Part 15 · Knowledge and Science
Spectacles
How to test eyesight with a home-made letter chart and a pinhole, choose the right lens for reading, long sight and short sight, grind it to strength, and fit it in a frame of horn or wire — plus the basic eye care that saves sight: getting grit out, treating infections, and knowing which blindness spectacles cannot help.
- Difficulty
- ●●●●●
- Time
- An hour to test someone's eyes; one to three days to grind a pair of lenses; a few hours for frames
- Steps from zero
- 8 prerequisites →
You need first
LensesThis unlocks
—The full path from nothing — 8 steps before this one
Do them roughly in this order. See it on the tech tree →
Why it matters
Almost everyone over about 45 years old gradually loses the ability to focus on things close up. Without help, the scribe can no longer read and the tailor cannot thread a needle — and these are the most experienced people you have. A pair of simple reading glasses gives each of them another 20 or 30 years of skilled work.
At the other end of life, many children and young people are short-sighted: the far world is a blur, from a hunter's quarry to a teacher's writing on the wall. Concave lenses fix this in a moment.
Spectacles may be the cheapest, most effective medical device ever made. No lens helps an eye that infection or injury has ruined, so this chapter also covers basic eye care.
How it works
The eye is a camera. The clear front window (the cornea) and the lens inside the eye bend light to form a sharp picture on the retina, the light-sensitive layer at the back. To look at something close, small muscles let the eye's lens bulge and grow stronger. This is focusing (doctors call it accommodation).
Three common faults:
- Short sight (myopia). The eye is a little too long, or too strong. Distant things blur; near things are clear. Corrected by a concave (minus) lens. Usually appears in childhood or the teens and grows for some years.
- Long sight (hyperopia). The eye is a little too short. Young people focus their way through it, at the cost of eyestrain and headaches; older people see blurred near and, later, far too. Corrected by a convex (plus) lens.
- Old sight (presbyopia). The eye's own lens stiffens with age, so it can no longer bulge to focus near. It happens to everyone. At 20 you can focus at 10 cm; at 40, at about 25 cm; at 50, at 50 cm; at 60, beyond a metre. Corrected by a convex lens for close work only.
A fourth, astigmatism, is a cornea curved more one way than the other, so lines in one direction look sharper than lines at right angles. It needs cylindrical lenses (see Going further); with mild astigmatism the best ordinary lens is usually enough.
Lens strength is measured in dioptres (D): 100 divided by the focal length in centimetres (Lenses). A +2 D lens has a focal length of 50 cm; a −4 D lens spreads light as if from a point 25 cm in front of it. Plus means convex; minus means concave.
What you need
| Item | Details |
|---|---|
| A trial set of lenses | Convex: +0.5, +1, +1.5, +2, +2.5, +3, +3.5, +4 D. Concave: −0.5, −1, −1.5, −2, −3, −4, −5, −6 D. Each 3–4 cm across, labelled on a wooden or Hides and Leather holder |
| A trial frame | A simple frame of wood or wire with clips or slots that hold a trial lens in front of each eye |
| Eye chart | Drawn in black Ink on white Paper or a whitewashed board (below) |
| Near card | Small text, fine print, a needle to thread |
| Pinhole card | Dark card or thin wood with a hole 1–1.5 mm across |
| Measuring tape or rod | 6 m of marked cord, and a ruler in millimetres (Measurement from Scratch) |
| Lens grinding tools | As in Lenses, one pair of tools for each strength you make |
| Frame materials | Cattle or goat horn, bone or hardwood; or brass, copper or iron wire 1.2–1.5 mm thick (Copper Wire) |
| Clean cloth and boiled water | For eye care |
Where to find it
- Horn: from cattle, goats, sheep. Boil it for 30–60 minutes until it softens, split it lengthwise and press it flat between warm boards (Horn and Bone Working). It becomes a tough, springy sheet that can be cut, filed and bent when warm — the classic frame material.
- Bone (boiled clean, sawn and filed) and drawn wire of copper, brass or iron (Copper Wire, Zinc and Brass).
- Pine resin and beeswax: melted together half and half, they make a cement for holding lenses in wooden frames and blanks on grinding handles (Tar, Pitch and Glue).
