Footwear

How to make sandals, moccasins, sewn leather turnshoes and carved wooden clogs; how to carve a last, add and replace soles, waterproof leather, and keep feet warm with socks, wraps and grass. Good shoes let people walk, work and survive winter.

Difficulty
●●●●●
Time
Sandals in an hour; moccasins in an afternoon; a pair of turnshoes in 2–3 days; clogs in 2–3 days of carving plus weeks of drying
Steps from zero
6 prerequisites →

You need first

Hides and LeatherSewing, Needles and Thread

This unlocks

—
The full path from nothing — 6 steps before this one
  1. Cordage and Rope
  2. Stone Tools
  3. Hunting and Trapping
  4. Spinning and Weaving Cloth
  5. Hides and Leather
  6. Sewing, Needles and Thread
  7. Footwear

Do them roughly in this order. See it on the tech tree →

Why it matters

Bare feet harden with time, but they still cut on flint and thorns, burn on hot sand, and freeze on snow. A thorn wound in the foot can kill through infection (Wound Care and Antiseptics); frozen toes are lost for good (Surviving Cold and Heat). A farmer, a smith, a soldier and a traveller all depend on their feet, and in many places a winter without good boots is a winter indoors.

Footwear is also a lesson in materials. It must be tough underneath and supple on top, grip without slipping, keep water out and still let sweat escape, and stay on the foot. Different peoples solved this in very different ways — woven grass, soft smoked buckskin, hard oak-tanned leather, solid wood — and each solution is worth knowing, because each uses what a different landscape offers.

How it works

A shoe has four jobs, and each part of it does one:

  • The sole takes the wear and protects against sharp and hot or cold ground. It must be thick and hard: thick leather (4–6 mm), rawhide, wood, plaited fibre, or layers of these.
  • The upper holds the sole to the foot. It must be thin and supple (1.5–2.5 mm leather), and it must follow the shape of the foot — which is why most shoes are made on a last, a wooden model of the foot.
  • The fastening — laces, straps, a toggle, a drawstring — stops the foot sliding forward and the heel lifting out.
  • The lining and filling keep the foot warm and dry: socks, wraps, felt, fur, dry grass. A loose boot full of dry grass is warmer than a tight boot of the best leather, because warmth comes from trapped air and blood flow, and tightness stops both.

Leather keeps water out only when its fibres are filled with fat and wax. Dry leather drinks water like a sponge; well-greased leather sheds it (Hides and Leather).

What you need

Item Notes
Sole leather Thick, firm bark-tanned cattle or horse hide, 4–6 mm (Hides and Leather). Rawhide also works but goes slippery and soft when wet
Upper leather Supple leather 1.5–2.5 mm: goat, calf, deer, or smoked buckskin for moccasins
Thread Heavy waxed linen or hemp (4–6 ply), or sinew (Sewing, Needles and Thread)
Awls A straight awl and a curved one, sharp, 4–6 cm, of bone, antler, or later steel
Needles Two blunt needles (bone or metal), or stiff hog bristles twisted onto the thread ends
Knife Very sharp, for cutting leather cleanly (Stone Tools, Axes, Chisels, Knives and Planes)
Lasts A pair of carved wooden feet; see below
Wood for clogs A green log of alder, willow, poplar, birch, sycamore or beech, 30–35 cm long and 15–20 cm thick
Carving tools Axe, a knife, a gouge or spoon knife, an auger (Axes, Chisels, Knives and Planes, Basic Woodworking, Drills and Boring)
Dubbin 2 parts tallow (or other animal fat) to 1 part beeswax, melted together

Where to find it

  • Leather and rawhide: Hides and Leather. The back and rump of the hide are thickest and best for soles; belly and shanks are thin and stretchy.
  • Sinew: Cordage and Rope.
  • Clog wood must be soft enough to carve, light, and not split. Alder — a tree of stream banks and wet ground with dark, cone-like little catkins and rounded leaves notched at the tip — is the classic; its wood turns orange when freshly cut. Willow and poplar are lighter; birch, sycamore and beech are harder-wearing.
  • Bast for woven shoes: the inner bark of lime (linden, basswood) and willow, stripped in spring (Cordage and Rope).
  • Grass and sedge for stuffing: tall, fine, dry sedge or meadow grass, combed and softened by rubbing.
  • Fat and wax: rendered tallow from cattle, sheep or deer (Soap), beeswax (Beekeeping), pine resin (Distillation, Tar, Pitch and Glue).

