Part 6 · Building
Arches, Vaults and Domes
How to span doorways, bridges and whole rooms with brick and stone and no beams at all — why an arch stands (the hanging chain turned upside down), how to build one on a wooden centering, how to roof rooms with barrel, groin and Nubian vaults and with domes, and how to stop it all pushing the walls over.
- Difficulty
- ●●●●●
- Time
- A day or two for a doorway arch; weeks for a vaulted room
- Steps from zero
- 6 prerequisites →
This unlocks
—The full path from nothing — 6 steps before this one
- Fire
- Finding and Preparing Clay
- The Kiln
- Bricks
- Lime
- Mortar and Concrete
- Arches, Vaults and Domes
Do them roughly in this order. See it on the tech tree →
Why it matters
Stone and brick are immensely strong when squeezed and weak when bent. A stone beam over a doorway snaps if it is much longer than a metre (Stone Masonry). But stones arranged in a curve, each pressing on the next, can span a doorway, a river or a great hall — with no timber and no steel. Arches built 2,000 years ago still carry roads and water.
Where timber is scarce — deserts, treeless plains, cleared lands — vaults and domes of mud brick or fired brick are the only way to put a roof over a room. They do not rot, burn or get eaten by insects. And the same ideas carry bridges (Roads and Bridges), aqueducts (Pipes, Plumbing and Aqueducts), sewers (Sewers and Wastewater), kilns, ovens and cisterns (Wells and Cisterns).
How it works
The hanging chain
Hang a chain or a string of beads loosely between two nails. Under its own weight it takes a particular curve, called a catenary. Every link pulls on its neighbours in pure tension — no link is bent.
Now turn that curve upside down. An arch of stones in that shape is in pure compression: each stone simply pushes on its neighbours along the curve, with no tendency to bend. That is the perfect arch for carrying its own weight. The English scientist Robert Hooke put it in a single line in 1675: "As hangs the flexible line, so but inverted will stand the rigid arch."
Use it to design your arch. Hang a light chain (or a string of clay beads) from two pegs on a board at the span and rise you want, trace the curve, and flip the drawing. If your arch will carry a wall or a road above it, hang small weights from the chain in proportion to the loads at each point: the chain will change shape, and that new curve is the right arch for that load.
The thrust line and the middle third
A real arch is never exactly the ideal shape, but it does not need to be. The pressure running through the stones (the thrust line) only needs to stay inside the thickness of the arch for it to stand — and if it stays in the middle third of the thickness, no joint will ever try to open. An arch fails when the thrust line escapes the stones: joints open like hinges, and when four hinges form, it falls.
So:
- Thicker arches are safer. For small brick or stone arches, make the ring at least one-tenth of the span deep, and never less than one brick on edge (about 11 cm).
- Fill the haunches (the shoulders of the arch, between the curve and the wall above) with masonry up to about a third of the arch's height. The extra weight there pushes the thrust line back inside a semicircular arch.
- Load arches evenly. A heavy weight on one side pushes the thrust line out on the other.
The push at the feet
An arch pushes down and outward on whatever holds its feet. The flatter the arch, the bigger the outward push: halve the rise and you roughly double the push. A pointed arch pushes outward least, a semicircular one a little more, and a flat or shallow segmental arch most.
The walls or piers at each end — the abutments — must take this push without sliding or tipping. For a semicircular arch in a wall, make each abutment at least a quarter of the span wide; for a flatter arch, a third or more. In a row of arches, as in an arcade or a bridge, the pushes of neighbouring arches balance each other — but the arches at the ends need big abutments.
What you need
| Item | Notes |
|---|---|
| Bricks or stone | Fired Bricks are easiest. For vaults without centering, light mud bricks with lots of straw (Cob, Adobe and Rammed Earth) |
| Mortar | Lime mortar (Lime, Mortar and Concrete); mud mortar for mud-brick vaults; pozzolanic mortar for anything wet |
| Timber for centering | Planks for ribs, boards for lagging, props, and hardwood for wedges (Timber Framing and Log Building) |
| A chain, cord, pegs, a board | For designing the curve |
| A trammel | A straight rod pivoting on a peg, for setting out curves and building domes |
| Plumb line, level | Measurement from Scratch |
Building an arch on centering
- Set out the curve. Draw the arch full size on a flat floor: for a semicircle, swing a cord from the centre; for a catenary, trace a hanging chain.
