◆ Rebuild

Part 13 · Electricity

Electric Bells, Buzzers and Alarms

An electromagnet that switches itself off and on makes a hammer strike a gong twenty times a second. That trembler bell, a push button and two cells make a doorbell; add numbered flaps and it calls servants or nurses; wire it through door contacts and heat detectors and it guards a house against burglars and fire. How to build each, and how to make alarms that sound even when the wire is cut.

Difficulty
●●●●●
Time
An evening for a buzzer; a day or two for a bell and doorbell circuit; a week to wire a house alarm
Steps from zero
18 prerequisites →

You need first

The ElectromagnetThe Battery

This unlocks

—
The full path from nothing — 18 steps before this one
  1. Fire
  2. Cordage and Rope
  3. Stone Tools
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Hunting and Trapping
  7. Basic Woodworking
  8. Charcoal
  9. Pottery
  10. Hides and Leather
  11. Fermentation
  12. Bellows
  13. Copper Smelting
  14. Iron (the Bloomery)
  15. Blacksmithing
  16. The Battery
  17. Copper Wire
  18. The Electromagnet
  19. Electric Bells, Buzzers and Alarms

Do them roughly in this order. See it on the tech tree →

Why it matters

A bell is the simplest useful thing electricity can do, and one of the most important. A doorbell tells you someone is at the gate a hundred metres away. A call bell brings a nurse to a patient's bed at night (Running a Hospital, Nursing the Sick). A bell on a The Telegraph or The Telephone line says "answer me". A bell that rings when a door is forced, or when the ceiling of a barn grows hot, wakes a whole household before the thief or the fire can do their worst (Firefighting).

Bells need very little: an The Electromagnet, a strip of spring, a gong, a push button, two or three cells from The Battery, and some thin wire. They are the right first project once you can wind a coil, and the same ideas — a contact that interrupts its own current, a relay that holds itself in — reappear in the The Induction Coil, the The Relay Computer and the The Automatic Telephone Exchange.

How it works

The trembler bell

Gongbronze or brass cupHammerbrass ball, 2–3 mm offContact screwsilver tip, locknutArmaturesoft iron, 1–2 mm offTwo coils400 turns of 0.5 mm eachSoft iron yokeFlat springsteel, 0.25 mmContact springsilver dotBrass pillarCellsPushBA
Fig. 1 The trembler electric bell. Current from the cells flows through the push button, round the two coils of the horseshoe electromagnet, through the contact screw and the contact spring, and back through the armature's spring. The magnet pulls the armature, the hammer strikes the gong — and the contact opens, cutting the current. The spring pulls the armature back, the contact closes, and it all happens again, twenty times a second.
  1. Press the button. Current flows round the coils of a horseshoe electromagnet, through a contact at the back of the armature, and back to the cells.
  2. The magnet pulls the soft iron armature towards its poles. The hammer on the armature's end strikes the gong.
  3. As the armature moves, its contact spring lifts off the contact screw. The circuit is broken; the magnet lets go.
  4. The armature's spring throws it back; the contact closes; the magnet pulls again.

This make-and-break — the same trick as the interrupter of the The Induction Coil — repeats 15–30 times a second for as long as the button is held, giving the familiar rattling ring.

Variations on one idea

  • Single-stroke bell: no contact; the coil is wired straight to the terminals. One press gives one stroke. Used where strokes are counted — railway block signals (Railway Signalling and Safety), fire station codes, ship's telegraphs.
  • Buzzer: a trembler with no hammer and no gong; a light, stiff reed vibrates fast (100–300 times a second) and hums. Quieter, for a desk, a telephone set or Morse practice (The Telegraph).
  • Continuous-ringing bell: rings on after the button is let go, until someone resets it. Needed for alarms (see below).
  • Polarised ringer: worked by alternating current from a hand magneto, used on telephones (The Telephone).

Open and closed circuits

A doorbell is an open-circuit system: no current flows until a push closes the circuit. The cells last a year or more because they rest almost all the time. Its weakness, for an alarm, is that a cut wire or a dead cell simply makes it silent.

A closed-circuit system has a small current flowing all the time through a loop of wire and every guarded contact, holding a relay pulled in. Anything that breaks the loop — a door opening, a window lifting, a burglar cutting the wire, a fuse melting in a fire — lets the relay drop, and its back contact rings the bell. It fails noisily instead of silently. That is the rule for every serious alarm.

