Part 5 · Cloth and Clothing
The Loom
Build a frame loom with a rigid heddle for your first fast weaving, then a floor loom where your feet open the sheds and a reed spaces and beats the cloth. Learn to warp it, thread it and weave plain cloth and twill — and add the flying shuttle that doubled a weaver's speed.
- Difficulty
- ●●●●●
- Time
- 2–4 days for a rigid-heddle frame loom; 3–6 weeks for a floor loom; a day to warp it; then about a metre of cloth a day
- Steps from zero
- 4 prerequisites →
This unlocks
Linoleum, Oilcloth and FloorclothsRopewalks and SailclothBlankets, Curtains, Rugs and TowelsTextile MachineryThe full path from nothing — 4 steps before this one
Do them roughly in this order. See it on the tech tree →
Why it matters
On a backstrap or warp-weighted loom (Spinning and Weaving Cloth), your hands do everything: lift the heddle rod, hold the shed open, pass the weft, and beat. A floor loom hands the shedding to your feet and the spacing and beating to a swinging frame, so your hands only throw the shuttle and pull the beater. A weaver on a floor loom makes several times as much cloth in a day as on a backstrap loom, and with four or more shafts can weave twills and patterns with no extra effort.
The loom is also where the industrial age began. The flying shuttle (1733) let one weaver make wide cloth twice as fast — so fast that spinners could not keep up, which drove the invention of the spinning machines and then the power loom (Textile Machinery). The Jacquard loom's punched cards later inspired the first programmable machines (The Computer).
How it works
Every loom does three things over and over:
- Shedding — lifting some warp threads and lowering others to open a gap (the shed).
- Picking — passing the weft through the shed.
- Beating — pushing the new weft tight against the cloth (the fell).
Then it changes the shed, and repeats. A floor loom mechanises shedding and beating:
- Heddles are loops of strong thread (or wire), each with an eye in its middle. Every warp thread passes through the eye of one heddle.
- The heddles hang on shafts (also called harnesses) — frames of two horizontal bars that can rise and fall. Threads on shaft 1 move together; threads on shaft 2 move together, and so on.
- Treadles under your feet are tied to the shafts. Press a treadle, and its shafts move. In a counterbalance loom, the shafts hang in pairs from cords over a roller at the top: when one shaft is pulled down, its partner rises. That opens a clean shed.
- The reed is a comb, closed top and bottom, with evenly spaced gaps (dents). It keeps the warp threads evenly spaced across the full width and, held in a swinging beater (batten), it packs each weft against the cloth.
- The warp beam at the back stores the unwoven warp, rolled up; the cloth beam at the front rolls up the finished cloth. Each has a ratchet and pawl so it holds the warp tight and can be advanced a few centimetres at a time.
Plain weave needs two shafts: odd threads on shaft 1, even on shaft 2. 2/2 twill needs four shafts, threaded 1-2-3-4, 1-2-3-4, and four treadles tied to lift (or lower) shafts 1+2, 2+3, 3+4, 4+1 in turn.
What you need
For a four-shaft counterbalance loom that weaves cloth up to 90 cm wide:
| Part | Size | Notes |
|---|---|---|
| Frame | About 130 cm wide, 140 cm deep, 150–170 cm tall | Posts and rails 8 × 8 cm or 10 × 10 cm of oak, ash, beech or maple, joined with pegged mortise and tenon |
| Warp beam and cloth beam | Round or eight-sided rollers 8–10 cm thick, 110 cm long | Turn in holes in the side frames; each with a ratchet wheel and pawl |
| Back beam and breast beam | Smooth rails 6–8 cm thick, 110 cm long | The warp runs over them |
| Shafts | 4 frames, 100 cm wide, of two bars 2 × 4 cm joined by end pieces | Heddles slide on the bars |
| Heddles | About 8–12 per cm of cloth width, so 700–1,000 | Linen or cotton thread, about 25–28 cm long, with a 6–8 mm eye in the middle |
| Reed | 100 cm long, 10–12 cm tall; 5–8 dents per cm for wool, 10–12 for linen | See below |
| Beater (batten) | A frame 110 cm wide holding the reed, swinging from the top or from the floor | Heavy enough to pack the weft |
| Treadles | 4–6 boards 3 × 6 cm, 80–100 cm long | Hinged at the back or front |
| Lamms | 4 bars under the shafts | Link shafts to treadles |
| Counterbalance roller | A round bar 6–8 cm thick at the top, with cords | Or pulleys (Simple Machines) |
| Shuttles | Boat shuttles 30–35 cm long holding a bobbin | Stick shuttles to start |
| Warping board | A frame 1 × 1.5 m with 10–12 pegs | For measuring the warp |
| Raddle | A bar with pegs every 1 cm | Spreads the warp while beaming |
Tools: saws, chisels, augers, a spokeshave or drawknife, ideally a The Lathe for the beams and shuttles (Basic Woodworking, Drills and Boring). A smith can forge ratchet pawls; hardwood ones work.