- Make the ribs. Cut two or more ribs to the inside curve of the arch from planks, built up in two layers with the joints staggered and nailed or pegged together. Space them 60–90 cm apart and join them with cross-pieces.
- Lag it. Nail boards (lagging) across the ribs to make the surface the bricks sit on. Leave small gaps so you can see the mortar joints from below.
- Prop it on folding wedges. Stand the centering on props or on ledges in the wall, with a pair of hardwood wedges, sloping opposite ways, under each prop. Tap the wedges to set the centering exactly at the right height.
- Lay from both sides at once. Start at the springing (where the curve begins) on each side and work up evenly, so the centering is loaded evenly. Each brick or stone (voussoir) points to the centre of the curve. Joints are thin at the inside (intrados) and thicker at the outside (extrados) — no more than about 15 mm thick there; for deeper arches, use wedge-shaped bricks or several separate rings of bricks laid on edge, one over the other.
- Key it. Set the last stone or brick at the crown — the keystone — firmly, driving it in with a mallet so the arch is locked tight.
- Fill the haunches and build the wall above evenly on both sides.
- Wait. Leave the centering in place at least one to two weeks for lime mortar on a small arch, a month or more on a large one.
- Strike it gently. Knock the wedges out a little at a time, all around, so the centering drops a few millimetres at once and the arch settles onto itself. Watch and listen. Then lower it fully and remove it. Stand clear while striking.
Vaults
A vault is an arch stretched out to make a roof.
- Barrel vault — a long half-cylinder. It pushes outward along the full length of both side walls, which must be thick (at least a quarter of the span for a semicircular vault) or have buttresses, or be tied across with timber or iron tie rods at the springing.
- Groin vault — two barrel vaults crossing at right angles. All the push gathers at the four corners, so the walls between can be opened with doors and windows. Square bays only, and the diagonal edges ("groins") are tricky to build.
- Rib vault — arches (ribs) are built across and diagonally first on centering, and the thin panels between them are filled in afterward, needing only light formwork. European builders developed it from about 1100, and it became the mark of Gothic churches.
- Fan, cloister and other vaults follow the same rules.
Build barrel vaults on centering exactly like a long arch, moving the centering along as each section sets, or use the leaning method below.
The Nubian vault: no centering at all
In Egypt, Sudan and across the Sahel, builders have long roofed rooms with mud bricks alone.
- Build the room's walls of mud brick, 40–60 cm thick, with a solid end wall at one end rising above the side walls. Draw the curve of the vault on the end wall — a tall catenary or parabola, its rise at least half the span. Spans of 2.5–4 m are usual.
- Bricks. Make light, thin bricks: about 25 × 15 × 5 cm, with plenty of straw. Drag two fingers across one face of each while wet to make grooves that grip the mortar.
- Mortar. Thick, sticky mud mortar of the same earth.
- Start against the end wall. Lay the first bricks on the side walls, leaning against the end wall, and build up both sides in a small half-arch.
- Lean each course back. Each new course of bricks is laid leaning back at about 20–30° from vertical against the previous one, stuck to it by mortar and suction, working from both sides to meet at the top. Because each course leans on the last, nothing falls while the mortar is wet.
- Fill the haunches with brick and mud as you go, and finish the open end against another wall or a buttress.
- Protect it. Plaster the outside with mud or lime and, in rainy climates, give it a waterproof skin or a light roof over it.
The architect Hassan Fathy revived this method in Egypt in the 1940s, and builders across West Africa still use it today.
Domes
A dome is an arch spun around a vertical axis. It has a great advantage: each horizontal ring, once closed, holds itself up, because every brick in the ring is squeezed by its neighbours. So a dome can be built ring by ring with little or no centering.
- Base. Build a circular wall, or put the dome on a square room using squinches (small arches across the corners) or pendentives (curved triangles) to turn the square into a circle.
- The trammel. Fix a pivot at the centre of the dome's curve and attach a straight rod exactly the dome's inner radius long. Swing it to any position: its tip shows where the inside of each brick goes, and the rod's line shows the angle to tilt it.
- Lay ring by ring, each brick tilted inward toward the centre, using quick-setting, sticky mortar. Complete each ring before starting the next. Near the top, the rings get steep; a light former or a few props may be needed for the last metre, or leave an open oculus (round hole) at the top.