Testing eyesight
1. Make the chart
Draw rows of letters, or the letter E facing different ways (up, down, left, right) so that people who cannot read can point. Each letter is a square; the bars and gaps are each one-fifth of its height. For a chart read at 6 m (about 7–8 paces):
| Row | Letter height | Means |
|---|---|---|
| 1 | 87 mm | Seen by a normal eye at 60 m |
| 2 | 52 mm | at 36 m |
| 3 | 35 mm | at 24 m |
| 4 | 26 mm | at 18 m |
| 5 | 17.5 mm | at 12 m |
| 6 | 13 mm | at 9 m |
| 7 | 8.7 mm | at 6 m — normal vision |
If you only have 3 m of room, halve every height. Hang the chart in good, even daylight, at eye height, out of glare.
Vision is written as distance / row: "6/6" is normal; "6/18" means this person needs to stand at 6 m to read what a normal eye reads at 18 m. 6/12 or better in the better eye is good enough for most work; worse than 6/18 makes many tasks hard and dangerous.
2. Test each eye
- Stand the person at 6 m. Cover one eye with a palm (not pressing) or a card.
- Point to letters from the largest row down. Note the smallest row where they get most letters right.
- Repeat with the other eye, then both.
3. The pinhole test
Have them look at the chart through the pinhole card with each eye in turn.
- Sees better through the pinhole (two or more rows) → the eye is out of focus: short, long or astigmatic. Spectacles will help.
- Sees no better → the problem is inside the eye: cataract, a scarred cornea, glaucoma or a damaged retina. Spectacles will not help. See Eye care.
The pinhole lets through only a thin pencil of light, which needs no focusing. It is the most useful test in this chapter.
4. Near vision
Give them print about 1 mm tall and ask them to hold it where they read best. A young normal eye reads it easily at 30–40 cm. If they push it to arm's length, or cannot read it, they need reading glasses.
Choosing the lens
Reading glasses (presbyopia)
Start from age, then try:
| Age | Usual reading lens |
|---|---|
| 40–45 | +0.75 to +1.5 D |
| 45–50 | +1.25 to +2 D |
| 50–55 | +1.75 to +2.5 D |
| 55 and over | +2.25 to +3 D |
- Put the lens from the table in the trial frame. Give them fine print at their usual working distance — about 35–40 cm for reading, 25–30 cm for needlework or close craft.
- Try half a dioptre stronger and weaker. Choose the weakest lens that lets them read comfortably there; too strong a lens forces work too close.
- A person who is long-sighted already needs more; a short-sighted person needs less, or may read fine with no glasses at all.
Short sight (myopia)
- Find the far point. Cover one eye. Have them hold fine print close and slowly move it away until it just starts to blur. Measure that distance in centimetres. The lens they need is about −100 ÷ that distance. Blur beyond 50 cm → about −2 D; beyond 25 cm → about −4 D.
- Check on the chart. Put that lens in the trial frame and test at 6 m. Try half a dioptre more and less.
- Choose the weakest minus lens that gives the best distant vision. Extra minus makes letters smaller and blacker but not sharper, and tires the eyes. Do not over-correct, especially in children.
- Repeat for the other eye. The two eyes often differ.
Long sight (hyperopia)
Suspect it in a young person who sees well far away but gets headaches or blurring when reading, or in a young child whose eye turns inward (a squint). Try plus lenses at the chart: a long-sighted person will still read the 6 m line with +0.5 to +2 D in front of the eye. Give the strongest plus lens that does not blur the distance.
Warning A child with a squint, or one eye much worse than the other, must be dealt with before about age 7. The brain stops using the blurred or turned eye and the sight in it is lost for life ("lazy eye"). Glasses to correct the focus, plus covering the good eye with a patch for a few hours each day for some weeks, can save it. Treatment works best when young; after about age 8 it helps less, though it is still worth trying up to about 12.
