◆ Rebuild

Part 12 · Transport

Jet Engines

Squeeze air, burn fuel in it, and let the hot gas spin a turbine that drives the squeezer, then blow the rest out of the back. How the compressor, combustion chamber and turbine work together in turbojets, turbofans, turboprops and power-station gas turbines; how each part is really made; the heat-resisting nickel alloys they cannot do without; and the honest path from a turbocharger on a bench to an airliner engine.

Difficulty
●●●●●
Time
Months for a bench gas turbine built round a turbocharger; decades and a whole metals industry for a flight engine
Steps from zero
38 prerequisites →

You need first

Gliders and AeroplanesThe Steam TurbineAlloy and Stainless Steels

This unlocks

Spaceflight and Spacecraft
The full path from nothing — 38 steps before this one
  1. Stone Tools
  2. Cordage and Rope
  3. Fire
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Basic Woodworking
  7. Hunting and Trapping
  8. Charcoal
  9. Pottery
  10. The Kiln
  11. Spinning and Weaving Cloth
  12. Hides and Leather
  13. Bricks
  14. Fermentation
  15. The Wheel and Axle
  16. Firebrick and Refractories
  17. Bellows
  18. Distillation
  19. The Lathe
  20. Gears
  21. Iron (the Bloomery)
  22. Copper Smelting
  23. The Waterwheel
  24. Blacksmithing
  25. The Blast Furnace and Cast Iron
  26. Magnets
  27. Steel
  28. The Steam Engine
  29. Copper Wire
  30. Steel in Quantity
  31. Machine Tools
  32. Petroleum and Refining
  33. The Generator
  34. The Electric Arc Furnace
  35. The Internal Combustion Engine
  36. The Steam Turbine
  37. Alloy and Stainless Steels
  38. Gliders and Aeroplanes
  39. Jet Engines

Do them roughly in this order. See it on the tech tree →

Why it matters

A piston engine (The Internal Combustion Engine) works in pulses, and every part must stop and start thousands of times a minute. A gas turbine does the same four jobs — breathe, squeeze, burn, exhaust — all at once and without stopping, in four places along one spinning shaft. Nothing goes back and forth, so it can be made enormous, runs smoothly for tens of thousands of hours, and gives far more power for its weight than any piston engine.

That changed the world. Piston airliners crawled across oceans at 400–500 km/h, shaking, with frequent engine failures. Jet airliners cruise at 850–900 km/h at 10–12 km height, above most weather, and an engine failure in flight is now so rare that most pilots never see one. The same machine, standing on the ground, drives generators in power stations that can start in minutes when demand jumps (Power Lines and Distribution), pumps Natural Gas and Helium down pipelines, and powers ships, helicopters and the turbopumps of rockets.

The idea is older than the aeroplane. What held it back for forty years was heat: the turbine must spin red-hot, at the edge of what any metal can bear. A jet engine is a test of a whole society's metallurgy, machining and quality control.

How it works

Suck, squeeze, burn, blow

Follow a parcel of air through the engine.

  1. Intake. Air is drawn in through a smooth, rounded mouth.
  2. Compressor. Rows of spinning blades squeeze it to several times — in a modern engine, 30 to 50 times — the pressure of the outside air. Squeezing air also heats it: at 40 times pressure it leaves the compressor at about 600 °C without any fire at all.
  3. Combustion chamber. Fuel — kerosene, the lamp oil of Petroleum and Refining — is sprayed in and burns continuously, like a blowtorch inside a can. The gas gets far hotter, so it expands, but the pressure stays about the same.
  4. Turbine. The hot, high-pressure gas rushes through rows of blades on a wheel, exactly like steam in a The Steam Turbine, and spins it. The turbine is on the same shaft as the compressor and drives it.
  5. Nozzle. The gas still has pressure and heat left over. It is allowed to expand through a narrowing pipe and leaves the back of the engine at high speed — 400 to 600 m/s in a plain jet.
Intake smooth mouth Compressor blades squeeze the air Combustion chamber fuel burns in flame tubes Turbine spun by hot gas Nozzle fast jet out Shaft joins turbine to compressor Fuel spraykerosene mist 1 bar, 15 °C 4 bar, 190 °C 4 bar, 800 °C 2 bar, 620 °C jet about 550 m/s
Fig. 1 A turbojet in cutaway. Air is squeezed by the compressor, burned with fuel in the combustion chamber, and drives the turbine, which turns the compressor through a shared shaft. What energy is left leaves the nozzle as a fast jet. The numbers are typical of a simple early engine.

