Part 2 · Earth and Fire
Glass Fibre and Glass Wool
Glass pulled thinner than a hair stops being brittle and becomes a flexible thread. Drawn onto a turning drum it gives continuous fibre that can be twisted and woven into fireproof cloth; blown or spun into a tangle it gives glass wool, which does not rot, burn or feed vermin — for insulating houses, boilers and cold stores, and for filtering acids and air. Molten furnace slag or basalt gives a coarser cousin, mineral wool.
- Difficulty
- ●●●●●
- Time
- An afternoon to draw first fibres from a rod; a week to set up a drum and a clay bushing; a day to make a batch of wool
- Steps from zero
- 7 prerequisites →
You need first
GlassThe full path from nothing — 7 steps before this one
- Fire
- Finding and Preparing Clay
- The Kiln
- Pottery
- Lime
- Lye and Potash
- Glass
- Glass Fibre and Glass Wool
Do them roughly in this order. See it on the tech tree →
Why it matters
A sheet of glass breaks if you bend it. A glass thread a few hundredths of a millimetre thick bends round your finger and springs back. In that thin form glass becomes a new material:
- Glass wool — a loose tangle of fibres — traps still air between millions of threads. It insulates as well as sheep's Wool or dry straw, but it does not burn, rot, go mouldy, or harbour insects and mice, and it stands heat up to about 450 °C. It lags steam pipes and Boilers and Pressure Vessels, fills walls and roofs (Insulation and Keeping Buildings Warm or Cool), insulates ice houses and cold stores (Ice and Refrigeration), and lines ovens and furnace doors.
- Mineral wool blown from molten iron-furnace slag or basalt stands even higher temperatures, and turns a waste heap into insulation.
- Filters: a plug of glass wool in a funnel strains liquids that would eat through cloth or paper — strong acids, lye, hot oils (Laboratory Glassware, Sulfuric Acid). Pads of it clean air.
- Glass cloth woven from continuous fibre is fireproof and does not conduct electricity: welding and forge curtains, gaskets and packing (Packing, Gaskets and Seals), electrical insulation for coils and motors that run hot (The Electric Motor, The Transformer).
- Glass-reinforced plastic: glass cloth soaked in a resin that hardens (Resins: Phenolic, Polyester and Epoxy, Composites: Fibreglass, Carbon Fibre and Honeycomb) makes a light, strong, rot-proof material for boat hulls, pipes, tanks and roofs.
How it works
Why thin glass is strong and flexible. Glass breaks from tiny cracks and scratches on its surface. A thick piece is full of them. A freshly drawn fibre has a pristine surface and is so thin that it has few flaws; such fibres are, weight for weight, stronger than steel wire. And because bending stretches the outside of a fibre by an amount proportional to its thickness, a thin fibre can bend sharply without its surface stretching enough to crack. A fibre 10–20 micrometres across (a fifth to a tenth of the thickness of a human hair) bends easily; one 0.2 mm across snaps.
How fibres are made. Hot glass is a thick, sticky liquid. Between about 900 and 1,250 °C soda-lime glass (Glass) is like warm honey or toffee: pull on it and it stretches into a thread instead of breaking or dripping. The thread cools and hardens in a fraction of a second as it leaves the heat. The faster you pull it, the thinner the fibre. Every method below is a way of pulling molten glass very fast.
Why wool insulates. Heat passes poorly through still air. Glass itself conducts heat quite well, but a fluffy mat of fibres is more than 95% air, held still in tiny pockets so that it cannot circulate. Packing it too tightly lets more heat through the glass; packing it too loosely lets the air move. A density of about 15–30 kg per cubic metre — a fist-sized handful that springs back when squeezed — is right for walls; denser mats (60–100 kg/m³) for hot pipes and ovens.
Which glass. Ordinary soda-lime glass makes perfectly good wool and filters. But its alkali slowly leaches out in damp, and over years the fibres weaken. For cloth that must last, use a glass with less soda or potash and more lime, a little clay (for alumina) and borax (see the recipe below). Factory glass fibre is made from a nearly alkali-free glass of this kind.
