Part 13 · Electricity
The Telephone
Carry the human voice along a wire. A magnet, a coil and a thin iron disc make an earpiece; a pinch of carbon grains makes a microphone. With a battery, a bell and a pair of wires, two houses — or a whole village through a switchboard — can talk.
- Difficulty
- ●●●●●
- Time
- A day for a pair of magnet telephones; a week or two for full sets with bells; a season for a village exchange
- Steps from zero
- 19 prerequisites →
You need first
The TelegraphThis unlocks
Loudspeakers, Microphones and HeadphonesNetworks and the InternetRadioRecording SoundThe Automatic Telephone ExchangeThe full path from nothing — 19 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Hunting and Trapping
- Basic Woodworking
- Charcoal
- Pottery
- Hides and Leather
- Fermentation
- Bellows
- Copper Smelting
- Iron (the Bloomery)
- Blacksmithing
- The Battery
- Copper Wire
- The Electromagnet
- The Telegraph
- The Telephone
Do them roughly in this order. See it on the tech tree →
Why it matters
The The Telegraph needs a trained operator at each end and a code to learn. The telephone needs neither: anyone who can speak can use it, at once, in their own words, with their own voice. A doctor can be talked through an emergency (Emergencies); a mill can be told the river is rising; a family can hear each other across a valley. It is also the beginning of a much larger story: the microphone and earpiece of this chapter become the voice of Radio, of Recording Sound, and, sent as data, of computer networks.
The first working telephone in this chapter needs no battery at all: two magnets, two coils, two thin iron discs and a pair of wires. Build that first. It will convince you that it works, and every later improvement builds on it.
How it works
Sound is a quick back-and-forth trembling of the air — a few hundred to a few thousand times a second for speech. Put a thin, springy disc (a diaphragm) in front of your mouth and it trembles in step with your voice.
The earpiece (receiver)
A permanent magnet holds a thin iron diaphragm pulled slightly towards its pole. Around the pole is a coil of fine wire. A current in the coil adds to or subtracts from the magnet's pull, so a current that varies with a voice makes the diaphragm tremble with the same voice — and you hear it.
The magnet is essential. Without it, a current flowing either way would pull, and the diaphragm would tremble at twice the right frequency, garbled. The magnet makes the pull stronger for one direction of current and weaker for the other.
The same device works backwards
Speak into the earpiece and the trembling diaphragm changes the magnetism through the coil, which induces a tiny current, just as in the The Generator. That current, sent along a wire to a second earpiece, makes it speak. Two identical earpieces are a complete telephone. This is Alexander Graham Bell's telephone of 1876–77. Its weakness: all the energy comes from your voice, so it is faint and works only over a few kilometres.
The carbon microphone
Carbon conducts electricity, but loose grains of it conduct better when pressed together and worse when loosened, because they touch at more points or fewer. Put a pinch of hard carbon grains between a fixed carbon plate and a carbon plate fixed to a diaphragm, and pass a current from a battery through them. Your voice presses and releases the grains hundreds of times a second, and the current swells and shrinks in step. Your voice now only controls the current; the battery supplies the energy. The carbon microphone gives a far louder signal than the magnet telephone — it is in fact an amplifier, the only one there was until the The Vacuum Tube.
The induction coil
The microphone works best in a short, low-resistance circuit with its battery. A long line has a high resistance. To match them, the microphone circuit goes through the primary (a few turns of thick wire) of a small The Transformer called the induction coil, and the secondary (many turns of thin wire) sends the voice out along the line at a higher voltage. This was the change that made the telephone useful over tens of kilometres.
