A hot wire in a vacuum gives off electrons, and a positive metal plate collects them — so current flows through the empty space one way only. Add a wire mesh between them and a tiny voltage on the mesh controls a large current. How to make the diode and the triode from a light bulb's glass and vacuum, and how to use them as rectifiers.

Difficulty
●●●●●
Time
Months of trials for a first working tube; then one tube every day or two once the method is settled
Steps from zero
25 prerequisites →

You need first

The Light BulbThe Vacuum Pump

This unlocks

Amplifiers and OscillatorsRadar and MicrowavesDetecting RadiationPhotomultipliers and Scintillation CountersSemiconductors and the TransistorCathode Rays and TelevisionX-Rays
The full path from nothing — 25 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. The Kiln
  9. Pottery
  10. Charcoal
  11. Hides and Leather
  12. Lime
  13. Mercury
  14. Lye and Potash
  15. Fermentation
  16. The Wheel and Axle
  17. Glass
  18. Bellows
  19. The Lathe
  20. Copper Smelting
  21. Laboratory Glassware
  22. Pumps
  23. The Battery
  24. The Vacuum Pump
  25. The Light Bulb
  26. The Vacuum Tube

Do them roughly in this order. See it on the tech tree →

Why it matters

Before the vacuum tube, electricity could be switched (by a key or a relay) but not amplified smoothly. A weak signal stayed weak. The tube changes that: a few thousandths of a volt on its grid control a current hundreds of times more powerful. That one ability gives you:

  • Amplifiers that make a faint radio signal or telephone voice loud (Amplifiers and Oscillators).
  • Oscillators that make the clean, continuous radio waves needed to carry speech and music, and to reach across oceans.
  • Long-distance telephone, with tube "repeaters" every hundred kilometres or so to boost the voice (The Telephone).
  • Electrical sound recording and loudspeakers (Recording Sound).
  • The cathode-ray tube of Cathode Rays and Television and the oscilloscope.
  • Electronic computers — the first ones used thousands of tubes as fast switches (The Computer).

The simpler two-electrode tube, the diode, is a one-way valve for electricity. It detects radio signals and turns alternating current into direct current (rectifies it).

This is one of the hardest chapters in the book. You need everything from The Light Bulb — glass-working, a glass-to-metal seal and a mercury The Vacuum Pump — and then a better vacuum and cleaner metals still. Start with the diode: it is little more than a light bulb with an extra wire in it.

How it works

The Edison effect

Every metal holds a sea of tiny negatively charged particles, electrons, that carry electric current. Heat the metal enough and some electrons boil off its surface into the space around it — thermionic emission ("emission by heat"). In air they are stopped at once; in a good vacuum they fly freely.

Put a second piece of metal, the plate (or anode), in the vacuum near the hot filament (the cathode), and connect a battery between them:

  • Plate positive: it pulls the electrons across. A current flows round the circuit.
  • Plate negative: it pushes the electrons back. Nothing flows. The cold plate gives off no electrons of its own to go the other way.

So current flows one way only. This is the diode.

The grid

Put a mesh or spiral of thin wire — the grid — between the filament and the plate, much closer to the filament. Electrons must pass through the gaps in it to reach the plate.

  • Make the grid a little negative and it repels the electrons; fewer get through; the plate current drops. A few volts negative cuts it off altogether.
  • Make it less negative and more get through.

Because the grid is so close to the filament, one volt on the grid changes the plate current as much as many volts on the plate would. The ratio is called the amplification factor; for a home-made triode expect 3 to 10, for a good factory tube 10 to 100. And a negative grid collects no electrons itself, so it takes almost no current — it controls without consuming. That is amplification: a small, weak voltage steers a large current drawn from a battery. This three-electrode tube is the triode.

