◆ Rebuild

Part 4 · Food and Farming

Vinegar and Pickling

Make vinegar by the barrel from wine, cider, beer, honey or fruit scraps — slowly by the Orléans method or in days in a quick generator packed with wood shavings — measure how strong it is, and use it to pickle vegetables and eggs and make chutneys and relishes that keep for a year, with the acid rules that keep pickles safe.

Difficulty
●●●●●
Time
Vinegar in 1–3 months (Orléans) or 3–10 days (quick generator); pickles ready in 1–4 weeks; chutney matures in 1–2 months
Steps from zero
5 prerequisites →

You need first

FermentationSalt

This unlocks

—
The full path from nothing — 5 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Pottery
  4. Salt
  5. Fermentation
  6. Vinegar and Pickling

Do them roughly in this order. See it on the tech tree →

Why it matters

Vinegar is the simplest acid you can make, and acid is one of the great preservers. Vegetables, eggs, fish and fruit soaked in vinegar strong enough keep for months — no smoke, no cold, and no special skill. Pickles carry vitamins and flavour through winter.

Vinegar is also the household acid: it cleans scale from kettles, neutralises spilled lye (Lye and Potash), sets dyes (Dyes and Mordants), curdles milk for glue and plastics (Glues and Adhesives, Early Plastics), and is the first acid of chemistry (Acids, Bases and Testing).

The basic way to turn wine into vinegar in a pot is in Fermentation. This chapter is about making it in quantity, knowing its strength, and using it safely.

How it works

Vinegar is made in two fermentations:

  1. Sugar → alcohol. Yeast, without air, turns the sugar in fruit juice, honey water or malted grain into alcohol (Fermentation, Beer, Wine and Cider).
  2. Alcohol → acetic acid. Vinegar bacteria (acetic acid bacteria), with air, turn the alcohol into acetic acid — the sour in vinegar. They live at the surface, where oxygen is, and build a slimy, rubbery skin there: the mother of vinegar.

Rule of thumb: each 1 % of alcohol becomes about 1 % of acid. So a liquid with 5–7 % alcohol — ordinary cider, wine diluted half-and-half, or strong beer — becomes vinegar of 5–7 %. To make 1 % alcohol, yeast needs about 17 g of sugar per litre; so for 6 % vinegar, start with about 100 g of sugar per litre. Fresh apple juice (10–12 % sugar) or grape juice (15–25 %, dilute it) is about right.

Air is everything. The bacteria need oxygen, and air reaches the liquid only at its surface. The two big methods differ only in how they give the bacteria air:

  • Orléans (surface) method: a large surface of liquid in a barrel open to the air. Slow (weeks), but simple, and gives the best flavour.
  • Quick (generator) method: the liquid trickles in a thin film over a tall column of wood shavings, with air rising through it. Enormous surface; vinegar in days.

Why acid preserves. Most dangerous bacteria, including Clostridium botulinum, which makes the botulism poison, cannot grow below about pH 4.6 — the acidity of a mild tomato (pH, Indicators and Buffers). Pickling means making food acid enough, all the way through, to stay below that line. Ordinary vinegar is about pH 2.5; vegetables are pH 5–6.5; when they soak together the vegetable releases water and the acid is diluted. That is why pickling rules are about ratios.

What you need

Item Notes
Alcoholic liquid Wine, cider, perry, beer, mead, palm wine, rice wine, or fermented fruit scraps (Beer, Wine and Cider)
Mother or live vinegar A piece of mother, or a jug of unheated vinegar from the last batch
Barrels or crocks Oak barrels (Barrels and Cooperage), lead-free glazed stoneware (Stoneware and Porcelain) or glass. Never metal.
For a quick generator A tall barrel or wooden tower; a sackful of curled beech or other hardwood shavings, corn cobs or grape stalks
Cloth Tightly woven, to keep out vinegar flies
Jars and crocks for pickles Glass jars (Glass) or stoneware crocks, with cork, wax or cloth seals (Canning and Bottling)
Salt Plain salt, without additives (Salt)
Spices Mustard seed, dill, coriander, peppercorns, chilli, garlic, bay, ginger, horseradish, cloves
Testing Chalk or eggshell, red cabbage indicator (Acids, Bases and Testing), a balance if you have one (Measurement from Scratch)