- Hold in the base. In a hemispherical dome, the lower part (roughly the bottom 40% of the curve, measured from the base) is pushed outward and tends to split in vertical cracks. Resist this with a thick base wall, a ring of timber or a chain of iron (The Blast Furnace and Cast Iron, Blacksmithing) set around it, or by giving the dome a taller, pointed or catenary profile that stays in compression throughout.
Corbelled domes — each course of stones projecting a little beyond the one below until they meet — are not true domes, but they are easy. Never let a stone project more than one-third of its length beyond the one below, and weight the back of each stone with the next course. The beehive tombs of Mycenae, Irish stone huts and the trulli houses of southern Italy are built this way.
Buttresses and ties
Every arch, vault and dome pushes out. There are only three ways to resist it:
- Mass. Thick walls and buttresses — projecting piers of masonry against the outside of the wall where the push arrives. The combined push and weight must land within the base of the buttress, ideally within its middle third. Heavy pinnacles on top help by turning the push more downward.
- Flying buttresses carry the push over an aisle or a street to a buttress further out, with a half-arch.
- Ties. A beam or rod across the springing of the arch holds the feet together, as a tie beam holds a roof (Roofs). Iron ties let thin walls carry vaults.
How to tell it worked
- After striking the centering, the crown of a small arch drops no more than a few millimetres, and no joints open.
- Sight along a vault: its curve is even and its line straight.
- The walls and abutments stay plumb; check them with a plumb line after striking and again after a month.
- Hairline cracks at the crown of a vault are common; a crack that widens over weeks, or cracks at the haunches and springing together, means the feet are spreading.
Note Troubleshooting. The arch sags and cracks at the crown and the haunches when the centering is struck → the feet are spreading. Add a tie or bigger abutments; rebuild with a higher rise. Joints open at the haunches → too thin a ring, or haunches not filled. Fill them. A Nubian vault course slides as you lay it → mortar too wet or bricks too heavy. Use lighter bricks and stickier mortar, and lean the course back more. A dome cracks vertically near the base → hoop tension. Bind the base with a tie ring or thicken it. Bricks keep slipping on a steep dome → mortar too slow to grab. Use stickier mortar, or prop each brick briefly until the ring is closed.
Dangers
Danger Arches and vaults can collapse all at once. The most dangerous moments are while building — before the keystone or the last ring is in — and when the centering is struck. Nobody stands beneath or beside an arch or vault while the centering is lowered. Build up both sides evenly; never take the centering out early; never load the top of a fresh arch on one side only. An unbuttressed vault on thin walls can push its walls over without warning, especially in an earthquake.
- Falls from vaults and domes under construction — use scaffolds with rails (Scaffolding and Ladders).
- Earthquakes. Unreinforced vaults and domes are dangerous in earthquake country unless tied. Use ties, keep spans modest, and keep walls thick (Building Against Earthquakes and Storms).
- Lime mortar burns skin and eyes — see Lime.
Going further
- Stone and brick bridges: Roads and Bridges. Aqueducts: Pipes, Plumbing and Aqueducts. Vaulted sewers and cisterns: Sewers and Wastewater, Wells and Cisterns.
- Timbrel (Catalan) vaults are built of thin flat tiles in two or three layers, stuck with fast-setting gypsum plaster, with no centering (Gypsum and Plaster of Paris).
- Concrete vaults and domes — the Roman way — need Mortar and Concrete and, much later, Reinforced Concrete.
How it was first done
Mud-brick arches and vaults were being built in Mesopotamia and Egypt by about 3000–2000 BC. The great storehouses at the Ramesseum, near Luxor in Egypt, built around 1250 BC, are long mud-brick vaults laid without centering, and many still stand. At about the same time the Mycenaeans built the "Treasury of Atreus", a corbelled stone dome 14.5 m across that remained the widest dome in the world for over a thousand years. The Romans made the arch the backbone of their engineering — aqueducts like the Pont du Gard in France, bridges, and the Pantheon in Rome, whose 43 m concrete dome, finished around AD 126, still stands. Byzantine builders set the dome of Hagia Sophia on pendentives in 537. Gothic masons of the 1100s–1200s perfected rib vaults and invented flying buttresses to make walls of glass. Filippo Brunelleschi built the dome of Florence cathedral (1420–1436) without centering, using herringbone brickwork. Robert Hooke explained the arch with the hanging chain in 1675, and the architect Antoni Gaudí designed his churches in Barcelona by hanging weighted strings and turning them upside down.
Source: content/entries/building/arches-and-domes.md