◆ Rebuild

Part 8 · Chemistry

Citric and Tartaric Acid

The two clean, safe, food-grade acids of the kitchen and the workshop. Cream of tartar is scraped from wine casks, tartaric acid is made from it, and citric acid comes from lemons or from a black mould grown on sugar. Together they give baking powder, sour drinks and jams that set, brighter dyes, blueprint paper and a gentle cleaner for scale and rust.

Difficulty
●●●●●
Time
A day to purify cream of tartar; three to four days for tartaric or citric acid from it or from lemons; two weeks for a mould fermentation
Steps from zero
11 prerequisites →

You need first

FermentationSulfuric Acid

This unlocks

—

Objects made here

baking powder
The full path from nothing — 11 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Sulfur
  4. Pottery
  5. The Kiln
  6. Lime
  7. Fermentation
  8. Lye and Potash
  9. Glass
  10. Saltpeter
  11. Sulfuric Acid
  12. Citric and Tartaric Acid

Do them roughly in this order. See it on the tech tree →

Why it matters

Most acids in this book burn skin and eat metal (Sulfuric Acid, Hydrochloric Acid, Nitric Acid). Citric and tartaric acid are the sour taste of lemons and grapes. You can eat them and keep them in a paper bag on a shelf, yet they do real chemical work:

How it works

Grapes store tartaric acid; lemons and limes store citric acid. Both are weak acids: a 5% solution is about as sour as lemon juice (pH about 2) and does not burn skin. Both are separated from their sources by the same three-step trick, the calcium salt route:

  1. Neutralise with chalk. The acid fizzes with chalk (calcium carbonate). Its calcium salt, calcium citrate or calcium tartrate, hardly dissolves and falls as a white powder. Sugar, colour and gums stay in the liquid and are poured away.
  2. Release with sulfuric acid. Sulfuric acid takes the calcium away as gypsum (calcium sulfate), which also hardly dissolves. The fruit acid is left free in the liquid.
  3. Crystallise. Filter off the gypsum, boil the liquid down gently, and let crystals grow as it cools.
1 Neutralise 2 Release 3 Filter 4 Crystallise chalk CO₂ fizzes calcium salt diluted sulfuric acid gypsum on cloth crystals gentle steam juice or dissolved tartar, boiling; pour away liquid with sugar and colour stir washed salt into water, add acid, keep warm an hour; gypsum forms gypsum stays behind; clear fruit acid runs through simmer to a thin syrup, then cool slowly for days The same route works for lemon juice (citric acid) and for cream of tartar (tartaric acid).
Fig. 1 The calcium salt route. Lemon juice or dissolved cream of tartar is neutralised with chalk; the calcium salt settles out and is washed. Sulfuric acid takes the calcium away as gypsum, leaving the pure fruit acid in solution to be boiled down and crystallised.

Cream of tartar is tartaric acid half-neutralised by potassium. Grape juice is rich in both, and as alcohol builds up during fermentation and the wine cools, cream of tartar comes out of solution as the crust on cask walls. It dissolves about 0.6 g in 100 mL of cold water but about 6 g in 100 mL of boiling water. That tenfold difference is how you purify it.

What you need

Item Amount (for one batch) Notes
Wine tartar (argol) or dried lees 500 g From casks and vats (Beer, Wine and Cider)
Lemons or limes 25–30 fruit, giving about 1 litre of juice Or any very sour citrus
Chalk, finely powdered 150 g Or crushed seashells or limestone (Lime)
Sulfuric acid, strong About 100 g (55 mL) Diluted before use (Sulfuric Acid)
Calcium chloride 30 g Chalk dissolved in Hydrochloric Acid and dried, or use more chalk and accept a lower yield
Charcoal, powdered 20 g To take out colour; bone charcoal or Activated Charcoal is best
Glazed pots or enamelled pans, 5–10 L 3 No bare iron, copper or zinc: the acids dissolve them and turn dark
Cloth filters, wooden paddle, shallow glazed dishes Fine linen or cotton, doubled
Fuel For boiling 15–20 litres of water

