◆ Rebuild

Part 4 · Food and Farming

Growing Mushrooms

Grow oyster mushrooms on straw and logs and shiitake on oak logs — getting "spawn" from a wild oyster mushroom, from stem butts or from colonised wood, keeping it clean, moist and shaded, and harvesting flush after flush from waste you would otherwise burn. And why you must never eat a wild fungus you cannot identify for certain.

Difficulty
●●●●●
Time
Oysters on straw — about 4–6 weeks to the first harvest; mushrooms on logs — 6–18 months, then fruiting for 3–6 years
Steps from zero
2 prerequisites →

You need first

Farming from Seed

This unlocks

—
The full path from nothing — 2 steps before this one
  1. Stone Tools
  2. Farming from Seed
  3. Growing Mushrooms

Do them roughly in this order. See it on the tech tree →

Why it matters

Mushrooms turn things nobody can eat — straw, sawdust, small logs from thinning a wood, corn stalks — into food. They need no field, no sun and little work once started. They grow in shade, in cellars, under trees, in old sheds, in the dark corners of a farm.

Fresh mushrooms are not a staple: they are about 90 % water, with roughly 30 kcal and 2–3 g of protein per 100 g. But they give flavour, protein and B vitamins to a plain diet, dry well for winter, and grow on waste. The spent straw or sawdust left after the harvest is half-rotted already and makes excellent compost or mulch (Compost and Manure), and cattle and pigs will eat spent straw.

This chapter covers the two easiest and most reliable mushrooms: oyster mushrooms, which grow on almost any plant waste, and shiitake, which grow on hardwood logs.

How it works

What a mushroom is. The part you eat is only the fruit of a fungus. The fungus itself is the mycelium: a mass of fine white threads (hyphae) that grows through wood, straw or soil, digesting it from outside with enzymes. When the mycelium has used up much of its food, and conditions change — a soaking, a cold snap, more light and air — it pushes up mushrooms to scatter spores (the fungal "seeds", too small to see one by one).

Spawn. You cannot practically plant spores; they are tiny, slow, and each grows into a different strain. Growers plant spawn instead — something already full of living mycelium of the right mushroom: colonised grain, sawdust, wooden pegs, cardboard, or pieces of the mushroom's base. Spawn is to mushrooms what a cutting is to a fruit tree (Fruit Trees and Orchards).

The race. Your substrate (the material the mushroom will eat — straw, logs) is also food for moulds, bacteria and wild fungi. Mushroom growing is a race: give your mushroom a head start — lots of spawn, a substrate with the competition reduced, at a temperature your mushroom likes — so it fills the substrate before anything else can.

  • Straw is cleaned of most competitors by pasteurising it — hot water at 65–80 °C kills most moulds and bacteria but leaves some harmless ones that help protect it. Full boiling or sterilising is not needed and lets mould in faster afterwards.
  • Logs are clean inside if they come from a living, healthy tree cut in the dormant season, and are inoculated before wild fungi arrive (within about 6 weeks).

The four needs:

Need Spawn run (mycelium growing) Fruiting (mushrooms growing)
Moisture Moist, never wet: squeeze a handful of straw and only a few drops fall Air very humid (85–95 %): mist or sprinkle 2–3 times a day
Temperature 20–25 °C oyster; 20–27 °C shiitake 10–20 °C for most strains (some oysters 18–28 °C)
Air Little needed; can be in a closed bag Lots of fresh air — stale air gives long stems and tiny caps
Light Dark or dim Dim daylight, enough to read by. No direct sun.

What you need

Item Notes
Spawn See "Getting spawn" below
Straw Wheat, barley, oat, rice or rye straw, dry and not mouldy; or chopped maize stalks, reeds, banana leaves, sawdust
Logs Fresh hardwood, 8–20 cm thick, about 1 m long. Oak for shiitake; poplar, willow, alder, birch, beech or maple for oyster
Pot or drum For pasteurising straw — 100–200 litres; a big clay pot, a cauldron, or a pit lined with clay and filled with water heated by hot stones (Pottery, Cooking Without Pots)
Containers Woven sacks, baskets lined with leaves, wooden crates, clay pots, or any bags
Drill or auger A hand drill or brace and bit, 8–12 mm (Drills and Boring); or a sharp chisel or gouge
Wax Beeswax or tallow, melted, to seal holes in logs (Beekeeping)
A shady place Under trees, on the north side of a building, in a shed, cellar or cave
Water Clean. A tub large enough to soak logs.

