◆ Rebuild

Part 15 · Knowledge and Science

The Telescope

How to build a telescope — first a simple spyglass of two lenses in a tube, then a Newtonian reflector with a mirror you grind, polish, test and silver yourself — how to mount it steadily, and what it gives you in astronomy, navigation and surveying.

Difficulty
●●●●●
Time
A day for a spyglass from lenses you already have; four to eight weeks of evenings for a first reflecting telescope
Steps from zero
25 prerequisites →

You need first

LensesMirrors

This unlocks

Radio Telescopes and Microwave LinksMeasuring Angles: Theodolite and SextantBuilding an ObservatorySignal Fires, Flags, Semaphore and Heliographs
The full path from nothing — 25 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Sulfur
  7. Hunting and Trapping
  8. Basic Woodworking
  9. The Kiln
  10. Pottery
  11. Charcoal
  12. Hides and Leather
  13. Lime
  14. Lye and Potash
  15. Glass
  16. Bellows
  17. Saltpeter
  18. Copper Smelting
  19. Lead
  20. Sulfuric Acid
  21. Lenses
  22. Gold and Silver
  23. Nitric Acid
  24. Silver Nitrate and Silver Salts
  25. Mirrors
  26. The Telescope

Do them roughly in this order. See it on the tech tree →

Why it matters

A telescope brings far things near. That is useful in very practical ways long before it is used for the stars:

  • At sea and on land: identifying a ship, a coastline, a landmark, smoke, a herd, a signal flag or fire at 10–20 km (Navigation, Boats and Sails). A semaphore line of hilltop towers with telescopes carries messages hundreds of kilometres in an hour (Signal Fires, Flags, Semaphore and Heliographs).
  • In surveying: a telescope with crosshairs makes every sighting instrument — levels, theodolites, the The Compass — ten times more accurate, and lets you measure distance by reading a marked staff (Surveying and Levelling, Maps and Mapmaking).
  • In astronomy: the moons of Jupiter, the phases of Venus, the rings of Saturn, the mountains of the Moon. These sights overturned the old belief that everything circles the Earth, and the clockwork of Jupiter's moons gave the first accurate way to fix longitude on land (Astronomy, The Calendar).
  • For science: precise timing of stars for clocks (The Mechanical Clock), the measurement of the Earth, the speed of light.

How it works

Every telescope has two parts:

  1. The objective — a large lens or a concave mirror — gathers light from a distant object and forms a small real image of it at its focus, one focal length (F) away.
  2. The eyepiece — a small, strong lens of focal length f — magnifies that image, like a magnifying glass.

Magnification = F ÷ f

An objective of focal length 100 cm with an eyepiece of 4 cm gives 25 times.

Aperture is what matters most. The width of the objective (its aperture, D) decides how much light is gathered and how fine a detail can be seen. A 10 cm objective gathers four times the light of a 5 cm one and shows details half the size. As a rule, the most useful magnification is about 1 to 2 times the aperture in millimetres: up to 50–100× for a 5 cm lens, 150× for a 15 cm mirror — less if the optics or the air are poor. Pushing beyond that only gives a bigger blur.

The focal ratio is F ÷ D. A mirror 15 cm across with a focal length of 120 cm is "f/8". Long focal ratios are easier to make well and forgive mistakes; short ones are brighter and more compact but much harder.

Galilean: concave eyepiece before the focus upright image, narrow field; spacing = F − f objective concave eyepiece focus Keplerian: convex eyepiece after the focus upside-down image, wide field; spacing = F + f objective convex eyepiece crosshair at the focus F (objective focal length) f magnification = F ÷ f
Fig. 1 Two kinds of refracting telescope. In the Galilean, a concave eyepiece placed before the focus gives an upright image — good for a spyglass, but a small field of view. In the Keplerian, a convex eyepiece placed after the focus gives a wider, upside-down image, and a crosshair placed at the focus is seen sharp across the object.