Measuring and the last

Stand on a piece of bark, board or leather, with your weight on the foot, and draw round it with a charcoal stick held straight up. Mark the widest point across the ball of the foot, and measure the girth (round the foot over the ball) and the instep (round the foot over the top, from the heel bone).

A last is a carved wooden model of the foot, a little bigger. It lets you shape the upper and pull it tight while sewing.

  1. Split a block of hardwood (beech, maple, birch, hornbeam) a little bigger than the foot. Season it dry for a few months if you can; green wood shrinks and changes shape.
  2. Draw the foot outline on the bottom. Add 5–10 mm extra at the toe (feet slide forward in walking) and 2–3 mm around the rest.
  3. Carve the shape: flat bottom, rounded toe, the instep rising to about the height of your own. Check the girth and instep with a cord against your foot measurements, plus about 5 mm to allow for socks.
  4. Make a left and a right. Smooth with sandstone and wax.

Method 1: Sandals

Leather sandals: cut a sole of thick leather or rawhide to your foot outline plus 5 mm all round. Cut three slots: one between the big toe and the next, and one on each side just in front of the ankle bone. Thread a long thong (1 cm wide leather strip, 1.5–2 m long) up through the toe slot, knotting it underneath, and lace it back through the side slots and round the ankle. Glue (pine resin and charcoal, Glues and Adhesives) or stitch a second sole layer underneath to cover the knot.

Woven sandals (the Japanese waraji and the bark sandals of many peoples): twist two long cords of rice straw, grass or bast (Cordage and Rope) into a loop and use them as a warp, held by your toes, and weave twisted straw back and forth over them (Baskets and Containers) to make a sole as long as your foot. Leave loops at the sides for tying. They last only days of hard walking, but cost nothing.

Method 2: Moccasins

PATTERN margin2.5–3cm Sole piecetraced round the foot Vampfoot-wide, halfthe foot long Heel tabfolds up over the heel seam holes5 mm SEWN Puckered seamsole gathered onto the vamp Cuff8–15 cm Tie Heel seamstraight up the back,covered by the tab
Fig. 1 A two-piece moccasin. The sole piece wraps up round the foot and is gathered onto a U-shaped vamp over the toes and instep; the heel seam is closed at the back, and a cuff and tie hold it on.

Moccasins are soft shoes of smoked buckskin or other supple leather (Hides and Leather). They are quick to make, silent and warm, and need no last. Their soles wear through quickly on rock; add a sole of rawhide or thick leather for hard country.

  1. Cut the sole-and-sides piece. Stand on the leather and trace your foot. Draw a second line 2.5–3 cm outside it all round (about two fingers wide), making the toe end a smooth round. At the heel, extend the piece back 5 cm as a tongue-shaped tab.
  2. Cut the vamp — the top piece over the toes and instep. It is a U-shape, as wide as the foot at its widest point, and about half the length of the foot, from the toe tip to just above where the foot bends at the ankle.
  3. Pierce the holes. Using an awl, make holes 3–4 mm in from the edge: every 5 mm round the toe of the sole piece, and every 3–4 mm round the edge of the vamp. The sole piece has a longer edge, so it is gathered in small puckers as you sew it to the shorter vamp edge.
  4. Sew the toe. Turn both pieces inside out (flesh side out), centre the vamp on the toe of the sole piece, and sew round with sinew or waxed thread, whipstitch or a running stitch pulled tight, pulling each stitch to gather the puckers evenly. Turn it right side out.
  5. Close the heel. Put the moccasin on. Pull the sides together behind the heel, mark the seam line, and cut off the extra. Sew the heel seam straight up, and fold the tab at the bottom up over the seam and sew it down — this stops the heel seam wearing through.
  6. Cuff and ties. Sew a strip of leather 8–15 cm high round the top for a cuff (taller for snow). Cut slits round the ankle and thread a thong through to tie it.

Method 3: The turnshoe

The turnshoe was the everyday shoe of medieval Europe: a leather upper sewn to a single leather sole inside out on the last, then turned right side out. The seam ends up hidden inside, where it does not wear. It needs only an awl, two needles and thread.