The trick: hot gas expanding gives more work than cold air needs to be squeezed. Heated, each kilogram of air swells to two or three times its volume, and expanding it back to outside pressure returns far more work than compressing it took. The turbine keeps just enough to drive the compressor — half to two-thirds of what it could deliver — and the rest is yours, as a fast jet or as power on a shaft.

Why hotter and tighter is better

Two numbers decide how good a gas turbine is.

  • Pressure ratio — how many times the compressor squeezes the air. The more it squeezes before burning, the more of the fuel's heat becomes work. Even a perfect engine turns only about a third of its fuel into work at a pressure ratio of 4, half at 10, and two-thirds at 40. Real engines of the 1940s managed 12–18%; the best today, 40% and more.
  • Turbine entry temperature — how hot the gas is when it hits the first turbine blades. The hotter, the more work each kilogram of air gives, so the smaller and lighter the engine for a given power. Early engines ran at about 750–850 °C. Modern ones run at 1,500–1,700 °C — hotter than the melting point of the blades, which survive only because cool air is blown through them and over them.

Where the push comes from

A jet engine pushes the aeroplane forward by throwing air backwards, the same reaction as a rocket (Helicopters, Rockets and Submarines (Overview)) — but it takes its "throwing mass" from the air instead of carrying it. The push, called thrust, is:

Thrust = mass of air per second × (speed the jet leaves − speed the aeroplane flies)

You can get the same thrust by throwing a little air very fast or a lot of air gently. Throwing a lot of air gently wastes much less energy — the same lesson as the Wrights' big slow propellers in Gliders and Aeroplanes. That is why the plain jet has been replaced, on almost every aeroplane, by engines that move more air: the turbofan and the turboprop.

The family of gas turbines

Turbojet all thrust from a fast, hot jet Turbofan a big fan blows most air round the core: quieter, half the fuel bypass bypass Turboprop turbine turns a propeller through a gearbox gearbox weak jet Gas turbine a free turbine drives a generator or pump Generator exhaust to boiler compressor burner turbine
Fig. 2 Four ways to use the same hot core. A turbojet uses only its jet. A turbofan uses part of the turbine's power to drive a big fan that blows extra air around the core. A turboprop uses nearly all of it to turn a propeller through a gearbox. A shaft turbine on the ground drives a generator or pump instead.

Turbojet

The simplest jet: compressor, combustion chamber, turbine, nozzle. All the thrust comes from the hot jet. It is light and simple and works well at very high speeds, but it is noisy and thirsty at the speeds airliners fly. A turbojet of the 1940s was about 1 m across, weighed 300–900 kg, and gave 4–9 kN of thrust (the push needed to hold up 400–900 kg).

Its compressor comes in two kinds:

  • Centrifugal — one wheel, like a pump impeller, that flings air outwards into a ring of diverging passages (the diffuser) where it slows down and its pressure rises. Rugged, short, easy to make, with a pressure ratio of about 4 in one stage, but fat for its power. Whittle's engines and most small gas turbines use it.
  • Axial — many rows of small blades on a drum, each row followed by a row of fixed blades (stators) that straighten the flow. Each row raises the pressure only 15–40%, but you can line up 10–15 rows and squeeze 20–40 times in a slim engine. The blades are small wings (Gliders and Aeroplanes); pushed too hard, they stall, and the air rushes backwards with a bang — surge — which can wreck the engine.

