Part 6 · Building
Fire Extinguishers and Alarms
The things that win the first minute of a fire — sand buckets, fire blankets, water and soda-acid extinguishers that one person can carry and use — and the bells, gongs and rattles that wake a household or a town, with heat-operated alarms in outline. Plus the fire drill and the escape route, which save more lives than any machine.
- Difficulty
- ●●●●●
- Time
- A sand bucket in an hour; a fire blanket in a day; a soda-acid extinguisher in a week of sheet-metal work; a fire drill in ten minutes, twice a year for ever
- Steps from zero
- 31 prerequisites →
This unlocks
—The full path from nothing — 31 steps before this one
- Stone Tools
- Cordage and Rope
- Fire
- Finding and Preparing Clay
- Finding and Identifying Ores
- Sulfur
- Measurement from Scratch
- Writing and Numbers
- Basic Woodworking
- Hunting and Trapping
- Pottery
- The Kiln
- Charcoal
- Arithmetic and Fractions
- Hides and Leather
- Tiles and Clay Pipes
- Lime
- Salt
- Surveying and Levelling
- Lye and Potash
- The Wheel and Axle
- Glass
- Bellows
- Saltpeter
- The Lathe
- Lead
- Sulfuric Acid
- Pumps
- Pipes, Plumbing and Aqueducts
- Soda Ash and Baking Soda
- Firefighting
- Fire Extinguishers and Alarms
Do them roughly in this order. See it on the tech tree →
Why it matters
Almost every fire that destroys a house began small enough to put out with a bucket, a lid or a blanket — in the first minute. After a few minutes a room fire is too big for anyone. Firefighting covers the brigade and the fire engine, which come later. This chapter covers what waits beside the stove, the forge and the bed: sand buckets and fire blankets; portable extinguishers one person can use; bells, gongs, rattles and automatic heat alarms; and the escape routes and drills that get everyone out when a fire cannot be fought.
How it works
Fire needs fuel, heat and oxygen (Fire). Each tool takes away one of them, and which tool works depends on what is burning:
| Kind of fire | Examples | Works | Never |
|---|---|---|---|
| Solids | Wood, straw, cloth, paper | Water, soda-acid, sand or earth, blanket on a small one | — |
| Burning liquids | Lamp oil, tar, turpentine, alcohol, petrol | Sand, foam, dry baking soda, a lid | Water jet: it splashes the burning liquid about |
| Cooking fat and oil | A pan on the stove | Lid or fire blanket, then heat off | Water — it flashes to steam and throws a ball of burning fat |
| Live electricity | Wiring, motors, generators | Cut the power first (Wiring and Electrical Safety), then treat as solids; dry powder or sand meanwhile | Water and soda-acid: they conduct |
| Burning metals | Magnesium, molten metal spills | Dry sand only | Water, and damp sand: steam explosions (Magnesium) |
Water cools; sand, blankets and lids smother; foam floats on a burning liquid and does both. A portable extinguisher holds only 9–10 litres and empties in a minute, so it wins only against a fire still smaller than a person. Its value is that it is already there.
What you need
| Item | For | Notes |
|---|---|---|
| Iron or copper sheet, rivets, solder | Buckets, extinguisher bodies | Sheet Metal and Rolling, Soldering and Brazing |
| Brass or bronze | Caps, nozzles, valves | Cast and threaded (Zinc and Brass, Screws, Nuts and Bolts) |
| Clean dry sand | Sand buckets | Sieved, dried |
| Baking soda (sodium bicarbonate) | Soda-acid, foam, dry powder | Soda Ash and Baking Soda |
| Strong sulfuric acid | Soda-acid | Sulfuric Acid |
| Alum or aluminium sulfate | Foam (outline) | Dyes and Mordants; or clay dissolved in hot sulfuric acid |
| Wool cloth or felt; glass cloth | Fire blankets | Spinning and Weaving Cloth, Felt, Glass Fibre and Glass Wool |
| Hardwood, ash or hickory | Rattles | Basic Woodworking |
| Iron bar 20–25 mm | Alarm gong | Blacksmithing |
| Bismuth, lead, tin | Fusible links | Antimony and Bismuth, Lead, Tin and Pewter |
| Hemp rope 14–16 mm | Escape ropes | Ropewalks and Sailcloth |
Sand buckets and fire buckets
The simplest extinguisher, and for oil, tar and metal fires the best.
