◆ Rebuild

Part 10 · Machines

Precision Grinding

A wheel of bonded grit spinning at 30 metres a second cuts hardened steel that no lathe tool can touch, and takes it to size within a few thousandths of a millimetre. How to make and mount grinding wheels, dress them true, and grind flat, round and centreless work to finished size after hardening.

Difficulty
●●●●●
Time
A week to make and fire a batch of wheels; months to build a surface or cylindrical grinder once you have a good lathe and planer
Steps from zero
20 prerequisites →

You need first

Machine ToolsAbrasives and Grinding Stones

This unlocks

—
The full path from nothing — 20 steps before this one
  1. Stone Tools
  2. Cordage and Rope
  3. Fire
  4. Finding and Preparing Clay
  5. Finding and Identifying Ores
  6. Basic Woodworking
  7. Hunting and Trapping
  8. Charcoal
  9. Pottery
  10. Abrasives and Grinding Stones
  11. Hides and Leather
  12. The Wheel and Axle
  13. Bellows
  14. The Lathe
  15. Iron (the Bloomery)
  16. Copper Smelting
  17. Blacksmithing
  18. Steel
  19. The Steam Engine
  20. Machine Tools
  21. Precision Grinding

Do them roughly in this order. See it on the tech tree →

Why it matters

A lathe tool can only cut metal softer than itself. But the parts that wear — bearing races and balls, shafts, gauges, dies, cutters, piston pins, cams — must be hardened to last, and hardening warps them by a few hundredths of a millimetre. Once a part is glass-hard, the only practical way to bring it back to size is to grind it.

A grinding wheel is a disc of hard grains held by a bond. Every grain that meets the work is a tiny cutting tool taking a chip finer than a hair. Because the cuts are so small and the wheel so fast, a good grinding machine holds a size to 0.002–0.005 mm and leaves a finer surface than any turned or planed one. This is how Making Ball and Roller Bearings, gauges, crankshafts and every sharp cutting tool are finished. Grinding is the last step of the toolmaker's climb that began with three plates in Machine Tools.

How it works

A wheel sharpens itself. As each grain cuts, its point dulls and the force on it rises. In a well-chosen wheel the bond then breaks, the dull grain falls out, and a sharp one underneath takes over. If the bond is too hard, dull grains stay in, the wheel rubs, heats and glazes (goes shiny). If it is too soft, good grains tear out and the wheel wears away and loses its shape.

The rule: hard work wants a soft wheel; soft work wants a hard wheel.

Makers stamp five things on a wheel, in this order:

Property Meaning Typical marks
Abrasive The grain A = aluminium oxide (corundum, emery); C = silicon carbide
Grit Grain size: sieve wires per inch it just passes 24 coarse, 46 medium, 60–80 fine, 120–220 very fine
Grade How hard the bond holds E–H soft, I–P medium, Q–Z hard
Structure How open the wheel is 1–4 dense, 5–8 medium, 9–14 open
Bond What holds the grain V vitrified (fired clay), S silicate, E shellac, R rubber, B resin

A general wheel for hardened steel reads A 46 J 8 V. Aluminium oxide is tough and suits steels; silicon carbide is harder but brittle, for cast iron, brass, stone and glass.

Speed. Grinding works best at a wheel surface speed of 25–33 metres per second — a hundred times faster than a lathe tool:

Turns per minute = surface speed (m/s) × 19,100 ÷ wheel diameter (mm)

A 200 mm wheel at 30 m/s runs at about 2,900 turns a minute. Every wheel has a maximum safe speed, and a wheel run faster can burst.

Heat. Most of the work becomes heat right at the surface; each spark is a red-hot chip. If the surface passes about 200 °C, hardened steel softens (straw, brown or blue temper colours — see Steel) or cracks. Light cuts, a sharp wheel and plenty of coolant prevent it.