What you need
| Item | Amount | Notes |
|---|---|---|
| Glass | 1–5 kg per session | Cullet or fresh batch (Glass); clean, one kind only |
| Glass furnace and crucible | 1 | As in Glass, able to hold 1,200 °C |
| Spirit lamp and blowpipe, or blast lamp | 1 | For drawing from rods (Laboratory Glassware) |
| Wooden drum | 40–60 cm across, 15–20 cm wide | On an axle with a crank and a gear-up, or driven by a treadle or belt (Belts, Chains and Power Transmission) |
| Fireclay | 2–3 kg | For the bushing pot (Firebrick and Refractories) |
| Bellows | 1 | Strong, steady blast for blowing wool (Bellows) |
| A collecting chamber | A box or shed 1–2 m long | Lined with cloth or wire screens |
| Starch or thin oil | A cupful | "Size" for fibres to be woven |
| Gloves, long sleeves, eye protection, cloth mask | For everyone | See Dangers |
Where to find it
- Glass: make it from sand, lime and plant-ash alkali (Glass), or melt clean broken glass (cullet) of one kind — mixing different glasses makes fibres that crack.
- Borax for a better fibre glass: a white mineral crust in dry salt lakes and desert playas (Water Glass (Sodium Silicate), Soldering and Brazing).
- Clay for alumina: any clean white clay or kaolin (Finding and Preparing Clay); or crushed feldspar from granite.
- Slag: the glassy black or greenish waste tapped from iron and copper furnaces (Iron (the Bloomery), The Blast Furnace and Cast Iron, Copper Smelting). Big heaps lie near old ironworks.
- Basalt: dark, heavy, fine-grained volcanic rock, from lava flows and dark column-jointed cliffs (Rocks and Minerals).
A good batch for fibres that last (by weight, roughly): sand 55, limestone or crushed shells 25, white clay or feldspar 10, borax 8, potash or soda 5. It is much stiffer than window glass: factory fibre glass of this kind is melted at about 1,400–1,500 °C and drawn at about 1,200 °C, so it may not melt properly in a simple wood-fired furnace. Melt a small test batch first. If it stays stiff, add borax a little at a time (it lowers the melting point without making the glass weak in damp) until it flows. For wool alone, ordinary window or bottle glass is fine.
Method 1: Drawing fibre from a rod
This is the simplest way to see glass become thread, and gives enough fibre for experiments, filters and small woven pieces.
- Draw glass rods 3–5 mm thick from a gather in the furnace (Glass, Beads and rods), or use thin tubing (Laboratory Glassware).
- Mount a wooden drum 40–60 cm across on an axle, with a crank geared up so that one turn of your hand turns the drum three or four times. Its rim should be smooth and slightly rough-textured (wrap it in paper) so that fibre grips it.
- Heat the tip of a rod in a hot flame — a spirit lamp blown by a mouth blowpipe or a small bellows jet — turning it, until the tip is bright orange and soft, about 1,000 °C.
- Touch the soft tip to the drum rim and pull away a few centimetres: a fine thread follows. Stick the thread to the drum with a dab of wax.
- Turn the drum steadily and fast — the rim moving at 2–5 metres a second (a 50 cm drum turning 2–3 times a second). Hold the rod still, feeding it slowly into the flame as the tip is used up. A continuous fibre winds onto the drum.
- Move the rod slowly sideways as you go, so the fibre winds in an even band and does not pile up.
- When the drum is full, cut across the band and peel it off: a hank of parallel fibres as long as the drum's circumference.
Expect fibres of roughly 20–50 micrometres from a hand-cranked drum — about the fineness of a thin hair. Faster turning, a smaller hot zone and a thinner rod give finer fibres. If the fibre keeps breaking, the tip is too cool, or you are turning too fast for the heat.
Method 2: The clay bushing (many fibres at once)
This is the principle of every glass-fibre factory: molten glass flowing out through small holes and pulled down fast. Factories use heated plates of platinum alloy; you can use fireclay.