Where to find it

Recognising oyster mushrooms in the wild

Oyster mushrooms (Pleurotus species) grow around the world, mostly in autumn and winter in temperate lands and after rains in the tropics. Learn them carefully: they are your source of spawn.

On dead hardwoodoverlapping shelves,caps 5–25 cm, grey, brown,cream or blue-grey Underneathwhite gills running down onto ashort, off-centre stem Spore printcap gills-down on paper,covered, 4–12 hours white to pale lilac Never on soil. Be suspiciousof any on conifer wood. No ring on the stemNo cup at the base Mild smell, sometimes of aniseed; firm white flesh If any one feature does not match, do not eat it and do not grow from it.
Fig. 1 The oyster mushroom: shelf-like caps in overlapping clusters on dead or dying hardwood; white gills that run down onto a short off-centre stem; no ring and no cup; a white to pale lilac spore print. Check every feature, every time.
  • On wood — dead or dying broad-leaved trees (beech, poplar, willow, oak, elm, maple), standing or fallen. Never on soil, and be suspicious of any on conifers.
  • Shape: shell- or fan-shaped caps, 5–25 cm across, in overlapping shelves like roof tiles. Grey, brown, cream, blue-grey or white; smooth, slightly greasy when wet.
  • Gills: white to cream, crowded, running down onto the stem (the gills continue down the stem instead of stopping at its top).
  • Stem: short, thick and off-centre or missing; whitish, often hairy at the base. No ring (skirt) on the stem and no cup at the base.
  • Smell: pleasant, mild, sometimes faintly of aniseed. Flesh white and firm.
  • Spore print white to pale lilac-grey. To make a spore print, cut off a cap, lay it gills-down on paper that is half white and half dark, cover it with a bowl, and leave it 4–12 hours. The spores drop in a powder pattern of their own colour.

Look-alikes: angel wings (thin, small, pure white, on conifer wood — have been linked to deaths in people with kidney disease); the jack-o'-lantern and ghost fungus (Omphalotus — orange in the northern hemisphere, cream and glowing faintly in the dark in Australia; they cause violent vomiting); Crepidotus (small, brown spore print); Lentinellus (saw-toothed gill edges, very bitter). If anything does not match — the wood, the gills, the spore print — do not eat it and do not grow from it.

Shiitake

Shiitake (Lentinula edodes) grows wild only in the forests of China, Japan and Korea, on fallen oak, chestnut and related trees. Elsewhere you can get it only from someone already growing it: a colonised log, a fresh mushroom, or spawn. It has a brown, often cracked cap 5–15 cm across, white gills that do not run down the stem, a tough, central to off-centre stem, and a white spore print.

Other materials

Getting spawn

You need living mycelium of a known mushroom. In order of ease:

1. Stem butts (oyster mushrooms). The tough base of a cluster of oyster mushrooms, where it joined the wood, is full of living mycelium.

  1. Cut a fresh, firm oyster cluster with its base. Trim off the caps (eat them); keep the bases.
  2. Tear corrugated cardboard (if you have any), clean paper, or a handful of pasteurised straw (below) into pieces; soak in boiled, cooled water and squeeze out until only a drip or two falls.
  3. In a clean crock, jar or bag, layer the damp material with thin slices of stem butt, pressing them together. Cover loosely (a little air), keep in the dark at 20–25 °C.
  4. In 2–4 weeks, white threads spread through the layers. When it is all white, this is your spawn. Use a quarter of it to start the next batch of spawn the same way.

2. Colonised wood. Find a log or stump fruiting with oyster mushrooms you have identified for certain. Cut or chisel out chunks of wood that are white and soft with mycelium, just under the mushrooms. Use them as plugs in fresh logs (below) or lay them between fresh logs.

