Part 8 · Chemistry
Hydrogen Peroxide and Oxygen Bleach
Water with one extra oxygen atom, which it gives up readily — so it bleaches and kills germs and leaves nothing behind but water and oxygen. Made in dilute form from barium peroxide and sulfuric acid, or in a works by electrolysis; used at 3 % to clean wounds and mouths, at 3–6 % to whiten wool, silk, bone and hair where chlorine would destroy them, and locked into dry crystals of perborate as the oxygen bleach of the laundry. This book stays at household and medical strengths.
- Difficulty
- ●●●●●
- Time
- A week of furnace work to make the first barium peroxide; an hour to turn it into a litre of 3 % peroxide; an afternoon for a batch of perborate
- Steps from zero
- 23 prerequisites →
This unlocks
—The full path from nothing — 23 steps before this one
- Fire
- Cordage and Rope
- Stone Tools
- Finding and Preparing Clay
- Finding and Identifying Ores
- Sulfur
- Hunting and Trapping
- Basic Woodworking
- Pottery
- The Kiln
- Charcoal
- Hides and Leather
- Lime
- Salt
- Lye and Potash
- Fermentation
- Glass
- Bellows
- Saltpeter
- Copper Smelting
- Sulfuric Acid
- The Battery
- Electrolysis
- Hydrogen Peroxide and Oxygen Bleach
Do them roughly in this order. See it on the tech tree →
Why it matters
Chlorine and Bleach is powerful, cheap and essential for drinking water, but it is rough. It yellows and rots wool and silk, eats feathers and hair, leaves a smell and makes poisonous gas with acids. Hydrogen peroxide bleaches by releasing oxygen, and when it has finished there is nothing left but water. That makes it the bleach for:
- protein fibres — wool, silk, feathers, fur, hair — which chlorine destroys (Wool, Silk);
- bone, ivory, horn and skulls for tools, handles and teaching (Horn and Bone Working);
- cleaning wounds and mouths at 3 %, where its foaming lifts out dirt and dried blood (Wound Care and Antiseptics, Dentistry);
- laundry: locked into dry crystals of sodium perborate, it becomes oxygen bleach, a powder that whitens cotton and linen in the hot wash without the damage of chlorine (Laundry and Bleaching Cloth, Detergents and Wetting Agents);
- small jobs in the workshop and laboratory: etching copper boards, testing, and making a little oxygen.
It does not keep well and at high strength it is dangerous, so this chapter deliberately goes no higher than about 30 %; the reasons are given below.
How it works
Water is two hydrogen atoms and one oxygen atom. Hydrogen peroxide has two of each. The second oxygen is held loosely and comes off easily:
hydrogen peroxide → water + oxygen
That freed oxygen is very active for a moment. It attacks the coloured parts of stains and fibres (which is bleaching) and the outer skins of germs (which is disinfecting).
The breakdown happens slowly on its own and much faster when the peroxide meets:
- heat — it roughly doubles in speed for every 10 °C;
- light, especially sunlight;
- alkali — soda, lye or ammonia;
- traces of metals — iron, copper, manganese — and dust and rust;
- living things: blood, yeast, raw potato and liver all contain an enzyme (catalase) that tears it apart in seconds. This is the fizz when peroxide touches a wound.
So keep it cool, dark, slightly acid, clean and away from metal; and warm it and make it slightly alkaline when you want it to bleach fast.
Strength: percent and "volumes"
Peroxide is sold and described in two ways. Percent is grams of peroxide in 100 g of liquid. Volume strength says how many millilitres of oxygen gas 1 ml of the liquid gives off when it breaks down completely. The volume strength can be measured with a bottle and a jar of water (below), which makes it ideal when you have no other instruments.
| Strength | Volume | Use |
|---|---|---|
| 1.5 % | 5 vol | Mouth rinse, gargle |
| 3 % | 10 vol | Wounds, ear wax, surfaces, the standard household strength |
| 6 % | 20 vol | Bleaching wool, silk, bone; hair lightening |
| 9–12 % | 30–40 vol | Strongest hair lightening; workshop bleaching. Burns skin |
| about 30 % | about 100 vol | Laboratory reagent only. Burns skin white on contact, blinds. The ceiling of this book |
Warning Why this book stops at about 30 %. Above that, hydrogen peroxide changes character. It can set cloth, wood, leather and straw alight on contact as it dries; mixed with fuels, solvents or dust it can form mixtures that explode; and if it is contaminated, a container of it can boil and burst on its own as it breaks down, faster and faster, releasing its oxygen all at once. It has been used in rocket and torpedo fuels and in weapons. No task in a household, clinic, laundry or dye works needs it — every use in this book works at 3–12 % — and making it means distilling a liquid that can explode in the still. So this book gives no method for concentrating peroxide. The two routes below give dilute peroxide directly, and that is all you need.