Where to find it

  • Wine tartar is the hard, gritty crust inside casks and vats where wine has stood: pinkish from red wine, greyish from white. It is about half to four-fifths cream of tartar. Dried lees, the sludge at the bottom of a cask, hold a tenth to a fifth. Expect a few kilograms a year from a winery making 1,000 litres of wine.
  • Tamarind pods, from a tropical tree with feathery leaves, hold a sticky brown pulp that is about a tenth tartaric acid. Soak it in hot water, strain, and treat the liquid like lemon juice below.
  • Citrus fruit: lemon juice is about 5–6% citric acid, so one litre gives about 50 g. Limes are similar. Unripe, green fruit is the sourest. Oranges hold only about 1%.
  • Black mould (Aspergillus niger) is the sooty black powder on the outer skins of stored onions and on rotting fruit. Under a hand lens it is white threads with black pin-heads.
  • Chalk: soft white limestone, or crushed seashells or eggshells (Rocks and Minerals).

Method 1: Cream of tartar from wine tartar

  1. Crush 500 g of crude tartar to a coarse powder.
  2. Dissolve hot. Bring 8 litres of clean water to the boil in a glazed or enamelled pot. Stir in the tartar a handful at a time and keep it boiling for 15 minutes. Much of the colour and grit will not dissolve; that is expected.
  3. Clear the colour. Stir in 20 g of powdered charcoal and, for a very cloudy liquid, a handful of fine white clay stirred to a cream. Boil 10 minutes more.
  4. Filter hot, through a doubled cloth over a second pot kept on embers. If the liquid cools on the cloth, crystals block it.
  5. Cool slowly. Cover the pot with a board and leave it overnight. White crystals of cream of tartar grow on the bottom and sides.
  6. Collect. Pour off the liquid (keep it to dissolve the next batch). Scrape out the crystals, rinse them once with a cup of cold water, and dry them in the sun or a warm room.
  7. Repeat steps 2–6 once with the crystals for food-grade cream of tartar. Expect 250–350 g of white, gritty powder from 500 g of good crust.

Tip Grind the dry crystals to a fine flour for baking powder. Coarse crystals react slowly and leave sour spots in the cake.

Method 2: Tartaric acid from cream of tartar

  1. Neutralise half with chalk. Stir 100 g of cream of tartar into 1 litre of boiling water. Add 27 g of powdered chalk a pinch at a time; it fizzes hard each time. When it is all in and the fizzing stops, half of the tartar has become calcium tartrate, a white sandy powder, and the other half stays in solution as potassium tartrate.

  2. Bring down the rest. Dissolve 30 g of calcium chloride in a cup of water and stir it in. More white calcium tartrate falls at once. Let it settle while the pot cools.

  3. Wash. Pour off the clear liquid (boiled down, it gives potassium chloride for Chemical Fertilisers). Wash the white powder three times with cold water, letting it settle each time.

  4. Release the acid. Stir the wet calcium tartrate into 300 mL of water in a glazed pot. Separately, pour 50 g (27 mL) of strong sulfuric acid slowly into 100 mL of cold water, never the other way round. Add this diluted acid to the pot in a thin stream, stirring. Warm it to about 70 °C (too hot to keep a finger in) and stir often for an hour. The sandy tartrate turns into a fine, silky mass of gypsum.

    This is slightly less acid than the calculation asks for, so no free sulfuric acid is left in your product.

  5. Filter off the gypsum through cloth and wash it with two cups of hot water, adding the washings to the liquid.

  6. Concentrate gently. Simmer the liquid, never boiling hard, until it is reduced to about a fifth and looks like thin syrup. If it starts to darken, you are overheating it.