What you need

Item Size and notes
Soft iron Two rods 8 mm thick, 35 mm long; strip 50 × 12 × 4 mm for the yoke; armature 40 × 10 × 4 mm (Iron (the Bloomery), annealed)
Covered copper wire 0.5 mm, about 40 m for one bell; 0.6–0.9 mm "bell wire" for the circuits (Copper Wire)
Spring steel or springy brass Strip 0.25 mm thick, 10 mm wide (Springs)
Gong Bell bronze, brass or steel cup 7–10 cm across (Bronze, Sheet Metal and Rolling)
Contacts Silver, as small rivets or dots; platinum is best but rare (Gold and Silver)
Brass Pillars, screws, terminals, push springs (Zinc and Brass, Screws, Nuts and Bolts)
Hardwood Base boards, push bodies, boxes
Cells 2–3 Leclanché cells for open circuits (Dry Cells and Electric Torches); Daniell or gravity cells for closed circuits (The Battery)
Shellac, wax Varnishing coils; waterproofing wire (Copper Wire)

Every part is made in other chapters. The only new skill is adjusting springs and contacts patiently.

Making the electric bell

The magnet

  1. Cores: file two soft iron rods 8 mm thick to 35 mm long, flat-ended. Tap a thread on one end of each, or rivet them, into holes 25 mm apart in a soft iron yoke 50 × 12 × 4 mm. Anneal everything after shaping (The Electromagnet).
  2. Bobbins: wrap each core in two layers of shellacked paper, with fibre or hardwood cheeks 22 mm across at each end, leaving 30 mm to wind.
  3. Wind each with about 400 turns of 0.5 mm cotton- or silk-covered wire, both in the same direction as seen from the yoke. Join the inner ends so that, as with any horseshoe magnet, one pole becomes north and the other south. The pair will measure about 3 Ω: right for 2–3 Leclanché cells and a run of up to about 30 m of bell wire. For long lines, wind more turns of thinner wire (0.3 mm), making 10–20 Ω, and use more cells.
  4. Varnish, and screw the yoke to the hardwood base (10 × 15 cm, 15 mm thick) with the pole faces standing up.

The armature and contact

  1. Armature: a bar of soft iron 40 × 10 × 4 mm, riveted to a strip of spring steel 0.25 mm thick, 10 mm wide and 60 mm long. Screw the lower end of the spring to a brass pillar so the armature hangs across both pole faces, 1–2 mm away at rest.
  2. Hammer: a stiff steel wire 2 mm thick and 50 mm long, fixed to the top of the armature, ending in a brass ball 8–10 mm across.
  3. Contact spring: a thin springy brass strip riveted to the back of the armature, carrying a small silver dot.
  4. Contact screw: a brass screw with a silver tip, through a brass pillar behind the armature, with a locknut. It just touches the silver dot when the armature is at rest.
  5. Gong: mount it on a pillar or a screw through its centre so its rim sits 2–3 mm from the ball at rest. A cast bronze gong (about 78 parts copper to 22 of tin) sings longest; spun or hammered brass is louder than steel.
  6. Wire it: terminal A → one coil → the other coil → contact screw pillar; contact spring → armature spring → armature pillar → terminal B.

Adjust

  1. Connect two cells and a push. Turn the contact screw in until the bell rings, then find the setting that gives the loudest, steadiest ring at the lowest voltage. Tighten the locknut.
  2. Bend the hammer wire so the ball strikes the gong squarely and bounces clear. A ball resting on the gong makes a dull clack.

A good bell rings at once on every press, even with one cell; rings cleanly with only a pin-point spark at the contact; and keeps ringing for minutes without sticking. A bad one hums without striking (contact screw too far in), clicks once and stops (screw too far out, or armature touching the poles and sticking — put a scrap of paper or a brass pin on each pole face so iron never touches iron), or sparks heavily and soon burns its contact.

Tip Taming the spark. The coils store energy that leaps across the contact as it opens, burning it. A resistance of about 10 times the coil's resistance wired straight across the coils (a few metres of thin iron or German silver wire wound on a spool), or a condenser across the contact (Resistors, Capacitors and Coils), cuts the spark greatly.

Buzzer

Make a smaller magnet — a single core 6 mm thick and 25 mm long with 300 turns of 0.3 mm wire — under a stiff steel reed 0.4 mm thick and 40 mm long, clamped at one end, with a contact as for the bell. Mount it in a small wooden box, which acts as a sounding board. A shorter, stiffer reed buzzes higher.