Where to find it
- Timber: oak, ash, beech, maple, cherry or other dense hardwoods for the frame and beams; dry and stable, so the loom does not twist (Basic Woodworking). Old looms were built from riven, seasoned timber.
- Reed or cane for the reed dents: split cane, bamboo, or the stems of common reed (the same reed used for pens in Ink). Thin strips of hardwood or hammered brass or iron wire also work.
- Heddle thread: strong, smooth, plied linen (Flax, Hemp and Linen) or cotton (Cotton), waxed with beeswax.
- Cords for tie-ups and the counterbalance: hemp or linen (Cordage and Rope).
Method 1: A frame loom with a rigid heddle
This is the fastest loom to build and a big step up from the backstrap. It weaves plain cloth up to about 50–60 cm wide.
Build it
- The frame: two side pieces 80–100 cm long, 5 × 2.5 cm, joined by a back beam and a front beam (smooth rails 70 cm long) to make a rectangle. Rest one end on a table and the other against your waist, or give it legs.
- Two rollers below the beams at each end: round poles 3–4 cm thick, in holes in the side pieces, each with a peg handle and a simple ratchet — a notched wooden disc and a pawl (a stick that drops into the notches) — or simply a peg that pushes through a hole to lock it.
- The rigid heddle: make 100–200 slats of thin hardwood, cane or bone, each about 10 cm long, 5–8 mm wide and 2–3 mm thick. Drill or burn a 3 mm hole through the middle of each. Glue or bind them, evenly spaced with 3–4 mm gaps (the slots), between a top and bottom rail 2 × 2 cm. Every gap and every hole carries one warp thread, so slats 3 mm thick with 3 mm gaps give about 3–4 threads per cm.
- Rests on the side pieces hold the heddle in a raised position (a notch in a block above the warp) and a lowered position (a notch below), and in the middle for threading.
Warp and weave
- Wind a warp on a warping board (Spinning and Weaving Cloth), tie the cross, and tie one end to the back roller.
- Thread the heddle: one warp thread through each slot and each hole, alternately, across the width.
- Wind the warp onto the back roller under firm, even tension, then tie the front end to the front roller in small bundles. Tension must feel the same in every bundle.
- Raise the heddle: the hole-threads rise, slot-threads stay down. Pass the weft. Bring the heddle forward to beat.
- Lower the heddle: the hole-threads drop below. Pass the weft back. Beat.
- Advance the warp when the fell is about 5 cm from the heddle.
Method 2: The floor loom
Build the frame
- Make two side frames, each a rectangle of two posts and two rails, 140 cm deep and 150–170 cm tall, joined with pegged mortise-and-tenon joints (Basic Woodworking).
- Join them across the front and back with rails at the bottom, and at the top with a castle (cross-beam) to carry the counterbalance roller over the middle of the loom.
- Fit the breast beam at the front and the back beam at the back, both about 90–100 cm from the floor, rounded and smooth on top.
- Bore holes lower down in the side frames for the cloth beam (front) and warp beam (back). Fix a ratchet wheel — a wooden or iron disc with 12–20 slanted teeth — to one end of each beam, and a hinged pawl on the frame that drops into the teeth. The warp beam pawl holds back; the cloth beam pawl holds forward. Make a lever or handle to turn each beam.