Turbofan

A turbofan is a turbojet whose turbine also drives a large fan at the front. Most of the fan's air goes around the hot core in a duct and out of the back, cool and relatively slow; only a small part goes through the core. The ratio of air around to air through is the bypass ratio: about 1 in the first turbofans of around 1960, 5–6 in the engines of most airliners, and 10–12 in the newest. A big turbofan has a fan 2–3 m across, moves 500–1,500 kg of air a second, gets about four-fifths of its thrust from the fan, and burns roughly half the fuel of a turbojet for the same thrust. So that the fan can turn slowly while the core spins fast, the engine has two or three shafts, one inside the other, each joining a compressor section to its own turbine.

Turboprop

A turboprop puts nearly all of the turbine's spare work into a shaft, which turns a propeller through a reduction gearbox of about 10–15 to 1, because the turbine spins far faster than any propeller can. It is the most fuel-thrifty way to fly below about 650 km/h, so it is used on short routes and cargo planes. The same arrangement, driving a rotor instead of a propeller, is the turboshaft of a helicopter.

Gas turbine (on the ground)

A gas turbine in a power station, on a pipeline or in a ship is a turboshaft built heavy and long-lived instead of light. It drives a The Generator directly at 3,000 or 3,600 turns a minute, or through gears. On its own it turns 30–40% of its fuel into electricity. Its exhaust leaves at 500–600 °C, still hot enough to raise steam in a boiler (Boilers and Pressure Vessels) for a The Steam Turbine; such a combined cycle station turns about 60% of its fuel into electricity, the best of any heat engine. It starts in minutes, so the grid uses it to cover sudden peaks, burning Natural Gas and Helium, diesel, or cleaned Biogas and Wood Gas.

How a jet engine is really built

Each of the main parts is a separate craft. Here is what each is, what it is made of, and how a factory makes it.

The compressor

  • Centrifugal impellers are machined from a single forged block of Aluminium alloy (for small, cool engines) or Titanium, on a five-axis milling machine (Machine Tools, CNC Machines and 3D Printing). The tips move at 400–500 m/s, faster than sound, so the wheel must be flawless, polished, and balanced to within a few hundredths of a gram.
  • Axial blades in the front, cooler stages are forged and machined from titanium alloy (about 6% aluminium, 4% vanadium), which is as strong as steel at little more than half the weight. Big fan blades are hollow titanium or carbon-fibre composite; the hot rear stages are nickel alloy. Each blade's dovetail root slides into a slot in a forged disc, and tip gaps are kept to fractions of a millimetre, because air leaking round the tips is work lost.

The combustion chamber

Swirler spins air round the fuel Primary zone eddy holds the flame, ~2,000 °C Secondary and dilution holes more air finishes burning, then cools Fuel spray nozzle kerosene under pressure Cooling film air sliding along the inside wall Outer casing and flame tube nickel–chromium sheet, 1–1.5 mm To turbine Air from compressor (blue): about a quarter feeds the flame; the rest finishes burning, cools the gas and shields the wall.
Fig. 3 Inside the combustion chamber. Only about a quarter of the air enters the swirler at the front and burns with the fuel at around 2,000 °C. The rest enters through rows of holes along the flame tube, first to finish the burning and then to cool the gas, and a film of air sliding along the inside wall keeps the metal from melting.

The problem: kerosene burns properly only when mixed with about 15 times its weight of air, which makes a flame of about 2,000 °C. No turbine survives that. So the engine passes 50–60 times as much air as fuel overall, and only lets about a quarter of it into the flame. The flame tube (or liner) is a perforated can inside an outer casing:

  • At the front, a fuel spray nozzle atomises the kerosene, and a swirler — a ring of angled vanes — spins the air around it, making a slow eddy that holds the flame in place like the calm water behind a rock in a stream. Without it, the flame blows out.
  • Along the tube, rows of larger holes let in more air to finish the burning (secondary air), then still more to dilute and cool the gas down to what the turbine can bear (dilution air).
  • Thousands of tiny holes or overlapping louvres let a film of cool air slide along the inside of the wall, so the metal never touches the flame.