Plate positive Plate negative Triode: add a grid +− −+ Current flows electrons boil off the hotfilament and are pulledacross to the plate No current the plate pushes electronsback; the cold plate hasnone of its own to give grid: a few volts A small voltage steers a little negative on the gridthins the stream; more negativestops it — amplification filamentplate filamentplate filamentgridplate Dots are electrons. The glass is pumped to a high vacuum so nothing stops them.
Fig. 1 How a tube works. Left: a positive plate draws electrons from the hot filament, so current flows. Middle: a negative plate repels them, so nothing flows. Right: the grid sits close to the filament; a small change in its voltage opens or closes the stream to the plate.

Why the vacuum must be so good

Gas inside the tube spoils it in three ways. Electrons crashing into gas atoms knock off more charges and set the gas glowing blue or violet; the tube's current becomes erratic and runs away. Positive gas atoms slam back into the filament and wear it away. And oxygen or water vapour poisons the hot filament surface so it stops emitting.

A lamp-grade vacuum (about a millionth of an atmosphere, the best a Sprengel pump gives in reasonable time) makes a "soft" tube: it works, especially as a radio detector, but it is touchy and changes from day to day. The first commercial triodes (1906–1912) were soft. A "hard" tube needs roughly a thousand times less gas, and gets it by three tricks besides pumping: baking the glass, heating every metal part red-hot while pumping, and a getter, a chemical that swallows the last traces of gas after sealing.

The filament: three choices

Cathode Working heat Notes
Carbon (as in the lamp) Yellow-white, about 1,800–2,000 °C You can already make it. Weak emitter, gives off gas, but fine for a first diode — the Edison effect was discovered with one
Bare tungsten White, about 2,200 °C Needs a hard vacuum and drawn tungsten wire, which is very hard to make (Tungsten and Filament Wire). Long life
Oxide-coated platinum or nickel Dull orange, about 750–850 °C Best for a home-made tube. A thin coat of barium (and strontium) oxide gives off electrons hundreds of times more easily than bare metal, at a far lower heat. Low heat means less gas from the parts

This chapter uses the oxide-coated cathode.

What you need

Item Size / amount Notes
Soft glass tubing and bulbs Tubing 6 mm and 12 mm; bulbs 3–4 cm across Laboratory Glassware. Use one batch of glass for everything — mixing glasses cracks seals
Lead-in wire Platinum, 0.3–0.4 mm, about 1 cm per lead 3 leads for a diode, 4 for a triode. See The Light Bulb for alternatives
Filament wire Platinum or nickel, 0.1–0.2 mm, 4–6 cm Platinum and the Platinum Metals, Nickel and Cobalt
Grid wire Nickel, platinum, molybdenum or soft iron, 0.1–0.2 mm, 30 cm
Plate Nickel or soft iron sheet 0.1–0.2 mm thick, 3 × 4 cm Copper and brass give off gas and zinc vapour: avoid
Support wire Nickel or iron, 0.5–0.8 mm
Mica A few thin sheets Spacers to hold the electrodes apart
Barium carbonate 5 g Made from barite, below
Strontium carbonate 5 g (optional) From celestine, the same way
Mercury vacuum pump Sprengel type at least; a mercury diffusion pump for hard tubes The Vacuum Pump, High-Vacuum Pumps and Gauges
Oven A sheet-iron box that fits over the bulb, heated to 350–400 °C
Batteries Filament: 2–4 V, 1–2 A. Plate: 20–100 V (15–70 cells in series). Grid: a few cells The Battery, The Rechargeable Battery
Galvanometer Sensitive The Electromagnet, Measuring Electricity

Where to find it

  • Barite ("heavy spar") is barium sulfate. Look in mineral veins in limestone and sandstone, often with galena, fluorite and quartz. It is white, cream or pale pink, glassy, surprisingly heavy for a pale stone (about 4.5 times water — a fist-sized lump feels like lead next to quartz), soft enough to scratch with a knife, and breaks into flat plates. It does not fizz with acid (calcite, which looks similar, does).
  • Celestine (strontium sulfate) is similar: pale blue-grey or white, heavy, in limestone and with gypsum. Not essential, but a mix of barium and strontium oxides emits better than barium alone.
  • Platinum: grains in gold-bearing gravels; rare. See Platinum and the Platinum Metals.
  • Nickel: from green garnierite ore, or from the nickel matte of copper-nickel ores (Nickel and Cobalt).
  • Mica: books of clear sheets in pegmatite veins in granite (Rocks and Minerals).