What you need
| Item | For two complete sets | Notes |
|---|---|---|
| Steel bar magnets | 2–4 bars, 10–12 cm × 1 cm × 0.5–1 cm, hardened and strongly magnetised | Magnets, Steel |
| Soft iron | Short rods 1 cm thick for pole pieces; iron wire for induction coil cores | Iron (the Bloomery), annealed |
| Fine covered copper wire | 300–500 m of 0.2–0.3 mm; 50 m of 0.6 mm | Copper Wire; silk or shellac covered |
| Thin iron sheet | Discs 5–6 cm across, 0.2–0.3 mm thick | Sheet Metal and Rolling; tinplate is ideal (Tin and Pewter) |
| Hard carbon | A few grams of grains, two small polished plates or blocks | From anthracite, arc-lamp carbons or graphite (below) |
| Batteries | 2 cells per set (about 2–3 V) | The Battery |
| Bells and ringing | A bell or buzzer per set; or a hand magneto per set | The Electromagnet, The Generator |
| Hardwood | Cases, mouthpieces, bases | Basic Woodworking, The Lathe |
| Line wire | Two wires the length of the line, or one wire and earth plates | As for the The Telegraph |
Where to find it
- Hard carbon. Ordinary wood Charcoal is too soft and too poor a conductor. Better carbons:
- Anthracite, the hardest, shiniest black coal (Coal and Coke): crush it, sieve out grains about the size of coarse sand (0.2–0.5 mm), and roast them in a sealed clay crucible at bright red to orange heat (900–1,000 °C) for an hour or two. Let it cool sealed. This drives off the volatile matter and makes them conduct well. Grains of this kind filled most of the world's telephone microphones for a century.
- Arc-lamp carbons (see The Light Bulb) or gas carbon, the hard, ringing crust that builds up inside retorts where coal is heated to make gas: saw into blocks and file flat, or crush into grains.
- Graphite (see The Light Bulb and the materials list): soft, but fine for the blocks of a Hughes microphone.
- Mica for the microphone's sealing washer: thin clear sheets peeled from mica crystals in granite and pegmatite (see the materials list).
- Diaphragm iron: the thinner and flatter, the better. Hammer or roll soft iron sheet to 0.2–0.3 mm (Sheet Metal and Rolling), anneal, and flatten between boards. Tinned iron (tinplate) resists rust.
Method 1: Two magnet telephones (no battery)
- Magnet: take a hardened steel bar 10–12 cm long, magnetise it strongly (Magnets).
- Pole piece: fix a short soft iron rod (1 cm thick, 3 cm long) to one end of the magnet with a binding of wire, so the magnetism flows into it. File its tip flat and smooth.
- Coil: on a paper and card bobbin around the pole piece, wind 1,000–2,000 turns of 0.2–0.3 mm covered wire, giving roughly 20–80 Ω. Varnish it (Copper Wire). Bring the two ends out to terminals.
- Case: turn or carve a hardwood case — a handle with a hole bored lengthways for the magnet, and a round head 7–8 cm across. Inside the head, the pole piece stands with its tip just below the face.
- Diaphragm: an iron disc 5–6 cm across and 0.2–0.3 mm thick, clamped all round its edge between the head and a wooden cap. The cap has a hole 1.5–2 cm across in the middle, shaped like a shallow funnel (the mouthpiece and earpiece in one).
- Set the gap: the gap between the pole tip and the diaphragm should be about 0.3–0.5 mm. Make the magnet slide in the handle with a screw at the back to adjust it. Too close and the diaphragm sticks to the pole; too far and the sound is faint.
- Make two, and connect them with two wires.
Test: one person speaks loudly and clearly into one instrument; the other holds the second to the ear in a quiet room. Expect a faint but clear voice. Tap or scratch the first diaphragm: the second clicks loudly.
Method 2: The carbon microphone
The Hughes microphone (simplest)
- Glue two small blocks of hard carbon (or graphite) 1 cm square, one above the other, 3–4 cm apart, to a thin upright board of soft wood (a sounding board) 10 × 15 cm on a heavy base.
- In the facing surfaces of the blocks, drill small shallow cups.
- Shape a carbon pencil, 3–4 cm long and 4–5 mm thick, pointed at both ends, and stand it loosely between the two cups, leaning slightly against the board. It must be free to rattle.
- Connect one block, two cells, an earpiece from Method 1 and the other block in a loop.
- Speak towards the board. The voice in the earpiece is far louder than with two magnet telephones. It is sensitive to every knock of the table, but it proves the principle in an afternoon.
The carbon-grain button (practical)
- Cup: turn a shallow brass or hardwood cup 2–2.5 cm across inside and 0.6–0.8 cm deep. In its bottom, fit a polished disc of hard carbon, connected by a wire through the back to a terminal.
- Front electrode: a second polished carbon disc, slightly smaller than the cup's inside, fixed to the middle of the diaphragm by a small screw or post, facing into the cup.
- Fill the cup about two-thirds to three-quarters full of roasted carbon grains.