Method 1: The spyglass (refractor)

You already know how to grind the lenses (Lenses).

The objective

A weak convex lens: focal length 50–120 cm, 3–5 cm across. Grind it with tools of radius equal to the focal length (both sides alike) and polish it well.

The trouble with a single lens is colour: it brings blue light to a focus a little closer than red, so bright things have coloured fringes. Two cures, both used by the early astronomers:

  • Make it long. The longer the focal length for a given width, the less the colour error shows. Keep the focal length at least 25–30 times the width: a 4 cm objective at 100–120 cm.
  • Stop it down. A ring of card in front of the lens that hides its outer part makes the image sharper and less coloured, at the cost of brightness. Galileo did this.

The real cure is the achromatic doublet: a convex lens of ordinary (crown) glass cemented to a weaker concave lens of heavy lead (flint) glass, whose colour errors cancel. It needs two kinds of glass of known properties and careful calculation (Glass); it is the next step after this chapter.

The Galilean spyglass

  • Eyepiece: a concave lens of focal length 3–5 cm.
  • Placing: the eyepiece goes before the focus, at a distance F − f from the objective. With F = 100 cm and f = 4 cm, the lenses are 96 cm apart: 25×.
  • The image is upright, so it is natural to use on land and at sea. But the field of view is narrow, and above 10–15× it becomes tunnel-like. For a hand spyglass, 6–10× is right.

The Keplerian telescope

  • Eyepiece: a convex lens of focal length 2–5 cm, or a Huygens eyepiece of two lenses (The Microscope).
  • Placing: after the focus, at a distance F + f from the objective.
  • The image is upside down — no matter for stars — and the field is much wider. Because there is a real image at the focus, a crosshair of two fine hairs, silk fibres or spider threads stretched on a ring at that point is seen sharply on top of the object. This is what makes surveying and astronomical instruments possible.
  • To make it upright for land use, add an erecting pair of two more convex lenses between the focus and the eyepiece; this lengthens the tube by about four times their focal length.

The tube

  1. Make two tubes that slide one inside the other: rolled and glued paper, thin wood strips glued round a former, or Sheet Metal and Rolling. The outer one holds the objective, the inner one the eyepiece.
  2. Blacken the inside with soot and glue, and fit two or three card rings inside as baffles to stop stray light.
  3. Mount the objective in a cell at the front with its optical centre on the tube's axis, and fit a short dew shield — a 10 cm extension of the tube — in front of it.
  4. Focus by sliding the inner tube. Mark the focus for distant objects.

Method 2: The Newtonian reflector

A concave mirror has no colour error at all, and a mirror can be made far larger than a lens with ordinary materials, because the light does not pass through the glass — bubbles and streaks inside do not matter. This is the telescope that you can make with real power.

Main mirror felt pads, 3 tilt screws Diagonal flat, at 45°, 1/5 mirror width Eyepiece focus slides here Side bearings round, 15–25 cm, rest in V-notches on felt Box turns on a flat base Light from a star
Fig. 2 A Newtonian reflector on a simple box mount. Light enters the open end, reflects from the concave main mirror at the bottom, and is turned sideways by a small flat diagonal mirror to the eyepiece at the side of the tube. The tube rocks up and down on round side bearings; the box turns round on a flat base.

A first mirror: 11–15 cm across, focal length 110–150 cm (about f/10). At f/10 a carefully made spherical mirror is good enough without any further shaping, and the tube is still easy to handle.

1. The blanks

You need two discs of glass the same size, about 2–2.5 cm thick: one becomes the mirror, the other the grinding tool. Cast them in a flat clay or sand mould from your glass furnace (Glass), and anneal them slowly over two or three days in warm ash or the annealing oven: thick glass with any strain in it cracks during grinding. Bubbles inside do not matter; a bubble that opens on the mirror face only spoils a tiny spot. The tool may be of stone, cast iron, or glass with tiles of glass or hard stone stuck to it with pitch.