Inside the wheel, magnified Grain Bond Pore Bench grinder, from the side Guardcovers about ¾ of the wheel Tool restgap 3 mm or less face turns downtoward the rest Mounting, exploded slide on in this order Inner flangefixed to spindle Wheelring-tested first Outer flangesame size as inner,at least ⅓ of wheel Nutfirm, never forced spindle Blotterssoft paper washers Marked: A 46 J 8 V aluminium oxide · grit 46 · grade J (soft to medium) structure 8 (open) · vitrified bond · safe to 33 m/s
Fig. 1 Anatomy and mounting of a grinding wheel. Grains are held by bridges of bond with open pores between them for chips and coolant. The wheel is clamped between two equal flanges at least a third of its diameter, with soft paper washers between, and runs inside a guard.

What you need

Item Notes
Abrasive grain Crushed, sieved emery or corundum (Abrasives and Grinding Stones), or made silicon carbide or fused alumina (below)
Bond Fine clay and feldspar for vitrified wheels; Water Glass (Sodium Silicate); shellac (Glues and Adhesives)
Steel ring mould and a screw or hydraulic press For pressing wheels
Kiln reaching 1,250 °C The Kiln, Stoneware and Porcelain
A good lathe and planer To build the machines (The Lathe, Machine Tools)
Hardened spindle in close bearings Scraped plain bearings (Bearings and Lubrication) or Making Ball and Roller Bearings
Dressing tool Diamond in a steel holder, star-wheel dresser, or silicon carbide stick
Micrometer and dial indicator Precision and Interchangeable Parts
Coolant Water with 1–2% washing soda (Soda Ash and Baking Soda) against rust, or 2–5% soluble oil

Where to find it

Emery (dark, very heavy rock) and corundum (hard grey to brown crystals that scratch quartz) are described in Abrasives and Grinding Stones and Rocks and Minerals. Feldspar is the pink or white blocky mineral in granite that splits along flat faces. Bauxite is a reddish earthy rock of tropical soils (Aluminium). Diamond is the hard part: small cloudy industrial diamonds (bort) turn up rarely in river gravels with garnet, and in kimberlite "blue ground". Most workshops will manage without one (see dressing); a single good diamond, carefully kept, lasts years.

Making grinding wheels

Glued wheels and laps

The simplest grinding wheel is emery glued to wood. Turn a disc of seasoned hardwood 15–25 cm across, coat the rim with hot hide glue, roll it in graded emery, let it set, and repeat twice. Run it at only 10–15 m/s; re-coat it when it wears smooth. It sharpens tools and cleans up small hardened parts. A lap is the precision version: a disc or rod of soft cast iron, copper or lead with fine emery and oil rolled into its surface. Laps run slowly and finish gauges and holes better than any wheel (Precision and Interchangeable Parts).

Shellac and silicate wheels

Warm graded grain (grit 46–120) to about 120 °C, stir in 1 part powdered shellac to 9 parts grain by weight until it sticks like damp sand, press it hot into a steel ring mould with a greased plug for the hole, and bake it in the mould at 150 °C for several hours. Shellac wheels are slightly springy and cut cool — good for thin cut-off wheels and fine finishing, used wet. Silicate wheels use water glass instead, pressed cold, dried and baked at 250–300 °C; they are soft and good for edge tools.

The vitrified wheel

Nearly all precision wheels are vitrified: the grain is held by a thin glass of fired clay, exactly like stoneware. They do not soften with heat or water, and their grade can be set accurately.

  1. The bond. Grind very fine about 6 parts plastic clay, 3 parts feldspar and 1 part flint or quartz by weight. A fired test bar should be dense and glassy without slumping. More feldspar melts sooner; more clay stays stiffer.
  2. Mix about 85 parts grain to 15 parts bond by weight, with just enough water (or thin flour paste) that a squeezed handful holds its shape. More bond makes a harder wheel. Sawdust or ground coke in the mix burns out and leaves pores for an open wheel.
  3. Press. Fill the mould evenly, levelling with a straightedge, then press hard. A wheel denser on one side is out of balance and can burst.
  4. Dry slowly for several days.
  5. Fire flat on a bed of sand, heating over a day or two to 1,200–1,280 °C (bright yellow-white, The Kiln), hold several hours, and cool very slowly over days. Strain from fast cooling bursts wheels later.
  6. Finish: bore the hole true (bush it with lead if needed), true the faces and rim, then balance and speed-test it.