- Seal: close the gap between the front disc and the cup's rim with a ring of thin mica, silk or soft paper, so the grains cannot spill but the front disc can move freely.
- Diaphragm: here it need not be iron; a thin disc of aluminium, mica, or even tightly stretched varnished parchment 5–6 cm across will do. Clamp it in a wooden case with a funnel-shaped mouthpiece.
- Resistance: the finished button should measure roughly 20–100 Ω and drop noticeably when you press on the diaphragm (watch a galvanometer in series, The Electromagnet).
Method 3: A complete telephone set
The induction coil
- Core: a bundle of soft, annealed iron wires about 1 cm thick and 8–10 cm long.
- Primary: 150–250 turns of 0.6 mm covered wire next to the core (about half an ohm).
- Secondary: over the primary, with paper between, 2,000–3,000 turns of 0.2 mm wire (roughly 100 Ω).
Ringing
You need a way to call the other end. Two choices:
- Battery bell: a buzzer or trembler bell (Electric Bells, Buzzers and Alarms) at each end, and a push-button that connects a battery of 4–6 cells to the line. Simple, good for a short line.
- Hand magneto and polarised ringer (the classic). A small hand-cranked magneto (The Generator) of 3–5 horseshoe magnets and an armature wound with thousands of turns of thin wire gives 50–100 V of alternating current when cranked. At the other end it works a polarised ringer: a pivoted iron armature, biased by a permanent magnet, rocking between two coils, with a hammer on a stalk that strikes two bells. The alternating current rocks it back and forth — a loud, unmistakable ring. Because it is AC and high voltage, it pushes through long, leaky lines where a battery bell would fail, and needs no battery for ringing.
Wiring it
- Hook switch: a lever on which the earpiece hangs, with a spring. Earpiece down (on hook): the line is connected to the bell (and the ringing generator). Earpiece up (off hook): the bell is disconnected, the line is connected to the earpiece and the secondary of the induction coil, and the microphone circuit (microphone, battery, primary) is closed.
- The microphone battery only runs when the earpiece is lifted, so two cells last months.
- Mount everything in a wooden box on the wall: bells on top, crank on the side, microphone on the front at mouth height, earpiece on its hook.
Method 4: The line
- Two wires (a metallic circuit) are far better than one wire and the earth. An earth-return telephone line hums and crackles with every stray current in the ground, and picks up the clicking of any telegraph line on the same poles. Two wires on the same poles, about 30 cm apart, cancel most of this.
- Swap the wires over (transpose them) every few poles — wire A moves to B's insulator and B to A's — so that both pick up the same interference, which then cancels. Do this especially where the line runs beside a telegraph or power line.
- Wire: copper carries the voice much better than iron. Iron works for short lines; for lines over 10–20 km, use copper 1.5–2 mm, or thicker. Strung on poles and insulators as in The Telegraph.
- Range: with carbon microphones and induction coils, expect clear speech over 20–50 km of good iron or copper line, more on thick copper. Beyond that, the voice fades and blurs; long-distance lines needed thicker copper and, later, amplifiers.
- Lightning protection at every house where the line enters: a small spark gap to earth (two carbon blocks separated by a thin mica sheet with a hole in it) and a fuse. See The Telegraph.
Method 5: The switchboard
With two sets, you have one conversation. With twenty houses, stringing a line from every house to every other is absurd: twenty houses would need 190 separate lines. Instead, every house has one line to a central office — the exchange — where an operator connects any two lines together.
- Drops: for each line, a small electromagnet holding up a hinged shutter with the line's number on it. When the caller cranks their magneto, the ringing current pulls the electromagnet's armature, which releases the shutter. It falls and shows the number.
- Jacks: under each drop, a socket for that line — two spring contacts in a hole, one for each of the two wires.
- Cord pairs: flexible cords with a plug at each end. A plug has two insulated contacts: the tip and the sleeve (brass, separated by a ring of hard rubber, horn or shellac-soaked wood). The two plugs of a pair are wired together, and a key on the desk lets the operator switch either her own headset or her own ringing magneto onto the pair.
- Making a call:
- Caller cranks. Drop 7 falls.
- Operator puts the answering plug in jack 7, switches in her headset, and asks "Number, please?"
- Caller asks for 12. Operator puts the calling plug in jack 12 and cranks her magneto to ring house 12.
