Part 13 · Electricity
Magnets
How to find a natural magnet (lodestone), how to turn steel needles and bars into lasting magnets, and how to float one on water to point north. Magnets lead to the compass, the generator and the electric motor.
- Difficulty
- ●●●●●
- Time
- An afternoon once you have lodestone or a steel needle; finding lodestone may take weeks
- Steps from zero
- 11 prerequisites →
You need first
Iron (the Bloomery)The full path from nothing — 11 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Hides and Leather
- Bellows
- Iron (the Bloomery)
- Magnets
Do them roughly in this order. See it on the tech tree →
Why it matters
A magnet is a piece of stone or metal that pulls on iron from a distance, without touching it. That sounds like a curiosity, and for thousands of years that is all it was. Then two uses changed the world.
First, a magnet that is free to turn will swing until it points roughly north–south, day or night, in fog or under cloud. That is the The Compass, and with it you can travel, map and sail when there is no sun or star to steer by (compare Finding Direction).
Second, magnets are half of everything electrical. Move a magnet past a coil of wire and electricity flows in the wire: that is the The Generator. Push electricity through a coil near a magnet and the magnet moves: that is the The Electric Motor. You cannot make electricity in useful amounts, or turn it back into motion, without magnets. This chapter is the doorway to the whole Electricity part of this book.
How it works
Every piece of iron is made of countless tiny regions, each of which is already a little magnet. Call them domains — tiny magnetic patches, far too small to see. In an ordinary lump of iron they point every which way, so their pulls cancel out and the lump as a whole is not a magnet.
Magnetising means lining the domains up so that most of them point the same way. Then their pulls add together and the whole piece becomes a magnet.
Some facts that follow from this:
- Every magnet has two ends, called poles. One end is attracted towards the Earth's north and is called the north-seeking pole (or just "north", marked N). The other is the south pole (S).
- Like poles push apart; unlike poles pull together. N repels N; N attracts S. The Earth itself is a giant, weak magnet, and that is why a free magnet swings to point north.
- Breaking a magnet in half gives two magnets, each with its own N and S. You can never get a lone north pole.
- Iron, steel, nickel, cobalt and a few iron ores are attracted to magnets. Copper, brass, gold, silver, wood, glass and stone are not.
- Soft iron magnetises easily but forgets. Pure, soft wrought iron (see Iron (the Bloomery)) becomes strongly magnetic while a magnet is near, and loses almost all of it the moment the magnet is gone. That is exactly what you want in the core of an The Electromagnet.
- Hardened steel is hard to magnetise but remembers. In Steel that has been heated red and quenched in water, the carbon and the strained crystal structure jam the domains in place. Once lined up, they stay lined up for years. This is the only kind of metal that makes a good permanent magnet with the materials in this book.
- Heat destroys magnetism. Above about 770 °C (a bright cherry red), iron cannot hold any magnetism at all. Lodestone loses its magnetism above about 580 °C (a dull red). Hard knocks and dropping also shake domains out of line.
What you need
| Item | Notes |
|---|---|
| Lodestone (if you can find it) | Any size; a lump the size of an egg is plenty |
| Steel needles or thin bars | Hardened high-carbon steel. Sewing needles, 4–8 cm long, for compasses; bars 10–15 cm × 1 cm × 0.5 cm for bar magnets |
| A hammer and an anvil | For Method 2. See Blacksmithing |
| A forge | To harden steel and for the heat method |
| A bowl of still water | Wood, Pottery or a gourd — not iron |
| A float | A thin slice of cork, a flat chip of light wood, a short piece of dry straw or reed, or a leaf |
| Iron filings or small iron scraps | To test your magnets |
| Thread | Silk or fine plant fibre, for hanging a needle |
Where to find it
Lodestone is a naturally magnetised lump of magnetite, a common black iron ore (see Finding and Identifying Ores). Ordinary magnetite is attracted to a magnet but will not itself pick up iron. Lodestone is the rare magnetite that is a magnet.
Where it occurs:
- On or very near the surface, not deep in mines. The best explanation is that lodestone was magnetised by lightning strikes: the huge current in a strike makes a brief, very strong magnetic field that magnetises the rock around it. Look on exposed ridges, hilltops and outcrops of iron-rich rock — the places lightning hits.
- Where magnetite is common: dark, heavy rocks such as gabbro and serpentine; the black sand that collects behind boulders in rivers and on beaches (magnetite sand); and iron ore bodies. Historic sources include Magnesia in Greece (which gave magnets their name), the hills of Hebei in China, Sweden, the Urals, and Magnet Cove in Arkansas in North America.
How to recognise lodestone:
- It is black to dark steel-grey, heavy for its size, and often a little rusty on the outside.
- Its streak is black. Rub it hard on the back of a broken piece of unglazed pottery: magnetite leaves a black line (the red-brown iron ore haematite leaves a red line).