3. Grain spawn (any mushroom, from a fresh mushroom). This is the professional method and needs clean work:

  1. Simmer grain (wheat, rye, millet, sorghum) for 15–20 minutes until swollen but not burst. Drain and let it steam dry until no water clings to the surface.
  2. Fill jars two-thirds full, plug the mouths with dry cotton wool or a cloth wad, and sterilise: in a pressure canner for 90 minutes (Canning and Bottling), or — without one — by steaming for an hour on three days in a row (each cooling lets heat-resistant spores sprout, and the next steaming kills them).
  3. In the stillest, cleanest place you have (a closed room, dust settled, surfaces wiped with boiled water or alcohol — Sterilising Instruments and Dressings), tear open a fresh, clean mushroom and with a flamed knife tip drop a few pieces of its inner flesh into each jar. Close the jar.
  4. Keep at 20–25 °C. In 2–4 weeks the grain turns white. Throw out any jar that shows green, black, pink, orange or slimy patches, or smells sour.
  5. One jar of grain spawn can inoculate 10 more jars, or 10–20 kg of straw.

The same steps, using a clear jelly of agar (Agar and Culture Plates) or gelatin (Gelatin) in dishes instead of grain, let you select and purify strains — see Culturing Microbes.

Method 1: Oyster mushrooms on straw

1. Chopstraw 5–10 cm 2. Pasteurise65–80 °C for 1 hour 3. Drain, mixspawn 5–10 % by weight 4. Spawn rundark, 20–25 °C 5. Fruitlight, air, mist on a block, witha sickle or scythe too hot to hold ahand in; keep it hot cool below 30 °C;squeeze: a few drops 2–3 weeks untilwhite all through pins in 3–10 days;2–3 flushes
Fig. 2 Oyster mushrooms on straw. Chopped straw is soaked in hot water, drained, mixed with spawn and packed into sacks; after two to three weeks of white growth, holes are opened and mushrooms grow out of them.
  1. Chop dry straw into pieces 5–10 cm long — with a sharp sickle on a block, or by running a scythe through a bundle (Sickle, Scythe and Hand Harvest Tools).
  2. Pasteurise: pack the straw into a sack or basket and sink it in water heated to 65–80 °C — too hot to hold a hand in for more than a second — for 1 hour. Keep the temperature up: a pot over a low fire, or add hot stones. (No fuel? Soak the straw for 12–18 hours in water with 3–5 g of slaked lime per litre (Lime); the alkaline water kills most competitors. Rinse once.)
  3. Drain and cool. Lift out and let it drain on a clean sloping board until it is cool (below 30 °C) and damp, not wet: a squeezed handful should give only a few drops.
  4. Mix in spawn: 5–10 % of the wet straw's weight (more is faster and safer: 1 kg of spawn to 10–20 kg of wet straw). Break up the spawn and mix it evenly, with clean hands.
  5. Pack firmly into sacks, baskets lined with large leaves, or bags — about 5–10 kg each. Tie the top. Make a dozen small slits or holes (1–2 cm) all round with a clean knife, for air.
  6. Spawn run: keep them in the dark or dim, at 20–25 °C, for 2–3 weeks. The straw turns white and knits into a solid block. A little yellow liquid on the surface is normal.
  7. Fruiting: when the block is white all through, move it (or open up the room) to dim light, fresh air and high humidity: a damp shed, cellar or shaded spot with the floor kept wet. Widen the holes to 3–5 cm. Sprinkle or mist the bags and the air 2–3 times a day, but don't soak the mushrooms.
  8. Pins (tiny mushrooms) appear at the holes in 3–10 days and grow to full size in another 4–7 days.
  9. Harvest when the caps are flattened out but before their edges turn up and begin to drop clouds of spores. Twist or cut the whole cluster off at the base.
  10. More flushes: keep the bags moist; a second and often a third flush follow every 2–3 weeks. Together they give 0.5–1 kg of fresh mushrooms per kilogram of dry straw used.

When the bags stop fruiting, the spent straw goes to the compost heap, the garden as mulch, or the animals.