Grinding to strength
Grind as in Lenses. The strength depends on the radius of the tools. For ordinary glass (refractive index about 1.5):
| Lens strength | Both faces curved (equal radius) | One face curved, one flat |
|---|---|---|
| ±0.5 D | 200 cm | 100 cm |
| ±1 D | 100 cm | 50 cm |
| ±1.5 D | 67 cm | 33 cm |
| ±2 D | 50 cm | 25 cm |
| ±2.5 D | 40 cm | 20 cm |
| ±3 D | 33 cm | 17 cm |
| ±4 D | 25 cm | 12.5 cm |
| ±6 D | 17 cm | 8.3 cm |
The rule is simple: radius in cm = 100 ÷ dioptres for an equal double lens, half that for a flat-backed one. Convex lenses are ground in the concave tool; concave lenses in the convex tool.
Blanks and thickness. Use discs 4–4.5 cm across. A +2 D double-convex lens 4 cm across is only 0.4 mm deeper at the centre on each face, so an edge 1.5 mm thick gives a centre about 2.3 mm. A −4 D double-concave lens of the same size has a centre of 1.5 mm and an edge of about 3.1 mm.
Make many at once. Spectacle makers pitched 5–7 blanks side by side on one curved block and ground them together on a large tool. One pair of tools per half-dioptre step supplies a whole town.
Check every lens.
- Plus lenses: measure the focal length in sunlight (Lenses) and work out dioptres.
- Minus lenses: lay the concave lens against plus lenses of known strength. Look through the pair at a window frame far away and move them side to side. When the frame does not move at all, the two lenses cancel: the minus lens has the same strength as that plus lens.
- Which is which? Look through a lens at a distant edge and move the lens sideways. If the edge moves the opposite way, it is a plus lens; the same way, minus.
- Find the optical centre. Look through the lens at a cross drawn on a wall. Move it until the lines through the lens line up exactly with the lines outside. Mark that point on the lens with an ink dot. This point must sit in front of the pupil.
Making frames
Measure the pupils
Sit facing the person at arm's length, at the same eye height. Hold a ruler across the bridge of their nose. Close your right eye, have them look at your open left eye, and set the ruler's zero under the centre of their right pupil. Then close your left eye, open your right, have them look at it, and read the ruler under the centre of their left pupil. This is the pupil distance — usually 58–70 mm in adults, smaller in children. For reading glasses, subtract 3 mm, because the eyes turn in to read.
Set the optical centres of the two lenses this far apart. Within 2–3 mm is good enough for weak lenses; strong ones (over 4 D) must be closer, or they pull the eyes and cause headaches.
Shaping the lens edge
Nibble the lens edge round with the notched end of a soft iron bar ("grozing"), then grind it smooth on a flat stone with wet sand. For a grooved frame, grind a gentle V-shaped bevel all round the edge so it seats in the groove.
Frame 1: Rivet or bridge frame of horn
- From flat, softened horn 2–3 mm thick, cut two rings joined by an arch over the nose — or two rings with short handles joined by a rivet, like the first spectacles.
- Cut each ring's hole 1 mm smaller than the lens. With a knife point or a small file, cut a groove 1 mm deep round the inside of each hole.
- Drop the frame in boiling water for a few minutes until it softens. Spring the lenses into the grooves while it is hot. As the horn cools it shrinks and grips them.
- Leave the arch wide enough to sit on the nose without pinching; pad it with a strip of leather.
Frame 2: Wire frame with sides
- Wrap 1.2–1.5 mm brass or copper wire tightly round the bevelled edge of each lens to make its rim. Twist or solder the ends together at the outer side, leaving a small loop (Soldering and Brazing). Better: file a shallow groove along the inside of the wire first, so it holds the bevel.
- Bend a separate piece of wire into an arch for the bridge, about 18–22 mm across at the nose, and solder or bind its ends to the inner edges of the two rims at the height of the lens centres.
- Make two side arms 13–14 cm long. Form a loop at the front end to hinge through the rim's loop, and curve the back end down behind the ear.
- Adjust: the lenses sit about 12 mm in front of the eyes, square to the face, bottoms tilted slightly towards the cheeks.
Before side arms, cords looped round the ears held spectacles on; they work perfectly well.
How to tell it worked
- The chart. Short-sighted people should now read the 6/6 or 6/9 row at 6 m. Reading glasses: fine print clear at 35–40 cm.
- Comfort. After half an hour's reading, no ache, no double vision, no headache.
- The cross test. Wearing the glasses, look at a cross on the wall: it should look straight and unbroken through both lenses together.