Liners are nickel–chromium sheet 1–1.5 mm thick, rolled, pressed and welded (Sheet Metal and Rolling, Welding), with punched or laser-cut holes. Early engines had 8–14 separate cans round the shaft; modern ones, one ring-shaped (annular) chamber. A spark plug (The Induction Coil) lights it; then the flame keeps itself going.

The turbine — the heart of the problem

The first row of turbine blades sits right behind the combustion chamber in gas at well over 1,000 °C, and spins so fast that each blade pulls on its root with the force of many tonnes. A metal held hot and under load slowly stretches like toffee; this is creep, and it is what kills turbine blades. If a blade stretches a few tenths of a millimetre it rubs the casing; if it breaks, it can destroy the engine.

Superalloys. The answer is a family of nickel-based alloys: nickel (Nickel and Cobalt) with 10–20% chromium for resistance to scaling, cobalt, tungsten and molybdenum to stiffen the metal, and a few percent of aluminium and titanium. Heat-treated, the aluminium and titanium form billions of tiny cubes of a hard nickel–aluminium compound that lock the metal's structure and, unusually, get stronger as they warm, up to about 800 °C. The first such alloy, Nimonic 80, was invented in Britain in 1941 for Whittle's engines: roughly 75% nickel, 20% chromium, with 2–3% titanium and 1–2% aluminium. Modern blade alloys add tantalum, rhenium and hafnium, some of the rarest metals mined. These alloys must be melted and poured in a vacuum furnace, because the aluminium and titanium would otherwise burn away into the air.

Investment casting. Turbine blades are far too hard and complicated to machine. They are cast by the lost-wax method (Metal Casting, Jewellery, Beads and Medals):

  1. A ceramic core shaped like the blade's internal cooling passages is moulded from fine silica and alumina and fired (Firebrick and Refractories).
  2. Wax is injected around the core in a steel die, making a perfect wax blade with the core inside.
  3. Wax blades on a wax tree are dipped again and again in ceramic slurry and grit, building a shell 6–10 mm thick. The wax is steamed out and the shell fired.
  4. The superalloy is melted in vacuum at about 1,450–1,550 °C and poured into the hot shell.
  5. For the best blades, the mould is lowered slowly — a few centimetres an hour — out of the hot furnace onto a chilled copper plate, so the metal freezes from the bottom up. A small corkscrew passage at the bottom lets only one grain through, and the blade grows as one single crystal, with no grain boundaries for creep to work along.
  6. The shell is broken off, the core is dissolved out in hot caustic soda (Lye and Potash), and the root is ground to shape (Precision Grinding).

Cooling and coating. Compressor air (500–700 °C — cool, by comparison) runs up through the root and winding passages inside the blade, then out through holes 0.3–0.8 mm wide, drilled by laser or spark erosion, which spread a cool film over the surface. A sprayed ceramic thermal barrier coating of zirconia, a few tenths of a millimetre thick, keeps the metal a hundred degrees or more cooler still.

The whole blade Tip Film holes 0.3–0.8 mm Inside passages winding Platform Fir-tree root locks into the disc Cooling air from compressor Cut across hot gas 1,500 °C Ceramic coat zirconia, 0.2–0.5 mm Cooling air in passages Nickel-alloy wall one crystal, ~1,000 °C
Fig. 4 A modern cooled turbine blade, cut across. Cool air from the compressor enters through the root and runs through passages inside the blade, then leaves through rows of tiny holes that spread a cool film over the surface. A thin ceramic coat insulates the metal, and the fir-tree root locks the blade into the disc against the pull of spinning.

Shafts, bearings and the rest

The shafts run in oil-fed ball and roller bearings. Discs are forged from nickel alloy or titanium, checked by ultrasound and X-Rays for hidden flaws, and balanced (The Steam Turbine). A fuel control — once a mechanical governor, now a computer — meters fuel so the engine accelerates without surging or overheating, and a starter spins it to about a quarter of running speed before fuel is lit.

