Part 7 · Home and Daily Life
Violins, Guitars and Harps
How to build the violin family (fiddle, violin, viola, cello) with their bows, bridges and sound posts; lutes and guitars with frets placed by a simple rule; and the frame harp — plus how to make strings of gut, silk and steel and the pegs that tune them. These are the instruments that carry a melody across a hall.
- Difficulty
- ●●●●●
- Time
- A box fiddle in a week; a first violin or guitar in one to three months of evenings; a lap harp in two to three weeks
- Steps from zero
- 12 prerequisites →
This unlocks
—The full path from nothing — 12 steps before this one
- Stone Tools
- Cordage and Rope
- Fire
- Finding and Preparing Clay
- Basic Woodworking
- Hunting and Trapping
- Charcoal
- Pottery
- Hides and Leather
- Tar, Pitch and Glue
- Musical Instruments
- Glues and Adhesives
- Violins, Guitars and Harps
Do them roughly in this order. See it on the tech tree →
Why it matters
The drums, flutes and lyre of Musical Instruments make music for a village gathering. The instruments here hold a hall: a fiddle plays a dance tune loud enough for a barn full of dancers, a guitar or lute carries a storyteller's song, and a harp gives whole chords. One good fiddler is a community's dance band, its wedding music and its comfort at a funeral.
Building them is also the finest training in woodworking there is. A violin top is carved to 2.5–3 mm and must not split under 20 kg of string pull. Splitting wood by its grain, bending thin wood with heat, fitting joints with no gap and measuring to a tenth of a millimetre are the same skills clocks and scientific instruments need.
How it works
A string alone barely moves the air. Every instrument here has three working parts:
The string sets the pitch, by its length, tension and weight per metre (Musical Instruments):
Tension (newtons) = (2 × length in m × frequency)² × mass per metre (kg)
Mass per metre = density × cross-section area. Gut is about 1,300 kg per cubic metre, steel 7,850, brass 8,500. Divide newtons by 9.8 for kilograms of pull.
A gut violin A string 0.7 mm thick, 328 mm long, tuned to 440 vibrations a second, pulls about 4.5 kg; a steel E string 0.26 mm thick at 659 vibrations, about 8 kg.
The bridge carries the vibration down into the top.
The soundboard (top, or belly) is a thin plate of light, stiff wood that pushes the air; the hollow body adds its own resonance. Spruce is the best wood because it is very stiff along the grain for its weight.
A bow does not pluck. Rosin on the hair grips the string, drags it sideways until it snaps back, then grips again, hundreds of times a second, making a tone that lasts as long as the bow moves.
Frets each shorten the string by the same fraction — about 1/17.8 of what is left — raising the note one semitone (a twelfth of an octave). Twelve frets halve the string.
What you need
| Item | For | Chapter |
|---|---|---|
| Spruce (or fir, cedar), quarter-split, knot-free | Soundboards, bass bars, sound posts | Basic Woodworking |
| Maple (or sycamore, pear, poplar, willow) | Backs, ribs, necks, bridges | — |
| Dense hardwood: boxwood, pear, plum, oak | Fingerboards, pegs, bow frog | — |
| Gouges, knives, small planes, steel scrapers, files | Carving | Axes, Chisels, Knives and Planes, Files and Saws |
| Bending iron: a metal tube 5 cm across, heated from inside by charcoal or a hot bar, clamped to the bench | Bending ribs and sides | — |
| Hide glue, clamps, cord, wedges | Every joint | Glues and Adhesives |
| Calipers (two bent wires on a rivet), a ruler in mm | Thickness | Measurement from Scratch |
| Gut, silk, steel and brass wire; horsehair; rosin | Strings, bows | Below, Iron and Brass Wire |
| Oil or spirit varnish | Finish | Pigments, Paints and Varnish |
Why hide glue? It grabs fast, dries hard, does not creep under steady load — and softens again with heat, so an instrument can be opened to repair a crack. Glue the top on with thinner glue than the rest so it lifts cleanly.