Note Troubleshooting. Headaches, pulling feeling, double vision → the lens centres are not over the pupils. Re-measure and move them; check both lenses are the same strength if they should be. Can read but only very close → reading lenses too strong. Go 0.5 D weaker. Things look small, sharp but tiring → minus lenses too strong. Go 0.5 D weaker. Blurred whatever lens you try, even through a pinhole → the eye itself is damaged. See below. Lenses fall out of horn frames → the groove is too shallow; recut it, and seat the lens while the horn is hot.
Eye care
Spectacles only help a healthy eye. Much blindness in the world is caused by injuries, infections and poor diet that you can prevent or treat at home. This section covers what a spectacle maker meets most; Eye Health and Preventing Blindness covers eye disease fully.
Grit and splinters
- Do not rub. Rubbing scratches the clear window of the eye.
- Flush. Pour clean water (boiled and cooled if you have time) gently across the open eye from the inner corner outwards, for several minutes, or have the person blink with the face in a bowl of clean water.
- Look under the lower lid by pulling it down while they look up. Lift any speck with the twisted corner of a clean, damp cloth.
- Look under the upper lid: have them look down. Grasp the upper lashes, lay a clean thin stick or a straw across the lid about 1 cm above the lashes, and fold the lid up over it. Wipe the speck off with the damp cloth. Have them look up and blink to unfold the lid.
- A speck stuck on the clear front of the eye — especially a hot flake of metal from hammering or grinding, which leaves a rust ring — needs skilled hands and a fine instrument. Do not dig with a needle. Keep the eye closed and seek help.
A small scratch feels like grit for a day or two, then heals. If it is worse after two days, with pus, a white spot on the clear part or failing sight, it is infected — an emergency (Infectious Diseases).
Chemicals in the eye
Danger Lime, wet cement, lye, wood-ash lye, strong soap and acids can blind in minutes. Wash at once with whatever clean water is nearest — do not wait to boil it. Hold the eyelids wide open and pour water across the eye for at least 20–30 minutes for alkalis (lime, lye, cement), 15 minutes for acids, turning the head so the water runs away from the other eye. Pick out any lumps of lime with a damp cloth. Alkalis keep burning long after it stops hurting; keep washing. See Lime, Lye and Potash, Emergencies.
Blows and stabs
A blow that leaves blood in the coloured part, a misshapen pupil, or anything stuck into the eye: do not press, pull anything out or wash it. Tape a cup or a ring of cloth over the eye so nothing touches it, keep the person sitting up and still, and get the most skilled help you can (Basic Surgery).
Infections
- Red, sticky, gritty eyes ("pink eye", conjunctivitis), sight normal: usually clears in one to two weeks. Bathe away the discharge several times a day with cloth dipped in boiled, cooled water, wiping from the nose outwards with a fresh piece each wipe. Wash hands and give the person their own towel; it spreads fast.
- A newborn baby with pus from the eyes in the first weeks needs urgent help: infection caught at birth can destroy the eye in days. One drop of 1 % silver nitrate in each eye at birth prevents most of it (Silver Nitrate and Silver Salts, Safe Childbirth).
- A stye (a painful lump on the eyelid edge): hold a clean cloth wrung out in hot water against it for 10 minutes, 3–4 times a day. Do not squeeze it.
- Trachoma — the world's leading infectious cause of blindness — spreads by fingers, cloths and flies. Years of repeated infection scar the lid until the lashes turn inward and scratch the eye blind. Daily face washing and latrines (Sanitation and Germs) prevent it; lashes that already rub the eye can be plucked out every few weeks with small tweezers until a surgeon can turn the lid (Eye Health and Preventing Blindness).
Diet
Night blindness — seeing poorly at dusk — is the first sign of lack of vitamin A. In young children, especially after measles or diarrhoea, it can go on to melting corneas and permanent blindness. Liver, eggs, milk, butter, red palm oil, dark green leaves and orange vegetables prevent it (Nutrition and Deficiency Diseases, Eye Health and Preventing Blindness).
Danger signs — what spectacles cannot help
Get the most skilled help available for:
- Sudden loss of sight in one or both eyes.
- A painful red eye with blurred vision, pain in bright light, or a white spot on the clear front.