The doorbell

Push button

Push buttonAnnunciator dropHeat detector Bone buttonUpper springspringy brassLowerspring2–3 mmhardwood or porcelain body 4 CoilArmaturewith catchFlap held upout of sightSpringfalls behind the glassand shows the number ceiling blockSpring armpressed downby a springSolderedlinkmelts at ~95 °CFixed contactthe arm drops onto itand closes the circuit
Fig. 2 Left: the push button, cut in half. Pressing the bone or hardwood button bends the upper brass spring down onto the lower one, closing the circuit; letting go, it springs back. Centre: one window of an annunciator. Current from a room's push pulls the armature, which releases a catch, and the numbered flap falls into view. Right: a heat detector. A spring presses a contact arm towards a fixed contact, but a link soldered with low-melting metal holds it up; heat from a fire melts the solder and the arm drops onto the contact.
  1. Body: a round block of hardwood or porcelain 5–6 cm across with a hollow underneath and a hole through the centre of its cover.
  2. Springs: two strips of springy brass, each screwed to the base and to a terminal. The upper one arches over the lower with a gap of 2–3 mm; both have a silver or clean brass contact where they meet.
  3. Button: a peg of bone, horn or hardwood (Horn and Bone Working) that slides freely in the cover hole and rests on the upper spring.
  4. For an outside door, cover it with a brass plate and shed rain away from the hole; fill the space round the wires with wax. For a bedside, hang the same thing on a cord as a pear-shaped pendant push.

Wiring

  • Bell wire: 0.6–0.9 mm copper, double cotton-covered and waxed, run along skirting and under eaves on small insulated staples, kept out of the rain. Two wires, side by side.
  • Supply: 2–3 Leclanché cells in series in a dry cupboard. They rest between rings and recover, so they last a year or more. A Daniell cell is wrong here — it wears out by itself whether used or not. On a mains supply, use a small bell transformer giving 8–12 V (The Transformer): its primary must be fused and fully enclosed, its secondary wiring never joined to the mains.
  • Several pushes to one bell: wire them in parallel. Front and back door: a bell for one and a buzzer for the other, so you know which door to go to.
  • Long lines: over about 100 m, use thicker wire, more cells, or a relay at the far end switching a local battery.

Call-bell boards

An annunciator (indicator board) tells you which push rang. It is a glass-fronted box with a numbered window for each room, wired so each room's push passes current through its own small electromagnet, then on to a single common bell.

  • The drop: in each window, a light pivoted flap carrying the room's number, held up out of sight by a catch on a small iron armature. Current through the electromagnet (300 turns of 0.3 mm wire on a 6 mm core) pulls the armature; the catch slips; the flap falls into view and stays down.
  • Reset: a rod along the bottom of the box, worked by a knob outside, pushes all fallen flaps back up past their catches.
  • Wiring: one wire from each push to its drop; one common return wire from all the pushes to the cells; the bell in the common line. With ten rooms you need eleven wires to the board, not twenty.

Use it in hospitals (each bed's pendant push), hotels, offices and schools. Fit a key-switch at the board to test every drop each morning.

Burglar alarms

cell Door contactsclosed while shutWindow foilDaniell cell5–20 mA flows round the loop all the timeCut wirealso rings the bellRelay coil100–300 Ω; holdsthe lever downBack contactLatchBellbell cellsKey switchsets and resetsdashed: lever after the relay lets go
Fig. 3 The closed-circuit burglar alarm. A small, steady current from a Daniell cell flows round a loop through every door and window contact and through the coil of a relay, holding its armature down. If any door opens, or the wire is cut, the relay lets go. Its back contact closes the bell circuit, and a second contact on the relay latches it so the bell rings on until the key switch is turned.

The closed-circuit alarm

  1. The loop: a single pair of bell wires runs from the control box to every door and window and back. At each, a door contact — two springy brass strips on the frame, pressed together by a stud on the door when it is shut — is wired in series. All shut, the loop is complete.
  2. The relay: wound with many turns of thin wire, 100–300 Ω, so that one or two Daniell or gravity cells push only 5–20 mA round the loop. A Daniell cell gives such a small current steadily for months (The Battery). Adjust the relay so it holds firmly at that current and lets go at half of it.
  3. The bell circuit: the relay's back contact (closed when the armature is released) switches a loud bell from a separate set of Leclanché cells.
  4. The latch: a second contact on the relay, closed when it lets go, keeps the bell ringing even if the door is shut again. The simplest latch is mechanical: a drop like the annunciator's, released by the relay, that falls and holds the bell contacts closed until reset by hand.
  5. The key switch: a lock-worked switch on the box that disconnects the bell when you set or unset the alarm, and resets the latch. Put the box inside, out of sight, and the bell outside, high up in a strong box, plus a second bell indoors.

Other detectors

  • Pressure mat: two sheets of thin copper or tinned gauze, separated by a sheet of felt 3–5 mm thick punched full of holes 2 cm apart, sewn into a canvas envelope and laid under a rug. A foot presses the sheets together through the holes. This is a closing contact: wire it to a separate input that drops the relay by shorting its coil through a resistance, so the loop stays fail-safe.
  • Trip wire: a fine wire, part of the loop, stretched across a passage or window opening at shin height; it breaks or pulls out of a spring clip when touched.
  • Window foil: a strip of thin tin or lead foil (Tin and Pewter) varnished onto the glass round its edge, in the loop; breaking the glass breaks the foil.