- The bucket. Sheet iron or copper, 10–12 litres, with a strong bail handle. Give fire buckets a round or pointed bottom: they must hang on hooks, cannot stand on the floor, and so are never borrowed for milking or mortar and are always there. Paint them a bright colour that means "fire" in your town — red is usual.
- The sand. Sieve clean river or pit sand through a 3–5 mm mesh to take out stones, then dry it in the sun or on an iron sheet over a fire. Fill to 5 cm below the rim. Put a loose wooden or sheet-metal lid on it to keep out rain, ash and rubbish, and hang a small scoop or short shovel beside it.
- Where. Two by every forge, kiln and furnace; one at every store of oil, tar or spirits, in every workshop and by each boiler. Water buckets go by hearths and in barns (Firefighting).
Using sand. Do not throw the whole bucket from a distance. Scoop it and spread it from the near edge forward, covering the burning liquid in a layer 2–3 cm deep. On a spreading pool of burning oil, first throw a ridge of sand across its path to dam it. On molten metal spills and burning magnesium, cover generously and leave alone until cold.
Check monthly that the sand is loose and dry: wet sand cakes, and near molten metal it is dangerous.
The fire blanket
A fire blanket smothers a burning pan, a small fire on a table or floor, or a person whose clothes are alight.
What it is made of. Wool: it needs about 570–600 °C to ignite, chars instead of melting, and goes out when the flame is taken away. Use heavy, tightly woven or fulled (shrunk and thickened) wool cloth, or Felt 3–5 mm thick. Glass cloth (Glass Fibre and Glass Wool) does not burn at all. Linen and cotton must first be soaked in a fire-retardant — for example 7 parts borax and 3 parts boric acid in 100 parts warm water (Borax and Boric Acid) — and re-treated after every wash. Never use plastic fibre: it melts onto skin.
Making one.
- Cut wool cloth to 1.2 × 1.2 m for a kitchen, 1.8 × 1.2 m for wrapping a grown person.
- Hem all four edges so they cannot fray.
- Sew a strong tape or loop to each of two corners on one side — these are the handles.
- Fold it concertina-wise so the two tapes come out last, and keep it in a wall pouch of canvas or a sheet-metal tube by the kitchen door, at shoulder height, with the tapes hanging down. One hard pull on both tapes must bring it out ready to use.
Using it on a pan fire.
- Pull it out by the tapes and wrap the top corners round your hands, holding it up like a shield.
- Lay it over the pan, away from you — do not throw it — covering the whole rim.
- Turn off the heat if you safely can.
- Leave it 30 minutes. Lifted early, the still-hot fat re-ignites.
On a person: make them stop, drop to the ground and roll; wrap the blanket around them from the head and neck downward, pressing it on to smother flames, and keep the flames away from the face. Then cool the burns in clean cool water for 20 minutes (Wound Care and Antiseptics).
Water extinguishers
- The pump can — the first portable extinguisher: a tank of 10–15 litres with a small hand pump built in, a brass barrel 3–4 cm across with a leather-cupped plunger and two flap valves (Pumps, Packing, Gaskets and Seals), a short hose and a 4–5 mm nozzle. It throws 6–8 m, has no pressure vessel, and refills from any bucket. It is the stirrup pump of Firefighting, made self-contained.
- Stored pressure — later: 9 litres of water under air pumped to 7–10 bar (Bellows to Air Compressors), let out by a squeeze-lever valve through a dip tube and hose, 8–10 m for a minute. It needs a valve that holds pressure for months and a gauge (Pressure and Vacuum Gauges). Add salt where it may freeze.
The soda-acid extinguisher
The extinguisher of the late 19th and early 20th centuries, and the best you can build before you can make valves that hold pressure for months. It stays unpressurised until the moment of use: turning it upside down mixes acid into a soda solution, the gas made pushes the water out.
