◆ Rebuild

Part 8 · Chemistry

Methanol and Formaldehyde

Wood spirit — methanol from the smoke of a charcoal retort — mixed with air and passed over a glowing coil of copper turns into formaldehyde, a sharp-smelling gas that dissolves in water as formalin. Formalin preserves specimens for study, hardens casein into plastic, disinfects seed grain and instruments, and with phenol from coal tar makes Bakelite. Both substances are poisons and must be handled with respect.

Difficulty
●●●●●
Time
Days to collect enough wood spirit; an afternoon to set up the apparatus; 2–4 hours per run
Steps from zero
13 prerequisites →

You need first

Ether, Acetone and Solvents

This unlocks

—
The full path from nothing — 13 steps before this one
  1. Fire
  2. Finding and Preparing Clay
  3. Sulfur
  4. Pottery
  5. The Kiln
  6. Lime
  7. Fermentation
  8. Lye and Potash
  9. Glass
  10. Distillation
  11. Saltpeter
  12. Sulfuric Acid
  13. Ether, Acetone and Solvents
  14. Methanol and Formaldehyde

Do them roughly in this order. See it on the tech tree →

Why it matters

Methanol (wood spirit) is the simplest alcohol. You can already get it from the watery smoke of a charcoal retort (Ether, Acetone and Solvents). On its own it is a solvent, a lamp fuel and a dangerous poison. Its real value is as the raw material for formaldehyde, one of the most useful chemicals of the 1890s–1920s:

How it works

Methanol is a carbon atom carrying three hydrogens and an –OH group. Pull two hydrogen atoms off it and you have formaldehyde, a gas with a choking smell (it boils at −19 °C). Copper — or silver — at a dull red heat (500–650 °C) does exactly that. Some of the hydrogen leaves as gas; the rest burns with oxygen from the air to water, and that burning gives off enough heat to keep the copper glowing by itself once the reaction has started.

methanol + a little oxygen → formaldehyde + water (over hot copper)

The gas is then bubbled through cold water, where it dissolves. A strong solution — about 37–40% formaldehyde in water — is called formalin. A little methanol left in it (10–15%) stops it from slowly turning into a white solid, paraformaldehyde, so leftover methanol from your run is useful, not a fault.

The trick of the method is the mixture. Methanol vapour and air in between about 6% and 36% methanol make an explosive mixture. So you keep the methanol warm (45–50 °C) while air bubbles through it, so the gas leaving it carries more methanol than that and cannot explode, and you put a flame arrester — a plug of tightly packed copper wire that cools any flame trying to pass, like a miner's safety lamp (Coal and Coke) — between the methanol and the hot copper.

air Methanol, warm bath 45–50 °C keeps the mixture too rich to explode Flame arrester packed copper wire Copper roll, dull red glows by itself once started Lamp to start then lower or remove Cold water absorbers catch formaldehyde gas as formalin Aspirator water runs out, pulling gas through Outdoors. Never unattended. If the copper glows bright orange, reduce the air at once.
Fig. 1 The formaldehyde apparatus. Air is drawn through warm methanol, through a plug of copper wire that stops any flashback, over a glowing copper roll, and through bottles of cold water that catch the formaldehyde. An aspirator jar at the end pulls the gases through, so any leak draws air in rather than letting fumes out.

What you need

Item Amount Notes
Methanol (wood spirit) 200–500 ml per run 85–95%, rectified, from Ether, Acetone and Solvents, Method 1. Keep the first tenth of each distillation separate: it holds most of the acetone.
Copper A roll of fine copper gauze, or 2–3 m of thin copper wire wound into a loose coil 8–10 cm long Copper Smelting, Iron and Brass Wire. Silver gauze works even better (Gold and Silver).
Catalyst tube 1 Hard glass (Laboratory Glassware) or a short iron or fireclay tube, about 2 cm bore and 30 cm long
Spirit lamp or small charcoal burner 1 To start the copper glowing
Bubbler flask 1 Glass flask with a two-hole stopper; one tube reaching to the bottom
Water bath 1 A pot of water at 45–50 °C — too hot to keep your hand in for more than a moment
Flame arrester 1 A 10 cm length of tube packed hard with copper wire or turnings
Absorption bottles 2–3 Each half full of cold water, inlet tubes to the bottom, standing in cold water
Aspirator jar 1 A large closed jar or barrel full of water, with a tap at the bottom; as water runs out, it sucks gas through the whole train (Pottery, Barrels and Cooperage)
Corks or rubber stoppers and tubing Rubber, Laboratory Glassware
Chalk or marble chips A handful To neutralise acid in stored formalin

Where to find it

  • Methanol: from the wood vinegar of a charcoal retort (Charcoal, Ether, Acetone and Solvents). 100 kg of dry hardwood gives only about 1.5–2 litres of crude wood spirit, so collect it from every charcoal burn. Hardwoods — beech, birch, maple, oak — give far more than softwoods.
  • Copper: smelted (Copper Smelting) or native copper, drawn into fine wire (Iron and Brass Wire).
  • Chalk and marble: white rocks that fizz in acid (Rocks and Minerals, Lime).

