◆ Rebuild

Part 15 · Knowledge and Science

Printing

How to make hundreds of identical copies of a page — first by carving whole pages in wood, then with movable metal type cast in a hand mould and pressed onto paper in a wooden screw press. Printing is how knowledge stops being rare.

Difficulty
●●●●●
Time
A week to carve and print a woodblock; many months to make a fount of metal type and a press
Steps from zero
9 prerequisites →

You need first

PaperInkBasic Woodworking

This unlocks

Calculating AidsEngraving, Seals and EtchingLibraries and Preserving KnowledgeLithography and Offset PrintingScreen PrintingThe Typewriter
The full path from nothing — 9 steps before this one
  1. Fire
  2. Stone Tools
  3. Finding and Preparing Clay
  4. Basic Woodworking
  5. Pottery
  6. Charcoal
  7. Lye and Potash
  8. Ink
  9. Paper
  10. Printing

Do them roughly in this order. See it on the tech tree →

Why it matters

A scribe copying a long book by hand takes months, and every copy adds new mistakes. A wooden hand press worked by two people prints about 250 sheets an hour, every one identical. Once a page is set and checked, the thousandth copy is as correct as the first.

That changes everything. With printing, this manual, a farming almanac, a map, a set of measures or a medical guide can be in every village at once. Errors can be corrected in the next edition instead of multiplying. Ideas meet and argue in print, and knowledge builds on itself instead of being lost every time a library burns. The spread of printing in Europe after 1450 was followed within two centuries by the The Scientific Method and the scientific revolution — not by coincidence.

How it works

Every printing method uses the same idea: a raised, mirror-reversed image is coated with ink and pressed onto paper. Only the raised parts touch the paper, and the mirror image prints the right way round. (Try it with a carved potato: carve a letter "R" backwards, ink it, press it.)

There are two ways to make the raised image:

  • Woodblock printing. Carve a whole page into one block of wood. Simple, needs no metal, perfect for pictures — but every page is a separate block, and a mistake means re-carving.
  • Movable type. Make each letter as a separate small block (a sort), all exactly the same height. Arrange them into lines and pages, print, then break the page up and reuse the letters. An alphabet has only a few dozen letters, so this suits it perfectly.

What you need

For Item Notes
Woodblock Blocks of fine, even-grained hardwood Pear, cherry, apple, boxwood, maple; 2–3 cm thick, planed flat
Woodblock Carving knives and small gouges Good Steel edges make this far easier
Type Steel bar for punches, copper for matrices See Steel, Copper Smelting, Files and Saws
Type Type metal: lead, tin, antimony See below; roughly 25 kg for a small fount
Type Hand mould, ladle, small furnace or brazier See Metal Casting
Setting Composing stick, type cases, a flat iron or stone bed, an iron frame (chase), wedges Made from wood and iron
Press Heavy timbers, a wooden screw and nut See Simple Machines, Screws, Nuts and Bolts
Inking Oil-based printing Ink, two ink balls of soft leather and wool Soft leather (see Hides and Leather)
Paper Sized or unsized Paper, dampened Rag paper is best

Method 1: Woodblock printing

  1. Prepare the block. Saw a plank along the grain, about 2–3 cm thick and a little larger than the page. Plane and scrape one face perfectly flat and smooth.
  2. Write the page in ink on thin paper, exactly as it should look.
  3. Transfer it reversed. Brush the block with thin starch paste and lay the paper on it face down. When dry, wet the back and gently rub away the paper fibres until the ink shows through clearly, mirror-reversed.
  4. Carve. With a sharp knife, cut along both sides of every line of the letters, angled slightly outward so each stroke has a strong, sloping base. Then clear away all the background with gouges and chisels to a depth of 3–5 mm. Leave the letters standing.
  5. Ink. Brush the block evenly with ink. Water-based carbon ink thickened with a little starch paste works well on wood; oil ink works too.
  6. Print. Lay a sheet of paper on the block, and rub its back firmly and evenly with a flat pad (a coiled cord or a bundle of fibre wrapped in leaf or cloth), or a smooth bone. No press is needed. Peel it off and hang it to dry.