  7. Crystallise. Pour it into a shallow glazed dish, cover with a cloth, and leave it somewhere warm and dry for several days. Large, clear, glassy crystals of tartaric acid grow. Pour off the last syrup, add it to the next batch, and dry the crystals.

Yield: about 50–65 g of tartaric acid from 100 g of cream of tartar (the theoretical limit is 80 g).

Method 3: Citric acid from lemons

  1. Juice 25–30 lemons or limes to get about 1 litre. Strain it through cloth.
  2. Clear it. Let the juice stand covered for 2–3 days. A slimy sediment settles and a light fermentation eats some sugar. Pour the clear juice off.
  3. Neutralise hot. Bring the juice to the boil in a glazed pot. Stir in powdered chalk a teaspoon at a time; it fizzes strongly. You will need about 40 g. Stop when another pinch no longer fizzes and a drop of the liquid no longer turns red cabbage juice pink (Acids, Bases and Testing). A heavy white powder of calcium citrate forms.
  4. Filter while boiling. Calcium citrate is less soluble hot than cold, so filter it through cloth while the liquid is still at the boil. Wash it on the cloth with several cups of boiling water until the washings come through clear and no longer taste sweet.
  5. Release the acid. Stir the wet citrate into 250 mL of water. Dilute 36 g (20 mL) of strong sulfuric acid in 80 mL of water as before and stir it in. Keep it warm (about 70 °C) and stir for an hour. Gypsum forms.
  6. Filter, decolourise, concentrate. Filter off the gypsum. If the liquid is yellow, warm it for 15 minutes with a spoonful of charcoal and filter again. Simmer it down gently until a drop placed on a cold plate forms a crust of crystals.
  7. Crystallise. Cool slowly in a covered dish over 2–3 days. Citric acid comes out as clear, colourless prisms. Dry them in air. Yield: 35–45 g from a litre of lemon juice.

Tip For cooking, cleaning and dyeing, lemon juice is 5–6% citric acid. Crystallise only when you must store, carry or weigh it, or keep it dry.

Method 4: Citric acid from mould and sugar

The black mould Aspergillus niger, grown on a very sour sugar solution, turns half or more of the sugar into citric acid. Almost all the world's citric acid has been made this way since the 1920s. Any place that can make Sugar can make citric acid.

Cloth on a frame keeps dust out, lets air in Black spores on top of the mat White mould mat floats, thick and leathery Sugar liquid sour, pH 3 to 3.5 Glazed or glass tray Glass tube samples from under the mat 3–5 cm One spore head seen under a hand lens Keep at 28–32 °C for 8–12 days. Air reaches the mould only from above, so wide shallow trays work best.
Fig. 2 Citric acid by surface fermentation. Shallow trays of acidified sugar solution are seeded with black mould spores. The mould grows a white mat that floats on the liquid and turns black with spores on top; beneath it the sugar slowly turns into citric acid.

The culture liquid

For each 1 litre of water:

Ingredient Amount Why
White sugar 140 g Refined is best: iron in raw sugar or molasses makes the mould grow fat and make little acid
Sal ammoniac (ammonium chloride) 2 g Nitrogen (Ammonia)
Potassium phosphate, or a pinch of bone ash dissolved in a few drops of sulfuric acid 1 g Phosphorus (Chemical Fertilisers)
Epsom salt (magnesium sulfate) 0.25 g Magnesium (Magnesium)
Hydrochloric acid A few drops, to sour it to pH 3–3.5 The sourness keeps bacteria and other moulds out

Mix in rainwater or distilled water, in glass, glazed or enamelled vessels only. Iron vessels ruin the yield.

