inner edge.
  8. Cut the babiche. Soak dry rawhide until soft. Cut it in a continuous spiral strip, going round and round the hide from the outside in: 5–6 mm wide from the thick parts for the middle section, 2–3 mm wide from the thin parts for the toe and tail. A deer hide gives 50–100 m of strip.
  9. Lace the toe and tail with the fine babiche through the holes, in a hexagonal (six-sided) weave — the traditional pattern of three sets of strands crossing at 60°, which spreads load evenly. Keep it wet and pull each strand firmly.
  10. Lace the middle with the heavy babiche, wrapped round the frame itself and the two crossbars. First lay a strong toe cord: several strands across the frame about 10 cm behind the front crossbar, leaving an open toe hole about 10 cm long and 10 cm wide between it and the crossbar. Then weave the rest of the middle section in the same six-sided pattern, closer and tighter than the toe and tail.
  11. Dry and seal. Let the laced shoes dry slowly away from the fire for several days; the rawhide shrinks drum-tight. Then rub the lacing and frame with warm fat or melted beeswax and pine pitch, or several coats of boiled-oil varnish, to keep water out. Wet rawhide sags.
  12. The binding. A leather strap or wide lamp wick loop over the toes of the boot and a strap round the heel, fixed to the toe cord. Put the ball of the foot on the toe cord, so on each step the toes dip into the toe hole and the heel lifts freely while the tail drags.

Walking: walk with feet a little wider apart than usual, lift each shoe just clear of the snow, and let the tail drag. Uphill, kick the toe into the slope; downhill, lean back slightly and dig in the heels; across a slope, stamp the uphill edge flat. In deep snow, the person in front breaking trail works twice as hard: change leaders every 10–15 minutes.

Method 2: Skis

Side view tip up10–15 cm camber ~2 cmarch under the foot toe strapthrough a slot heel strapheel free to lift 2.5 cm thick at the foot,1 cm at the ends balance pointfront of the boot From below groove1 cm wide, 3 mm deep — runs straight; base tarred and waxed climbing skinfur, hairs pointing back, tied at tip and tail to tail
Fig. 2 A wooden ski in side view and from below. The tip is steamed and bent up; the ski is arched slightly under the foot (camber) so the weight spreads to both ends; a shallow groove underneath helps it run straight. A fur strip with the hairs pointing back grips for climbing. A toe strap and a heel strap hold the boot, leaving the heel free to lift.

Sizes. Length about your height plus 20–30 cm for open country, closer to your height for forest and steep ground. Width 7–10 cm; wider (10–12 cm) floats better in deep untracked snow. Thickness about 2.5 cm under the foot, tapering to 1 cm at tip and tail.

Step by step:

  1. Split two straight blanks of birch, ash or hickory a little longer, wider and thicker than the finished ski. Season them for a few weeks, or carve green and dry slowly.
  2. Shape each with axe and drawknife: flat on the bottom, the top slightly domed, tapering in thickness from the middle to each end, and slightly narrower at the waist than at the tip.
  3. Cut a groove down the middle of the bottom, about 1 cm wide and 3 mm deep, from 20 cm behind the tip to the tail. It helps the ski run straight.
  4. Bend the tip. Steam the front 40 cm for an hour and bend it over a curved form so the very tip rises about 10–15 cm. At the same time, clamp the middle of the ski up on a block about 2 cm high with both ends tied down, so it dries with an arch (camber) under the foot. Leave it on the form for one to two weeks.
  5. Find the balance point. Balance the ski on a knife edge. The front of the boot goes at or just behind this point, so the tip rises a little when the ski is lifted.
  6. Fit the binding. Cut a slot sideways through the ski under the toe of the boot (or fix two small blocks) for a leather toe strap, and add a heel strap of leather or twisted willow round the back of the boot, tight enough to hold the boot forward in the toe strap. The heel must lift freely.
  7. Tar the base. Brush warm pine tar (Tar, Pitch and Glue) on the bottom, heat it gently with a glowing ember or hot iron until it bubbles and soaks in, and wipe off the excess. Repeat. Tar waterproofs the wood and is the base for wax.
  8. Wax. For glide, rub on beeswax or hard tallow and polish it with a cork or smooth wood. For grip on flat ground, a softer, sticky mixture (pitch with a little wax) under the foot only.
  9. Climbing skins. Cut strips of hide with short, stiff fur, as wide as the ski and as long as from tip to tail, hair pointing backward. Tie or strap them on with cord through the tip and a loop round the tail. With skins on, you can walk straight up moderate slopes.
  10. Poles. Two straight poles of hazel, ash or bamboo reaching to the armpit, with a basket — a ring of willow 10–12 cm across tied a hand's width above the tip — so they do not sink. Or one long, stout pole, held in both hands, the old way: it steers and brakes.