Where to find it
- Spruce and fir grow in cold forests and mountains. Slow-grown trees give the best tops, with rings 1–2 mm apart. Split the log like a cake into wedges (quarter-split) so the rings run straight across each wedge's end; split wood follows the grain and does not crack.
- Maple and sycamore grow in temperate woods. Rippled "flame" maple looks fine; plain maple sounds as good.
- Season everything at least two years under cover with air between the pieces. Wood still drying shrinks and cracks after the instrument is done.
- Horsehair: white tail hair from a stallion or gelding (a mare's tail is soiled by urine).
- Gut, silk and resin: Musical Instruments, Silk, Tar, Pitch and Glue.
The violin family
The parts
| Part | Wood | Size (full-size violin) |
|---|---|---|
| Body length | — | 356 mm |
| Upper bout / waist / lower bout | — | 168 / 112 / 208 mm |
| Top | Spruce | 2.5–3 mm thick, arched 15–16 mm |
| Back | Maple | 4–4.5 mm in the centre, 2.5 mm at the edges |
| Ribs | Maple | 1.0–1.2 mm thick, 30–32 mm high |
| Bass bar | Spruce | 270 mm long, 5–6 mm wide, 11–12 mm high in the middle |
| Sound post | Spruce | 6 mm across |
| Neck with scroll | Maple | Nut to body edge 130 mm |
| Fingerboard | Dense hardwood | 270 mm |
| String length | — | 328 mm |
| Bridge | Maple | 41 mm wide at the feet, 33 mm high, 4 mm thick at the feet, 1.3 mm at the top |
The proportion that matters most: the neck (nut to body edge, 130 mm) to the stop (body edge to bridge, 195 mm) is 2 : 3. The bridge stands between the notches in the middle of the f-holes.
The sound post is a spruce dowel wedged, not glued, between top and back, 2–3 mm behind the treble (E-string) foot of the bridge. It carries vibration to the back and lets the bridge rock on it so the bass foot drives the top. The bass bar stiffens the top under the other foot. Moving the post 1 mm changes the tone; this is how violins are adjusted.
The fiddle (start here)
"Fiddle" and "violin" are the same instrument; "fiddle" just means one played for dancing. Start with a box fiddle: every working part of a violin, none of the carving.
- Sides: bend hardwood strips 3 mm thick, 45 mm wide round an outline 36 × 20 cm with rounded corners, on the bending iron or by steaming (Steam-Bending Wood). Glue blocks in the corners.
- Top and back: flat plates 3 mm thick, spruce for the top, any hardwood for the back. Glue two thin spruce strips across the inside of the top and a bass bar along the bass side.
- Cut two f-holes, or two round holes 2 cm across, one each side of the bridge.
- Glue on back and top. Fit sound post, bridge, a neck mortised into the top block, fingerboard, four pegs and tailpiece as for the violin below.
- Tune in fifths: G–D–A–E (196, 294, 440, 659 vibrations a second).
It sounds thinner than a carved violin, but it plays in tune and teaches the setup.
The carved violin
- Mould. Saw a 12 mm board to the body outline less the ribs, with recesses for six spruce or willow blocks (neck, tail, four corners), spot-glued so they break free later.
- Ribs. Plane maple to 1.1 mm and 32 mm wide. Heat the bending iron until a flicked drop of water sizzles and dances (about 150–200 °C). Wet the rib and press it over the iron, backed by a strip of thin metal, a little at a time. Too hot scorches; too cool cracks. Glue to the blocks, then glue willow linings (2 × 7 mm) round the inside edges.
- Plates. Saw a spruce wedge in half through its thick edge and open it like a book (book-matching). Plane the thick edges until they meet with no light between, and glue them with hot glue. Same for the maple back.
- Outline. Trace the rib garland on the plate, add 2.5 mm overhang, saw out.
- Arch the outside with gouge, finger planes and scrapers to 15–16 mm: a smooth hill rising from a shallow channel near the edge, no flat top.