Shafts, heddles and treadles
- Shafts: for each, two straight bars a little longer than the weaving width, held a heddle-length apart by thin end pieces, so the heddles can slide along the bars.
- Heddles: make a jig — a board with four pegs: two 26 cm apart for the heddle length, and two 6–8 mm apart in the middle for the eye. Tie each heddle round the pegs with a knot at the eye and at each end so all are identical. Wax them. It is slow work: a few hundred an evening.
- Counterbalance: hang the shafts in pairs (1 with 2, 3 with 4) by cords from horses — short rocking bars — which hang in turn from the roller at the top. When one shaft of a pair is pulled down, the horse tips and lifts the other.
- Lamms: hinge four bars to one side of the frame under the shafts, and tie each to the bottom of its shaft.
- Treadles: hinge 4 (or 6) boards at the back of the loom floor. Tie up each treadle to the lamms it should pull down. For plain weave: treadle A to shafts 1 and 3, treadle B to shafts 2 and 4 (with the warp threaded 1-2-3-4). For 2/2 twill: treadle 1 to shafts 1+2, treadle 2 to 2+3, treadle 3 to 3+4, treadle 4 to 4+1.
Make the reed
- Split cane, bamboo or reed into thin, flat strips (dents), all exactly the same thickness, about 2–3 mm wide and 0.5–1 mm thick, and 10–12 cm long. Smooth them.
- Take two pairs of thin half-round rods (top and bottom) the length of the reed.
- Set the dents upright one at a time between each pair of rods, and between each dent wrap a strong waxed or pitched thread round the rods several times. The number of wraps sets the spacing. Count dents per 10 cm often and adjust.
- Bind the ends with end posts. The finished reed must have perfectly even gaps; uneven dents give stripes in the cloth.
Fix the reed in the beater — two horizontal bars with a groove for the reed, joined by two swords (uprights) that swing from pivots on the top of the frame (an overhead beater) or on the floor.
Warp the loom ("dressing")
- Measure the warp on a warping board: decide length (cloth length + about 70 cm wastage for tying on and the end you cannot weave), number of threads (width × sett), and wind them in groups with a cross at one end (see Spinning and Weaving Cloth). Tie the cross securely and tie the warp in several places (choke ties) before taking it off.
- Spread it in a raddle (a bar with pegs every 1 cm) to the full width, so the threads go onto the warp beam evenly.
- Beam on: tie the end loops to a rod fixed to the warp beam, and wind the warp onto the warp beam while a helper holds it firmly from the front, combing out tangles. Lay sticks or stiff paper between layers so the threads cannot sink into each other.
- Thread the heddles: sit inside the loom. Taking the threads in order from the cross (held by lease sticks), pass each through the eye of a heddle on the right shaft — 1, 2, 3, 4, 1, 2, 3, 4... — using a hook made of bent wire or a slim stick. Check every few centimetres.
- Sley the reed: pass the threads through the dents in order, one or two per dent, from the centre outwards so the warp is centred.
- Tie on to a rod attached to the cloth beam in bundles of 2–3 cm, using a half-bow knot. Then go back and tighten each bundle until the tension feels the same across the whole warp — press your palm across it like a drum.
- Weave a header: a few picks of thick yarn to spread the bundles and even out the warp.
Weave
- Press a treadle. Throw the shuttle through the shed from one hand to the other, leaving the weft at a slight angle across the warp.
- Pull the beater firmly towards you to pack the weft.
- Change treadles, then beat again — many weavers beat on the closed or changing shed to lock the weft in.
- When the fell is about 8–10 cm from the reed, release the warp beam pawl, wind the cloth beam forward 5–8 cm, and re-tension.
- Keep the beat the same every time. An even beat gives an even cloth.
An experienced weaver on a floor loom weaves roughly a metre of medium cloth a day, more with plain weave and thick yarn.
The flying shuttle
On a wide loom, a weaver cannot reach across to pass the shuttle from hand to hand; wide cloth needed two weavers. The flying shuttle fixes this:
- The race: fix a smooth, flat, slightly sloping shelf, 5–7 cm wide, along the bottom of the beater, just in front of the reed. The bottom layer of the shed lies on it.
