◆ Rebuild

Part 1 · Staying Alive

Fire

How to make fire from nothing but wood, stone and patience — and how to keep it alive. Almost every other chapter in this book begins here.

Difficulty
●●●●●
Time
10 minutes to a few hours for your first success
Steps from zero
0 prerequisites →

You need first

Nothing — start here.

This unlocks

Lye and PotashCharcoalThe KilnPotterySaltPreserving FoodGrain, Flour and BreadSugarHorn and Bone WorkingLamps and CandlesSteam-Bending WoodSurviving Cold and HeatCooking Without PotsFinding and Purifying WaterBalloons

Why it matters

Fire is the first technology. It cooks food (which kills parasites and makes far more calories digestible), boils water clean, keeps you warm enough to survive the night, keeps predators back, dries wet clothes, gives light after dark, and hardens wooden tools. Later in this book, fire becomes the engine of everything else: it turns Finding and Preparing Clay into Pottery, wood into Charcoal, limestone into Lime, sand into Glass, and rock into metal.

If you learn one skill before anything else, make it this one. And once you have fire, never let it go out without a way to make it again.

What fire actually is

Fire is a fast chemical reaction between a fuel and oxygen from the air. It needs three things at once, and removing any one of them puts it out:

HEAT spark · friction · sunlight OXYGEN air — don't pack it too tight FUEL grass · wood · fat · charcoal
Fig. 1 The fire triangle. Take away any side — cool it with water, smother it with dirt, or let it run out of wood — and the fire dies.
  • Fuel — anything that burns: dry plant material, wood, fat, oil, charcoal.
  • Heat — enough to bring the fuel to its ignition temperature (for wood, roughly 250–300 °C).
  • Oxygen — from the air. A fire that is packed too tightly suffocates; a fire that gets plenty of air burns hotter.

Every method of starting a fire is just a way to concentrate enough heat in a tiny amount of fine fuel to make a glowing ember. You then grow that ember, step by step, into a flame and then a fire.

What you need

For every method you need the same three grades of fuel, gathered before you start making the ember. An ember lasts only a minute or two; you will not have time to go looking.

Grade Size Examples Amount
Tinder Fine as hair Dry grass, shredded inner bark (cedar, juniper, cottonwood), cattail fluff, thistle down, birch bark curls, old bird nests, dry pine needles Two double-handfuls
Kindling Matchstick → pencil → thumb Dead twigs that snap cleanly, split dry sticks An armful, sorted by size
Fuel wood Wrist → forearm Dead, dry branches and split logs (Firewood and Coppicing) Enough for the night, then double it
TINDERhair-fine, holds the ember KINDLINGmatchstick → pencil LARGE KINDLINGthumb-thick FUEL WOODwrist-thick and up ember goes in the hollow
Fig. 2 Building up from tinder to fuel. Each size catches from the size before it. Most failed fires skip a step.

Tip The snap test. Dry kindling breaks with a sharp crack. If a twig bends instead of snapping, it is too wet or still alive — leave it.

Where to find it

  • Dry wood in wet weather. Look for dead branches still attached to standing trees, especially the low dead twigs under evergreen trees — they stay off the wet ground. Standing dead trees are drier than fallen ones. Split a wet log open: the heart is often dry.
  • Fatwood. Old pine stumps and the bases of dead pine branches become saturated with resin. The wood is heavy, amber-coloured, sticky, and smells strongly of turpentine. Shavings of fatwood light even when wet and burn like a candle. Prize it.
  • Birch bark. The white papery outer bark of birch trees is full of oil and burns even when damp. Peel only loose strips from dead or fallen trees; stripping a living tree's bark all the way around kills it.
  • Tinder fungus. Hoof-shaped bracket fungi (the tinder fungus, Fomes fomentarius, on birch and beech) and the black, cracked chaga on birch both hold a spark and smoulder for a long time. The soft brown layer just under the fungus's hard crust is the part that catches.
  • Flint and other hard stones for spark methods: see Stone Tools and Finding and Identifying Ores. Pyrite ("fool's gold") — brassy, heavy, cubic crystals — throws sparks when struck hard with flint.

Method 1: The bow drill

The bow drill is the most reliable friction method for beginners because the bow does most of the work your hands would otherwise do. It takes practice. Expect to fail several times before your first ember; after that it becomes routine.