A good block prints thousands of copies, and a practised printer can rub out over a thousand sheets a day. Woodblocks remain a good way to print pictures, maps and diagrams even after you have type, until Engraving, Seals and Etching and Lithography and Offset Printing give finer lines.

Method 2: Movable type

Simpler kinds of type

Before attempting cast metal type, know the easier routes:

  • Wooden type. Carve each letter separately on the end of a small block of hardwood, all cut to exactly the same height. Good for large letters (posters, headings); too much work for small text.
  • Fired clay type. The first movable type, made in China around 1040, was carved in soft clay and fired. Make each letter on a small clay block, fire it, and grind the faces flat on a stone so they are all the same height. Set them in a frame on an iron plate spread with a mix of pine resin and wax; warm the plate to soften the mix, press the type flat with a board, and let it cool to lock them in place. Clay type is fragile, but needs only a The Kiln.
  • Sand-cast type. Carve one master of each letter in hardwood, press it into fine damp sand mixed with a little clay, and pour molten metal into the impression. This is how Korean printers cast bronze type in the 1300s. It is quicker to set up than punches and matrices, but each piece of type needs a fresh mould and comes out slightly different.

Cast type: punch, matrix and hand mould

This is Gutenberg's system, and it makes thousands of identical letters quickly. It is precise metalwork; expect months of practice.

R R end view top view strike moltentype metal matrix, heldby a spring jerkup Faceletter raised, reversed typeheight jetnick 1 · Punchhard steel, letter inrelief, mirror-reversed 2 · Matrixpunch struck into copper:sunken and right-reading 3 · Hand mouldpour, and jerk upwardin the same instant 4 · Sortbreak off the jet;type height about 23 mm
Fig. 1 Making type. A hardened steel punch carries the letter in relief; struck into copper, it leaves a sunken matrix. The matrix sits at the bottom of the hand mould; molten type metal poured into the mould comes out as a sort, ready to print.
  1. Cut the punch. File the end of a bar of Steel about 6 cm long and 6–8 mm square into the letter, standing up in relief and mirror-reversed. For hollow letters like "o", "a" and "e", first make a counterpunch — a small punch shaped like the hollow — and strike it into the end of the bar. Check the letter by smoking it in a candle flame and pressing it on paper. Then harden and temper the punch.
  2. Strike the matrix. Lay a small bar of soft Copper Smelting (about 3 × 1 × 0.5 cm) on an anvil and strike the punch into it with one sharp hammer blow, about 1–2 mm deep. This gives a sunken, right-reading impression. Justify it: file the face of the matrix flat so the impression has the same depth as every other matrix, and square its sides so the letter sits in exactly the same place.
  3. Make the hand mould. Two L-shaped halves of iron or brass, each fixed in a wooden casing to protect the hands, fit together to form a narrow rectangular channel. The channel's height (front to back) is the body of the type; its length is the type height — about 23 mm in the old standard. One wall slides, so the channel can be made wide for "m" and narrow for "i". The matrix is held against the bottom of the channel with a spring. A funnel-shaped mouth at the top takes the metal.
  4. Melt the type metal in an iron pot over a brazier. It is ready when a slip of paper dipped into it turns brown and begins to char, about 300–350 °C.
  5. Cast. Hold the closed mould in your left hand. Pour a small ladle of metal into the mouth and, in the same instant, jerk the mould sharply upward. The jerk drives the metal into the fine corners of the matrix. The metal sets in a second or two.
  6. Release. Open the mould, flick the matrix back, and tip out the sort. Break off the jet (the funnel-shaped waste at the foot) and remelt it. Rub the sides of each sort on a flat stone to remove burrs.

A practised caster makes several thousand sorts a day. For text you need many of each letter — far more "e"s than "z"s. A small shop needs 10,000 sorts or more: enough for several pages at once.