- They talk. When they hang up, each cranks briefly ("ringing off"); a clearing drop on the cord pair falls, and the operator pulls the plugs and resets the drops.
- Size: a single operator can handle 50–100 lines. Ten cord pairs allow ten conversations at once.
A small exchange is a natural job to combine with the The Telegraph office, the post office or the fire watch.
How to tell it worked
- Scratch test: scratch or tap the diaphragm at one end; a sharp click at the other means the line and instruments are connected.
- Hum test: hum a steady note. It should come through as the same note, not an octave higher (if it does, the receiver's magnet is weak or missing).
- Speech test: read a list of unfamiliar words, numbers and names; the listener writes them down. Words like "five" and "nine" are easily confused — spell numbers digit by digit ("one, two, three") and use a spelling alphabet for names.
- Ring test: crank (or press) at one end; the far bell rings loudly and the near bell does not.
Note Troubleshooting. Nothing at all → broken wire, a bad joint, or the hook switch not making contact. Check each with a galvanometer and cell. Speech faint but clear → magnet weak, gap too wide, or a magnet-only set used on too long a line. Remagnetise, adjust the gap, or add a carbon microphone and induction coil. Loud frying or crackling → microphone grains too fine, packed too tight, or damp. Use coarser grains, fill less, keep the button dry. Microphone works, then goes dead after a few minutes → grains packed together ("packing"); tap the case. Fill a little less. Hum and clicking from other lines → earth return or untransposed wires. Use two wires and transpose them. Bell rings but you cannot talk → hook switch wiring wrong, or the microphone battery dead. Diaphragm sticks to the magnet → gap too small. Back the magnet off.
Dangers
Danger Lightning comes in on the line. Telephones on overhead lines have killed and injured people during thunderstorms. Fit a spark-gap protector and an earth connection where every line enters a building. Do not use the telephone during a thunderstorm unless it is an emergency.
Danger Never let a telephone line touch a power line. Run telephone wires below power wires, never on the same cross-arm, and with a wide gap. A fallen power wire on a telephone line can kill the person holding the earpiece. See Wiring and Electrical Safety.
- Ringing voltage. A hand magneto's 50–100 V AC gives a painful jolt. Do not touch line terminals while anyone might crank, and put a notice on the switchboard's ringing key.
- Battery chemicals: see The Battery.
- Climbing and falling wire: see The Telegraph.
Going further
- Common battery. Instead of a battery at every house, put one large battery at the exchange; lifting the earpiece then automatically signals the operator with a lamp. This needs no crank and no house batteries.
- Automatic exchanges (The Automatic Telephone Exchange) replace the operator with rotating switches worked by pulses from a dial at the caller's set — stepping relays, close cousins of the The Relay Computer.
- Loudspeakers and amplifiers: the The Vacuum Tube amplifies the faint receiver current, and the telephone receiver with a horn becomes a loudspeaker for Radio and Recording Sound (Loudspeakers, Microphones and Headphones).
How it was first done
In 1861 the German schoolteacher Philipp Reis built a "Telephon" that sent musical tones and, at times, a few words, using a contact that opened and closed. The Italian inventor Antonio Meucci, working in New York, experimented with voice transmission in the 1850s and filed a caveat (a notice of invention) in 1871. On 14 February 1876, Alexander Graham Bell, a Scottish-born teacher of the deaf in Boston, filed his patent application, the same day as Elisha Gray filed a caveat for a similar invention. Bell's patent was granted on 7 March, and on 10 March 1876 he spoke to his assistant Thomas Watson over a wire: "Mr. Watson, come here — I want to see you." That first transmitter used a needle dipping in acidified water; the practical instruments that followed were the magnet telephones of Method 1.
Thomas Edison and Emile Berliner developed carbon and contact transmitters in 1877–78; David Hughes in London showed his loose-contact "microphone" in 1878; and in 1878 Henry Hunnings in England patented the carbon-grain transmitter, the ancestor of almost every telephone microphone until the 1980s. The first commercial switchboard opened in New Haven, Connecticut, in January 1878 with 21 subscribers. In 1891 Almon Strowger, an undertaker in Kansas City, patented an automatic exchange; the first opened in La Porte, Indiana, in 1892. Telephone calls crossed North America in 1915, once vacuum-tube amplifiers could boost the voice along the way.
Source: content/entries/electricity/telephone.md