Methanol from coal and air (outline). Since 1923, nearly all methanol has been made by passing carbon monoxide and hydrogen — made by blowing steam through white-hot coke ("water gas", Coal and Coke) — over a copper–zinc or zinc–chromium catalyst at 250–400 °C and pressures 50–300 times that of the air. It needs steel pressure vessels and compressors, as for Ammonia (Bellows to Air Compressors, Steel). Until you have those, wood is the source.

Step by step

Do the whole thing outdoors or under an open shed, with no other flames nearby except the starting lamp, and with the wind behind you.

  1. Assemble the train in this order: air inlet → bubbler of methanol in the warm water bath → flame arrester → catalyst tube with the copper roll in its middle → absorption bottle 1 → absorption bottle 2 (→ 3) → aspirator jar. Make every joint tight with clean corks or rubber; test by running the aspirator with the air inlet pinched shut: the water should stop flowing.
  2. Fill the bubbler no more than one-third full with methanol, and set it in the water bath at 45–50 °C. Keep the bath at that heat throughout; top it up with hot water.
  3. Fill the absorbers half full with cold water, and stand them in a bucket of the coldest water you have (spring water, or with snow or ice — Ice and Refrigeration).
  4. Heat the copper in the catalyst tube with the spirit lamp until it glows dull red — just visible in shade.
  5. Start the air. Open the aspirator tap so that air bubbles slowly and steadily through the methanol — about 2–3 bubbles a second. Within a minute the copper should keep glowing with the lamp moved away, and the first absorber should start to smell sharp.
  6. Adjust and watch. Remove or lower the lamp once the copper glows by itself.
    • Copper dark and dull → too little air, or the methanol bath is too cold; open the tap a little or warm the bath; reheat with the lamp.
    • Copper glowing bright orange or yellow, or sparks/flame in the tube → too much air. Close the tap partly at once.
    • The copper roll blackens on the inlet side and turns bright pink further in: normal.
  7. Run for 2–4 hours, or until the methanol is nearly gone. Never leave it unattended.
  8. Shut down: close the aspirator tap, remove the lamp, let the tube cool, then open the train. Pour the absorbers together into a glass bottle. Add a few marble chips or a spoonful of chalk to keep it from turning acid.

With a careful run, 100 ml of methanol gives a few tens of grams of formaldehyde in the absorbers — a solution of very roughly 15–30%, with some methanol in it. Call it crude formalin and test its strength before relying on it.

Making it the right strength

Many uses are given in terms of commercial formalin (37–40% formaldehyde). If your crude formalin is weaker, use correspondingly more.

Measuring strength (if you have sodium sulfite and a standard acid). Formaldehyde reacts with a neutral solution of sodium sulfite (made by passing burning-sulfur fumes into soda solution — Sulfur, Soda Ash and Baking Soda) and sets free an equal amount of caustic soda. Neutralise 50 ml of sulfite solution to a red-cabbage colour change (Acids, Bases and Testing), add 5 ml of your formalin, and titrate the alkali that appears back to the same colour with standard acid. Each 1 ml of 1-molar acid used means 30 mg of formaldehyde in the 5 ml. So 30 ml of acid → 900 mg in 5 ml → an 18% solution.

The practical test. Drop a cube of firm gelatin glue jelly or hard-boiled egg white into a 4% solution (your crude formalin diluted accordingly) for 24 hours. Properly fixed, it is rubbery and will not melt or soften in boiling water. Untreated gelatin melts at once.

Useful strengths

Formalin37–40% stock bottleglass, stoppered,poison label Specimens1 + 9 1 part formalin,9 parts water(about 4%) Casein1 + 7 4–5%hardening Footbath1 + 25 3–5% formalinfor foot rot Seed grain1 + 320 a cupfulin 80 litresdip 5–10 min Parts are by volume: strong formalin + clean water. If your formalin is weaker than 37%, use correspondingly more of it.
Fig. 2 Working strengths of formalin. Most uses are a simple dilution of strong formalin with clean water.
Use Strength How
Preserving specimens ("10% formalin") 1 part formalin + 9 parts water (about 4% formaldehyde) Use at least 10 times the specimen's volume. Slice organs no thicker than 1 cm; it soaks in only about 1 mm an hour. Open the body cavity of small animals. After 2 days, specimens can be kept in it or moved to 70% alcohol. Add marble chips.
Hardening casein 4–5% formaldehyde See Early Plastics
Hardening gelatin layers 1–2% A few minutes' dip for glue films or photographic plates
Seed grain against smut and bunt 1 part formalin in 320 parts water (about a cupful in 80 litres) Dip the grain in a sack for 5–10 minutes, or sprinkle and turn until all is wet. Cover with damp sacks for 2 hours, spread to dry, and sow within a few days. Treated grain is not food.
Footbath for foot rot in sheep and cattle 3–5% formalin Walk the animals through a shallow trough; do not let them drink it (Animal Health)
Instruments that cannot be boiled 10% formalin Soak overnight in a closed vessel, then rinse very well in boiled water (Sterilising Instruments and Dressings). It kills bacterial spores only slowly, so treat this as strong disinfection, not certain sterilisation; boil or steam whatever can stand it

Note Fumigation. Formaldehyde gas, boiled off from formalin in a sealed room, was once used to disinfect rooms, incubators and beehive boxes after infection. It is unpleasant and hazardous: the room must be empty of all people and animals, sealed for a day, then aired for a day or more. For houses, scrubbing with soap and hot water, sunlight, whitewash (Lime) and carbolic (Coal Tar Chemicals) are safer.