- Hollow the inside to the table's thicknesses, checking with calipers. Held to a bright window, a spruce top glows evenly where it is even; dark patches are thick. Held lightly one-fifth from an end and tapped, a good plate rings clearly. A finished top weighs about 60–70 g.
- F-holes: drill the round eyes, cut between them with a fine knife.
- Bass bar: scrape its face until it touches the arched top along its whole length, then glue it.
- Close the box: free the garland, glue back, then top. Inlaying a thin strip of wood (purfling) 3–4 mm in from the edge stops edge cracks running inward.
- Neck: carve neck, pegbox and scroll from a maple block 25 × 45 × 260 mm. Set it into a tapered mortise in the top block, tilted back so a straightedge on the fingerboard stands about 27 mm above the top at the bridge. Glue on the fingerboard.
- Varnish in thin coats of oil varnish or spirit varnish, each dried for days in sunlight (Pigments, Paints and Varnish). Leave the neck bare and oiled.
- Set up: pegs, a hardwood nut with four notches (16 mm between the outer two), tailpiece, end button, sound post and bridge.
The sound post and bridge
Sound post. Cut the dowel with its rings across the violin's grain. Cut both ends to the angle of the arch where it stands, so they sit flat, and to a length that stands by friction without forcing the top up. Lower it through the treble f-hole on an S-shaped steel hook (the setter), stand it up and tap it into place.
Bridge. Use hard, quarter-sawn maple cut to the table's sizes. Pare the feet until they touch the top all over (chalk on the top shows contact). Curve the top edge so each string can be bowed alone, highest under the G, about 1 mm lower under the E, with notches 11 mm apart. Tuning drags the bridge forward; keep it upright. String height at the end of the fingerboard: about 3.5 mm under the E, 5.5 mm under the G.
Viola and cello
The same instrument, scaled, by the same steps.
| Violin | Viola | Cello | |
|---|---|---|---|
| Body length | 356 mm | 380–430 mm | 750–760 mm |
| String length | 328 mm | 360–380 mm | 690 mm |
| Rib height | 30–32 mm | 35–40 mm | 115–125 mm |
| Tuning (low to high) | G D A E | C G D A | C G D A, an octave below the viola |
| Bow length / weight | 75 cm / 60 g | 74 cm / 70 g | 72 cm / 80 g |
A viola is a fifth lower than a violin but only a little bigger, so it sounds darker. A cello's top is 4–5 mm thick; it is played upright between the knees on an endpin pushed out from the tail block.
The bow
The simplest bow is a curved stick with hair tied at both ends, tightened by the player's thumb (Musical Instruments). The modern bow plays louder and more evenly:
- Stick: dense, springy, straight-grained hardwood — snakewood, ironwood, hard maple, even split bamboo (pernambuco is the classic). Plane it to 73 cm, tapering from 8.6 mm at the frog end to 5.3 mm at the head. Carve the head with a mortise for the hair.
- Camber: heat a few centimetres at a time over a clean lamp flame until too hot to hold comfortably, and bend so the middle dips 1.5–2 cm toward the hair. Hold till cool. Sighted from above, it must stay straight.
- Frog: a hardwood block 40 mm long sliding under the stick, with a threaded metal eyelet taking a screw that runs inside the stick to a button at the end (Screws, Nuts and Bolts).
- Hair: 150–200 hairs, 65 cm long, washed and combed. Tie one end, dip the knot in melted rosin and wedge it into the head with a tapered plug. Comb into a flat ribbon 10 mm wide and wedge the other end into the frog.
- Rosin: heat pine resin gently outdoors until the turpentine has steamed off and a cooled drop is hard and brittle. Pour into a paper mould. Rub new hair for several minutes before it will sound.
Slacken the hair after playing, or the stick loses its camber.
Lutes and guitars
The lute
- Carve a softwood mould the shape of the inside of the rounded back.
- Plane 9 to 13 ribs of maple, yew or plum about 1.5 mm thick, 3–5 cm wide in the middle and pointed at the ends; bend each to the mould on the bending iron.