- Make the bushing: a fireclay pot (Firebrick and Refractories) about 8 cm across and 8 cm deep, with a flat bottom 1.5 cm thick. Before firing, push a smooth wire 2 mm thick through the base to make 5–10 holes in a line, 1 cm apart, and smooth each hole. Fire it hard.
- Set it in the furnace so that its base pokes out through a hole in the furnace floor or side, with the holes facing down into open air. Wrap the projecting part in a ring of clay that the flames reach, so the base stays as hot as the glass inside.
- Fill it with clean, broken cold glass or pre-melted fibre glass, and bring it up to bright orange-yellow, about 1,150–1,250 °C. A bead of glass appears at each hole and slowly grows.
- Start the fibres: with a cold iron rod, touch the beads and pull them down together; they draw out into threads. Carry the bundle down 1–2 m to the drum, passing it over a pad soaked with size — thin starch paste or a light oil — which coats the fibres so they do not scratch each other.
- Wind fast: the drum must take up the fibre continuously and evenly. A treadle or water- or engine-driven belt (Belts, Chains and Power Transmission) gives a steadier speed than a hand crank. The bundle of fibres is called a strand.
- Keep the glass topped up with small pieces of cold glass, a little at a time, so the level and temperature stay steady. A drop in heat breaks every fibre at once.
Clay bushings wear: the holes enlarge, and specks of clay break off into the glass and cut the fibres. Expect a bushing to work for a few hours to a few days. Glaze the inside of the pot with the same glass before use; it lasts longer.
Method 3: Glass wool and mineral wool
Blowing
- Build a collecting chamber: a long wooden box or a small shed, 1–2 m long, lined with coarse cloth or wire screens, open at the far end so the air can escape.
- Melt glass (or slag, or crushed basalt) in a crucible with a pouring lip. Glass needs about 1,200 °C; slag and basalt need more — 1,350–1,450 °C, white heat — so use your hottest furnace (The Blast Furnace and Cast Iron, Firebrick and Refractories).
- Fix a bellows nozzle or a steam pipe from a small boiler (Boilers and Pressure Vessels) pointing across the place where the stream will fall, just 2–3 cm from it.
- Start a hard, steady blast. Pour a stream as thin as a pencil lead through the jet. The blast tears it into fibres and carries them into the chamber, where they drift down and pile up like dirty snow.
- Shot — small glass beads that were not drawn out — falls just beyond the jet. Keep it out of the wool, which it makes heavy and gritty.
- Gather the wool when cool. Fluff it, pick out lumps, and store it in sacks.
Chopping and carding
Fibre from Methods 1 and 2 can be cut into 3–10 cm lengths and fluffed by hand or with Wool cards into a soft, even wool. This is cleaner and finer than blown wool.
Making it usable
- Batts and blankets: lay the wool 5–10 cm thick between two layers of coarse cloth or paper and quilt it with stitches every 20 cm (Quilting, Down and Warm Clothing); or sprinkle a little thin glue, starch or Water Glass (Sodium Silicate) solution through it and press lightly while it dries, which binds the fibres into a springy mat.
- Pipe lagging: wrap hot pipes with 3–5 cm of wool, bind with wire or cloth, and plaster the outside with a mix of clay or lime and chopped wool.
- Filters: push a loose plug of clean wool into the neck of a funnel. For acids, wash the wool in hot water first.
Method 4: Glass cloth
- Twist strands from Method 2 (each of several fibres) into a yarn on a spinning wheel (The Spinning Wheel) with a light twist — glass yarn does not need much. Keep it sized; dry glass fibres rubbing on each other wear through.
- Weave on an ordinary loom (The Loom) in a plain weave. Keep the warp evenly tensioned and the shed gentle: glass yarn does not stretch, and snaps if jerked.
- Clean the finished cloth by heating it on an iron plate to about 400 °C — hot enough to char a wood shaving quickly, but not glowing — for several hours, until the cloth is white all through: the starch or oil size burns away. Do not take it to red heat: near its softening point the fibres weaken and stick together. Even at 400 °C, heat-cleaned cloth loses half or more of its strength, so clean only cloth that does not need to bear load, and handle it gently afterwards.