The chemistry. Sulfuric acid and baking soda give carbon dioxide gas:
sulfuric acid + baking soda → sodium sulfate + water + carbon dioxide
About 220 g of strong acid (120 ml) makes over 100 litres of gas. Sealed inside a 10-litre can, the gas pushes the pressure up to several bar within seconds and drives the water out. The recipe deliberately uses too little acid for the soda, so all of it is used up and the jet is only mildly alkaline, not acid.
Parts and sizes.
| Part | Size and material |
|---|---|
| Body | Cylinder about 18 cm across, 60 cm tall, holding 10 litres; copper sheet 1–1.5 mm with a brazed or riveted-and-soldered seam, and domed ends brazed in (Sheet Metal and Rolling, Soldering and Brazing). Tin the inside or coat it with pitch against corrosion. |
| Neck and cap | Cast brass neck 7–8 cm across, brazed into the top; screw cap with a leather or rubber gasket (Packing, Gaskets and Seals). |
| Acid bottle | Glass or stoneware, about 150–250 ml, standing in a wire or perforated-sheet cage hung from the neck. Its mouth is closed by a loose lead stopper that falls out when the can is upturned. |
| Outlet | A short brass pipe near the top (which becomes the bottom when inverted), with a fine strainer inside; a hose 50–60 cm long of rubber or leather; a nozzle 3–4 mm across. |
| Handles | One at the top, one at the bottom for turning it over. |
Charging it.
- Dissolve 600–700 g of baking soda in 9 litres of lukewarm clean water, in a separate bucket. Stir until it is all dissolved; pour it into the can through a cloth to keep out grit that would block the nozzle. Fill only to the marked line, which leaves room for the gas.
- Wearing gloves and eye protection, fill the bottle with about 120 ml of strong sulfuric acid (Sulfuric Acid), put in the loose stopper, set the bottle in its cage.
- Screw on the cap firmly. Hang the extinguisher on a hook, upright, by the door of the room it guards. Tie a paper label on it with the date charged.
Using it. Carry it upright to within 8–10 m. Turn it upside down and aim the jet at the base of the flames, sweeping across; it runs about a minute and cannot be stopped. Only on wood, cloth, straw and paper — never oil, fat or electrics. Recharge yearly and after every use, checking the inside for corrosion.
Testing the body. Before first use and every five years, fill the can full of water and pump it to 25 bar — about three times its working pressure — for five minutes: no leak, no weeping seam, no bulge. A body that fails a water test splits harmlessly instead of exploding (Boilers and Pressure Vessels).
The foam extinguisher (outline)
For burning oil, tar and spirit, use foam. The can is like the soda-acid one, but the body holds baking soda with a foam stabiliser (a few percent of liquorice-root or soapwort extract), and a large inner container holds aluminium sulfate solution (or, less well, alum). Inverted, they mix into 8–10 times their volume of stiff foam. Aim it at a wall or the far edge so the foam slides gently across the liquid.
Dry powder
Fine baking soda, kept bone-dry in a lidded tin with a scoop, knocks down small fat, oil and spirit fires when thrown at the base by the handful. Never use flour — flour dust in air is explosive.
Fire alarms
A fire found early is small. Everyone in a household or settlement must know one sound that means fire, and must hear it.
Bells and gongs
A bell rung fast and without stopping means fire everywhere; casting and hanging one is in Walls, Palisades and Watchtowers and Bronze. The alarm gong is quicker to make and nearly as loud:
- Forge a triangle from round iron bar 20–25 mm thick and about 2.5 m long, bent into a triangle with 80 cm sides, one corner left slightly open. Or use a ring cut from an old iron wheel tyre, a length of rail, or a disc of steel plate 3–5 mm thick and 40–60 cm across.
- Hang it free by a chain or a rope loop from one point — touching anything kills the ring.
- Chain a striker beside it: an iron rod 30–40 cm long, or a hammer. Strike it on the inside or near the edge, fast and repeatedly.
Hang one in every street, yard and barn, where a child can reach it. A good gong is heard 300–500 m on a still night.
The watchman's rattle
A hand rattle of hardwood makes a harsh, ratcheting clatter that carries several hundred metres and sounds like nothing else — night watchmen carried them for two hundred years. It needs no metal.