What you need
| Item | Amount | Notes |
|---|---|---|
| Barite (heavy spar) | 1–2 kg | For barium peroxide (Method 1). Recovered at the end and reused |
| Charcoal | 1 kg | Powdered, to reduce the barite (Charcoal) |
| Nitric acid or soda | To turn barium sulfide into nitrate or carbonate (Nitric Acid, Soda Ash and Baking Soda) | |
| Sulfuric acid | about 90 g pure acid per litre of 3 % peroxide | Diluted to 10 % (Sulfuric Acid) |
| Clay crucibles and a tube furnace | A clay or iron tube 5 cm bore, 60 cm long, in a charcoal fire, with a bellows (The Kiln, Bellows) | |
| Borax and caustic soda | 38 g and 8 g per batch | For perborate (Borax and Boric Acid, Lye and Potash) |
| Brown or dark glass bottles | With loose glass stoppers (Bottles, Drinking Glasses and Glassware) | |
| Ice or cold spring water | a bucket | To keep reactions cold |
| Test kit | A narrow-necked bottle, rubber or gut tube, a measuring jar, yeast or powdered black manganese ore; or permanganate solution (Potassium Permanganate) |
Glass, glazed stoneware and good porcelain are the only safe vessels. Never use iron, copper, brass or zinc.
Where to find it
- Barite is a strikingly heavy pale mineral in veins with lead ore and fluorite; it does not fizz in acid (Rocks and Minerals).
- Black manganese ore (pyrolusite) for the strength test: sooty black, stains the fingers (Potassium Permanganate).
- Borax from dry lake beds and hot springs (Borax and Boric Acid).
Method 1: Barium peroxide and acid
This is how peroxide was first made, in 1818, and how it was sold for the next 80 years. It is a long chain of furnace work, but at the end, barium peroxide and dilute sulfuric acid give clean 3 % peroxide in an afternoon, and the barium comes back as barite to be used again.
Barium oxide (outline)
- Reduce the barite. Grind barite fine and mix it with a quarter of its weight of powdered charcoal and a little flour paste. Pack it in a covered clay crucible and fire it at bright orange-yellow heat (about 1,000 °C) for 2–3 hours. The grey-black product is barium sulfide. It smells of rotten eggs when wet.
- Leach it with hot water, which dissolves the sulfide, and filter.
- Make barium nitrate. Add dilute Nitric Acid to the clear liquid, outdoors (it gives off poisonous rotten-egg gas, hydrogen sulfide), until it no longer fizzes. Boil down and let barium nitrate crystallise: white, heavy crystals.
- Make barium oxide. Heat the dry nitrate in a clay crucible at red heat (700–800 °C) until it stops giving off brown fumes, about an hour. Outdoors, upwind: the fumes are nitrogen dioxide. What is left is a grey-white, porous cake of barium oxide. It soaks up water and carbon dioxide from the air quickly: use it at once or seal it in a dry jar.
Barium peroxide
- Load the tube. Break the barium oxide into pea-sized lumps and fill a clay or iron tube with them, loosely, so air can pass. Lay the tube through a charcoal fire.
- Feed it air. Bring the tube to a dull red, just visible in shade (about 500–550 °C), and pump air through it slowly with a small bellows for 3–6 hours. The air must be dry and free of carbon dioxide: draw it first through a jar of lumps of quicklime (Lime), which takes out both.
- Do not overheat. Above a bright cherry red (about 700 °C) barium peroxide gives its oxygen back. That is the trick of the old Brin process: one heat to take oxygen from air, a hotter heat to release pure oxygen (Hydrogen, Oxygen and Gases).
- Weigh it. Cooled, the lumps should have gained close to one-tenth of their weight: 100 g of barium oxide becomes about 110 g of grey-white barium peroxide. A gain of 7–9 % is a fair first result.