TOP VIEW OF THE FIREBOARD socket V-notch ember pan Bearing blockhard wood or stone, greased Spindle20 cm long, thumb-thick Cordone turn round the spindle Footpins the board still Bowarm-length, stiff long, full strokes Fireboardsoft, dry, non-resinous wood Ember panleaf or bark
Fig. 3 The bow drill. The cord wraps once around the spindle; sawing the bow back and forth spins it fast against the fireboard. The fine hot dust that collects in the notch becomes the ember.

The parts

  1. Fireboard — a flat board about 2 cm thick, 5–8 cm wide and 30 cm long, of soft, dry, non-resinous wood. Good woods: willow, poplar, cottonwood, aspen, basswood (linden), cedar, juniper, buckeye, sycamore, yucca and sotol stalks. Test with a thumbnail: you should be able to dent it, but not easily.
  2. Spindle — a straight, dry stick about 20 cm long and as thick as your thumb (about 2 cm). Use the same wood as the fireboard, or slightly harder. Round the bottom end bluntly; sharpen the top end to a point so it has less friction in the bearing.
  3. Bearing block — a hand-sized piece of hard wood, bone, or a stone with a small hollow in it. It holds the top of the spindle. Grease the hollow with animal fat, a waxy leaf, or the oil from rubbing it on your nose and hair, so the friction happens at the bottom of the spindle, not the top.
  4. Bow — a stiff, slightly curved stick about as long as your arm, from armpit to fingertip.
  5. Cord — a bootlace, a strip of leather, or Cordage and Rope you twist from plant fibre. Tie it to both ends of the bow, leaving it just slack enough to wrap once around the spindle under tension.
  6. Ember pan — a dry leaf, a chip of bark, or a thin wood shaving placed under the notch to catch the ember.

Step by step

  1. Prepare the tinder nest first. Roll your finest tinder into a loose bird's-nest shape the size of two fists, with a small hollow in the middle. Keep it dry and within reach.
  2. Burn in a socket. Near one edge of the fireboard, carve a small starting dimple with a sharp stone. Wrap the spindle in the cord, put its blunt end in the dimple, and drill gently until the dimple has blackened into a round socket as wide as the spindle.
  3. Cut the notch. Cut a V-shaped notch from the edge of the board into the centre of the socket — about one eighth of the circle, like a slice of pie. This is where the hot dust collects and where air reaches it. No notch, no ember.
  4. Get into position. Kneel on your right knee (if right-handed) and put your left foot firmly on the fireboard, close to the socket. Hold the bearing block in your left hand and brace your left wrist hard against your left shin. This locks the spindle upright and steady — a wobbling spindle is the most common cause of failure.
  5. Start slow. Use the full length of the bow in long, smooth strokes. Press down lightly at first. When smoke starts, gradually press harder and bow faster.
  6. Push through. Keep going 10–20 seconds after there is plenty of smoke. The notch should fill with a dark brown to black powder.
  7. Check for the ember. Stop, carefully lift the spindle, and watch the powder in the notch. If it keeps smoking on its own for several seconds, you have an ember. Do not rush. Fan it very gently with your hand to let it grow.
  8. Move the ember. Tap the board to free the ember, lift the board away, and carry the ember on its pan to the tinder nest. Tip it into the hollow.
  9. Blow it to life. Fold the nest loosely around the ember and blow long, gentle, steady breaths through it. The smoke will thicken and turn yellow-white; then the nest bursts into flame. Put it straight into your prepared fire lay (below).

Note Troubleshooting the bow drill. Shiny, glazed socket and almost no dust → too little pressure or the wood is too hard; sprinkle a pinch of sand in the socket or choose softer wood. Lots of light-brown coarse dust but no ember → not enough speed; bow faster with longer strokes. Spindle keeps jumping out → your wrist isn't locked against your shin, or the socket is too shallow. Cord slips → tighten the cord or rough up the spindle's surface. Smoke but the dust won't hold together → the wood is damp. Dry it by a fire or in the sun for a day.

Method 2: Flint and steel (or flint and pyrite)

Strike the sharp edge of a piece of flint, chert, quartzite or jasper with a piece of high-carbon steel (see Steel) or with pyrite. Tiny shavings of metal are torn off and burn as sparks. Sparks are not hot enough to light grass directly; they must land on a material that catches sparks:

  • Char cloth — squares of cotton or linen cloth "cooked" without air: put them in a closed tin or clay pot with a tiny hole, set it in the fire until smoke stops coming out of the hole, and let it cool before opening. The black cloth catches a spark instantly. The same works with punk wood, cattail fluff, or tinder fungus — this "charring" process is the same as making Charcoal.
  • Tinder fungus (amadou) — boiled in water with wood ash (see Lye and Potash), pounded flat and dried, it catches sparks almost as well as char cloth.