- Handle and wheel. Turn or carve a handle 2.5 cm thick and 15 cm long of oak, ash or other hard wood. At its top end, fix a toothed wheel 6–7 cm across and 2.5 cm thick, cut with 8–10 sharp ratchet teeth, so it cannot turn on the handle (square the handle end into a square hole, glue and pin it).
- Frame. Two side cheeks of hardwood 22 × 4 × 1.5 cm, joined by a spacer block at the far end and a thin one beside the wheel. Bore both cheeks for the handle's round upper end, so the whole frame spins freely around the handle.
- Tongue. A thin, springy slat of ash, hickory or maple, 2.5 cm wide and about 16 cm long, planed from 6 mm at its fixed end down to 2–3 mm at its tip. Fix the thick end firmly between the cheeks at the far end; the tip must press on the wheel and catch each tooth. Two tongues side by side, on a wheel cut as two sets of teeth half a tooth apart, double the noise.
- Use. Hold the handle and swing the frame round in circles. Each tooth flicks the tongue, which snaps back with a crack.
Tell a good one: a loud, hard, even clatter at a slow swing. If it sounds soft, the tongue is too thick or the tip too far from the teeth; if the tongue snaps, it was too thin or of brittle wood.
Signals and codes
Agree one signal for fire — fast, continuous ringing, or the rattle — and use it for nothing else. In a town, number the districts; after the alarm the watch strikes the number (three blows, pause, three blows) so the brigade runs to the right place (Firefighting). Test at the same hour each week, so ringing at any other time means trouble. Horns, whistles (Musical Instruments) and later electric bells (Electric Bells, Buzzers and Alarms) carry the same codes.
Heat-operated alarms (outline)
A sleeping house needs an alarm that rings by itself. Three ways, from simplest:
- The burning thread. A cotton thread across the ceiling near the hearth holds a weighted hammer clear of a bell. The hottest gases of a fire collect under the ceiling first; the thread burns and the hammer falls. Renew the thread every few months.
- The fusible link. Two small brass strips overlapped 1.5–2 cm and soldered with 50% bismuth, 25% lead and 25% tin (Rose's metal), which melts at about 95 °C (Antimony and Bismuth). It holds the cord: when the ceiling air gets that hot, the link parts and the hammer falls — or a fire door swings shut, or a damper drops. Test one link from each batch, carrying its load, in slowly heated water: it must part before the water boils. Fusible alloys creep under load, so keep the pull to a few kilograms and renew links every few years.
- Electric. A bimetal strip of brass and iron riveted together bends as it warms; set it to touch a contact at 60–70 °C, closing a circuit from a The Battery to an electric bell (Thermostats and Automatic Control, Electric Bells, Buzzers and Alarms).
A fusible link holding shut a plug in a water pipe makes an automatic sprinkler (Pipes, Plumbing and Aqueducts). Later, smoke detectors — a lamp and a light cell in a dark box (Photocells and Sensors) — warn earlier still, because smoke reaches a sleeper long before flame.
Escape routes and fire drills
When the fire is bigger than you, the only thing that matters is getting everyone out. Most people who die in fires die of smoke, often without waking, or because they could not find a way out in the dark.
Building for escape.
- Two ways out of every place where people sleep or gather: a door, and a window that opens at least 50 cm wide and 60 cm high, low enough to climb through.
- Doors of halls, schools, workshops and theatres open outward, held by a simple latch or push bar, never locked while anyone is inside: a crowd cannot pull open an inward door.
- No one more than about 30 m from a way out; corridors and stairs at least 1 m wide and kept clear. Enclose stairs with a door at each floor so smoke cannot fill them, or build an outside stair of iron or stone.
- Upper rooms without a second stair get an escape rope: hemp 14–16 mm thick (Ropewalks and Sailcloth), reaching the ground, an overhand knot every 30–40 cm, tied to an iron ring set in the wall below the window. Test it with a person's weight once a year.
- Paint exit door frames white, and in public halls keep a lamp burning by each exit.
The household plan. Draw your house. Mark two ways out of each room. Choose a meeting place outside — a particular tree or gate. Teach everyone, children above all: shout "fire", get out, stay out; feel a door with the back of the hand before opening it; crawl low under smoke; close doors behind you; go to the meeting place; nobody goes back in.