How to tell it worked
- A single fibre can be wrapped round a pencil without breaking.
- A hank of fibres feels silky, not prickly, and is white or clear, not green with clay specks.
- A handful of wool springs back after squeezing. Held in a candle flame, it glows and shrinks but does not burn or smoke.
- Wrap a jar of hot water in 5 cm of glass wool and an identical jar in nothing: after an hour the wrapped one is still hot to the hand.
- Glass cloth held in a forge fire with tongs glows and slowly stiffens but does not burn.
Note Troubleshooting. Fibres keep breaking at the rod or bushing → glass too cold, or pulling too fast for the heat. Hotter glass, slower drum, then speed up. Fibres come out thick and few → glass too hot and runny (it drips instead of drawing), or holes too large. Lower the heat a little. Fibres green or speckled, snap in the middle → clay specks from the bushing, or unmelted batch. Use clean cullet; glaze the bushing. Blown wool all shot, no fibre → stream too thick or blast too weak. Thinner stream, harder blast, jet closer. Fibres turn powdery after months in damp → too much alkali in the glass. Use the fibre-glass recipe with more lime, clay and borax. Cloth wears through at folds → no size, or too sharp a bend. Keep it sized until in place; avoid creasing.
Dangers
Warning Glass fibres irritate skin, eyes and lungs. Broken fibres work into the skin and itch fiercely; in the eye they scratch; breathed in, very fine fibres lodge in the lungs. Always wear long sleeves, gloves, a close-woven cloth mask (damp is better) and eye protection when handling wool or cutting cloth. Work outdoors or in a draught. Wash your hands and face before eating, and wash work clothes separately. Do not try to make the finest wool possible by blowing: fibres thinner than about 3 micrometres hang in the air and reach deep into the lungs. Coarser fibres are safer and insulate almost as well.
- Molten glass and slag at 1,200–1,450 °C cause deep burns, and a drop of water or wet tool in molten slag explodes into spray. Keep everything dry, wear leather and wool (never plant fibres that flare), and keep the area clear of people (Glass, Iron (the Bloomery)).
- The drum can catch sleeves, hair and fingers. Tie back hair and keep sleeves tight.
- Bushing failure: a cracked pot dumps molten glass. Stand clear of the line under it; keep a bed of dry sand below.
What this unlocks
Glass wool makes efficient buildings, steam plant and cold stores possible without great quantities of wool, straw or cork (Insulation and Keeping Buildings Warm or Cool, Ice and Refrigeration, Boilers and Pressure Vessels). Glass cloth gives fireproof, rot-proof fabric and high-temperature insulation for motors and transformers. With a hardening resin it becomes glass-reinforced plastic for boats (Boats and Sails), tanks and pipes (Composites: Fibreglass, Carbon Fibre and Honeycomb, Resins: Phenolic, Polyester and Epoxy). Very pure, very even glass fibres, made from glass with a slightly different glass in the centre, carry light round corners: the optical fibres of modern communication (Fibre Optics, Networks and the Internet) — a long way off, but it begins with a thread drawn from a rod onto a drum.
How it was first done
Glassmakers in ancient Egypt and Phoenicia trailed threads of coloured glass around vessels more than 3,000 years ago, and Venetian glassmakers of the Renaissance drew fine glass threads for decoration. In the 18th century the French scientist René-Antoine Ferchault de Réaumur spun glass threads and suggested weaving them. Edward Libbey's glass company exhibited dresses woven from glass fibre and silk at the 1893 World's Columbian Exposition in Chicago. Slag wool was first made by blowing steam through molten iron slag in Wales around 1840, and made commercially in Germany and the United States from the 1870s; rock wool from basalt and limestone followed in the 1890s. Continuous glass fibre and glass wool for insulation were developed into large-scale industries in the 1930s in the United States by Games Slayter and colleagues at Owens-Illinois and Corning, who formed Owens-Corning Fiberglas in 1938. Glass-reinforced plastic boats and aircraft parts followed in the 1940s.
Source: content/entries/earth/glass-fibre.md