Turning it into peroxide
- Make the acid. Pour about 90 g of strong sulfuric acid into 800 ml of water (acid into water, slowly, stirring) to make about 10 % acid. Cool it in a bucket of ice or cold spring water to below 10 °C.
- Make a paste. Grind about 150 g of barium peroxide to a fine powder and stir it into 200 ml of cold water. It forms a creamy paste of hydrated peroxide.
- Add the paste to the acid, a spoonful at a time, stirring, with the pot standing in ice. Keep it below 10 °C. Each spoonful turns into heavy white barium sulfate, which is simply barite again.
- Stop while the liquid is still faintly acid: test paper just pink. If you overshoot to alkaline, the peroxide starts to break down; add a few drops of acid at once.
- Settle and filter. Let the white sludge settle for an hour in the cold. Pour off and filter the clear liquid through clean cloth or paper. You have about 1 litre of 3 % peroxide. Wash the sludge, dry it and keep it: it is barite, ready to start again.
- Check for barium. A drop of dilute sulfuric acid in a little of the liquid must give no cloud. If it clouds, add a few more drops of acid to the batch, settle, and filter again. Barium salts are poisons; the peroxide must be free of them before it touches a wound.
Method 2: Electricity (outline)
From 1908 most peroxide was made by electricity, and the chemistry is worth knowing because its first product is useful by itself.
- Persulfate. Electrolyse cold ammonium or potassium sulfate dissolved in sulfuric acid (Electrolysis) with a fine platinum wire anode at a very high current density — several amperes on a few square centimetres of wire — and a lead or graphite cathode, kept below 20 °C. At the anode the sulfate is joined in pairs into persulfate. Potassium persulfate is only slightly soluble and settles out as white crystals. It is a strong, dry, stable oxidiser in its own right: it etches copper for circuit boards (Building Circuits: Boards, Connectors and Cables), boosts hair bleach, and starts the reactions that make many Petrochemicals and Modern Plastics.
- Peroxide. Warmed with water, persulfate slowly turns into hydrogen peroxide and sulfuric acid. The factory then separates the peroxide from the acid in a special still. That is a works process, with the hazards described above, and this book does not describe it.
The modern anthraquinone process loads a recycled dye-like compound with hydrogen over a palladium catalyst, then blows it with air to release peroxide. It needs a full chemical industry (Organic Synthesis and Fine Chemicals).
Measuring strength
Home-made peroxide varies, and peroxide loses strength in storage. Measure every batch, and measure stock again before medical use.
The peroxide strength tester
- Build it from a small wide-mouthed bottle (100–200 ml) with a stopper bored for one tube; a bent glass tube or a length of gut or rubber tubing; and a measuring jar marked in 10 ml steps (mark it by pouring in water weighed on a balance — 1 g is 1 ml). See Hydrogen, Oxygen and Gases for collecting gas over water.
- Fill the jar with water and stand it upside down in a basin of water, with the end of the tube under its mouth.
- Put 10 ml of the peroxide in the bottle. Put a pea-sized lump of yeast paste, or a pinch of black manganese ore powder, in a small open thimble or tube and stand it upright inside the bottle so it does not touch the peroxide yet.
- Stopper the bottle tightly. Tip it so the yeast falls into the peroxide. It foams. Swirl it gently.
- When bubbling stops (5–15 minutes), level the water inside and outside the jar and read the volume of gas.
- Volume of gas ÷ 10 = volume strength. 100 ml means 10 vol, which is 3 %. 60 ml means 6 vol, about 1.8 %.
A good tester agrees within 5 ml on two runs; low, drifting readings mean a leaky stopper.
By permanganate
For a laboratory, titrate it (Potassium Permanganate, Acids, Bases and Testing). Dilute 10 ml of peroxide to 100 ml with water. Take 10 ml of that, add 10 ml of 10 % sulfuric acid, and run in permanganate solution of 3.16 g per litre from a burette until one drop leaves a pink colour that lasts 30 seconds. Each millilitre of permanganate used means 1.70 mg of peroxide. A 3 % solution needs about 17.6 ml.