- It picks up iron. Touch it to iron filings, a nail or a needle. Lodestone grabs them and they cling in tufts, mostly bunched at two places on the stone — its poles. Ordinary magnetite does nothing.
- It swings north. Hang a piece in a sling of thread, or float it on a chip of wood in a bowl of water. A lodestone turns and settles with the same side always towards the north.
Tip Finding magnetite sand. Drag a known magnet (or a lodestone wrapped in a cloth) through river sand where the sand is dark. The black grains that cling to it are magnetite. They tell you that magnetite rocks are upstream — and that lodestone may be found on the ridges there.
Hardened steel comes from Steel and Blacksmithing. If you have no lodestone at all, you can still make magnets: Method 2 below uses only the Earth's own magnetism.
Preparing lodestone ("arming" it)
A raw lodestone is weak because its pull leaks out in all directions. Find its two poles (where the filings bunch), then grind or chip two flat faces there. Fit two small caps of soft iron — bent strips about 3 mm thick — against those faces, with their ends sticking out on the same side like two feet, and bind the whole thing tightly with wire, cord or a Hides and Leather strap. This is an armed lodestone. The iron caps gather the stone's pull and bring both poles close together, and an armed stone can lift many times what it could lift bare. Some historic armed lodestones lifted dozens of times their own weight.
Method 1: Stroking with a lodestone or another magnet
This is the oldest and best method for small magnets such as compass needles.
- Harden the needle. If it is not already hard, heat it to a bright cherry red (about 800 °C) in the forge and plunge it into cold water. Test it with a file: hard steel makes the file skate instead of biting. A soft needle will take the magnetism and then lose it within days.
- Find the lodestone's poles. They are where the iron filings cluster. Choose one pole and mark it.
- Lay the needle flat on a wooden board. Hold one end down with a fingertip.
- Stroke. Place the chosen pole of the lodestone on the needle near the end under your finger, press gently, and draw it firmly along the whole length of the needle and off the far end.
- Lift away. At the end of the stroke, lift the lodestone high — at least a hand's width — and swing it back through the air to the starting end. Never drag it back along the needle; that undoes the last stroke.
- Repeat 30 to 50 times, always in the same direction, always with the same pole.
- Test the needle by picking up iron filings, or by floating it (below).
The end of the needle where your strokes finish becomes the pole opposite to the lodestone pole you used. If you stroke with the lodestone's north-seeking pole, the far end of the needle becomes a south pole.
For bigger bars, use divided touch: put two magnets with opposite poles down on the middle of the bar, then draw them apart towards the two ends at the same time; lift both away in arcs, bring them back to the middle, and repeat 20–30 times. Then turn the bar over and do the other side. This gives a stronger, more even bar magnet.
Tip Magnets multiply. Once you have one good needle, you can use it to magnetise others, and several magnetised bars tied together side by side (all N ends together) make a stronger stroking magnet than any single one. In the 1700s this is exactly how people built powerful steel magnets without any lodestone better than average.
Method 2: The Earth's field (hammering or heating)
The Earth's magnetism is weak, but it is everywhere. If you shake the domains of a piece of steel loose while it lies along the Earth's magnetic field, they settle a little more in line with it.
- Find magnetic north. Use the pole star or the sun at noon (Finding Direction). True north and magnetic north differ in most places by a few degrees to 20°, but that is close enough for this.
- Point the bar north and tilt it down. The Earth's field is not level: it dips into the ground. In the northern hemisphere, tilt the north end of the bar down steeply — about 60–70° below level in mid-latitudes (Europe, northern China, most of the United States); less near the equator, where the field is almost level. In the southern hemisphere tilt the south end down.
- Either hammer it: hold the bar in that position, resting its lower end on an anvil or stone, and strike the top end sharply 20–30 times with a hammer.
- Or heat it: heat a steel needle or bar to bright cherry red (above 770 °C), take it out with tongs, hold it pointing north and tilted down, and quench it in water while still in that position. This hardens and magnetises it in one step. Chinese writers described exactly this — a thin iron "fish" heated red and cooled pointing north — in 1044.
Both give a weak magnet: enough to make a floating needle point north, but much weaker than one stroked with a lodestone. Use it as a seed: stroke other needles with it, tie them together, and stroke again, building strength step by step.
Method 3: An electromagnet
Once you have a The Battery and Copper Wire, this is by far the strongest method. Wind 100–300 turns of insulated wire around a tube of paper or wood that the steel bar slides into. Put the hardened steel bar inside, connect the coil to the battery for a few seconds, and disconnect. The bar comes out as a strong permanent magnet — stronger than a lodestone can make it. Alternatively, stroke the bar across the poles of a powerful The Electromagnet, as in Method 1. Every good permanent magnet in the modern world is made this way (see Permanent Magnets). Keep the current on for a few seconds only: a coil straight across a battery is close to a short circuit, and the wire and battery heat up fast.