Method 2: Shiitake and oyster mushrooms on logs

15 cm 5–8cm Spawn, sealed with wax Holes 8–12 mm wide in staggered rows; about 30–50 in a 1 m log, 10–15 cm thick wax cap 2.5–3cmdeep Spawn runcrib stack, off the ground,in deep shade: 6–12 monthsfor shiitake, 3–6 for oyster To fruit shiitakesoak 12–24 h in cold water;mushrooms 7–10 days later
Fig. 3 Inoculating logs. Holes are drilled in a staggered diamond pattern about 15 cm apart along the log, filled with spawn and sealed with wax. The logs are stacked in shade for the spawn run, then soaked in cold water to make them fruit.

Logs take longer to start, but then fruit for years with almost no work.

  1. Cut logs in the dormant season from healthy, living trees: oak is the best for shiitake (also chestnut, hornbeam, beech, alder, sweetgum); poplar, willow, alder, birch, beech or maple for oyster. 8–20 cm thick (10–15 cm is easiest), about 1 m long. Leave the bark undamaged — it holds the moisture in.
  2. Rest them 2–4 weeks in shade, off the ground, so the living wood's own defences die down — but inoculate within 6 weeks of cutting, before wild fungi move in.
  3. Drill holes 8–12 mm wide and 2.5–3 cm deep, in rows along the log: holes 15 cm apart along each row, rows 5–8 cm apart around the log, staggered so the holes make a diamond pattern. A 1 m log 12 cm thick takes about 30–50 holes.
  4. Fill each hole firmly with spawn: grain or sawdust spawn pressed in with a stick, wooden pegs soaked in spawn, or plugs of colonised wood.
  5. Seal each hole and the cut ends of any damaged bark with melted beeswax or tallow, dabbed on with a brush or rag. This keeps the spawn moist and keeps out insects and wild fungi.
  6. Stack in shade — under trees, behind a north wall, under a roof of brushwood — off the ground on a layer of stones or branches. Criss-cross them in a crib (log cabin) stack or lean them against a rail. 70–80 % shade: dappled forest shade is ideal.
  7. Keep moist. If no rain falls for 2 weeks, soak or sprinkle the logs. Logs should never dry right out (cracks in the end grain and bark peeling are warnings) or sit waterlogged.
  8. Wait. The spawn run takes 6–12 months for shiitake and 3–6 months for oyster on soft woods. It is done when the cut ends show white patches or a white ring of mycelium, and the wood smells mushroomy. Sometimes the first mushrooms appear on their own after heavy rain.
  9. Fruiting shiitake ("shocking"): soak the logs in cold water — a stream, pond or tub, 5–10 °C colder than the air — for 12–24 hours. Stand them upright, leaning against a rail, in humid shade. Pins appear in 3–7 days; mushrooms are ready 7–10 days after soaking.
  10. Rest each log 6–8 weeks between soakings. With a few groups of logs soaked in turn, you can harvest every week or two through the warm half of the year.
  11. Oyster logs usually fruit by themselves in autumn after rains and cold nights; soaking helps too.

A shiitake log typically gives 1–2 kg of fresh mushrooms over a life of 3–6 years (longer for thick oak logs, shorter for thin soft logs). Twenty logs keep a family in mushrooms.

Harvesting, storing and cooking

  • Pick by twisting the whole cluster or mushroom off at the base, or cutting with a clean knife. Pick shiitake when the cap is 70–90 % open, edges still curled under.
  • Use fresh mushrooms within 3–5 days, kept cool, in a basket or cloth — not airtight, or they turn slimy.
  • Dry them for winter: slice and spread on racks in the sun or near a fire, or thread on strings, until crisp and brittle (see Preserving Food). Dried shiitake keep a year or more and have even more flavour. Soak 20–30 minutes before cooking. Mushrooms dried in sunlight, gills up, gain a large amount of vitamin D — useful in dark northern winters (Nutrition and Deficiency Diseases).
  • Always cook them. Raw oyster mushrooms upset some stomachs; raw or undercooked shiitake cause an itchy, whip-like rash in a few people ("shiitake dermatitis").