- Severe eye pain with headache and vomiting, haloes round lights, and an eye that feels hard as a stone when pressed gently through the closed lid: acute glaucoma, which can blind within a day or two.
- Flashes of light and a dark curtain spreading across the view: a torn retina.
Cataract
A cataract is the eye's own lens turning cloudy, usually with age, sometimes after injury, and faster with years of strong sun or furnace glare. Sight grows misty, lights dazzle, and in the end the pupil looks grey or white. The pinhole does not help.
Nothing but surgery cures it — removing the clouded lens through a tiny cut, which needs a trained surgeon, magnification, fine instruments, sterility and anaesthesia (Basic Surgery, Sterilising Instruments and Dressings, Anaesthesia). The ancient "couching" — pushing the lens back into the eye with a needle — often ended in infection and total blindness. Do not attempt it.
What spectacles can do: once a surgeon has removed a cataract, the eye has lost most of its focusing power, and a strong convex lens of about +10 to +12 D (tools of radius 8–10 cm, both sides) gives back useful sight — with about +3 D more for reading. Making these is well within your skill.
Prevent it where you can: wide hat brims and shade in strong sun; slit goggles on snow, sea and desert (below); never staring into furnace glow (The Thermometer).
Snow blindness and goggles
Sun glare off snow, ice, sand or water burns the surface of the eye; hours later the eyes feel full of sand and cannot bear light. It heals in one to three days with the eyes closed in the dark under cool wet cloths. Prevent it with slit goggles, as Arctic peoples have for thousands of years: wood, bone or antler shaped to the face, with a slit 1–2 mm wide for each eye, blackened inside with soot. With small glass windows instead of slits, the same goggles protect grinders and smiths from sparks.
Danger Never look at the sun — not through spectacles, not through smoked glass, not during an eclipse. It burns a permanent blind spot in the centre of sight, painlessly, in seconds.
Dangers
- Reading glasses worn while walking blur the ground and cause falls in the old. Take them off, or make half-height lenses to look over.
- Glass lenses can shatter in a blow. For children, smiths and hunters, keep them at least 2 mm thick and set deep in the frame.
- Wrong glasses cause headaches but do not damage the eyes; do not let fear of error stop you trying.
- Wash your hands before and after touching anyone's eyes.
Going further
- Bifocals. Cut a distance lens and a reading lens each in half and mount the top half of one above the bottom half of the other — Benjamin Franklin's design, about 1784.
- Meniscus lenses. A lens with one side convex and the other concave (shaped like a crescent in section) gives a wider clear view than a double-convex one. A +2 D reading lens can be ground with a front surface of radius 12.5 cm and a back of 25 cm.
- Astigmatism. Grind one face on a cylindrical tool (a rod ground against a matching trough with strokes only along its length) and turn its axis to where the person sees lines worst on a clock-face chart of radiating lines. Hard; most early spectacle makers never did it.
- Tinted glass (a little iron or manganese in the batch) makes sun spectacles (Glass).
- Magnifiers for the nearly blind: a strong +10 to +20 D hand lens or a reading stone (a half-sphere of glass laid on the page) lets some people with damaged eyes still read (Hearing Aids, Braille and Daily-Living Aids).
How it was first done
Seneca noted that letters look bigger through a globe of water, and Ibn al-Haytham explained the eye and lenses around 1021. Medieval scholars read through polished reading stones of rock crystal or beryl, and Roger Bacon wrote in 1267 that a curved glass helps old people to read. Spectacles were invented in northern Italy around 1286: in 1306 the preacher Giordano da Pisa told his Florentine congregation that it was "not yet twenty years" since the art of making eyeglasses was found. The oldest picture of a man wearing them is a 1352 fresco by Tommaso da Modena in Treviso. Concave lenses for short sight were made in Florence by the mid-1400s. Benito Daza de Valdés published the first book on fitting spectacles in Spain in 1623, and the London optician Edward Scarlett made frames with side arms around 1727. In 1862 the Dutch eye doctor Herman Snellen published the letter chart still used today, and in 1864 his teacher Franciscus Donders explained short, long and old sight in the terms used here.
Source: content/entries/knowledge/spectacles.md