Note Troubleshooting. Bell hums but does not ring → contact screw too far in; or armature rubbing. Bell clicks once and stops → contact screw too far out; armature sticking to the poles; or cells exhausted. Test each cell. Bell rings by itself → a push wet inside, or wires chafed together. Dry it; re-run the wire. Alarm triggers at random → a loose door contact; damp leakage making the current wander; the relay set too fine. Tighten contacts, check each with a galvanometer, raise the drop-out setting. Alarm does not ring when tested → relay sticking (paper on the pole face), bell cells flat, or the latch not falling. Test every week.

Fire alarms

Fire alarms use the same closed-circuit loop, with two kinds of trigger:

  • Call point ("break glass"): a small box with a thin glass front. Behind it, a spring contact is held closed by the glass. Breaking the glass with a fist or the attached hammer lets the spring open, breaking the loop. Put one by every exit and on every landing, at shoulder height, and paint the box red.
  • Heat detector: a springy contact arm held away from a fixed contact by a small link soldered with low-melting metal — Rose's metal, about half bismuth and a quarter each of lead and tin (Antimony and Bismuth), melts at about 95 °C. Heat from a fire melts the solder, the arm drops onto the contact, and that shorts the relay coil so it lets go. A bimetal strip set to close at 60–70 °C (Thermostats and Automatic Control) does the same job and can be tested and reused. A mercury The Thermometer with one wire sealed into the bulb and another into the tube at the 60 °C mark is the classic laboratory version (Mercury).
  • Siting: fix heat detectors on the ceiling, at the highest point of each room, no more than about 7 m apart, and never near a stove where normal heat will set them off. Hot air gathers at the ceiling first.
  • The bell: use a big gong, 15–25 cm, ringing continuously, and agree with everyone that this sound means fire, get out — different from the burglar bell and the doorbell.

Warning A heat detector only sounds once a fire is well under way. It buys minutes, not hours. It does not replace a night watch, safe stoves and chimneys, or a practised way out of every room (Firefighting, Fire Extinguishers and Alarms). Detecting smoke early needs a light beam and a photocell (Photocells and Sensors).

How to tell it worked

  • Every push, at the farthest end of the house, rings the bell at once.
  • The annunciator shows the right number for every room.
  • Alarm walk test: with the alarm set, open each door and window in turn, cut a test link in the loop, break a spare call-point glass, and warm each bimetal detector with a hot iron. Every one must ring the bell, and the bell must keep ringing until the key resets it.
  • Take a cell out of the loop battery: the alarm must ring (fail-safe).

Dangers

  • Mostly safe: bell circuits run at 3–12 V and cannot hurt you.
  • Bell transformers are joined to the mains on one side. Mount them in a closed box, fuse the primary, and never let a bell wire touch a mains wire (Wiring and Electrical Safety).
  • Cells contain acids or sal ammoniac paste that leak and corrode; keep them in a box away from children.
  • Mercury in a thermometer detector is poisonous if spilled (Mercury).
  • False alarms breed contempt. An alarm that rings for nothing teaches people to ignore it. Fix every false alarm at once, and test on a fixed day each week.

Danger Never let an alarm lock people in. Doors on escape routes must open from the inside without a key, whatever the alarm or the lock is doing (Locks and Keys).

What this unlocks

The self-interrupting contact is the heart of the The Induction Coil and the vibrating rectifier. Latching relays and indicator drops lead straight to the The Automatic Telephone Exchange and the The Relay Computer. Call systems belong in every hospital. Bells and alarm loops are the first step to Railway Signalling and Safety, automatic control (Thermostats and Automatic Control) and electric fire telegraphs that let any street corner call the fire station.

How it was first done

In 1831 Joseph Henry, teaching in Albany, New York, rang a small bell with an electromagnet at the end of more than a kilometre of wire. In 1837–39 Johann Philipp Wagner and Christian Ernst Neef in Frankfurt built the self-interrupting "Wagner hammer", the make-and-break that drives every trembler bell. Trembler bells were in use in telegraph offices by the 1850s. Georges Leclanché's cell of 1866, which rested well between uses, made the electric doorbell practical, and from the 1880s house bells and indicator boards spread through hotels and town houses, replacing the old pull-wires and cranks.

In 1852 William Channing and Moses Farmer put a fire alarm telegraph into service in Boston: a crank in a box on a street corner sent the box's number by telegraph to a central office. Augustus Russell Pope of Boston patented an electromagnetic burglar alarm in 1853; Edwin Holmes bought the rights a few years later and built up the first burglar-alarm business, and by the 1870s his company was watching banks and shops in New York from a central office by wire.

Source: content/entries/electricity/bells-buzzers-and-alarms.md