Using dilute peroxide
| Job | Strength | How |
|---|---|---|
| Cleaning a dirty wound | 3 % | Once, at first cleaning, after irrigation with boiled water: pour or dab it on; the foam lifts dirt and dried blood. Do not use it again and again — it also damages the healing tissue (Wound Care and Antiseptics) |
| Mouth rinse, sore gums | 1.5 % (3 % mixed 1:1 with water) | Swish for 1 minute, spit, rinse with water; 2–3 times a day for no more than a week. Never swallow |
| Ear wax | 3 % | 5–10 drops in the ear, lying on your side, for 5 minutes; then tilt out and rinse with warm water. Not if the eardrum may be torn |
| Surfaces and tools | 3–6 % | Wet thoroughly and leave 10 minutes. Kills most germs; not a substitute for boiling (Sterilising Instruments and Dressings) |
| Wool and silk | 1–2 % | See below |
| Bone, skulls, ivory, horn | 3–6 % | Clean and degrease first; soak 1–3 days, rinse, dry in the sun |
| Hair lightening | 6 % with a few drops of ammonia | Comb through, 15–30 minutes, rinse well. Test on one strand. Keep out of eyes (Toothpaste, Shampoo, Perfume and Cosmetics) |
| Etching copper boards | 2 parts 3 % peroxide to 1 part strong hydrochloric acid | Outdoors; rock the board in it until bare copper is gone (Building Circuits: Boards, Connectors and Cables, Hydrochloric Acid) |
Bleaching wool, silk and linen
- Wash the goods first: grease and size stop the bleach (Laundry and Bleaching Cloth).
- Make the bath: 3 % peroxide diluted with an equal volume of soft water (about 1.5 %), 20 litres of bath per kg of goods. Make it faintly alkaline: add washing soda or ammonia until a test paper shows pH 8–9 (blue-green on cabbage paper, pH, Indicators and Buffers). A spoonful of water glass per 10 litres (Water Glass (Sodium Silicate)) slows the waste of peroxide on dust and iron.
- Wool and silk: hold at 40–50 °C (hot bath water) for 4–8 hours or overnight, turning now and then. Hotter, and stronger alkali, damage them.
- Linen and cotton tolerate more: 80–90 °C for 1–2 hours, with 2–3 g of soda per litre.
- Rinse, then sour in water with a dash of vinegar, and rinse again. Dry in shade.
Oxygen bleach
Oxygen bleach is peroxide in a dry, safe, stable powder. In hot water it gives the peroxide back and bleaches tea, coffee, wine, fruit, grass and sweat stains, and keeps whites white, without the yellowing and rotting of chlorine. There are two kinds.
Sodium perborate (can be made from 3 % peroxide)
- Dissolve 38 g of borax and 8 g of caustic soda (Lye and Potash, made from soda ash and lime) in 100 ml of warm water. Cool it to room temperature.
- Pour it slowly, stirring, into 450 ml of cold 3 % peroxide (or 225 ml of 6 %) in a glass jar.
- Chill. Stand the jar in ice or the coldest spring water you have, around 5 °C, for 3–6 hours, stirring now and then. A fine, white, sandy powder settles: sodium perborate.
- Collect it on a cloth filter, rinse once with a little ice-cold water, and dry it in air below 40 °C, spread thin on paper in the shade. Heat drives off its oxygen.
- Yield: about 30–45 g. With 6 % peroxide it is better, because less stays dissolved.
Potash lye does not work here: potassium perborate stays dissolved. Use soda.
Sodium percarbonate (works only)
Sodium percarbonate is soda ash with peroxide locked into its crystals. It bleaches at lower temperatures than perborate and contains no boron. But it dissolves so easily that it can only be crystallised from peroxide near 30 % in a factory. Use perborate; it does the same job.
Using oxygen bleach
- In the wash: mix 1 part perborate with 4–5 parts of your washing powder (Detergents and Wetting Agents). It bleaches only in hot water, above about 60 °C, so it belongs in the hot or boiling wash of white cotton and linen.
- Stain soak: 1 level tablespoon (15 g) per litre of water at 60–70 °C. Soak the stained cloth for a few hours or overnight, then wash. Test coloured cloth on a hidden corner.
- Not for wool and silk above 40 °C: the hot alkaline liquid harms them. Use the peroxide bath above.
A good oxygen bleach is a dry, free-running white powder. A spoonful in a cup of hot water gives a steady stream of tiny bubbles, and a glowing splinter held just above a teaspoonful heated in a test tube flares up (that is oxygen). Caked, damp powder that does not fizz has lost its oxygen; make fresh. Store it in a closed, dry jar.