1. SEWN INSIDE OUT ON THE LAST (UPSIDE DOWN) Last Solegrain side against the last Edge-flesh stitch The awl goes into the edge of the sole and out of itsflesh side, then through the upper. It never goesthrough the face that will touch the ground. Upperinside out soak, turn 2. TURNED RIGHT SIDE OUT Upper room for the foot Solegrain down Seamnow inside,safe from wear
Fig. 2 The turnshoe. The upper and sole are sewn together inside out on the last with an edge-flesh stitch that does not go through the bottom of the sole. Then the shoe is soaked, turned right side out, and dried on the last again.
  1. Pattern. Make a pattern for the upper from cloth or bark by wrapping it round the last: the upper must cover the last from the edge of the sole up to above the ankle, with an opening at the front or side for the foot. A simple one-piece upper wraps round and has one seam at the inner side or the back. Add a 5-mm margin at the sole edge.
  2. Cut the sole from 3–5 mm firm leather and the upper from 1.5–2.5 mm leather.
  3. Soak the leather in water for 15–30 minutes, until it is limp. Let the surface dry a little ("cased" leather — damp throughout, dry on the surface), so it moulds and holds stitches without stretching.
  4. Last the sole. Turn the last upside down on your knee and tack the sole to its bottom, grain side against the last — inside out, like the upper. Its flesh side faces you.
  5. Sew upper to sole. Pull the upper over the last inside out (grain side in), and lay its edge over onto the margin of the sole. With the curved awl, make each hole into the edge of the sole and out through its flesh side, about 4 mm in — never through the grain side, which will become the bottom of the shoe. Then through the upper. Sew with two needles, saddle stitch (Sewing, Needles and Thread), stitches 5–6 mm long. Pull every stitch tight.
  6. Turn. Take it off the last, soak it again until supple, and turn it right side out, starting at the heel and pushing the toe through with a smooth rounded stick. Work it slowly; leather turned too dry cracks.
  7. Re-last the turned shoe and let it dry slowly for a day or two, away from fire.
  8. Fasten. Add a lace through holes punched round the opening, a toggle and loop, or a strap.

Add a second sole. For longer wear, stitch or peg (with small hardwood pins) a thick outer sole underneath. When it wears through, cut it off and sew on another — the shoe lasts years.

Tip Welted shoes came after turnshoes: the upper and a narrow strip of leather (the welt) are sewn together round the edge of an inner sole, and a thick outer sole is then stitched to the welt. Shoes built this way can be resoled again and again and have been the standard for good shoes and boots for 500 years.

Method 4: Wooden clogs

Clogs are carved from a single block of wood (Dutch klompen, French sabots), or made of a wooden sole with a leather upper nailed on (English and Scandinavian clogs). They are cheap, very hard-wearing, warm (wood insulates), and keep feet dry in mud and wet fields, farmyards and workshops.

1. Split a green logalder, willow or poplar;one half per clog 2. Rough out with an axe2–3 cm longer than the foot,toe curved up (rocker) 3. Bore and scoopauger first, then aspoon gouge to the toe FINISHED CLOG, CUT THROUGH LENGTHWAYS Walls8–10 mm Sole15–20 mm thick Hollowfitted to the foot with its sock Toerocker Dry slowly in shade, 2–6 weeks.
Fig. 3 A whole-wood clog roughed out with an axe from a green block, then hollowed with an auger and a spoon gouge. Walls are left 8–10 mm thick and the sole 15–20 mm.
  1. Choose green wood. Cut a fresh log of alder, willow or poplar, and split it into halves. Each half makes one clog. Carve green: dry wood is too hard to work.
  2. Rough out the outside with an axe: the shape of a shoe 2–3 cm longer and 1–2 cm wider than the foot, with a raised toe (the sole curves up at the front so it rocks forward as you walk).
  3. Bore the hollow. With an auger (Drills and Boring), bore a ring of holes into the heel opening and forward into the toe. Do not go too deep: stop 15–20 mm above the bottom.
  4. Scoop it out with a spoon gouge or a curved knife, working toward the toe. Leave walls 8–10 mm thick and a sole 15–20 mm thick.
  5. Fit it often to the foot (with the sock you will wear), and adjust.
  6. Dry slowly. Stuff with wood shavings and dry in shade, out of sun and wind, for 2–6 weeks, or smoke it gently over a smouldering fire for a few days. Fast drying splits it.
  7. Finish with oil or wax, and stuff with straw for warmth.

Leather-topped clogs: carve a sole only, 2–3 cm thick, with a rocker curve and a ridge round the edge; cut a leather upper and nail it on round the edge with tacks through a strip of leather. Iron strips ("clog irons") nailed to the bottom make them last for years.