Tip Fire one wheel from each batch first and grind a hardened file with it. If it glazes and burns the steel, use less bond; if it crumbles away as you watch, use more.

Better grain. Natural emery is only half corundum. The The Electric Arc Furnace makes two far better grains. Silicon carbide (carborundum): a trough of firebrick packed with about 50 parts quartz sand, 35 coke, 10 sawdust and 5 salt, round a core of crushed coke between two carbon electrodes, heated by heavy current for a day or more to 2,200–2,500 °C, grows a ring of glittering black-green crystals. The furnace gives off a great deal of poisonous carbon monoxide: run it in the open and keep upwind. Fused alumina: bauxite melted with a little coke and iron at about 2,000 °C sheds its impurities as a sinking iron alloy, leaving a block of brown corundum to crush.

Mounting and testing a wheel

Most grinding injuries come from bursting wheels. Do every step, every time.

  1. Ring test. Hang the wheel on a peg through its hole and tap it lightly with a wooden handle about 45° either side of the bottom. A sound vitrified wheel rings clear; a dull thud means a crack — break it up and throw it away.
  2. Check the speed of the spindle against the wheel's safe speed.
  3. Flanges: two of the same size, at least one-third of the wheel diameter, recessed so they grip only near their rims, with a blotter (soft paper or thin leather washer) between each flange and the wheel. The wheel slides on the spindle without force or shake.
  4. Tighten the nut only firmly by hand with a short spanner.
  5. Guard: cast iron or thick steel, leaving bare no more than about a quarter of the wheel.
  6. Stand clear — out of the wheel's plane — and let it run at full speed for a full minute before you use it.

Balancing. Roll the wheel and flanges on a straight arbor across two level, hardened knife-edge rails — a balancing stand. The heavy side rolls down. Shift the small weights in the flange groove until the wheel stays wherever you leave it. Balance again after truing.

Dressing and truing

Truing makes the wheel round and true to its spindle; dressing breaks off dull grains and clogged metal to open the face. Usually one pass does both.

  • Diamond. Hold a diamond set in a steel rod on the table, pointing 10–15° in the direction the wheel turns and just below centre. Flood it with coolant and pass it across the running wheel, 0.02–0.03 mm at a time, finishing at 0.005–0.01 mm. A slow pass leaves a smooth face for finishing; a fast pass an open, sharp face for heavy cutting. Turn the diamond in its holder now and then, and never let it run dry: heat shatters it.
  • Without diamond. For bench grinders, a star-wheel dresser — a handle carrying hardened steel discs cut like stars, free to spin — is pressed against the wheel on the rest and crushes its face open. For finer work, press a hard silicon carbide stick across the face, or use a small silicon carbide wheel on its own spindle held back by a brake, so it rubs the grinding wheel true.

Bench and tool grinding

The bench grinder — two wheels 150–250 mm across on one spindle, coarse (36–46) on one end and fine (60–80) on the other — shapes lathe tools, sharpens drills and chisels, and cleans forgings. Keep the tool rest within 3 mm of the wheel: a wider gap drags the work, and your fingers, into it. Grind on the rim, never the side of a straight wheel. Dip carbon-steel tools in water every few seconds; a blue edge has lost its temper (Axes, Chisels, Knives and Planes). Shaping cutters to exact angles needs a tool and cutter grinder, a small wheel on a slide with a table that holds the cutter at a set angle.

Surface grinding: flat work

The surface grinder finishes flat faces: gauge blocks, die plates, slides, hardened washers and bearing rings. A heavy cast iron base carries a table that slides back and forth under the wheel on V and flat ways, like a small planer (Machine Tools). The wheel head sits on a column, lowered by a fine screw graduated in 0.002–0.005 mm; a second screw moves the table across a little after each stroke. Wheels are 150–300 mm across and 13–25 mm wide.

The magnetic chuck holds steel parts: a thick steel top with strips of brass between alternating iron poles, over coils of insulated copper wire fed with direct current (The Electromagnet). Afterwards, pass the parts slowly through a coil fed with alternating current, or reverse the chuck current briefly, to demagnetise them. Without electricity, hold parts with low toe clamps against a stop, or stick thin ones down with warm shellac.