Where to find it

  • Sugar sources: windfall and cull fruit, apple and pear peelings and cores, grape pressings, overripe berries, honey (Beekeeping), sugar-cane and palm sap (Sugar), malted grain (Grain, Flour and Bread). Vinegar is the classic way to use fruit too damaged to store.
  • Mother of vinegar: if you have none, leave a bowl of unpasteurised wine, cider or fruit-scrap ferment covered with cloth in a warm place; wild bacteria (carried by tiny vinegar flies) arrive within 1–3 weeks and form a skin.
  • Vegetables for pickling: small firm cucumbers, small onions and shallots, red cabbage, beetroot, carrots, green beans, cauliflower, peppers, green tomatoes, green walnuts, samphire, nasturtium seeds (like capers).
  • Spice plants: mustard, dill, coriander, horseradish, garlic and wild garlic (Foraging Wild Food).

Method 1: Fruit-scrap vinegar (small, from waste)

  1. Fill a wide crock loosely with apple, pear or other fruit scraps.
  2. Dissolve 100 g of sugar or honey per litre of boiled, cooled water and pour it over to cover the fruit. Weigh the fruit down under the liquid.
  3. Cover with cloth. Stir daily for 1–2 weeks while it bubbles (alcohol stage).
  4. Strain out the fruit and return the liquid to the crock, add a splash of live vinegar, cover, and leave undisturbed in the warm (25–30 °C) for 3–8 weeks until sharply sour, as in Fermentation.

Method 2: The Orléans barrel (steady supply)

Funnel tubenew wine goes in below themother, never breaking it Air holes3–5 cm, screened air in Mother of vinegarfloating skin ofvinegar bacteria Vinegarbarrel two-thirds full,25–30 °C Tapdraw off 1/10–1/6 a week Air spacea big surface forthe bacteria fresh wine
Fig. 1 The Orléans barrel. Wine or cider is added through a funnel tube that reaches below the mother, so the floating skin is never broken; air enters through screened holes above the liquid; finished vinegar is drawn off from the tap below.

One barrel gives a steady trickle of fine vinegar for years.

  1. The barrel. Use a clean oak barrel of 100–250 litres that has held wine or vinegar (never oil, spirits treated with anything, or chemicals). Lay it on its side on a stand. Bore 2–3 holes, each 3–5 cm across, in each end, above the liquid line, and cover them with tightly woven cloth or fine mesh against flies. Fit a wooden tap near the bottom of one end.
  2. The funnel tube. Through the bung hole on top, fit a wooden or glass tube, open at both ends, reaching to just below the middle of the liquid — below the mother. You will pour new wine through this so it never sinks or tears the skin.
  3. Start it. Pour in about one-quarter strong live vinegar and three-quarters wine or cider, up to about two-thirds of the barrel's height. The vinegar sours the mix at once, so wild yeasts and moulds cannot start, and seeds it with bacteria. Lay a piece of mother on the surface if you have one.
  4. Keep it warm: 25–30 °C is ideal; a warm room, near (not beside) a stove or in a sunny shed. Below 15 °C it nearly stops; above 35 °C the bacteria suffer and alcohol evaporates.
  5. Wait. A grey-white skin forms in days, then thickens. The first vinegar is ready in 4–10 weeks, when it is sharp with no taste or warmth of alcohol left.
  6. Draw and feed. Each week draw off about one-tenth to one-sixth of the contents (10–20 litres from a 200-litre barrel) and replace it with the same amount of wine or cider through the funnel tube. Never draw off more than about a third at once.
  7. Clean up every few years: the mother thickens into a heavy leathery slab that sinks. Lift out the old layers, save a healthy piece, and carry on.