- Shuttle boxes: extend the race 35–40 cm beyond each side of the warp, with a back wall, a front wall and a lid, to form a box the shuttle fits into.
- Pickers: a block of hard leather or wood in each box, sliding on a smooth rod (spindle) along the length of the box.
- Picking cords run from each picker to a single wooden handle — the picking stick — hanging in front of the beater's centre.
- The shuttle: a boat-shaped piece of hard, polished wood (boxwood or apple), 35–40 cm long, with metal-tipped points, small rollers or a waxed underside, holding a pirn (a long, thin bobbin of weft) that feeds out through an eye in its side.
To weave: one hand holds the beater, the other the picking stick. Jerk the stick towards one side: the picker flicks the shuttle across the race through the shed and into the far box. Beat, change the shed, jerk the other way. With practice, a weaver can throw 40–60 picks a minute and weave cloth of any width alone.
How to tell it worked
- Clean sheds: when a treadle is pressed, the shed opens wide (at least 4–5 cm at the reed) with no threads straggling in the middle.
- Even cloth: edges straight, width constant, picks evenly spaced, no stripes from uneven dents, no floats (skipped threads).
- Even tension: the warp feels equally tight everywhere, and stays so as the cloth is wound on.
Note Troubleshooting. A thread stays in the middle of the shed → threading mistake, crossed thread, or a heddle missing. Find and re-thread it. Shed too small → shafts not hanging level, cords stretched, or warp too slack. Level the shafts and retension. Weft streaks, thin and thick bands → uneven beat, or uneven reed dents. Cloth narrows (draw-in) → weft too tight. Lay it at a steeper angle before beating. Broken warp threads → weak warp yarn, too much tension, or a rough reed or heddle. Tie in a repair thread with a weight hanging off the back. Flying shuttle falls out of the shed → race not sloping slightly back towards the reed, shed too small, or the beater was moving when you threw. Throw only when the beater is fully back.
Dangers
Warning Flying shuttles fly. A shuttle that leaves the race travels fast enough, with its metal tips, to break teeth or blind an eye. Mill weavers were often hurt this way. Fit a shuttle guard — a wire or wooden bar along the front of the beater — keep the race clean and smooth, and never stand to the side of a running loom at shuttle height.
- Pinched fingers between beater and breast beam, and in ratchets. Keep hands clear when beating and releasing pawls.
- Heavy beams full of warp are awkward to lift; lift with two people.
- Posture. Set the bench height so your thighs are level and your elbows just above the breast beam; long days at a badly set loom cause back and shoulder pain.
What this unlocks
Cloth in quantity: Making Clothes, bedding, sacks, sailcloth for Boats and Sails, belting for Belts, Chains and Power Transmission. Patterned and dense cloths for upholstery (Mattresses and Upholstery, Blankets, Curtains, Rugs and Towels) and heavy wear. The loom's mechanisms — shafts lifted by cams, a shuttle thrown by a picker, beams advanced by ratchets — were the first things to be driven by water and steam: the power loom and the Jacquard loom (Textile Machinery). The Jacquard's punched cards, choosing which threads rise for each pick, were the ancestors of the cards of tabulating machines (Punched-Card Tabulating Machines) and early The Computers.
How it was first done
The first looms were the horizontal ground loom of Egypt (painted on a bowl about 6,000 years old), the backstrap loom and the warp-weighted loom (Spinning and Weaving Cloth). The treadle loom with heddles moved by the feet appears in China, probably by the Han dynasty around 2,000 years ago, and spread west; by the 11th century, horizontal treadle looms were working in Europe's cloth towns, and weaving became a full-time trade organised in guilds. In 1733 John Kay, from Lancashire in England, patented the flying shuttle. Weavers feared for their jobs and attacked his house, and manufacturers refused to pay him royalties; he died poor in France. But the flying shuttle spread, roughly doubling a weaver's output and creating a hunger for yarn that led to the spinning jenny (1764), the water frame (1769), Edmund Cartwright's power loom (1785) and Joseph-Marie Jacquard's card-controlled loom (1804).