Basic technique: on the flat, kick and glide — push down and back with one foot while sliding the other forward, arms swinging opposite as when walking. Climb a gentle slope with the tips pointing outward in a herringbone; a steep one by side-stepping or zig-zagging. To slow or stop on a slope, push the tails apart into a wedge (snowplough). If you are going too fast, sit down to the side.

Method 3: Sledges

Toboggan (for deep, soft snow — it floats where runners sink):

  1. Split or saw 3–4 boards of ash, birch or tamarack about 1 cm thick, 10–15 cm wide and 2.5–3 m long.
  2. Lay them side by side to make a bed 30–45 cm wide and lash crossbars across them every 40 cm with rawhide through holes, the knots on top.
  3. Steam the front 60 cm and curl it up and back into a scroll, tying it to the first crossbar with rawhide.
  4. Run a lashing rope along each side for tying the load, and a towing rope from the curl.

Runner sledge (for packed snow, trails and ice):

  1. Two runners of hardwood 2–3 m long, 15 cm high, 5 cm thick, their front ends curved up.
  2. Crossbars across the top every 30–40 cm, lashed, not nailed — a flexible sledge survives rough ice; a rigid one breaks.
  3. Shoe the runners with strips of hard bone, antler or iron (Blacksmithing) to stop wear. In hard cold, Arctic peoples coated wooden runners with a layer of mud or peat, then wiped them with water to build a thin, glass-smooth skin of ice that glided better than anything else.

Hauling by hand. A padded belt round the hips and a strap over the shoulders, joined to the sledge by two stiff poles (not rope) so it cannot run into your legs downhill. One fit person can haul 40–80 kg over good snow for a full day.

Dogs. A strong northern dog of 25–40 kg can pull about its own weight all day on a good trail, more for short hauls.

  • Harness: a padded loop of leather or thick webbing over the head and round the chest, with two traces running back along the dog's sides to a short spreader bar behind it, then a single line to the sledge. The pull must come on the chest and shoulders, never the throat.
  • Hitch: in forest, the gangline — dogs in pairs along a central line, a trained leader in front. On open tundra and sea ice, the fan hitch — each dog on its own line to the sledge, spread out like a fan, so one dog through the ice does not drag in the rest.
  • Care: working dogs in the cold need 1–2 kg of fatty meat or fish a day, water and rest. Check their feet every evening for ice balls and cuts; sew hide booties for icy trails (Keeping Animals, Animal Health).

Horses and oxen haul heavy sleighs on packed winter roads; their shoes need studs to grip ice (Draft Animals and Harness, Wagons and Carriages).

Travelling safely on snow and ice

Ice thickness — for clear, hard, black or blue ice, newly formed:

Thickness Safe for
Under 10 cm Nobody. Stay off.
10 cm One person on foot
12–15 cm A group walking in single file, well spaced; a hand sledge
20–30 cm A horse and sleigh; a loaded dog team
Over 30 cm Heavy loads

White, snowy or cloudy ice is about half as strong: double these figures. Grey, wet, honeycombed spring ice may be rotten at any thickness — stay off it. Salt-water ice is weaker and more flexible than lake ice.

Where ice is thina frozen lake from above stream inletmoving water spring under snowinsulated: thinner outlet reed edges pressure ridge test holesevery 10–20 m If you fall inseen from the side 1. Breathe; turn backtoward the ice that held you 2. Arms on the ice, kick flat,pull forward with the picks 3. Roll away; do not standuntil on thick ice. Then warm up fast.
Fig. 3 Ice safety. Test new ice by chopping holes every 10–20 m. Danger spots are where water moves or the ice is insulated: river currents, inlets and outlets, springs, edges near reeds and rocks, and under thick snow. If you fall in, turn back towards the ice that held you, kick your legs up behind you, pull yourself out with ice picks, and roll away.
  • Test it. On unknown ice, chop a hole with an axe or ice chisel every 10–20 m and measure. Tap ahead with a pole: a dull thud is solid; a hollow sound or a crack is not.
  • Avoid river ice over current, mouths of streams, outlets, springs, ice near reeds, rocks, trees and docks, pressure ridges, and ice under deep snow (snow insulates it so it freezes thinner).
  • Spread out, 5–10 m apart, in single file, ideally roped together. Carry a long pole crossways. Wear ice picks — two short wooden handles with nails set in the ends, joined by a cord round the neck. Loosen pack straps and ski bindings so you can shed them.
  • If you fall in — the 1-10-1 rule. You have about 1 minute of gasping cold shock: keep your head up and get your breathing under control. You then have about 10 minutes of useful strength: turn back toward the direction you came from (that ice held you), get your arms onto the ice, kick your legs up behind you until you are nearly flat, and pull yourself forward with the picks or your elbows. Roll away from the hole; do not stand until you are on thick ice. You have roughly 1 hour before the cold makes you unconscious. Then get to a fire and dry clothes at once (Surviving Cold and Heat).
  • Rescuing someone: never run to the hole. Reach with a pole, branch, ski or rope while lying flat; throw a rope; or form a chain of people lying flat, each holding the ankles of the one in front.