Method 3: The quick vinegar generator

Distributor trayholes with string wicks;pour feed in here Beech shavingssoaked in live vinegar;bacteria live on them 1.5–3 m air in Warm air outinside 28–35 °C: warmto the hand, never hot Pour back3–5 times, untilno alcohol is left False bottomgrid 30 cm up Vinegarcollects and is drawn off
Fig. 2 The quick vinegar generator. Alcoholic liquid drips from a perforated tray over a tall column of wood shavings coated with vinegar bacteria. Air enters through holes near the bottom and rises through the warm column. Vinegar collects below and is drawn off, then passed through again.

This turns weeks into days by giving the bacteria a huge surface of thin, airy film.

  1. The tower. A tall barrel or wooden vat 1.5–3 m high and 60–100 cm across, standing upright on blocks.
  2. False bottom. About 30 cm above the real bottom, fit a wooden grid or perforated board. The space below collects the finished vinegar; fit a tap at the lowest point.
  3. Air holes. Just above the collected liquid but below the false bottom, bore a ring of 6–8 holes, each 2–3 cm, sloping slightly downward from inside to outside so vinegar cannot run out. Screen them.
  4. The packing. Fill the column above the false bottom with curled shavings of beech (or another hardwood that gives no taste — maple, birch, alder), loosely, so air passes freely. Corn cobs, vine twigs, grape stalks or lumps of charcoal also work. Soak the packing in strong live vinegar for a day or two before use, so it is acid and coated with bacteria.
  5. Distributor. Near the top, fit a wooden tray with dozens of small holes, each with a twist of cotton or linen string hanging down as a wick, so the liquid drips evenly over the whole surface. Cover the top with a loose lid with a few vent holes.
  6. The feed. Mix the alcoholic liquid to about 6–8 % alcohol and add about one part live vinegar to three parts. A feed that is already acid stops other microbes.
  7. Run it. Pour the feed into the distributor tray a few litres at a time, several times a day. It takes hours to trickle down. The bacteria working on the shavings produce heat: inside the tower should be 28–35 °C. Air is drawn in through the bottom holes and out the top — like a chimney.
  8. Recirculate. Draw off the liquid from the bottom and pour it back in at the top, 3–5 times, until it tastes sharp with no alcohol left. Or run two or three towers in a row.
  9. Watch the heat. Put your hand flat on the outside of the tower: it should feel distinctly warm, like bathwater. Too hot (above about 38 °C — uncomfortably hot to the hand) → feed less often or partly close the air holes; the bacteria die and alcohol is lost as vapour. Too cool → feed more often, insulate the tower with straw, or warm the room.

A tower gives a batch of 5–8 % vinegar every 3–10 days. The cost: about 10–15 % of the alcohol is lost as vapour, and the flavour is plainer than slow vinegar.

Tip Stronger vinegar. Vinegar left outdoors in a hard frost partly freezes; the ice is mostly water. Pour off the unfrozen liquid — it is stronger. Distilling vinegar (Distillation) gives clear "distilled" vinegar and leaves the colour and solids behind.

Finishing and storing vinegar

  1. Settle and strain. Let new vinegar stand for a few weeks, then pour or siphon off the clear part, and strain through cloth or a layer of clean sand.
  2. Stop it. To keep it from forming new mother, or to kill vinegar eels (below), heat it to 65–70 °C — too hot to keep a finger in — for 30 minutes, in a glass or stoneware pot, never metal. Or fill bottles right to the top and seal them; without air, the bacteria stop.
  3. Store in glass or stoneware, corked or waxed (beeswax over cork works well). Kept full and cool, vinegar keeps for years and improves.