Making barium carbonate

  1. Crush 100 g of clean barite to a fine powder and mix it with 25 g of fine charcoal powder (Charcoal).
  2. Roast without air. Pack it in a lidded clay crucible, seal the lid with clay, and heat to a bright orange-yellow (about 1,000–1,100 °C) for 2–3 hours in a The Kiln or forge. The charcoal pulls the oxygen out of the sulfate and leaves barium sulfide, a grey-black cake.
  3. Dissolve the cooled cake in 500 ml of hot water. Stir, let it settle, and pour or filter off the clear liquid. It smells of rotten eggs.
  4. Precipitate. Stir in a strong solution of washing soda (Soda Ash and Baking Soda) a little at a time until no more white solid forms. This is barium carbonate.
  5. Wash it: let it settle, pour off the liquid, add clean water, stir, settle — at least five times, until the wash water no longer smells. Dry it.

Make strontium carbonate from celestine in exactly the same way.

Method 1: The Fleming diode

The quickest working tube, and a test of your whole process.

  1. Make a carbon filament lamp exactly as in The Light Bulb, but seal a third lead-in wire into the stem.
  2. On this third lead, fix a small plate: a strip of nickel or iron 1 × 2 cm, or a little open cylinder round the filament, about 3–5 mm from it at every point. It must not touch the filament.
  3. Pump, heat the filament to drive out its gas, and seal off as for a lamp.
  4. Test. Light the filament from its battery. Connect the plate through a sensitive galvanometer to the positive end of a second battery of 10–20 V whose negative end goes to the filament. The galvanometer should show a current. Reverse the second battery: the current should fall to nothing.

This is the Fleming valve, and it works as a radio detector in place of the crystal in a Radio receiver: plate to the tuned circuit, filament to the earphone side. It is steadier than a cat's whisker, but no more sensitive.

Method 2: The triode

Pumping tubemelted shut after pumping Getter mirrorsilvery film that swallows gas getter (optional) Platenickel or iron cylinder, 10–12 mmacross, 2.5 cm long Gridwire spiral 4–5 mm across,turns 1 mm apart Filamentplatinum or nickel, coated withbarium oxide; dull orange in use Pinch sealglass squeezed round theplatinum lead-ins four leads out: filament (2),grid, plate Mica spacer Mica spacerholds parts apart Filament supportsmall spring keepsthe filament taut Glass stemsoft glass, one batchfor the whole tube Bulb 3–4 cm acrosspumped to a high vacuum
Fig. 2 A home-made triode in cross-section. The oxide-coated filament runs up the middle, inside a spiral grid, inside a cylindrical plate. Four lead-in wires pass through a pinched glass seal. Mica discs hold the parts apart. The tube is pumped through the narrow tube at the top, which is then melted shut.

1. Clean every metal part

Gas hides in and on metal. Cut and shape all parts, then:

  1. Wash them in strong alcohol (Ether, Acetone and Solvents) to remove grease. From now on never touch them with bare fingers; use clean tweezers.
  2. Heat them red-hot for a few minutes buried in charcoal powder in a closed crucible (to burn off dirt without rusting), and let them cool in the crucible.

2. Make the electrodes

  • Filament. A straight piece of 0.1–0.2 mm platinum or nickel wire, 3–4 cm long, stretched between two support wires. A light spring of thin wire at the top end keeps it taut as it expands.
  • Coating. Mix barium carbonate (or half barium, half strontium carbonate) with a few drops of a thin binder — a weak solution of nitrocellulose (Early Plastics) in a solvent, or failing that, plain alcohol — to a thin cream. Paint the filament with a fine brush, let it dry, and repeat 5–10 times, until the wire is evenly white and about twice its original thickness. Keep the coating off the support wires.
  • Grid. Wind 0.1–0.2 mm wire round a 4–5 mm rod in a spiral with 1 mm between turns, 2.5 cm long. Fasten it along one stiff support wire by twisting each turn round it (or by spot-welding, see Welding). Slide it off the rod. The filament will run down its centre, about 2 mm from every turn.
  • Plate. Roll the sheet into a cylinder 10–12 mm across and 2.5 cm long, fastened to a support wire. It will stand round the grid with about 3 mm of space all round.
  • Mica spacers. Two discs of mica a little larger than the plate, with holes punched to hold the filament supports, the grid support and the plate support in their exact places. One at the bottom, one at the top. They stop the parts touching when they get hot.