How to tell it worked

  • Smell: a sharp, stinging smell from the first absorber within minutes; your eyes water if you lean close (don't).
  • Silver mirror: to 2 ml of silver nitrate solution (Nitric Acid) add ammonia water a drop at a time until the brown cloud just clears; add a few drops of your product and warm the tube in hot water. A mirror of silver forms on the glass. Pour it out at once into dilute acid — this silver–ammonia mixture must never be kept, as it can form an explosive solid on standing.
  • Fixing test: gelatin or egg white made rubbery and heat-proof, as above.
  • Specimens: a small fish or a mouse in 10% formalin is still firm, with no smell of rot, after a month.

Note Troubleshooting. Copper will not stay glowing → too little methanol in the air (bath too cold) or too little air; warm the bath, open the tap a little. Copper glows white and the tube cracks → too much air. Reduce the flow; the mixture must stay methanol-rich. Product smells only of methanol → the copper was not hot enough; heat it brighter before starting the air. Product smells sour (vinegar-like) → over-oxidised to formic acid; less air. Add chalk to the bottle. White sediment in the bottle → paraformaldehyde. Store above 15 °C; warm gently to redissolve, or add a little methanol. Aspirator draws but nothing bubbles → a leaking joint. Re-seal.

Dangers

Danger Methanol blinds and kills. As little as 15–30 ml swallowed can kill or blind, and even 10 ml has caused permanent blindness; symptoms come 12–24 hours later. It looks and smells like drinking alcohol. Colour and mark every bottle as poison, and never store it near food or drink (Ether, Acetone and Solvents, Emergencies).

Danger Formaldehyde poisons and causes cancer. The vapour stings the eyes and nose at very low levels and damages the lungs at higher ones; long exposure causes cancer of the nose and throat, and probably leukaemia. Swallowing 30 ml of formalin can kill. It hardens and cracks skin and makes many people allergic for life. Work outdoors or in a strong draught, keep vessels covered, wear gloves and eye protection, and never sniff it directly. Splashes in the eyes: rinse with water for 15 minutes.

Danger Explosion and fire. Methanol vapour and air explode over a wide range of mixtures, and methanol burns with an almost invisible flame in daylight. Keep the bubbler warm so the mixture stays rich, always fit the flame arrester, keep the only flame the starting lamp, and keep a damp sack and a bucket of sand by you.

  • Spills of formalin: cover with ammonia water (Ammonia), which turns formaldehyde into a far less volatile solid, then wash away with plenty of water.
  • Store formalin and methanol in glass, tightly closed, labelled, cool but not freezing, out of reach of children, and away from acids and from strong oxidisers such as saltpeter and bleach.
  • Specimens and treated seed are poisonous: never feed treated seed to animals or people.

What this unlocks

Permanent teaching collections for How the Body Works, Cells, Life and Evolution and the The Microscope; healthier grain crops and flocks (Farming from Seed, Animal Health); casein buttons and Bakelite switches, insulators and telephone cases (Early Plastics, The Telephone, Wiring and Electrical Safety); waterproof plywood glues (Glues and Adhesives); hardened photographic plates (Photography). The method itself — a gas passed over a hot metal catalyst that speeds a reaction without being used up — is the same idea behind sulfuric acid by the contact process (Sulfuric Acid), ammonia from the air (Ammonia) and most of modern chemical industry.

How it was first done

Robert Boyle noticed a spirit in the products of distilling wood in 1661, and in 1834 Jean-Baptiste Dumas and Eugène Péligot in Paris showed that wood spirit was a distinct alcohol, methyl alcohol. In 1859 the Russian chemist Alexander Butlerov made formaldehyde, without quite recognising it. In 1867 August Wilhelm von Hofmann in Berlin passed methanol vapour and air over a glowing platinum spiral and identified the gas properly. The German chemist Oscar Loew showed in 1886 that copper worked as a catalyst, and from 1889 Auguste Trillat in France made formaldehyde commercially; it was soon sold as "formalin".

In 1893 the Frankfurt doctor Ferdinand Blum found by accident that formaldehyde hardened the skin of his fingers, and introduced it to preserve tissue — it is still the standard fixative in hospitals. In 1897 Henry Bolley of North Dakota showed that formalin killed the smut on seed wheat. In 1907 Leo Baekeland turned phenol and formaldehyde into Bakelite. Synthetic methanol from carbon monoxide and hydrogen was first made on a large scale at BASF in Leuna, Germany, in 1923.

Source: content/entries/chemistry/formaldehyde.md