2. Rough grinding

  1. Fix the tool face up on a solid post or barrel at waist height, so you can walk round it.
  2. Put a teaspoon of wet coarse grit (emery, or sharp sand) on the tool, lay the mirror blank on it, and push it back and forth in strokes about one-third of its width, with the centre of the mirror passing over the centre of the tool. After every few strokes, turn the mirror a little in your hands, and step a little way round the post. Mirror on top, the mirror becomes concave; the tool becomes convex.
  3. Check the depth often. The hollow at the centre must reach D² ÷ (16 × F): for 15 cm and 150 cm, 0.94 mm; for 11 cm and 110 cm, 0.69 mm. Lay a straight edge across the wet mirror and slide stacks of thin metal foil or paper of known thickness under its middle. Or simply measure the focus: wet the hollow and reflect the sun or a distant lamp from it onto a card; the distance to the sharpest spot is F.
  4. To deepen faster, use longer strokes; when deep enough, switch to short strokes, sometimes with the tool on top, to keep the curve from going deeper.

3. Fine grinding

Wash everything perfectly, then grind with each finer grade — four to six grades, each graded by settling in water (Lenses) — for 30–60 minutes each, with one-third strokes. A thin pencil grid drawn on the mirror should grind away evenly all over in a minute or two: then the two surfaces fit everywhere. Finish when the surface, held at a low angle to a lamp, shows an even, fine, satin grey with no pits.

4. Polishing

  1. Pour a 5–6 mm layer of softened pine pitch onto the warmed tool (Tar, Pitch and Glue). While it is soft, press the wet mirror into it (with rouge water between, so it does not stick) to take the exact curve. Cut channels in it, 3 mm wide, in a grid of 2–3 cm squares.
  2. Polish with rouge or tin oxide and water, the same one-third strokes, light pressure, turning and walking as before.
  3. It takes 5–10 hours. Stop when a strong lamp beam shows no grey haze over the whole surface, even at the edge.

5. Testing — the knife edge

Léon Foucault's test lets you see errors smaller than a ten-thousandth of a millimetre with nothing but a lamp and a blade.

Mirror on edge twice the focal length (the centre of curvature) Pinhole lamp hole 0.3 mm Razor blade slides into the beam eye Perfect sphere darkens evenly, all at once Blade not at focus shadow sweeps across; move the blade in or out Turned-down edge bright rim at the edge; polish with shorter strokes Zone a ring lit on one side, dark on the other
Fig. 3 The Foucault knife-edge test. A pinhole light and a razor blade stand side by side at the centre of curvature, twice the focal length from the mirror. As the blade cuts the returning beam, a perfect sphere darkens evenly all over; zones, a turned-down edge or a hole show up as shadows and rings.
  1. Stand the mirror on edge at one end of a dark room or long passage.
  2. At twice the focal length away (the centre of curvature: 3 m for an F = 150 cm mirror), set up a lamp behind a sheet of tin pierced with a pinhole about 0.3 mm across, aimed at the mirror. The mirror returns the light to a point right beside the pinhole.
  3. Fix a razor blade on a block that slides sideways, at the point where the light returns, and put your eye right behind the blade. You will see the whole mirror filled with light.
  4. Slide the blade slowly into the beam.
    • If the blade is exactly at the point of focus and the mirror is a perfect sphere, the whole mirror darkens evenly all at once — it goes uniformly grey, then black.
    • If the blade is in front of or behind the focus, a shadow sweeps across the mirror from one side or the other. Move the block nearer or farther until the darkening is even.
    • A raised zone or a dip shows as a ring that looks lit on one side and shadowed on the other, as if the mirror were a landscape lit from the side.
    • A turned-down edge (very common) shows as a bright rim on the side away from the blade's shadow.
  5. Correct by polishing: shorter strokes work the centre more; longer ones, the edge. Test after every 15–20 minutes of polishing.