Vinegar eels are tiny harmless worms, 1–2 mm long, that wriggle in old unheated vinegar; strain them out or heat them dead.

Testing strength

You need to know your vinegar is strong enough to pickle safely: at least 5 % acid.

  1. Taste and fizz (rough): sharp enough to make you wince; crushed chalk fizzes hard for a long time.
  2. The chalk weighing test (needs a balance — Measurement from Scratch):
    1. Measure exactly 1 litre of vinegar into a crock.
    2. Weigh out 100 g of finely crushed chalk, limestone or baked eggshell — all nearly pure calcium carbonate.
    3. Stir it in a little at a time. It fizzes. Stir now and then for a day, until no more bubbles appear.
    4. Pour the liquid off carefully, rinse the leftover powder with a little water, dry it completely in the sun or near a fire, and weigh it.
    5. Chalk used (g) × 1.2 = grams of acid per litre. Divide by 10 for the percentage. Example: 58 g remaining → 42 g used → 42 × 1.2 = 50 g per litre = 5 %.
  3. Titration — the accurate way, using a known-strength soda solution and cabbage indicator: see Acids, Bases and Testing. Each millilitre of the standard soda solution neutralises 60 mg of acetic acid.
  4. Compare with a known vinegar. Keep a bottle of a measured batch as a reference. Put a spoonful of it and a spoonful of the new vinegar into two cups with a few drops of cabbage indicator, and add weak ash-lye drop by drop to each until it turns from red to blue-green. If the new one needs as many drops or more, it is as strong or stronger.

Pickling

The safety rules

  1. Use vinegar of at least 5 % acid, tested as above. If you cannot test, use the strongest you have undiluted.
  2. Never dilute vinegar with more than an equal amount of water. One part vinegar to one part water is the weakest pickling liquid. Stronger (more vinegar) is always safer.
  3. Cover completely. Pack vegetables into the jar, then pour in liquid to cover them by at least 1–2 cm. The jar should hold roughly as much liquid as vegetable — don't jam it so tight that only a little liquid fits.
  4. Fresh, sound produce only, washed well. Trim off the flower end of cucumbers (it holds enzymes that soften them).
  5. Check it. After 2–3 days, dip some liquid from the middle of the jar into cabbage indicator (Acids, Bases and Testing). It must turn clearly red or pink, meaning pH below about 4. Purple means not acid enough — the batch is not safe to keep; eat it within days, kept cold, or drain and re-cover with stronger vinegar.
  6. Never pickle in metal (iron, copper, brass, zinc, tin or aluminium pots or lids). Vinegar dissolves metals — copper and brass into poisonous green salts. Old recipes that boiled pickles in copper pans "to green them" were poisoning people. Use glass, lead-free stoneware, enamel or wood, and wooden spoons. Never use lead-glazed pots (Glazes).
  7. For storing at room temperature more than a few weeks, seal jars and heat them in a boiling-water bath (Canning and Bottling) — 10–15 minutes for jars up to 1 litre. Otherwise keep pickles in a cool cellar, below about 10 °C.

Warning Garlic, herbs or peppers kept in oil are not pickles. Oil keeps air out and lets botulism grow in low-acid foods at room temperature. Pickle them in vinegar first, or keep oil infusions cold and use within a week.

Recipe 1: Quick vinegar pickles (cucumbers, beans, carrots, onions, beetroot)

Pickling liquid (for about 4 litres of jars): 1 litre of vinegar (5 %+), up to 1 litre of water, 40–60 g of salt, 0–200 g of sugar or honey to taste.

Spices per 1-litre jar: 1 teaspoon of mustard seed, a head or two of dill or 1 teaspoon of dill seed, 2 cloves of garlic, 6 peppercorns, a bay leaf, a small dried chilli; for crispness, 1–2 fresh vine, oak or horseradish leaves.