3. The stem and pinch seal

  1. Heat the end of a 12 mm glass tube until soft, then lay four platinum lead-ins side by side, about 3 mm apart, in the soft end, and squeeze it flat with heated tongs so the glass closes round them. This is the pinch seal. Each platinum piece must be fully buried in the glass for about 5 mm.
  2. Join copper wires to the outside ends and the support wires to the inside ends, by twisting tightly or by welding.
  3. Anneal the stem by cooling it slowly in warm ash. See The Light Bulb for testing seals.

4. Assemble and seal into the bulb

  1. Build the electrodes on the supports with the mica discs. Check under a lens (Lenses) that nothing touches — filament, grid and plate must be centred.
  2. Blow a bulb 3–4 cm across with a 6 mm pumping tube at the top (Laboratory Glassware).
  3. Slip the mount into the bulb and seal the stem to the bulb's neck in the flame, turning steadily. Anneal.

5. Pump, bake and activate

This is where tubes are made or lost. Go slowly.

  1. Pump with the mercury pump until it reaches its best vacuum — an hour or more.
  2. Bake. Lower the iron box over the bulb and heat it to 350–400 °C (paper put against it browns quickly; lead just melts at 327 °C) for 1 hour, still pumping. Gas sticking to the glass comes off. Let it cool.
  3. Heat the filament slowly from its battery through a rheostat (a long resistance wire with a sliding clip) — dull red at first. The carbonate coating breaks down into oxide, giving off carbon dioxide; the pump will labour. Raise it over 20–30 minutes to bright orange (about 1,000 °C) for one or two minutes, then back down. This is called activating the cathode.
  4. Clean the plate and grid. With the filament at dull orange, put the highest voltage you have on the plate (100 V or more) and let the electron stream pound it until it glows dull red. Gas pours out again; keep pumping. Do the same with the grid connected as a plate. If you have a few millimetres of magnesium ribbon (Electrolysis) fixed near the plate as a getter, heat it the same way at the end until it flashes into a silvery mirror on the glass; it will swallow gas for the life of the tube.
  5. Seal off. With the filament warm and the pump at its best, melt the pumping tube shut with a small, hot flame and draw it apart.
  6. Age. Run the tube with filament and a modest plate voltage for several hours. Emission usually rises and settles.

6. Running it

  • Filament: about 0.5–1.5 A at 1–2 V for the sizes above; adjust with the rheostat until the coated part glows dull orange. Hotter does not help — it shortens the life of the coating.
  • Plate: 20–100 V, positive, through whatever is being driven (an earphone, a resistance).
  • Grid: 1–3 V negative ("grid bias"), from a few cells.

Rectifiers

A diode lets current through only when its plate is positive. Feed it alternating current — from a The Generator or a The Transformer — and only the forward halves get through: the output is one-way, though bumpy. That is a rectifier (Rectifiers: Turning AC into DC covers all the kinds). Smoothing the bumps into steady direct current with capacitors and an iron-cored coil is covered in Amplifiers and Oscillators and Power Supplies and Regulators.

  • Power diodes need a larger filament and plate: two or three filaments in parallel and a plate 2–3 cm across. A tube with two plates round one filament, fed from a transformer with a centre tap, uses both halves of the AC wave (full-wave rectifier).
  • Electrolytic rectifier (no vacuum at all). A plate of Aluminium and a plate of lead or iron, in a strong solution of borax or washing soda. Aluminium forms a thin oxide skin that blocks current when the aluminium is positive and lets it pass when negative. Each jar stands about 40 V of AC; use several in series for more. They warm up and must be kept cool, but they are cheap and need no vacuum. Use them first.
  • Crystal rectifiers — galena, silicon — handle only tiny currents, for radio detection (Radio).
  • For big currents, the mercury-arc rectifier (a glass bulb with a pool of mercury as the cathode) was used for a century in railways and electrolysis plants. It is beyond a first workshop.