- Glue them edge to edge over the mould from the centre outward (only to each other, not to the mould), with paper or cloth strips across every joint inside.
- Top: spruce 1.5–2 mm, with a carved rose instead of an open hole, and 5–7 thin bars across the grain.
- Strings run in pairs (courses), 6–8 courses, at a string length of 60–70 cm, tied to a light bridge glued to the top. Frets are loops of gut tied round the neck.
A simpler folk lute is carved from one block: hollow a log into a half-pear with walls 4–5 mm thick and glue a spruce top over it.
The guitar
| Part | Classical (gut-strung) guitar |
|---|---|
| String length | 650 mm |
| Body length | 480–490 mm |
| Lower bout / waist / upper bout | 360 / 240 / 280 mm |
| Side depth | 95–100 mm |
| Top | Spruce or cedar, 2–2.5 mm, with 5–7 thin "fan" struts under the lower half |
| Sound hole | 85 mm across |
| Tuning (low to high) | E A D G B E (82, 110, 147, 196, 247, 330 vibrations a second) |
Bend the sides as violin ribs, but 2 mm thick. Glue on the back (3–4 cross braces) and the braced top with linings. The bridge is a hardwood bar about 19 × 2.5 cm glued to the top, holding a hard saddle of bone. Make the string length to the saddle 2–3 mm longer than 650 mm under the bass strings and 1 mm under the trebles; this corrects the stretch of pressing a string down. A steel-string guitar pulls about twice as hard and needs X-shaped top bracing and a steel rod inside the neck.
Placing the frets
Distance from the nut = string length × (1 − 0.5^(fret number ÷ 12))
Or: divide the remaining length by 17.82 and measure that far to the next fret.
| Fret | 1 | 2 | 3 | 4 | 5 | 7 | 12 | 19 |
|---|---|---|---|---|---|---|---|---|
| mm from nut (650 mm scale) | 36.5 | 70.9 | 103.4 | 134.1 | 163.1 | 216.2 | 325.0 | 433.1 |
Saw each slot 0.6 mm wide and 2–3 mm deep and press in brass wire hammered to a mushroom section (Iron and Brass Wire). File all fret tops level with a long file, round and polish. The string sits 3–4 mm above the 12th fret.
The harp
A harp is a triangle: a soundbox, a neck across the top and a pillar joining them. Each string runs from the soundboard up to a tuning pin in the neck and plays one note. The strings try to fold the triangle shut; the pillar holds it open.
A lap harp of 22–26 strings, about 90 cm tall:
- Soundbox: a tapered box of 6 mm hardwood, 8 cm wide at the treble end and 25–30 cm at the bass.
- Soundboard: spruce 3–5 mm, grain running across the box so the line of string holes cannot split it, with a hardwood string rib 2–3 cm wide and 4–5 mm thick glued down the inside centre.
- Neck: curved hardwood 5–6 cm thick, glued from two or three layers with crossing grain. Drill tuning-pin holes at 13–14 mm centres.
- Pillar: hardwood about 5 × 5 cm, mortised strongly into neck and base (Doors, Windows and Joinery).
- Strings pass through the soundboard and rib and are knotted over small toggles inside. Start the top string at about 8 cm; lengthen each one, but keep the longest bass string to about 90 cm and make up the rest of the drop in pitch with thicker strings.
- Tuning pins: tapered steel pins 6 mm thick in tapered holes, turned with a T-shaped key. Hardwood pegs do for a small gut-strung harp.
The old Irish and Scottish harp (clàrsach) was strung with brass wire and played with the fingernails; it rings longer but needs a much stronger frame.
Strings
- Gut (Musical Instruments): rough sizes — violin E 0.6 mm (2–3 strands), A 0.7 mm, D 0.9 mm; guitar trebles 0.7–1.0 mm. Polish dry strings on fine abrasive and rub with oil to keep out damp.
- Silk: twist 16 to over 100 reeled filaments (Silk), boil in thin glue, dry under tension. Soft, quiet and very even; traditional on the Chinese qin.