  1. Prepare the vegetables. Small cucumbers whole or halved; carrots in sticks; green beans topped, blanched 2 minutes in boiling water; beetroot boiled until tender, peeled and sliced; cauliflower in florets.
  2. Salt firm, watery vegetables first for crisp pickles: onions, cucumbers, cauliflower and cabbage are layered with salt (about 2 tablespoons per kg) or soaked overnight in brine of 100 g of salt per litre, then rinsed and drained. This draws out water that would otherwise dilute the vinegar.
  3. Scald jars and lids with boiling water.
  4. Put the spices in the jars, pack the vegetables in snugly, upright where possible.
  5. Bring the liquid to the boil and pour it over, hot, to cover by 1–2 cm. Press out air bubbles with a wooden stick.
  6. Seal. For long storage at room temperature, process in a water bath (Canning and Bottling); otherwise store cool.
  7. Wait 1–3 weeks before eating, for the acid and flavours to soak in.

Pickled onions (the classic): peel small onions, soak 24 hours in strong brine (100 g salt per litre), rinse and drain, pack into jars and cover with undiluted spiced vinegar, cold. Ready in 4 weeks; crisp for 6 months.

Pickled red cabbage: shred, layer with salt, leave 24 hours, rinse and drain, pack loosely, cover with undiluted spiced vinegar. Ready in a week; eat within 2–3 months before it softens.

Recipe 2: Pickled eggs

  1. Hard-boil 12 fresh eggs for 10–12 minutes. (Very fresh eggs are hard to peel; use eggs 1–2 weeks old — see Poultry and Eggs.) Cool in cold water, peel, and rinse.
  2. Liquid: 500 ml vinegar, 250 ml water, 1 tablespoon salt, a few slices of onion, mustard seed, peppercorns; add a little beetroot juice for pink eggs. Boil it for 5 minutes.
  3. Pack the eggs loosely into a scalded jar, pour over the hot liquid to cover by 2 cm, and seal.
  4. Keep them cold — below 5 °C if at all possible (an ice house, spring house or winter cellar; see Ice and Refrigeration). Ready after 1–2 weeks; eat within 3 months.

Danger Pickled eggs kept warm have killed people. Acid soaks into a whole egg slowly, and the yolk can stay low-acid for days. A case of botulism was traced to home-pickled eggs left on a kitchen counter. Make small batches, keep them cold, never store them at room temperature, and do not try to "can" them in a water bath.

Recipe 3: Chutney

Chutney is fruit or vegetables cooked slowly with vinegar, sugar and spice until thick. It uses up gluts and damaged fruit and keeps a year or more.

Basic recipe: 1.5 kg of fruit or vegetables (apples, plums, green tomatoes, marrow, rhubarb, pears, mangoes, or a mixture), chopped; 500 g onions, chopped; 250 g raisins or dried fruit (optional); 400–500 g brown sugar; 600 ml vinegar; 1–2 tablespoons salt; spices: a thumb of ginger, 1 tablespoon mustard seed, 1–2 chillies, a few cloves.

  1. Put everything except the sugar in a wide, heavy earthenware or enamelled pot — not bare iron, copper or aluminium.
  2. Simmer gently, uncovered, stirring often, for about 1 hour until soft.
  3. Add the sugar and stir until dissolved. Simmer 1–2 hours more, stirring more and more often as it thickens, so it does not catch and burn.
  4. It is done when a spoon drawn across the bottom of the pot leaves a clear channel that fills only slowly, and there is no pool of thin liquid on top.
  5. Ladle hot into hot, scalded jars, almost to the top. Seal at once with waxed paper discs and a cork, or a cloth tied over and painted with melted wax. No bare metal lids — vinegar eats through them.
  6. Leave 1–2 months to mellow. Unopened, it keeps 1–2 years in a cool, dark place.

A relish uses the same ingredients chopped finer and cooked only 20–30 minutes; keep it cool and use within a few months, or process in a water bath. Ketchup is a relish sieved smooth.