What a rebuilt society needs first

A flight engine needs all of these, at once:

Need From
Nickel, chromium, cobalt, molybdenum, tungsten in quantity Their ores and electrolytic refining (Nickel and Cobalt, Alloy and Stainless Steels)
Aluminium and titanium Aluminium, Titanium
Vacuum melting and investment casting The Vacuum Pump, The Electric Arc Furnace, Metal Casting, Firebrick and Refractories
Precision forging, machining, grinding, balancing Machine Tools, Precision Grinding, Precision and Interchangeable Parts
Hidden-flaw inspection X-Rays, ultrasound, Detecting Radiation
Clean, consistent kerosene Petroleum and Refining refining
Aerodynamics and stress calculations Calculus, Strength of Materials, wind tunnels (Gliders and Aeroplanes)
A test bed and the patience for thousands of hours of running Organisation

The honest summary: a rebuilt society that can make good Alloy and Stainless Steels and run a The Steam Turbine power station can build a stationary gas turbine running at modest temperature. A useful flight engine needs nickel superalloys and a precision industry on the scale of the 1940s. The single-crystal, film-cooled engine of an airliner needs the whole modern world.

The stepping stones

Take them in order. Each one teaches what the next needs.

  1. Turbines with steam. The small impulse turbine in The Steam Turbine teaches nozzles, blades, balancing and fast bearings without fire.
  2. A centrifugal blower with curved blades in a spiral casing, belt-driven (Bellows to Air Compressors). Pressure rises with the square of tip speed: double the speed, four times the pressure. This is your compressor.
  3. A turbocharger on a piston engine (Rotary Compressors and Turbochargers). A turbocharger is a gas turbine without its own burner: a turbine wheel in the exhaust of an The Internal Combustion Engine engine drives a centrifugal compressor that blows extra air into the cylinders. Exhaust is only 600–850 °C, so the turbine wheel can be cast from heat-resisting steel (about 25% chromium, 20% nickel) and the compressor wheel from aluminium alloy, running on oil-fed bronze sleeve bearings at 50,000–150,000 turns a minute. Here you learn to cast, machine and balance tiny fast wheels.
  4. A bench gas turbine. Give the turbocharger its own combustion chamber, in outline: a flame tube of heat-resisting steel sheet with rows of holes, inside an outer casing, taking all the compressor's air and returning it to the turbine inlet. Start it by blowing air into the compressor with a blower, light a gas flame from a spark, and slowly increase the fuel until the engine runs on its own and the starting air can be removed. It gives little useful power, but it proves you can make a gas turbine self-sustaining — the way many amateurs and engineering schools have learned. In the 1980s the German model-maker Kurt Schreckling built tiny working jet engines at home, with compressor wheels of plywood and carbon fibre and turbine wheels cut from heat-resisting steel sheet.
  5. A power gas turbine. Add a second, separate free turbine after the first, on its own shaft, to drive a The Generator or pump. Keep the turbine entry temperature low — below about 650 °C for good austenitic steels — and accept modest efficiency. The first power-station gas turbine (1939) ran at about 550 °C and still turned 17% of its fuel into electricity.
  6. A flight turbojet. Only now: nickel alloys, centrifugal compressor, can-type combustion chambers, a single-stage turbine — Whittle's layout. Ground-test for hundreds of hours before anything is put in an airframe.
  7. Turboprop and turbofan. Add a gearbox, or a fan and a second shaft. Then axial compressors, cooled blades, and the long climb to modern engines.

How to tell it worked

  • Self-sustaining. Remove the starting air: the engine keeps running and accelerates as you add fuel. If it slows and stops as soon as the starter is removed, the compressor or turbine is not good enough, or air is leaking.
  • Exhaust colour and temperature. The turbine casing and exhaust pipe should show no glow or, at most, a dull red in the dark (about 550–650 °C). A bright cherry-red glow, or flames coming out of the exhaust, means too much fuel and too much heat at the turbine.
  • Steady sound. A smooth, rising whine. Popping or rumbling through the intake is surge.
  • Thrust or power. Hang a small engine on a pendulum or on a cart pulling a spring balance (Balances, Steelyards and Weighing Machines): measure thrust directly. For a power turbine, load the generator with lamps or heaters and measure the electrical output (Measuring Electricity).
  • Run-down. After the fuel is cut, the engine coasts smoothly for many seconds without grinding.