Surface downfeed Wheel25–33 m/s Work Chuckmagnetic Table table moves to and fro; crossfeed after each stroke Between centres (from above) Dog Wheel infeed Work work traverses Dead centres neither one turns; the dog drives Centreless (end view) work sits above the line of centres Work Blade Grinding wheelfast, 30 m/s Regulating wheelslow, rubber-bonded
Fig. 2 Three ways to grind. A surface grinder passes the work back and forth under the wheel. A cylindrical grinder turns the work slowly between two fixed centres while the wheel cuts its side. A centreless grinder lets the work ride on a blade between the grinding wheel and a slow rubber regulating wheel, set a little above centre.
  1. Dress the wheel; clean the chuck and the part (one chip under a part tilts it).
  2. Set the stroke so the wheel runs 2–3 cm past each end, and lower it until it just whispers sparks at the high point.
  3. Rough: down 0.02–0.03 mm per pass, crossfeed a quarter to a third of the wheel width per stroke, table 8–20 m a minute.
  4. Finish: redress slowly, feed 0.005 mm, crossfeed an eighth of the wheel width.
  5. Spark out: two or three passes with no feed, until the sparks die. The machine springs back a little under each cut; this takes out the last of it.
  6. Thin hardened parts bow as one face is ground. Turn them over and over, taking less each time.

A good machine holds flatness and parallelism within 0.002–0.005 mm over 150 mm.

Cylindrical grinding: round work

The cylindrical grinder finishes shafts, pins, spindles and plug gauges. It is like a long, very rigid lathe: a sliding table carries a headstock and tailstock, each with a hardened, ground 60° centre, and the wheel head behind is fed in by a screw graduated in 0.002–0.005 mm of diameter.

Both centres stand still. The headstock turns only a faceplate, which drives the work by a dog clamped to its end. The work turns on two motionless points, so no wobble in the headstock bearings can reach it. Lap the work's centre holes true at 60° before grinding, and keep them oiled.

Speeds. The work turns slowly — surface speed 15–30 m a minute (a 25 mm shaft at 200–400 turns a minute) — in the same rotational direction as the wheel, so their surfaces meet moving opposite ways. The table moves half to two-thirds of the wheel width per turn of the work for roughing, an eighth to a quarter for finishing.

  1. Turn and harden the part, leaving 0.2–0.4 mm on the diameter to grind (0.4–0.6 mm on large or long parts).
  2. Mount it between centres; set the table stops so the wheel runs a third of its width off each end.
  3. Dress the wheel; flood coolant exactly where wheel meets work.
  4. Feed 0.02 mm on the diameter at each end of the stroke until about 0.03 mm remains; redress slowly; feed 0.005 mm at a time to size; spark out.
  5. Measure both ends. If one is bigger, swivel the upper table slightly and try again. Measure cool: steel grows about 0.001 mm per 100 mm per degree, so a part sized hot is undersize when cold.
  6. Support long, thin work every 6–10 diameters with steady rests — adjustable hardwood or bronze shoes bearing behind and below.

Plunge grinding feeds a wheel wider than the part straight in, for crankshaft journals and collars. Bores are ground with a small wheel on a fast slender spindle (internal grinding).

Centreless grinding

The centreless grinder grinds pins, rollers, piston pins and bar with no centre holes — thousands of identical parts, fast. The work lies on a work-rest blade between the fast grinding wheel and a slow regulating wheel of rubber-bonded abrasive (surface speed 15–40 m a minute) turning the same way. The grippier regulating wheel holds the work to its own slow speed, so the grinding wheel cuts.

  1. Set the work above centre — its centre above the line joining the two wheel centres by about half its diameter (no more than 10–15 mm). Exactly on the line, a bump on the work lifts it at each wheel, and you grind a three- or five-lobed shape that measures the same across every diameter but is not round.
  2. The blade: hardened steel, a little thinner than the work, its top bevelled about 30° down toward the regulating wheel.
  3. Throughfeed: tilt the regulating wheel 1–5° and it screws the work along past the grinding wheel. Feed speed = regulating wheel surface speed × sine of the tilt: a 250 mm wheel at 50 turns a minute tilted 3° pushes work through at about 2 m a minute. Dress the regulating wheel at the same tilt.
  4. Infeed parts with heads or shoulders: set the tilt near zero and push the regulating wheel in until the part is to size.