Step by step

  1. Get the mould. Rub a black-dusted onion skin over bread soaked in culture liquid; keep it covered and warm. In a week it is furred black. Take spores from the cleanest black patch. Keep spores from your best batch on dry sterilised bran in a corked bottle; they live a year or more (Culturing Microbes).
  2. Sterilise. Boil the culture liquid for 10 minutes, cover it, and let it cool to blood warm.
  3. Fill the trays to a depth of 3–5 cm. A tray 40 × 60 cm holds about 10 litres.
  4. Seed with a pinch of black spores tapped evenly over the surface. Cover with a cloth on a frame.
  5. Keep warm, at 28–32 °C (pleasantly warm to a bare arm), for 8–12 days. A white skin forms in two days and thickens into a wrinkled, leathery mat that turns black on top.
  6. Follow the sourness. From day six, draw a spoonful from under the mat daily with a glass tube and taste or titrate it (Acids, Bases and Testing). When the sweetness has gone and the sourness stops rising, it is done.
  7. Harvest. Lift the mat aside, pour off the liquid, and filter it. Treat it exactly like lemon juice, from step 3 of Method 3.

Expect 40–70 g of citric acid per 100 g of sugar with a good strain and steady warmth; beginners often get half that. Save spores only from the trays that gave the most acid.

Warning Check for oxalic acid. If the liquid is not sour enough, or the mould strain is poor, it makes oxalic acid as well, which is poisonous. Test every batch made for food: dissolve 1 g of your crystals in 10 mL of cold water and add a few drops of calcium chloride solution. Clear means no oxalic acid. A white cloud at once means oxalic acid is present; use that batch only for cleaning.

Baking powder

Baking powder is a dry mix of baking soda (sodium bicarbonate, made in Soda Ash and Baking Soda) and a dry acid, kept apart from damp by starch. Wet it and carbon dioxide bubbles through the dough.

The standard recipe, by weight:

Ingredient Parts For a 500 g jar
Baking soda 1 120 g
Cream of tartar, finely ground 2¼ 270 g
Dry starch (maize, potato, wheat or rice) 1 110 g

That ratio exactly uses up the soda, so nothing tastes soapy, and it gives off about an eighth of its weight as gas.

  1. Dry everything. Spread each powder on a tray in a warm, dry place (an oven that has cooled to "hot to the hand", below 50 °C) for an hour. Damp powder reacts in the jar and goes dead.
  2. Sieve each one separately through fine cloth or a hair sieve.
  3. Mix them by sieving all three together three times, or shaking in a closed jar for 5 minutes. The soda must be spread perfectly evenly, or you get yellow, soapy-tasting spots in the cake.
  4. Store in a tight-lidded glass or tin jar, in a dry place. It keeps 6–12 months.

Use about 4–5 g (one level teaspoon) per 100 g of flour, and bake at once: cream of tartar acts as soon as it is wet. With tartaric acid instead, use 1 part soda to 0.9 part acid; it acts almost instantly. "Double-acting" powders add a slow acid that works only in oven heat, such as calcium acid phosphate made from bones and Sulfuric Acid.

Fizz powder: 1 part citric acid, 1 part baking soda and 4–6 parts fine sugar, kept dry, makes a soft drink in cold water, or pressed, an effervescent tablet (Making Medicines).

Other uses

In the kitchen.

  • Jam sets only when it is sour enough (pH about 3). For sweet, low-acid fruit (strawberries, pears, figs, sweet cherries) add 2–3 g citric acid or the juice of one lemon per kilogram of fruit.
  • Bottling tomatoes, which are borderline acid: add ¼ teaspoon (1.5 g) of citric acid per half-litre jar before processing (Canning and Bottling).
  • Stop browning of cut apples, pears and potatoes with a dip in 1% citric acid (10 g per litre).
  • Syrup and meringue. A pinch (0.5 g) of cream of tartar per 250 g of sugar stops syrup turning grainy; a pinch per egg white makes beaten whites stable.

In dyeing. Add cream of tartar at 6–7% of the dry weight of wool to the alum mordant bath (Dyes and Mordants). The wool stays soft and the colours come out brighter and more even.