How to tell it worked

  • One-way current. With the filament lit, a positive plate gives a current on the galvanometer; a negative plate gives none. If current flows both ways, two electrodes are touching.
  • The grid controls. Note the plate current with the grid joined to the filament. Make the grid 2 V negative: the current should fall clearly. A few volts more negative should stop it. Make it slightly positive: the current rises.
  • No glow. In a darkened room, with 100 V on the plate, a hard tube shows no light between the electrodes (a faint blue glow on the glass itself is harmless). A blue-violet glow filling the space means gas: the tube is soft. It may still work as a detector.
  • The spark test. Connect an The Induction Coil to two leads of the tube, with a spark gap of 2 cm in air alongside. In a good vacuum the coil's spark prefers to jump the air gap rather than pass through the tube.

Note Troubleshooting. No plate current at all → filament not hot enough, coating not activated, or coating poisoned by air. Re-activate; if that fails, the tube has leaked. Current flows, then fades over minutes or hours → gas coming off the parts and poisoning the cathode. Degas the plate longer; bake longer; add a getter. Blue glow and a sudden rush of current → too much gas. Reduce plate voltage at once; re-pump. Filament burns through → too much current, or a thin spot. Use a rheostat, and turn up slowly. Coating flakes off → painted too thick at once, or the wire was greasy. Thinner coats, cleaner wire. Grid barely controls → grid too far from the filament or its turns too wide apart. Wind it closer and finer. Seal cracks while cooling → wrong glass for the lead-in, or cooled too quickly. See The Light Bulb.

Dangers

Danger Imploding glass. An evacuated bulb is crushed by the air with great force. If cracked, or heated unevenly, it collapses and then flings glass outwards. Wear eye protection whenever a bulb is under vacuum, being heated, or being sealed, and keep your face to one side.

Danger Mercury vapour. The mercury pump gives off invisible, poisonous vapour, worse when warm — and the oven sits right beside it. Work in a well-aired room, keep the mercury covered, catch every spill in a tray, and never heat mercury in the open. See Mercury.

Danger Barium compounds are poisonous. Barite itself is harmless because it does not dissolve, but barium sulfide and barium carbonate dissolve in stomach acid and can kill. Keep them labelled and away from food, wash hands, and never use cooking pots. The roasting also gives off carbon monoxide and the sulfide gives off rotten-egg gas (hydrogen sulfide), which is poisonous: work outdoors.

  • Plate voltage. A battery of 100 V or more gives a painful, sometimes dangerous shock, and an The Induction Coil far more. Switch off before touching connections. See Wiring and Electrical Safety.
  • Burns. From the glass flame, the oven, and hot metal parts.

What this unlocks

How it was first done

In 1880–1883, while trying to stop his carbon lamps blackening, Thomas Edison's team sealed an extra metal plate into a bulb and found a current flowed from the hot filament to the plate only when the plate was positive; Edison patented it in 1884 as a voltage indicator but found no real use for it. In Britain, John Ambrose Fleming, who had advised Edison's company, made the effect into a radio detector, the "oscillation valve", and patented it in November 1904. In 1904 Arthur Wehnelt in Germany discovered that metal coated with barium and calcium oxides emits electrons at low heat. In 1906 Lee de Forest in the United States added a zig-zag grid between filament and plate — his "Audion" — though he did not fully understand how it worked; his early tubes were soft and erratic. Around 1912–1913 Harold Arnold at Western Electric and Irving Langmuir at General Electric showed that a much higher vacuum gave steady, powerful tubes, and in 1915 tube amplifiers carried the first telephone call across the United States, from New York to San Francisco. Tubes ruled electronics until transistors replaced them from the late 1950s.