Tip Is a sphere good enough? For a perfect star image, the mirror should be a paraboloid, slightly deeper in the middle than a sphere. For a 15 cm mirror at f/10 or longer, or an 11 cm mirror at f/8 or longer, the difference is smaller than the errors your eye can notice; a good sphere will do. Faster mirrors need parabolising — polishing with longer, overlapping W-shaped strokes until the knife edge shows a gentle "doughnut" shading — a skill best learned on a second mirror.

6. Silver it

Coat the front of the finished mirror with silver (Mirrors), let it dry, and polish it very lightly. Keep it covered when not in use.

7. The diagonal flat and the tube

  • The diagonal: a small, flat mirror at 45°, about one-fifth of the main mirror's width (3 cm for a 15 cm mirror). Flat surfaces are made by grinding three discs against each other in turn — A on B, B on C, C on A — because only flat surfaces can fit all three pairs. Silver it like the main mirror. A small right-angled glass prism works too.
  • The tube: wood or thick rolled cardboard, square or round, its inside width about 5 cm more than the mirror, and about as long as the focal length. Blacken it inside. An open frame of wooden rods covered with black cloth is lighter.
  • The mirror cell: a wooden board at the bottom of the tube, with the mirror resting on three pads of felt or cork and held by three small clips at the edge — loose, never squeezed — and three screws with springs that tilt it for adjustment.
  • The eyepiece holder goes in the side of the tube a short way from the top: the diagonal sends the image out through a hole in the tube wall to a sliding tube that holds the eyepiece. Fix the diagonal on a thin stalk or on three thin strips of metal across the tube (a "spider"), so it blocks as little light as possible.

Lining it up (collimation). Take out the eyepiece and look through its holder. Tilt the diagonal until you see the whole main mirror centred in it; then adjust the three mirror screws until the reflection of the diagonal sits centred in the main mirror. Mark the exact centre of the main mirror with a small ring of ink before silvering — it makes this easy, and the diagonal's shadow covers it anyway.

Eyepieces for the reflector

With F = 150 cm: an eyepiece of 4 cm gives 38× (finding things, the Moon whole, star clusters); 2.5 cm gives 60× (Jupiter's moons, Saturn's rings); 1.2 cm gives 125× (fine detail on a steady night). Use the Huygens design from The Microscope for the longer ones.

Mounts

A telescope that shakes is useless: at 60×, a shake you cannot see with the bare eye throws the object out of view.

  • For a spyglass: a wooden tripod with a simple swivel head, or rest it on a padded stick or a wall.
  • The box mount (often called a Dobsonian after its modern popularizer): a wooden box holds the tube on two large round side bearings (15–25 cm across) resting in V-shaped cut-outs; the box turns on a flat base board round a central bolt. Pads of leather, felt or waxed hardwood give smooth, firm motion. It is simple, steady, and can be made in a weekend (Basic Woodworking).
  • The equatorial mount: tilt one axis so it points at the celestial pole — parallel to the Earth's axis, at an angle from level equal to your latitude (Finding Direction, Navigation). Then a single slow turn on that axis follows the stars as the Earth turns, and a clockwork drive can do it for you (The Mechanical Clock). Needed for long observing, timing, and photography.

What to look at

Target What you see Power
The Moon Craters, mountains, long shadows along the line between day and night 20× and up
Jupiter Four bright moons in a line, changing place night by night; cloud bands 15–60×
Venus Phases like a little moon 25× and up
Saturn The rings 30–60×
The Pleiades, the Milky Way, star clusters Many more stars than the eye can see 10–40×
Double stars Pairs too close for the eye; a test of your optics 60–150×
The Sun Sunspots — by projection only, below Any

Projecting the Sun. Use only a simple spyglass or a small refractor, with a plain single-lens eyepiece (no cemented lenses). Cap any finder. Without looking through it, point the telescope at the sun by making its shadow as small and round as possible. Hold a white card 20–30 cm behind the eyepiece and focus: a bright disc of the sun appears, with any sunspots as dark specks. Never leave it pointed at the sun — the eyepiece heats up and can crack.