Waterproofing

  • Dubbin: melt 2 parts tallow with 1 part beeswax; a spoonful of pine resin or fish oil makes it more water-repellent. Warm the leather (and the dubbin), and rub it in thoroughly with the fingers, especially into the seams and where the upper meets the sole. Repeat every few weeks of wet use.
  • Soles can be soaked in hot tallow, or brushed with pine tar (Tar, Pitch and Glue), which makes them harder-wearing and waterproof.
  • Fill seams with a wax-and-resin mixture.
  • Dry shoes slowly, stuffed with dry grass or paper and well away from the fire. Leather dried by fire turns brittle and cracks within days.

Socks, wraps and fillings

  • Foot wraps (portyanki): rectangles of wool or linen cloth, about 40 × 90 cm. Lay the foot diagonally across one end, wrap the end over the toes, then wind the long end round the foot and up the ankle, and pull on the boot. Wrinkle-free wraps don't blister; damp wraps can be rewrapped so the dry end is at the toes. Armies used them until the 21st century.
  • Knitted or nålbound socks of wool (Knitting, Crochet and Netting).
  • Felt liners and insoles (Felt); felt boots for extreme cold.
  • Dry grass or sedge: Ötzi, the Alpine traveller of 5,300 years ago, stuffed his shoes with hay. Sámi herders still pack fine dried sedge round their feet in their fur boots; it absorbs sweat and is changed every day.
  • Fur inside out, hair against the foot.

How to tell it worked

  • Walk a day. Any rubbing point turns red before it blisters. Stop, find the spot, and soften, stretch or pad it.
  • Fit. With socks on, you should be able to wiggle your toes freely and fit a finger behind the heel when you push your foot forward. The heel should not lift much when walking.
  • Water. Stand in a shallow stream for a minute. Well-dubbined leather boots stay dry inside; the seams are usually where water gets in.
  • Seams should not open when you flex the shoe hard.

Note Troubleshooting. Blisters at the heel → the heel lifts. Tighten the fastening across the instep, or add a heel counter (a stiff leather piece inside the heel). Toes pinch → too short, or a pointed toe. Add length to the last. Turnshoe cracks while turning → leather too dry or too thick. Soak longer; use thinner upper leather. Moccasin sole wears through in a week → add a rawhide or thick leather outer sole; avoid sharp rock. Clog splits while drying → dried too fast, or the pith of the tree was left in. Use split halves, dry in shade, wrapped in a damp cloth at first. Boots go hard after drying → dried by the fire. Soften with warm fat; dry slowly next time.

Dangers

Danger Wet, cold feet can be lost. Feet kept wet and cold (even above freezing, 0–15 °C) for a day or more develop trench foot: numb, swollen, white then red and painful, and in bad cases the tissue dies. In freezing weather, tight or wet boots bring frostbite within hours. Change into dry socks at least once a day, dry feet and wraps at night, never sleep in wet socks, and never wear boots so tight they squeeze the foot. See Surviving Cold and Heat.

  • Blisters and small wounds on the feet easily become infected. Keep them clean and covered; don't pop a blister unless it will burst anyway, and then drain it with a boiled needle (Wound Care and Antiseptics).
  • Awls slip and stab the hand holding the work. Keep the hand behind the line of the awl, and use a leather palm guard.
  • Clogs and leather soles slip on wet stone and ice. Nail iron studs or wrap grass rope round soles for ice; walk carefully on wet rock.
  • Old fire and hot coals burn through thin soles. Thick soles at the forge (Blacksmithing).

Going further

How it was first done

The bones of people's toes became slightly weaker about 40,000 to 26,000 years ago in western Eurasia, which suggests that shoes were by then worn regularly. The oldest surviving shoes are sandals woven from sagebrush bark found in Fort Rock Cave in Oregon, about 9,000–10,000 years old. The oldest leather shoe, from Areni-1 cave in Armenia, is about 5,500 years old: a single piece of cowhide laced round the foot like a moccasin, stuffed with grass. Ötzi (about 3,300 BC) wore shoes with bearskin soles, deerskin uppers and a net of grass cord holding hay round his feet. Turnshoes were the shoe of medieval Europe until welted shoes replaced them around 1500. Wooden clogs were made in the Low Countries by the 1200s; the oldest surviving Dutch ones come from Amsterdam and Rotterdam. Shoes made specially for the left and the right foot became common only in the 1800s.