Type metal

Metal What it does Where from
Lead, about 75% The bulk: cheap, melts at 327 °C Smelted from galena — see Lead
Antimony, about 15% Makes the alloy hard and makes it expand slightly as it sets, so it fills the sharp corners of the matrix Heat stibnite (antimony ore) with scraps of Iron (the Bloomery): the iron takes the sulfur and antimony metal collects at the bottom (Antimony and Bismuth)
Tin, about 10% Makes the metal flow well and toughens it Smelted from cassiterite — see Tin and Pewter and Finding and Identifying Ores

The exact proportions vary; anything near these works. Honest alternatives: lead with 5–10% tin, and no antimony, casts acceptably but gives softer type with slightly rounded corners that wears out sooner — fine for a first fount. Pure lead is too soft and shrinks from the corners. Pewter-like tin-lead alloys work. Wear down type, melt it, and cast it again: type metal is endlessly reusable.

Setting type

  1. Cases. Keep the sorts in shallow wooden trays divided into compartments, one for each letter. Capitals traditionally went in the upper tray and small letters in the lower — which is why we call them "upper case" and "lower case".
  2. The composing stick. A small hand-held tray, as long as a line of text, with a sliding stop that sets the line length. Hold it in your left hand and pick sorts with your right, placing them left to right with the nick (a groove cast into each sort's front) facing out, so you can tell by touch that each one is the right way round. The letters are mirror-reversed; with practice you read them easily.
  3. Spaces. Between words, put blank pieces of type metal that are lower than type height, so they don't print. To justify a line — make it fill the stick exactly — adjust the spaces.
  4. The forme. Slide finished lines onto a flat tray (a galley). When a page is complete, tie it round with cord, put it on the press bed, surround it with an iron frame (the chase) and wedge it tight with wooden blocks and wedges. Plane the type down gently with a flat block of wood and a mallet so every letter stands at the same height. Locked up, the whole page can be lifted as one piece.
  5. Proof it: print one copy, read it carefully for errors, and fix them with tweezers before the run.

The press

heavy frame, braced to floor and ceiling Headholds the nut Screwhardwood, 8–10 cm Platenflat and heavy Formeinked type Bedflat stone in asliding carriage bed rolls in and out on rails Barpull: a quarter-turn Tympan and friskethinged frames that holdthe paper over the type Ink ballsleather stuffed with wool
Fig. 2 A wooden screw press. Pulling the bar turns the screw, which drives the platen down onto the paper and inked type. The bed slides in under the platen and back out on rails.

A press gives a hard, even squeeze over a whole page at once. The type of press Gutenberg used was adapted from the wine and olive presses of his day.

  1. The frame. Two upright timbers (the cheeks), about 2 m tall and 15–20 cm thick, joined by a heavy crossbeam at the top (the head) and another lower down. Brace it to the floor and ceiling; the press must not rock.
  2. The screw. A hardwood screw about 8–10 cm across, turning in a threaded nut set in the head. Mark the thread by wrapping a paper triangle around the round shaft: if the triangle's base equals the shaft's circumference and its height equals the pitch (about 3–4 cm), its sloping edge traces a perfect spiral. Saw along the line to the thread depth and chisel out the groove. For the nut, bore a hole in a block, split the block in two lengthways, carve half the thread in each half, and clamp the halves together with iron bands. See Screws, Nuts and Bolts and Simple Machines.
  3. The platen. A flat, heavy block of hardwood (or later, iron) hung from the bottom of the screw, so it moves straight up and down without twisting. It is usually half the size of the sheet; you pull twice to print a full side.
  4. The bar. A lever fixed into the screw. A quarter-turn of the bar drives the platen down a centimetre or two with great force.
  5. The bed. A flat stone set in a wooden carriage that slides on rails, wound in and out under the platen by a handle and straps. The forme sits on it.
  6. Tympan and frisket. Hinged to the carriage: the tympan, a frame covered with parchment and padded with a blanket or felt, holds the paper; the frisket, a thin frame covered with paper with page-shaped holes cut in it, folds over to keep ink off the margins.