How to tell it worked

  • Spawn and substrate turn evenly white, firm, and smell fresh and mushroomy, like raw button mushrooms.
  • Pins appear at the holes or bark within days of the fruiting trigger, and grow into firm, clean mushrooms with the same features as the parent: same colour, same gills, same spore print.
  • Logs show white rings in their ends after the spawn run and fruit after soaking.

Note Troubleshooting. Green, black, pink or orange patches; sour or rotten smell → contamination by moulds or bacteria. Straw too wet, not pasteurised hot enough or long enough, too little spawn, or dirty hands and containers. Throw contaminated bags far from your growing area, and next time drain the straw better and use more spawn. White growth stalls halfway → too cold, too dry, or competitors. Move somewhere warmer; check moisture. Mushrooms with long thin stems and tiny caps → not enough fresh air (too much carbon dioxide). Ventilate more. Pins appear then dry up and turn yellow or brown → air too dry, or a draught blowing on them. Mist more often, shelter from wind and sun. Logs never fruit → logs from dead or diseased trees, inoculated too late, dried out, or too much sun. Keep logs shaded and moist, and be patient: shiitake may take more than a year. Tiny flies around the bags → fungus gnats; harmless to people but their larvae eat mycelium. Cover with fine cloth, keep the area clean, remove spent substrate promptly.

Dangers

Danger Never eat a wild fungus you have not identified with complete certainty. A few common mushrooms kill: the death cap and destroying angels (white gills, a ring on the stem and a cup at the base, on soil near trees) cause about nine out of ten mushroom deaths, and their poison shows no symptoms for 6–24 hours, by which time the liver is failing. Cooking, drying and boiling do not destroy it. Mushroom poisoning has no reliable "test" — not silver spoons, not peeling, not animals eating them, not the universal edibility test (Foraging Wild Food). Grow your mushrooms from spawn you are sure of, and check every harvest: if something different appears on your logs or straw, throw it away.

  • Contamination of your crop. Occasionally a wild fungus fruits from your logs or straw. Learn your crop's features, compare every flush, and discard anything that does not match.
  • Spores in the lungs. Picking large amounts of oyster mushrooms indoors, especially if caps are left to release spores, causes coughing, fever and long-term lung inflammation ("mushroom worker's lung"). Harvest before caps release spores, ventilate well, and wear a cloth over nose and mouth in a closed growing room.
  • Hot water and fire when pasteurising; lime water stings eyes and skin — wear eye protection (Lime).
  • Lifting and drilling logs: wet oak logs weigh 15–25 kg each.

What this unlocks

Mushrooms turn Forestry and Tree Nurseries and farm waste into food and compost and fit any corner of the farm: logs under the orchard trees (Fruit Trees and Orchards), straw bags in the cellar or the shade of a barn. The clean culture methods used for grain spawn — sterilising, working in still air, picking out contaminated jars — are the same as those for brewing yeast (Fermentation) and for growing medicines such as Penicillin (Culturing Microbes). Spent mushroom compost improves heavy soils (Understanding Soil), and the oyster mushroom's ability to digest straw and wood is a first step towards turning plant waste into animal feed.

How it was first done

People have gathered wild mushrooms since before history; the "Iceman" who died in the Alps about 5,300 years ago carried birch polypore and tinder fungus (Fire). Cultivation began in China: by about AD 600 wood-ear mushrooms were being grown on logs, and shiitake cultivation in the mountains of Zhejiang province is recorded from the Song dynasty, credited by legend to a woodsman named Wu San Gong, who found that cutting and beating logs made them fruit. Japanese growers cut oak logs and placed them near fruiting ones to catch spores — a slow, chancy method until Kisaku Mori developed pure-culture wooden spawn plugs in the 1940s.

In Europe, melon growers around Paris began growing button mushrooms on horse manure in the 17th century, and later moved into the cool limestone quarries and catacombs under the city. Oyster mushrooms were first deliberately cultivated in Germany during the First World War, on logs and stumps, as a source of food in a time of hunger — exactly the situation this book is written for.

Source: content/entries/food/mushroom-growing.md