The fire drill, for every school, workshop, hospital and public building:
- Name a warden for each floor or group, carrying the list of names.
- Sound the real alarm, without warning.
- Everyone leaves everything and walks by the nearest exit to an assembly point at least 20 m away. Wardens check rooms and close doors behind them.
- Wardens count against their lists and report anyone missing, so no one is sent back in for someone already outside.
- Time it: a school or workshop should be empty in 2–3 minutes. Block one exit in some drills.
- Talk over what went wrong. Drill at least twice a year, every term in schools, sometimes at night where people sleep. Plan for those who cannot walk; in a hospital, move patients sideways through a fire door first (Running a Hospital).
How to tell it worked
- Monthly round: sand buckets full, dry and hanging; blankets in their pouches; extinguishers upright on their hooks, labels dated within a year.
- Test fire: once a year, on bare ground, put out a tray of oily rags and a small woodpile with sand, a blanket and an extinguisher due for recharging, everyone taking a turn. A soda-acid can should throw a solid jet 8 m or more for 45–60 seconds.
- Alarm test: is the gong heard in the farthest house, at night, doors shut?
- Drill: the building emptied within the target time and every person counted.
Note Troubleshooting. The extinguisher dribbles instead of jetting → nozzle or strainer blocked by grit or crystals, a leaking cap gasket, or the acid bottle never emptied. Clean, re-gasket, check the stopper is loose. It started working by itself → it was knocked over or hung tilted. Hang it upright, at a height where it will not be bumped. The sand will not pour → damp and caked. Dry it, and fit a better lid. People crowded at one exit in the drill → they went the way they came in. Mark and teach the nearest exit for each room.
Dangers
Danger Old pressure vessels kill. A soda-acid can whose body or cap has been eaten by years of acid and damp can burst when inverted, with enough force to kill the person holding it. Inspect the inside every year, pressure-test every five years, and scrap any extinguisher that is dented, pitted or more than about 20 years old. Never block the nozzle while it runs.
Danger Never throw water on burning fat or oil, and never use water or soda-acid on live electrical equipment. Never put damp sand or water on molten metal or burning magnesium — the water turns instantly to steam and throws molten metal about.
- Strong sulfuric acid burns skin and blinds. Fill acid bottles wearing gloves and eye protection, with water at hand to wash off splashes (Sulfuric Acid).
- Do not make carbon tetrachloride extinguishers, sold in the early 20th century: in a fire the liquid turns into deadly phosgene gas.
- Know when to leave. A fire taller than you, or smoke spreading across the ceiling, is past an extinguisher. Get out, close the door, raise the alarm. Always keep the exit behind you when you fight a fire.
What this unlocks
Small fires put out early let a village grow into a town (Planning a Settlement). The fusible link and the bimetal strip lead to automatic control (Thermostats and Automatic Control); electric alarm circuits and the The Telephone lead to street fire-alarm boxes and an emergency number. Sprinklers make large mills safe to run.
How it was first done
Buckets of leather and wood, wet blankets, and sand have fought fires since antiquity. In 1723 the chemist Ambrose Godfrey in London patented a fire "extinguisher" that burst a cask of liquid in the flames with a small charge. George William Manby, an English barrack-master, invented the first portable pressurised extinguisher in 1818: a copper vessel holding 3 gallons (about 14 litres) of potash solution under compressed air. François Carlier in France patented a soda-and-acid extinguisher in 1866, and the soda-acid design with sulfuric acid was patented in the United States by Almon Granville in 1881; it remained standard until the 1960s. The Russian teacher Aleksandr Loran invented chemical foam in 1904. Night watchmen with rattles patrolled European towns for centuries; London's police carried rattles until the 1880s. William Channing and Moses Farmer built an electric fire-alarm telegraph in Boston in 1852, and Francis Robbins Upton patented an automatic electric fire alarm in 1890. Rules on outward-opening doors and school fire drills followed disasters such as the Iroquois Theater fire in Chicago (1903) and the Collinwood school fire in Ohio (1908), in which about 170 children died.