Making a floating-needle compass
- Use a magnetised needle 4–8 cm long.
- Lay it on a float: a thin disc of cork, a sliver of light wood, a leaf, or push it through a 3 cm piece of dry straw.
- Float it in the middle of a bowl of still water at least 10 cm across. Keep iron and steel (knives, axes, nails) at least an arm's length away — they pull the needle off line.
- It will turn and settle within a few seconds. Turn it away by hand and let go: it should return to the same direction every time.
- Mark the north-seeking end with a scratch or a dab of colour, once you have checked against the sun or stars which end it is.
A dry version: balance the needle on a sharp vertical point (a thorn or another needle), or hang it from its middle by a single fine thread (silk is best — it does not twist much) inside a jar out of the wind. These lead to the proper The Compass.
How to tell it worked
- The pick-up test. A good compass needle picks up iron filings at both ends but few in the middle. A good bar magnet 10 cm long should lift a small nail.
- The swing test. Floated or hung, it settles in the same direction every time.
- The two-needle test. Bring the N end of one magnetised needle near the N end of another floating one: the floating one should swing away. Unlike ends pull together. (Plain unmagnetised iron is attracted to both ends of a magnet; only another magnet is ever repelled. Repulsion is the only proof that something is a magnet.)
- The keeping test. Check again after a week. If it has gone weak, the steel was not hard enough.
Note Troubleshooting. Needle picks up nothing after stroking → the lodestone is too weak or you stroked back and forth. Stroke in one direction only, with lifts. Strong at first, weak after a few days → the steel is soft. Harden it (red hot, quench in water) and magnetise again. Floating needle won't settle, or always points the same way whatever you do → there is iron nearby, or the float is touching the side of the bowl. Use a wider bowl. Needle tips and sinks → the float is too small. Use a bigger float or a lighter needle. Both ends pick up filings but it does not point north → it may have two poles of the same kind at the ends and an extra pole in the middle (from careless stroking). Heat it red to wipe it clean, harden, and start again.
Looking after magnets
- Store bar magnets in pairs, side by side with opposite poles together, with a short bar of soft iron (a keeper) laid across each pair of ends. A horseshoe-shaped magnet should always have an iron bar across its two ends. This closes the magnetic loop and keeps the magnet strong for years.
- Do not drop, hammer or heat them.
- Keep them away from each other N to N — strong magnets pushed together like poles can weaken each other.
- Remagnetise weakened magnets by stroking again. It costs nothing but time.
Dangers
Magnets made with these methods are weak and almost harmless. The risks are in the work around them:
Warning Hardened steel shatters, and quench water spits. Hammering or bending a hardened needle or bar can snap it and throw sharp splinters at your eyes; shield your face and work with the bar pointing away from you. Plunging red-hot steel into water throws scalding steam and droplets: hold it in long tongs at arm's length.
- Forge work. Heating and quenching steel means red-hot metal and burns: see the dangers in Blacksmithing.
- A compass you trust too much. A magnetic compass points to magnetic north, which can be 20° or more away from true north in some regions, and iron objects or iron-rich rocks nearby can drag it far off. Check it against the sun and stars (Finding Direction) whenever you can, and write down the difference for your area.
- Lightning. Do not go looking for lodestone on exposed ridges during thunderstorms — the very places that make lodestone are the places lightning strikes.
What this unlocks
- The The Compass, for travel, mapping and sailing (Boats and Sails).
- The The Generator: magnets spinning past coils of Copper Wire make electricity.
- The The Electric Motor and the moving-coil meters of Measuring Electricity.
- Stronger alloy magnets (alnico, ferrite) in Permanent Magnets.
- A way to detect electricity: a magnetised needle next to a wire swings when current flows (see The Electromagnet and the galvanometer there).
- The The Telephone earpiece, which uses a permanent magnet.
How it was first done
Greek writers knew that lodestone attracts iron by about 600 BC; the word magnet comes from Magnesia, a lodestone region of Greece. Chinese texts from about the same period also describe it. The Chinese were the first to use magnetism to find direction: by the 1000s the scholar Shen Kuo (1088) described needles rubbed on lodestone and hung by a silk thread, and noted that they point not exactly south but slightly east of it — the first record of magnetic declination. A military manual of 1044 describes the heated-iron "south-pointing fish" floated on water. The compass reached Europe and the Islamic world by the late 1100s; the Englishman Alexander Neckam described a needle for sailors in about 1190.
In 1269 Petrus Peregrinus, a French scholar, wrote a short letter describing poles, attraction and repulsion, and how breaking a magnet makes two. In 1600 William Gilbert, an English physician, published De Magnete, showing by experiment that the Earth itself is a great magnet and that iron hammered while pointing north becomes magnetic. In the 1740s and 1750s Gowin Knight and John Michell in England made strong steel bar magnets by repeated stroking of hardened bars, and from the 1820s onwards, magnets were made with electric currents.