Surveying and navigation uses

  • Telescopic sights. A Keplerian telescope with a crosshair, fixed to a level or a sighting compass, points to within a fraction of a minute of angle.
  • Stadia hairs: two extra horizontal hairs at the focus, spaced so that the length of staff seen between them, times 100, is the distance to the staff. Set them by sighting a staff at a measured 50 m and placing them 50 cm apart on the staff (Surveying and Levelling).
  • Longitude by Jupiter's moons. The four moons are eclipsed by Jupiter at moments that can be predicted and timed. Comparing the local time of an eclipse with its time in a printed table for your home observatory gives the difference in longitude. It works well on land, but is nearly impossible on a rolling ship; at sea the answer was the Chronometers and Stopwatches (Navigation).

How to tell it worked

  • A star test. Point at a bright star at high power and slowly move the focus in and out. Just inside and just outside focus, a good telescope shows the same evenly lit disc with a few rings on both sides. Different patterns on the two sides mean a poorly figured mirror or lens; a triangular or elongated shape means a pinched mirror or bad collimation.
  • The moons of Jupiter at 20–30× as sharp points, and Saturn's rings clearly separated from the ball at 50×.
  • Reading: a printed page should be readable at 100–200 m with a spyglass of 10×.

Note Troubleshooting. Coloured fringes round everything (refractor) → stop the objective down, or use a longer focal length. Image soft everywhere (reflector) → collimate first; then Foucault-test the mirror again. Stars look like crosses or triangles → the mirror is pinched in its cell. Loosen the clips. Image boils and wobbles → warm air. Let the telescope cool outdoors for an hour before use, observe away from roofs and chimneys. Low contrast, washed out → stray light. Blacken and baffle the tube; add a dew shield. Dew on the mirror or lens → a longer dew shield; store it indoors and bring it out an hour before use.

Dangers

Danger Never look at the Sun through any telescope, binoculars, finder or spyglass — not for an instant, not at sunset, not through smoked glass. It burns a blind spot into the retina immediately, painlessly and permanently. Keep telescopes capped in daylight, and watch children around them. Use projection only.

  • Glass blanks can crack during grinding and leave razor edges. Bevel the edges of mirror and tool with a stone before you start.
  • Silica dust from dry grit: always grind wet and clean up wet (Abrasives and Grinding Stones).
  • Silvering chemicals: see Mirrors — leftover silvering solution can explode.
  • Heavy tubes on tall mounts fall over. Make the base broad and weight it.
  • Night work: cold, uneven ground, and stumbling in the dark. Use a dim red light (a lamp behind red glass or cloth) — it does not spoil your night vision.

Going further

How it was first done

In October 1608 the spectacle maker Hans Lipperhey of Middelburg in the Netherlands applied for a patent on an instrument "for seeing things far away as if they were nearby"; others, including Jacob Metius, claimed the idea at the same time. In 1609 Galileo Galilei in Padua heard of it and built his own, grinding lenses to reach about 20×; in January 1610 he discovered four moons circling Jupiter, and soon the phases of Venus. Johannes Kepler described the two-convex-lens design in 1611. To fight colour fringes, astronomers such as Christiaan Huygens built very long telescopes — some over 40 m, with the objective hung on a pole. In 1668 Isaac Newton made the first working reflecting telescope with a speculum mirror and a flat diagonal, and in 1721 John Hadley made the first truly good one. Chester Moor Hall (1733) and John Dollond (1758) made achromatic lenses. William Herschel, a musician in Bath, ground his own speculum mirrors and in 1781 found the planet Uranus. In 1857–1858 Léon Foucault in Paris introduced silvered glass mirrors and his knife-edge test, which made it possible for anyone with patience to make a fine telescope — and in the 1920s groups of amateurs in America and Britain began doing exactly that, as you can now.

Source: content/entries/knowledge/telescope.md