Note Troubleshooting. Will not run on its own: leaks between compressor and turbine, a turbine nozzle area that does not match the compressor, or a compressor too inefficient — the margin is small, so every loss counts. "Hot start" — flames from the exhaust on lighting: too much fuel before the engine is turning fast enough; cut the fuel, keep blowing, try again with less. Banging and air puffing out of the intake (surge): fuel added too fast, or the turbine nozzle too small; accelerate more gently. Turbine glowing bright red: too much fuel or a poorly mixed flame; the dilution holes may be too few. Rising vibration: imbalance or a bearing failing — shut down at once.

Dangers

Danger A bursting wheel is a bomb. A turbine or compressor wheel at 50,000–100,000 turns a minute stores enough energy to hurl fragments through steel sheet and through a person. Never stand in line with the spinning wheels (the "plane of rotation"). Run every test engine inside a thick steel ring or behind a wall of sandbags or earth, controlled from the side. Real engines have containment rings that must catch a broken blade.

Danger Fire, fuel and burns. Unburned fuel pooling in a cold engine ignites with a whoosh on the next start. Keep fuel lines short, tight and away from hot parts; keep a fire extinguisher and sand at hand. Exhaust pipes stay hot enough to burn skin for many minutes after shut-down.

  • Intake suction pulls in rags, hands and clothing: fit a wire guard and keep clear of the front.
  • Noise of 120–140 dB close up causes permanent deafness: wear ear protection.
  • Exhaust contains carbon monoxide and is hotter than it looks a metre behind the nozzle: run only outdoors.
  • Flight. A working turbojet is not a flying machine. Everything in Gliders and Aeroplanes about the safe order of work applies with greater force at jet speeds.

What this unlocks

The jet airliner, fast air freight and airmail; turboshaft helicopters; gas-turbine and combined-cycle power stations on the Power Lines and Distribution; pipeline compressors for Natural Gas and Helium; ship propulsion. The turbopumps that feed liquid-fuelled rockets are small gas turbines, so this chapter is a step towards Spaceflight and Spacecraft. The materials science it demands — superalloys, single crystals, ceramic coatings, inspection — feeds back into every other high-temperature industry.

How it was first done

In 1791 the Englishman John Barber patented a gas turbine on paper. In 1903 the Norwegian Ægidius Elling built the first that gave out more power than its own compressor needed — about 8 kW net. Others failed for decades: compressors too inefficient, metals too weak.

In 1930 Frank Whittle, a young British Royal Air Force officer, patented the turbojet. Starved of money, he ran his first engine on a test bed in April 1937. In Germany, Hans von Ohain, working independently with the aircraft maker Heinkel, built an engine that flew first, in the Heinkel He 178 on 27 August 1939. Whittle's engine flew in the Gloster E.28/39 on 15 May 1941. Both used centrifugal compressors. In 1939 the Swiss firm Brown Boveri installed the first power-station gas turbine, at Neuchâtel: 4 MW at about 17% efficiency. The Nimonic alloys developed for Whittle's engines proved decisive: German engine makers, short of nickel and cobalt, built engines whose turbines lasted only tens of hours.

The first jet airliner, the British de Havilland Comet, entered service in 1952; the Boeing 707 followed in 1958 and made jet travel ordinary. Rolls-Royce's Conway of about 1960 was the first bypass engine in service, and the high-bypass turbofans of the late 1960s — the General Electric TF39 and the Pratt & Whitney JT9D that powered the first Boeing 747 in 1970 — set the pattern of every airliner since. Directionally solidified blades entered service in the late 1960s and single-crystal blades in the early 1980s, and turbine temperatures have climbed by roughly 10 °C a year ever since.

Source: content/entries/transport/jet-engines.md