Storing peroxide
- Dark, cool, clean. Brown glass, or clear glass wrapped in paper or kept in a closed clay jar, in the coolest place you have.
- Slightly acid. Add 1 drop of dilute sulfuric acid per 100 ml to home-made peroxide; it keeps far better than neutral peroxide.
- Vented, never sealed tight. Use a loose glass stopper, or a cork with a fine groove cut down its side, so gas can escape. Fill bottles only three-quarters full.
- Never pour unused peroxide back into the stock bottle, and never let metal, dust or a dirty dropper into it.
- Label it with the strength and the date. Clean 3 % keeps most of its strength for months in the dark; dirty or warm peroxide can lose half in weeks. Measure again before medical use.
How to tell it worked
- It foams on blood, yeast or raw potato, at once and strongly.
- The strength tester gives about 100 ml of gas from 10 ml for 3 %.
- Starch and iodide test. A drop in a little starch water with a pinch of potassium iodide (Iodine) and a drop of vinegar turns deep blue within a minute.
- It bleaches. A strip of brown wool in the 1.5 % alkaline bath is visibly paler overnight.
Note Troubleshooting. Little or no gas from the barium peroxide batch → the barium oxide had soaked up carbon dioxide, or the tube ran too hot. Dry the air through quicklime, keep the tube at dull red, and weigh for the one-tenth gain. The batch foamed while you added the paste → too warm, or it went alkaline. Use more ice, add the paste more slowly, and keep it faintly acid. Peroxide loses strength in a week → light, warmth, dust or a trace of metal, or no acid stabiliser. Use brown glass, add the drop of acid, keep it cool. No perborate crystals → too warm, too dilute, or potash used instead of soda. Chill colder and longer, or use 6 % peroxide.
Dangers
Danger Barium compounds are poisons. Barium sulfide, carbonate, nitrate, oxide and peroxide all poison the heart and muscles if swallowed — a few grams can kill. (Barite itself is harmless because it does not dissolve at all.) Wear gloves, wash hands, keep them locked and labelled, and always check the finished peroxide for barium as in step 14. Making barium sulfide and nitrate gives off hydrogen sulfide and nitrogen dioxide, both deadly: outdoors only.
Danger Strong peroxide burns and blinds. Even 6–12 % stings and whitens skin and can scar the eyes; 30 % burns skin white at once and can blind. Wear eye protection when handling anything stronger than 3 %; if it splashes in an eye, rinse with running water for 20 minutes. Peroxide spilled on cloth, wood, straw or paper can start a fire as it dries: rinse spills away with plenty of water. Never mix it with fuels, solvents or other chemicals, and never keep it in a tightly sealed bottle.
- Swallowing even 3 % causes vomiting and a stomach full of foam; stronger solutions can release enough gas to block blood vessels. Keep it out of reach of children, and in bottles that look nothing like drinks.
- Not for repeated wound washing. Use it once to lift dirt, then plain boiled water or salt water.
- Perborate is mildly poisonous if swallowed in quantity; store laundry powder away from food.
What this unlocks
- Gentle bleaching of wool, silk, feathers and fur (Wool, Silk, Dyes and Mordants): white grounds for the brightest dyes.
- Better laundry with oxygen bleach (Detergents and Wetting Agents, Laundry and Bleaching Cloth).
- Clean bone and horn for tools, combs and buttons (Horn and Bone Working).
- Persulfate for etching boards and starting plastics (Building Circuits: Boards, Connectors and Cables, Petrochemicals and Modern Plastics); peroxide reagents for chip-making (Making Microchips).
How it was first done
The French chemist Louis Jacques Thénard discovered hydrogen peroxide in 1818 by treating barium peroxide with acid, and called it "oxygenated water". Barium peroxide routes supplied it through the 1800s; the brothers Arthur and Léon Brin in France in the 1880s used the same oxide to take oxygen from air and release it pure, and their process sold both oxygen and peroxide. The first electrolytic peroxide works opened at Weissenstein, Austria, in 1908, using persulfate. Sodium perborate was first made in 1898, and in 1907 the German firm Henkel sold it with water glass as Persil, the first "self-acting" washing powder. The anthraquinone process was worked out at IG Farben in the 1930s and took over the world's production after the 1950s.
Source: content/entries/chemistry/hydrogen-peroxide.md