If you cannot make a screw, a lever press works: a long, heavy beam hinged at one end, with the platen under its middle and a weight or your body on the far end.

Inking and printing

  1. Dampen the paper the day before: dip every fifth sheet in water and stack them under a board. Damp paper takes a far crisper, blacker impression.
  2. Make ink balls. Stuff a cup-shaped wooden handle with wool or horsehair, cover it with soft leather, and nail the leather round the rim — a ball about 15 cm across. Make two. Keep the leather supple by soaking it overnight and wringing it out before use.
  3. Ink. Spread a little printing ink on a stone slab. Dab the balls in it and rub them against each other to spread it thin and even. Then beat the forme all over with quick rocking dabs. Thin and even is the goal: too much ink fills in the letters.
  4. Pull. Lay the damp sheet on the tympan, fold the frisket down over it and the tympan down over the forme. Wind the bed in, pull the bar, wind further, pull again, wind out. Lift the tympan and peel off the sheet. Hang it on a line to dry.

One person inks while the other pulls. Print all copies of one side, let them dry, then print the other side.

How to tell it worked

  • Every letter is sharp and evenly black. Grey patches mean too little ink or uneven type height; blobby, filled-in letters mean too much ink.
  • The impression is even across the page. A weak corner means the platen or bed is not flat, or the type is not planed level; pack thin paper under the tympan to fix it.
  • The text reads correctly — no mirrored letters, no upside-down "u"s or "n"s, no confusion between b, d, p and q.

Note Troubleshooting. Type comes out of the mould with rounded, incomplete letters → metal too cold, mould too cold, or not jerked; preheat the mould by casting a few throwaway sorts. Sorts stand at different heights → mould channel not square or matrices not justified to the same depth. Ink smears → paper too wet, or ink too thin; use stiffer ink. Ink won't stick to the type → it is water-based; metal type needs oil-based ink.

Dangers

Danger Molten metal and water explode. A single drop of water — on a damp ladle, in a wet mould, or on a cold, damp floor — turns instantly to steam under molten metal and throws it outward. Preheat every tool that touches the metal, keep the casting area bone dry, and wear heavy clothing and eye protection.

Warning Lead and antimony are poisons. They build up in the body over months and years, causing stomach pain, weakness, damage to the nerves and brain, and in children permanent harm to growth and learning. Melt them outdoors or under a strong draught, never breathe the fumes, wash your hands before eating, never eat, drink or smoke in the type room, and keep children and pregnant women away from casting and setting.

  • Fingers get crushed in presses. Keep hands clear of the platen when the bar is pulled.
  • Burns from the ladle and mould are common; keep the wooden casings on the mould.

What this unlocks

Printing turns Writing and Numbers into mass knowledge. It allows standard forms, tables, almanacs and calendars, textbooks for teaching many people at once, and the accurate copying of drawings and maps. Printed sheets are folded and sewn into books (Bookbinding). The same precision skills — punch cutting, matching parts to the hundredth of a millimetre — feed into Screws, Nuts and Bolts, clocks and Machine Tools.

How it was first done

Woodblock printing began in China by the 7th century AD; the oldest dated printed book, a Buddhist text called the Diamond Sutra, was printed in 868. Around 1040 a Chinese commoner named Bi Sheng made movable type of fired clay, as described by the scholar Shen Kuo. Korean printers cast metal type in the 1200s; the oldest surviving book printed from metal type, the Jikji, dates from 1377. In Mainz, Germany, around 1440–1450, the goldsmith Johannes Gutenberg combined the punch-and-matrix hand mould, a lead-based type metal, oil-based ink and a screw press. His Bible, finished around 1455, was printed in about 180 copies. By 1500 there were printing shops in more than 200 European towns, and many millions of books had been printed.

Source: content/entries/knowledge/printing.md