How to tell it worked

  • Vinegar smells and tastes sharp, clean and fruity or malty, with no warmth of alcohol and no rotten or nail-polish smell, and tests at 5 % or more.
  • Pickles are firm and crisp, evenly coloured all the way through, and the liquid stays clear (some cloudiness from spices is fine). The liquid turns cabbage indicator red.
  • Chutney is thick, glossy, dark, and smells richly sweet-sour; no mould on the surface after months.

Note Troubleshooting. Vinegar stays sweet or winey → too cold, too little air, or alcohol too strong (over 10 %). Warm it, use a wider vessel, dilute strong wine with water, add live vinegar. Vinegar goes flat and weak after being sharp → left too long with air after the alcohol ran out; the bacteria began eating the acid. Draw it off and seal it full once it is sharp. Fuzzy coloured mould on vinegar → acidity too low at the start. Throw it out; next time start with a quarter live vinegar. Soft, slimy pickles → vinegar too weak, vegetables not covered, cucumber flower ends left on, or produce not fresh. Discard slimy pickles. Hollow or shrivelled pickles → cucumbers picked too long before pickling, or vinegar or salt far too strong at first. Chutney weeps liquid or ferments → not cooked down enough, or too little sugar and vinegar. Recook it and rejar. Pickles darken or taste metallic → metal pot, lid or spoon. Throw them out if a metal was green or corroded.

Dangers

Danger Botulism. Under-acid pickles, pickled eggs kept warm, and low-acid food under oil can grow Clostridium botulinum, whose poison causes drooping eyelids, double vision, slurred speech, difficulty swallowing and breathing, and death — often with no bad smell or taste in the food. Follow the acid ratios, test with indicator, keep anything doubtful cold, and never taste food from a bulging, leaking or spurting jar — boil it for 10 minutes, then bury it. See Canning and Bottling and Emergencies.

  • Metal poisoning. Vinegar dissolves copper, brass, zinc, lead and iron. Never make, store or cook it in metal or lead-glazed pots.
  • Hot vinegar spatters and its steam stings the eyes and throat; keep your face back when boiling it, and work with a window open.
  • Strong vinegar in the eyes stings badly; rinse with plenty of clean water at once. Concentrated (freeze- or distil-strengthened) vinegar can burn skin — handle it like other acids (Acids, Bases and Testing).
  • Fruit flies carry vinegar bacteria to your wine and beer. Keep vinegar making well apart from brewing, with separate pots and spoons (Fermentation).

What this unlocks

Vinegar and pickles extend the harvest through winter alongside salting, drying and cold storage (Preserving Food, Canning and Bottling). As the household acid, vinegar feeds into cleaning, dyeing (Dyes and Mordants), casein glue and plastics (Glues and Adhesives, Early Plastics), and simple chemistry (Acids, Bases and Testing); its salts — lead, copper and calcium acetates — were among the earliest chemicals made deliberately. Distilled and concentrated, acetic acid becomes a solvent and raw material for Ether, Acetone and Solvents and later industrial chemistry.

How it was first done

Vinegar is as old as wine and beer, since any open jar of either sours. Babylonian texts from about 5,000 years ago mention vinegar made from date wine, and Roman soldiers drank posca, vinegar mixed with water. The vinegar makers of Orléans in France — where wine spoiled on the river journey from the vineyards was turned to vinegar — formed a guild in 1394 and gave their name to the slow barrel method.

The quick method was devised in Germany by Karl Sebastian Schützenbach in 1823. In the 1860s Louis Pasteur showed that vinegar is made by a living organism in the mother, not by the air alone, and explained how to make it reliably and how to stop it spoiling.

Pickling in brine and vinegar is thousands of years old, and Roman cooks preserved everything from turnips to fish in vinegar. The word chutney comes from the Hindi chatni; British traders brought the idea home in the 17th century.

Source: content/entries/food/vinegar-and-pickling.md