- Steel: hard-drawn high-carbon music wire, the strongest wire there is (Iron and Brass Wire, Steel). Violin E 0.25–0.27 mm.
- Wound strings: a plain gut bass string would be thick and dull. Wrap fine copper, brass or silver wire tightly round a gut, silk or steel core, stretched between two hooks, one turned by a crank geared about 1 : 10. Feed the wire at a slight angle through a leather pad so every turn touches the last.
If a string breaks below its note, it is too thin for that length and pitch. If it sounds dull and floppy, it is too thick or too slack.
Pegs: friction pegs tapered 1 in 30 (Musical Instruments) — chalk stops slipping, soap stops sticking. A guitar's machine head is a small worm gear, about 14 : 1, that the string cannot turn backwards (Gears). Harps, harpsichords and pianos use steel wrest pins in hardwood, turned with a key.
How to tell it worked
- Finished plates ring clearly when tapped; a short thud means too thick, cracked or loose.
- Every string speaks quickly and evenly, low to high, with no buzz and no "wolf" (a howling, unstable note).
- The octave is true: the note at the 12th fret matches the harmonic made by lightly touching the open string at its midpoint.
- It holds tune through an evening, and after a month at full tension the top has not sunk, the neck has not pulled forward and no joint has opened.
Note Troubleshooting. Buzz → loose brace, open seam, high fret or something rattling inside; tap all over, re-glue with hot glue worked in on a thin knife. Weak, nasal tone → top too thick or sound post too tight. Harsh, edgy tone → bridge too heavy, or post too close to the bridge; move it back a millimetre. Out of tune up the neck → the 12th fret is not at the middle of the string; the 12th-fret-to-saddle distance should be slightly longer than nut-to-12th. Bow skates → not enough rosin or greasy hair; wash and re-rosin. Pegs creep back → taper does not match the hole; ream and refit.
Dangers
Danger Snapping strings and collapsing frames. A steel string breaking at tension whips back hard enough to cut an eye. Look away while tuning a new string up, and never tune above its note. A harp or guitar at full tension stores a great deal of energy; a weak neck or pillar can fail suddenly. Slacken strings before working on any instrument, and test a new design at half tension for a few days first.
- Gouges and knives slip on curved wood. Clamp the work and cut away from the holding hand.
- The bending iron burns deeply. Mount it so it cannot roll; keep water by it.
- Varnish and its solvents are flammable. Cook oil varnish outdoors with a lid ready to smother a flare-up.
- Dust of some tropical hardwoods irritates skin and lungs; cover nose and mouth.
- Raw gut and hide carry infection; see Musical Instruments.
What this unlocks
The bending iron, plate carving and hide-glue work lead straight to the harpsichord and piano in Horns, Pianos, Organs and Accordions, whose soundboards are big violin tops. Wound strings and music wire are the craft of Springs. A violin maker's calipers and scrapers start Scientific Instrument Making, and the study of vibrating plates led into Sound, Pitch and Acoustics, the The Telephone and Recording Sound.
How it was first done
Bowed instruments probably began in Central Asia and spread west through the Islamic world; the Arab rebab and Byzantine lyra were bowed by the 10th century AD. The violin family took shape in northern Italy in the early 16th century: Andrea Amati of Cremona made some of the earliest surviving violins in the 1560s, and Antonio Stradivari (1644–1737) and Giuseppe Guarneri "del Gesù" (1698–1744), also of Cremona, made the instruments players still prize most. François Tourte settled the modern bow in Paris around 1780–1790.
The lute descends from the Arab oud (al-'ūd, "the wood"), which reached Europe through Muslim Spain and Sicily by the 13th century. Wound bass strings appear in Bologna in the 1660s. Antonio de Torres Jurado fixed the size and fan bracing of the classical guitar in Spain in the 1850s–1860s. Harps are among the oldest instruments, shown in Mesopotamia and Egypt before 2500 BC; the triangular frame harp with a pillar appears in northern Europe by about the 9th century AD.