In blueprints. Citric acid with iron and ammonia makes ferric ammonium citrate, the light-sensitive salt of the blueprint (Blueprints and Cyanotypes).

For cleaning.

  • Kettles and boilers. Warm 15 g of citric acid in 500 mL of water in the scaled vessel for 30 minutes. The crust fizzes away. Rinse well.
  • Rust stains on cloth and dull copper and brass: a paste of cream of tartar and lemon juice, an hour in the sun, then wash (Laundry and Bleaching Cloth).

Warning Not on stone. Fruit acids dissolve marble, limestone and lime mortar just as they dissolve kettle scale. Never use them on a marble table, a limestone floor or a plastered wall.

How to tell it worked

  • Cream of tartar is white, gritty and sour; it barely dissolves in cold water but fully in boiling water, and crystallises again on cooling.
  • Tartaric and citric acid form clear crystals that dissolve quickly in their own weight of water, fizz hard with baking soda, and turn red-cabbage juice pink-red.
  • Burn test. Heat a few crystals on a clean iron spoon: they melt, froth, char, and smell of burnt sugar. Any white, unburnable residue is gypsum or potash: your crystals are not pure.
  • Baking powder test. Stir half a teaspoon into half a glass of hot water. It should fizz hard and at once, with foam rising nearly to the rim. Weak fizzing means it has taken up damp and gone dead.

Note Troubleshooting. No crystals from cream of tartar → too much water. Boil the liquid down by a third and cool again. Syrup that turns brown and will not crystallise → overheated, or too much sulfuric acid charring the last traces of sugar. Next time simmer, never boil hard, and use the slightly short measure of acid. Crystals taste sharp and leave a burning feeling → free sulfuric acid. Redissolve, add a little calcium citrate or tartrate, warm, filter and crystallise again. Mould mat green, pink or slimy → contamination. Discard, scald the trays, sour the next batch more. Thick mat but little acid → iron from a vessel or raw sugar, or the liquid not sour enough. Cake soapy, crumb yellow-green → too much soda or poor mixing.

Dangers

Warning Strong sulfuric acid is the one truly dangerous material in this chapter. A splash blinds and burns deep, and water poured into the strong acid boils and spits it out of the pot. Always pour the acid slowly into cold water, never the reverse, wearing eye protection and with a bucket of water at hand to flood any splash on skin. See Sulfuric Acid.

  • Oxalic acid in mould-made citric acid is poisonous (Oxalic Acid). Use the calcium test above on every batch meant for food.
  • Mould spores. Breathed in, Aspergillus spores can cause serious lung infection in people who are ill or weak, and allergy in anyone. Wet mats before handling, wear a damp cloth over nose and mouth, and keep people with lung disease away from this work.
  • Lead and copper. Do not boil fruit acids in lead-glazed pots, pewter or bare copper: they dissolve the metal into your food (Lead).

What this unlocks

How it was first done

Wine tartar was used in medicine and dyeing by the ancient Greeks and Romans, and purified cream of tartar was traded from the wine regions of Europe by the Middle Ages. The Swedish chemist Carl Wilhelm Scheele isolated tartaric acid from cream of tartar in 1769 by the chalk and sulfuric acid method above, and citric acid from lemon juice in 1784 the same way. Commercial citric acid was first made in England in the 1820s, from Sicilian lemon juice; Italy kept a near monopoly, shipping calcium citrate, for a century.

In Birmingham in 1843, Alfred Bird made a yeast-free baking powder because his wife could not eat yeast or eggs; Eben Horsford's phosphate powder followed in America in the 1850s.

Carl Wehmer in Germany showed in 1893 that some moulds make citric acid from sugar, but unreliably. James Currie of the United States Department of Agriculture published in 1917 that Aspergillus niger in a strongly acid sugar solution gave high yields. Pfizer began production in Brooklyn in 1919, and within a decade mould-made citric acid had ended the dependence on Italian lemons.

Source: content/entries/chemistry/fruit-acids.md