Avalanches happen mostly on open slopes of 30–45° — about as steep as a staircase — after heavy snowfall (30 cm or more in a day), on slopes where wind has piled snow, and in sudden thaws. Warning signs: recent slides nearby, cracks shooting out from your skis, a hollow "whumpf" as the snow settles. Travel on ridges, in thick forest, or on flat valley floors well away from the foot of slopes; cross any dangerous slope one at a time, the others watching; avoid gullies and the ground under overhanging snow (cornices).

Other winter rules: dress in layers and avoid sweating; wear slit goggles against snow blindness (Surviving Cold and Heat); carry fire-making kit, a dry layer and food; tell others your route; navigate carefully in whiteouts (Finding Direction).

How to tell it worked

  • On snowshoes you sink no more than 10–20 cm in powder where boots sink to the knee or more.
  • Skis glide forward a metre or more with each kick on flat snow, and climb moderate slopes with skins.
  • A loaded sledge slides with a steady pull and does not dig in or tip on side slopes.
  • You come home dry inside your clothes, with all fingers and toes warm.

Note Troubleshooting. Snowshoe frame cracks while bending → not steamed long enough, grain runs out of the side, or wood too dry; use fresh, split green wood and bend over a strap on the outside of the curve. Lacing sags → it got wet; dry the shoes slowly and seal them better with fat, wax or varnish. Snowshoes sink too deep → they are too small for your weight and load; make bigger ones, or pack the trail first. Skis stick and gather balls of snow → the base is wet or bare; dry it, tar and wax it. Warm, wet snow sticks to everything: rub on more wax. Skis slip backwards → too much glide wax under the foot; add grip wax or use skins. Sledge digs in → runners too narrow for soft snow; use a toboggan, or pack a trail.

Dangers

Danger Thin ice and avalanches kill quickly and silently. Never cross ice you have not measured, never travel alone on ice or avalanche ground, and turn back when in doubt. A day lost going round a lake is better than a life lost crossing it.

  • Exhaustion and sweating lead to hypothermia when you stop. Pace yourself, and stop early to make camp (Surviving Cold and Heat, Shelter).
  • Frostbite of feet in wet bindings or tight boots; check toes at every stop.
  • Falls on skis break legs and wrists. Learn on gentle slopes, and carry the means to splint and haul an injured person (The First Aid Kit, Wound Care and Antiseptics).
  • Runaway sledges downhill crush the person in front; use stiff shafts or a rope brake (a loop of rope thrown under the runners), and lead dogs and horses down steep slopes slowly.
  • Steam scalds when bending wood; open the steam box with a stick.

What this unlocks

Winter becomes a season for hauling timber and ice (Ice and Refrigeration), hunting, trapping and trade. Sledge-runner ideas lead to sleighs for Draft Animals and Harness, and skis became the basis of whole armies, postal routes and, later, a sport. Packed winter roads and frozen rivers link settlements in winter as well as boats do in summer (Roads and Bridges, Boats and Sails).

How it was first done

Fragments of skis and sledge runners about 8,000 years old have been found at Vis I, a peat bog in northern Russia; at Zhokhov Island in the Siberian Arctic, people bred and used sled dogs about 9,000 years ago. A ski about 5,000 years old was dug from a bog at Kalvträsk in Sweden, and rock carvings at Rødøy in Norway show a skier more than 4,000 years ago. Snowshoes probably developed in northern Asia and reached perfection among the Indigenous peoples of North America; a snowshoe of birch and plant fibre about 5,800 years old melted out of a glacier in the Italian Alps. In 1206 two Norwegian skiers carried the infant prince Håkon across the mountains to safety — an event still remembered by the Birkebeiner ski race. In the 1860s Sondre Norheim of Telemark, Norway, added a firm heel binding of twisted willow and shaped skis narrower at the waist, the beginnings of modern skiing; in 1888 Fridtjof Nansen crossed the Greenland ice cap on skis, hauling sledges by hand.

Source: content/entries/transport/snowshoes-and-skis.md