Hold the char cloth on top of the flint, under your thumb, close to the sharp edge. Strike down glancingly with the steel. When a spark lands, it makes a glowing red spot that spreads. Fold it into the tinder nest and blow, as with the bow drill.

Pyrite with flint works — a 5,300-year-old man found frozen in the Alps carried exactly this kit with tinder fungus — but its sparks are weaker and fewer than steel's.

Method 3: Focused sunlight

On a bright day a magnifying lens (see Lenses), a clear piece of ice shaped into a lens, or even a round clear bottle filled with water can focus sunlight onto a dark spot of char cloth, punk wood or dark tinder. Move the lens until the bright spot is as small as possible; it will smoke within seconds. This method needs no strength at all, but it needs sun.

Method 4: Hand drill and fire plough

Without a cord, you can spin a long straight stalk (60–80 cm, of mullein, cattail, yucca, horseweed or elderberry) between your flat palms on a fireboard. Rub your hands down the stalk as it spins, then quickly return to the top and repeat. It is harder than the bow drill, and blisters are common, but it needs nothing but two plants.

The fire plough is a hard stick rubbed fast back and forth along a groove in a soft board until the dust at the end of the groove ignites. It is common in tropical islands, where the dry, soft woods (such as hibiscus) suit it.

Building and keeping a fire

wind TEEPEEhot, fast, easy to light LOG CABINsteady bed of coals for cooking LEAN-TObig log shields it from the wind
Fig. 4 Three useful ways to lay a fire. The teepee lights easily and burns hot; the log cabin gives a steady bed of coals for cooking; the lean-to shelters a small fire from the wind.
  1. Choose the place. Clear a circle 3 metres wide down to bare earth. Stay away from overhanging branches, dry grass and roots (roots can smoulder underground for days and start a fire far away). Do not build on wet river stones — trapped water can turn to steam and crack them explosively.
  2. Build the lay before you light. For a teepee: put the tinder nest in the middle, lean the smallest kindling around it in a cone, then larger kindling around that, leaving a "door" on the windward side to slip the burning tinder in.
  3. Feed it gradually. Add the next size of wood only once the current size is burning well. Too much too fast smothers it.
  4. Bank it for the night. Before sleeping, push the glowing coals together and cover them with a layer of ash and then a few large logs laid tight. In the morning, scrape away the ash, add tinder and blow — the coals are often still alive.
  5. Carry it. People have carried fire between camps for hundreds of thousands of years. Pack a smouldering lump of tinder fungus, punk wood or dry dung, with a glowing coal in the middle, inside a clay pot, a hollow horn, or a bundle of green leaves bound with bark. It will smoulder for hours.

Dangers

Danger Smoke in enclosed spaces kills. Burning in a closed shelter or cave without airflow produces carbon monoxide, which has no smell and causes headache, dizziness, confusion and then death in sleep. Always leave a vent for smoke to escape and a gap at ground level for fresh air.

  • Wildfire. A single escaped ember in dry grass can burn an entire valley — and your food, shelter and stores with it. Keep water or loose dirt ready, never leave a fire unattended in dry, windy weather, and drown and stir the ashes until they are cold to the touch before leaving.
  • Toxic smoke. Never burn poison ivy, poison oak or oleander; their smoke damages the lungs and eyes. Avoid burning painted or treated wood and plastics from old ruins.
  • Burns. Cool any burn in cool running water for 20 minutes. Do not put fat, butter or ash on it. See Wound Care and Antiseptics.
  • Exploding stones. Wet, porous rocks (especially from riverbeds) can burst in a fire.

What fire unlocks

With fire you can cook, boil Finding and Purifying Water safely, and survive cold nights. Once you can keep a fire hot — by feeding it air with a Bellows and enclosing it in a The Kiln — you can make Pottery, Charcoal, Lime, Glass and metals. Nearly every path through this book starts here.

How it was first done

Our ancestors were using fire at least one million years ago; burned bones and plant ash have been found in Wonderwerk Cave in South Africa. For most of that time, people probably collected fire from lightning strikes and kept it alive rather than making it. Deliberate fire-making by friction and by striking stones was certainly known tens of thousands of years ago. The friction match, which made fire effortless, was invented only in 1826 — less than two hundred years ago. Until then, everyone who used fire had to keep it, carry it or make it by hand, as this chapter describes.

Source: content/entries/survival/fire.md