Once set, it turns out part after part within 0.002–0.005 mm; check a sample every few minutes with a go/no-go gauge (Precision and Interchangeable Parts).

How to tell it worked

  • Size: within tolerance by micrometer, at room temperature, at both ends and several points round.
  • Roundness: turned slowly in a V-block under a dial indicator, round work moves the needle less than 0.002 mm. A lobed part shows highs and lows that a micrometer misses.
  • Flatness: smeared thinly with red marking paste and rubbed on a surface plate, a flat face marks all over.
  • Finish: soft satin grey, reflecting a window frame clearly. Regular dull and bright patches are chatter.
  • No burn: pale grey all over. To check, dip the part a few seconds in 5% nitric acid in alcohol (Nitric Acid) and rinse: burnt, softened spots etch darker. Mix the etch a little at a time by pouring the acid slowly into cold alcohol, never stronger than 5%, and never keep it in a tightly stoppered bottle: stronger or stored mixtures can react violently and burst. Wear eye protection; it burns skin and eyes. Burnt parts can show a fine net of cracks; scrap any cracked bearing or gauge part.

Note Troubleshooting. Wheel glazes, work burns → wheel too hard, too fine or dull. Dress faster, use a softer, more open wheel, more coolant, lighter cuts. Wheel wears fast and loses shape → too soft, or cuts too heavy. Chatter → unbalanced or out-of-round wheel, loose spindle, slack belt, or work flexing. Balance and true; add steadies. Work tapered → table not parallel to the wheel; swivel it. Lobed work on the centreless grinder → work centre too low; raise the blade. Size drifts during a run → the machine is warming up. Run it half an hour first and keep the coolant at one temperature. Scratches in a fine finish → dirty coolant. Settle and filter it.

Dangers

Danger Bursting wheels. A vitrified wheel at working speed throws pieces through a wooden wall. Never exceed its marked safe speed; never run a wheel that fails the ring test or has been dropped; always use flanges, blotters and a guard; never grind on the side of a straight wheel; stand out of its plane when starting it. Speed-test every wheel you make at 1½ times working speed inside a heavy box before it goes on a machine.

Danger Dust. Grinding dust — especially from sandstone, quartz and silica-bonded wheels — scars the lungs (silicosis) slowly and without warning. Grind wet where you can, put a hood and fan over dry wheels, and wear a mask when truing wheels (Mining and Tunnelling).

  • Eyes: wear goggles or keep the glass shield down.
  • Hands: keep the rest close; hold small parts in pliers; no gloves, loose sleeves or loose hair near a wheel.
  • Fire: sparks light oily rags and wood dust; magnesium and aluminium dust burn fiercely.

What this unlocks

Grinding finishes the races, balls and rollers of Making Ball and Roller Bearings, the plugs and rings of gauges, crankshafts for the The Internal Combustion Engine engine and the The Motor Vehicle, and the cutters every other machine tool uses. Lapping after grinding reaches the accuracy of Watches and Small Clocks and Scientific Instrument Making. The same wheels and dressing methods grind glass for Lenses and stone in Gem Cutting and Lapidary work.

How it was first done

Simple machines that ground parts with emery wheels appeared in the 1830s and 1840s, and Joseph R. Brown of Brown & Sharpe in Providence, Rhode Island, built the universal grinding machine in 1876, ancestor of every cylindrical and tool grinder. Bonded wheels improved quickly: in the 1870s Sven Pulson at the Norton pottery in Worcester, Massachusetts, fired the first successful vitrified wheels. Edward Acheson made silicon carbide in an electric furnace in 1891, and fused alumina followed around 1900. From about 1900 Charles H. Norton showed that wide wheels on very rigid machines could grind parts to size from the rough faster than lathes could turn them, and grinding became central to car making. The magnetic chuck appeared in the 1890s, and the centreless grinder, patented in the United States around 1915, was developed in the 1920s for bearings and cars.

Source: content/entries/mechanics/precision-grinding.md